Sstpc Sinopec Sabic Tianjin Hdpe 5502xa

SSTPC (Sinopec SABIC Tianjin) HDPE 5502XA

    • Product Name: SSTPC (Sinopec SABIC Tianjin) HDPE 5502XA
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 134097
    Polymer Type High-Density Polyethylene (HDPE)
    Density 0.954 g/cm³
    Melt Flow Rate 0.35 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 26 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 600%
    Flexural Modulus 1100 MPa
    Notched Izod Impact Strength At 23 C 20 kJ/m²
    Vicat Softening Temperature 124°C
    Heat Deflection Temperature 70°C
    Environmental Stress Crack Resistance >1000 h
    Hardness Shore D 65
    Melting Point 130-135°C
    Molecular Weight Distribution Broad

    As an accredited SSTPC (Sinopec SABIC Tianjin) HDPE 5502XA factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SSTPC Sinopec SABIC Tianjin HDPE 5502XA is supplied in 25 kg bags, 40 bags per pallet, 1000 kg total, stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL container loading of SSTPC (Sinopec SABIC Tianjin) HDPE 5502XA, in 25 kg bags, palletized, securely stowed for shipment.
    Shipping SSTPC (Sinopec SABIC Tianjin) HDPE 5502XA is shipped as a non-hazardous solid resin, typically in 25 kg bags or 500–1,000 kg jumbo bags, palletized and stretch-wrapped. It is transported in dry containers by sea, truck, or rail, away from heat, moisture, and direct sunlight. Not regulated for transport; no special placards required.
    Storage Store SSTPC (Sinopec SABIC Tianjin) HDPE 5502XA in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original bags or containers sealed, clean, and palletized. Avoid moisture, contamination, and prolonged UV exposure. Do not stack excessively. Use first-in, first-out. Maintain ambient temperature. Separate from strong oxidizers. Ensure good ventilation. Follow local regulations and manufacturer’s recommendations.
    Shelf Life Typically 24 months from manufacture when stored in original packaging, cool, dry, ventilated, away from direct sunlight and excessive heat.
    Application of SSTPC (Sinopec SABIC Tianjin) HDPE 5502XA

    On continuous shuttle lines producing 20–30 L UN-rated jerricans, Sinopec SABIC Tianjin HDPE 5502XA is processed as a high-molecular-weight blow moulding grade with a melt flow rate of 0.22 g/10 min at 190 °C/2.16 kg per ISO 1133-1 and a density of 0.955 g/cm³ at 23 °C per ISO 1183-1. On a 60–75 mm grooved-feed extruder with 24–30:1 L/D, the die-entry melt temperature is normally set at 195–205 °C; the barrel front zone is held 5–10 °C lower to avoid low-molecular-weight tail formation. Because the melt viscosity is higher than that of a 0.35 g/10 min blow moulding comparator, head pressure may rise 8–12 % at constant screw speed, so start-up should trim screw speed against motor amperage rather than against cycle-time targets. The initial die ring flat gap is widened 0.2–0.5 mm beyond the comparator setting to compensate for higher die swell, then closed by the parison programmer to a final gap of 1.2–1.5 mm for sidewall control. Pre-blow air is set at 0.6–0.8 MPa, final blow at 0.8–1.0 MPa, and mould cooling water at 12–18 °C; operation below 8 °C at relative humidity above 60 % causes condensation pitting on mould faces and rejects at the station.

    Wall-thickness distribution is regulated by a 10-point parison programmer, with ultrasonic scanning of the finished container on a 20-point grid. The limiting feature in drop tests is the pinch-off seam root; worn pinch lands below 0.8 mm produce seam-root thinning even when the sidewall remains within tolerance. Pinch lands are inspected every 5,000 cycles and reground when wear exceeds 0.1 mm. In-line granulation of flash is acceptable up to 30 wt% regrind if the scrap is dry, ink-free, and passed through a 10 mm protection screen; once regrind exceeds 35 wt%, the -18 °C UN drop test on the chime and closure neck should be repeated because weld-line impact properties begin to degrade before low-temperature ductility is visible in routine tensile tests.

    For chemical resistance, the base grade carries no UV stabilizer or antistatic agent. Outdoor storage of jerricans therefore requires a UV package added at the blow moulder, typically 0.15–0.25 wt% hindered amine light stabilizer plus 0.05–0.10 wt% UV absorber. Hydrocarbon packing lines must not use generic HDPE permeation coefficients to set shelf-life thresholds; published permeation coefficients for 5502XA in formulated agrochemical mixtures with ester solvents, surfactant fractions, or aromatic hydrocarbons are limited, and the packer should test the actual fill liquid at 40 °C under ASTM D2684 or an equivalent internal protocol before committing to a shelf-life specification.

    What Limits Parison Sag, Not Just ESCR, in Six-Layer Automotive Fuel Tanks?

    Six-layer coextrusion of 5502XA into automotive fuel tanks places the resin in the outer and inner virgin layers of an HDPE/regrind/tie/EVOH/tie/HDPE stack on accumulator-head machines with 2–5 kg shot capacity. The process control variable that determines scrap rate is parison sag between accumulator discharge and mould close; the high viscosity of 5502XA reduces sag but lengthens accumulator refill time. Barrel zones in the HDPE extruder are set 5–10 °C higher than monolayer jerrican processing, with die-head melt temperature held at 200–210 °C and the accumulator body held at 190–205 °C to preserve melt strength. Residence time in the accumulator should not exceed 8 min at 210 °C; longer hold times generate gel specks and black specks on the tank inner wall that are not removed by downstream fluorination.

    Virgin HDPE outer and inner layers together usually account for 30–50 % of the 5–7 mm wall, the regrind core for 40–60 %, and the tie/EVOH/tie barrier package for 3–5 %. The pinch-off seam is compressed at 25–35 N/mm² and should not be thinned below 2.5 mm at the seam root; seam-root thinning below that value creates a plane for crack propagation during pressure cycling under SAE J1737. Because unmodified HDPE 5502XA does not by itself control hydrocarbon permeation, the EVOH barrier and closure system are the primary compliance elements; fluorination of 10–40 µm depth may be applied to the virgin layer, but the exact depth is fuel-grade specific and must be validated by the fluorination contractor. Mechanical release testing on specimens cut from the tank wall under ASTM D638-14 shows that the axial tensile yield can differ from compression-moulded plaques by 10–20 % because of blow orientation; therefore release limits must be set from blow moulded specimens, not from raw material certificates.

    Coextrusion die design for 5502XA in fuel tank service uses a multi-manifold accumulator head, not a spiral mandrel die, because the outer HDPE layer must be switched from virgin to regrind during the shot. Layer-adapter flow channels are kept above 190 °C but below 220 °C; local hot spots above 230 °C in the adapter generate gels that appear as elongated streaks in the sidewall. The die gap is trimmed on a 6-point radial adjuster to correct side-to-side wall variation above 0.2 mm; ultrasonic wall scans after each start-up are compared against a golden-tank thickness map. If the outer virgin layer drops below 0.8 mm at any scan point, fluorination coverage can be discontinuous and hydrocarbon permeation rises outside the pass band.

    Indicative extrusion blow moulding envelope for HDPE 5502XA across three downstream configurations
    Control variableUN 3H1/Z220 jerrican 20–30 LSix-layer automotive fuel tankClosed-head 220 L drum
    Die-entry melt temperature195–205 °C200–210 °C190–205 °C
    Blow pressure0.6–1.0 MPa0.8–1.1 MPa0.8–1.2 MPa
    Mould cooling water12–18 °C8–15 °C8–12 °C
    Maximum regrind30–35 wt%40–60 wt% in core layer20–30 wt% post-industrial
    Release gateUN drop at -18 °CFuel permeation under SAE J1737Hydrostatic 100 kPa × 24 h

    Closed-head 220 L drums blow moulded from 5502XA on single-station accumulator machines require melt delivered at 190–205 °C from a 120 mm grooved-feed extruder with 30–36:1 L/D. Ultrasonic wall thickness scanning on a 20-point grid is used to keep the chime corner above 2.0 mm, because the top chime absorbs most of the UN 1H1/Z200 drop energy. Aluminium mould cooling water is held at 8–12 °C, with internal air blast after extraction until inner wall temperature falls below 60 °C; release above that threshold produces base dimpling and loss of stacking flatness. Cycle time for a 220 L drum is 4–7 min and is dominated by cooling, not by extruder throughput.

    The pinch-off compression ratio is maintained at 5:1–8:1 to produce a weld line that survives hydrostatic testing at 100 kPa for 24 h without weeping. After demoulding, the weld tail is trimmed flush; a ragged tail concentrates stress during stacking and vibration testing. Post-industrial regrind is limited to 20–30 wt% because drums processed with higher regrind levels show lower ASTM D1693 Condition B failure energy in 10 % Igepal CO-630 at 50 °C; post-consumer drum scrap is not recommended for UN-certified service unless it passes melt filtration through a 120 µm screen and a visual contamination check under 200 lux.

    The blow mould for 220 L drums is run with sequence-controlled pressure: pre-blow at 0.4–0.6 MPa for the first 1.5–2.5 s, then final blow at 0.8–1.2 MPa. Pre-blow that is too high stretches the bottom corners and thins the chime; pre-blow that is too low does not push melt into the top band before the wall freezes. Venting of the mould cavity is through 0.02–0.05 mm vent channels at the top bead area; blocked vents cause entrapped air marks and local weld-line porosity. The extruder screen pack is 40/60/80 mesh during start-up and is replaced or inverted after 24 h of continuous running if head pressure exceeds the safe upper limit of the extruder flange.

    Interior Water Tank Stress Cracking and Chlorine Resistance; a Test Cut from the Weld Line

    Water storage vessels from 200–1000 L are blow moulded as vertical cylinders with integrally moulded fittings, using die-head melt temperature of 190–205 °C, blow pressure of 0.8–1.1 MPa, and aluminium mould temperature of 10–20 °C. The stress-cracking mechanism in chlorinated potable water is oxidative attack at weld lines rather than aliphatic hydrocarbon absorption, so the release gate is not a standard hydrocarbon ESCR test. Specimens cut from the tank base weld line are exposed to 2 % chlorinated water at 60 °C for 1000 h; this protocol is adapted from ISO 16770 full-notch creep testing and is specific to the fabricator, because the welded fitting geometry controls stress concentration. The weld region must not show a visible flow line or a notch deeper than 0.2 mm. Post-mould shrinkage of 5502XA in large flat side walls is 1.5–2.0 % after 24 h, so mould dimensions must include this allowance and the first-shift inspection must measure the diagonal of the tank mouth.

    Compliance for potable water contact is governed by the finished article under NSF/ANSI 61 or AS/NZS 4020, not by the resin raw material certificate alone; the tank fabricator must qualify the complete construction including welded fittings, gaskets, and any post-mould machining. In production audits, the most frequent defect is a blow-pin witness mark pinhole at the nozzle, caused by inner wall temperature above 70 °C during bladder release or by incorrect pre-blow delay. Pre-blow delay is set at 0.5–1.2 s after mould close; early pre-blow traps air at the pinch, while late pre-blow allows the parison to sag and the top wall to thin. These settings are machine-specific and cannot be transferred directly between shuttle and accumulator platforms.

    In potable water tank production, cooling channel spacing in the aluminium mould is 40–60 mm, with cooling water at 10–20 °C and a Reynolds number above 4,000 in the circuit to maintain turbulent heat transfer. Low-flow laminar cooling produces differential shrinkage across the sidewall, visible as waviness and high residual stress after demoulding. The mould is fitted with mechanical ejectors and air ejectors; ejection air pressure is limited to 0.2–0.4 MPa to avoid localized surface deformation. Stacks of finished tanks are aged for 24 h before welding of fittings, because immediate welding of warm, shrinking parts shifts the fitting alignment and creates a high-stress heat-affected zone.

    During blow moulding of diesel exhaust fluid storage tanks with 32.5 wt% aqueous urea, the controlling failure mode is stress cracking initiated at heated connectors, welded inserts, and squeeze-pinch zones, not permeation through the shell. Specimens cut from the squeeze-pinch zone are exposed at fixed strain of 1.0 % in 32.5 wt% urea at 60 °C for 500 h; published data for 5502XA in this specific urea environment is limited, so OEM qualification must include this exposure and should not rely on generic detergent ESCR results. HDPE extruder barrel temperatures are held at 185–200 °C, with die-head melt at 190–200 °C; the lower temperature limit reduces thermal degradation of the melt while maintaining hot-plate weldability of fittings. Contact between molten HDPE and brass tooling is avoided during start-up purging, because copper migration into the surface layer can accelerate oxidative degradation in aqueous urea service.

    Hot-plate welding of caps, spuds, and brackets to the DEF tank shell is performed at 205–215 °C with 0.3–0.6 MPa weld pressure and bead squeeze-out of 0.5–1.0 mm; the squeeze-pinch region is permitted to contain regrind only if the regrind stream is sourced from unpainted, unfilled DEF tank scrap. The final assembly is pressure-tested at 30 kPa for 30 min and vibration-tested with the tank 50 % filled; failures are normally located at weld lines where the wall thickness has fallen below 1.5 mm or where the hot-plate bead has been shaved too aggressively.

    Welded inserts in DEF tanks are produced from the same HDPE family or an approved HDPE compound; mixing with polypropylene inserts is rejected because the weld strength at the dissimilar interface drops below 10 MPa and failure occurs under cold impact. Insert and tank body are cleaned with 70 % isopropanol and dried before hot-plate welding; surface moisture above 0.1 g/m² produces steam bubbles at the weld plane and reduces burst pressure. The weld bead is not shaved below 0.5 mm; shaving to the parent surface removes stress-bearing material and opens a notch at the weld root.

    For pharmaceutical and food-powder intermediate containers, the selection of 5502XA is governed by long environmental stress crack resistance and high weld strength after multiple drop cycles, not by optical clarity or low-temperature impact alone. The blow moulder verifies migration under EU 10/2011 or FDA 21 CFR 177.1520(c) for the finished liner, not for the raw resin alone, because additives and masterbatches added downstream determine final compliance. Cold start-up requires purging with a low-density polyethylene at 170–180 °C before introducing 5502XA; direct extrusion below 150 °C is avoided because the high melt viscosity at low temperature generates excessive screw torque and surface melt fracture. When the line stops for more than 15 min, the die head is held at 180 °C and the next 2 kg of melt is purged before production resumes.

    Liners intended for dry food powders are tested for stress cracking with the actual filling medium because coconut oil, mineral oil, and fine powders can alter surface wetting and crack initiation even though the base resin is chemically resistant. Published data for 5502XA in dry powder and pharmaceutical intermediate contact is limited; packers must conduct a migration test under ASTM D4754 or the applicable food-contact protocol using the actual finished article. Pre-drying is not normally required for HDPE 5502XA, but silo transfer at low temperature into a warm humid plant can condense surface moisture; if condensation is visible, the resin is brought to ambient temperature and the surface moisture removed before the extruder throat to prevent streaking and die-lip deposit formation.

    Cleaning between dark coloured and natural runs of 5502XA uses a purge sequence of low-density polyethylene at 170–180 °C followed by the next product's own scrap. Colour change without adequate purge leaves streak contamination in the first 50–100 kg of production; therefore a 100 kg purge buffer is common when moving from black to natural food-contact liners. The purge material is segregated and cannot be returned to food-contact regrind unless it meets the same migration specification. If a melt pump is installed, differential pressure across the pump is kept below 8 MPa; higher differential pressure indicates screen pack plugging and poor melt quality.

    Free Quote

    Competitive SSTPC (Sinopec SABIC Tianjin) HDPE 5502XA prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SSTPC HDPE 5502XA is a high-density polyethylene copolymer manufactured and supplied by Sinopec SABIC Tianjin Petrochemical Co., Ltd. The resin is positioned for extrusion blow molding of rigid packaging, including narrow-neck bottles, jerry cans, and intermediate bulk containers for detergent, solvent, food, and pharmaceutical fluids. Technical data sheets characterize the product by a nominal density of 0.955 g/cm³ (ASTM D1505) and a melt flow rate of 0.35 g/10 min at 190 °C/2.16 kg (ASTM D1238). The high-load melt index at 190 °C/21.6 kg is typically 9.0 g/10 min. This combination yields a flow rate ratio of approximately 25.7:1, which indicates a broad molecular-weight distribution that supports parison melt strength, die-swell stability, and shear-thinning behavior in blow molding tooling. The resin is used where containers must withstand stacking, drop impact at low temperatures, and environmental stress cracking from aggressive formulations. These performance attributes are typically measured by ASTM D1693, ASTM D638, and ISO 180/A. The product is not intended for high-speed thin-wall injection molding, rotational molding, or blown film extrusion.

    The XA suffix in SSTPC nomenclature does not represent a standardized comonomer or catalyst designation across all polyolefin producers. Public technical literature identifies the suffix as a commercial variant with a specialized additive package for packaging lines; the full additive formulation is proprietary. Converters should therefore treat 5502XA as a distinct commercial specification with the same base polymer architecture as the 5502 range but with stabilized handling and packaging performance. When exact additive composition is critical for end-use certification, formal documentation should be requested from the supplier because published data for this specific configuration is limited.

    Resin architecture and molecular-weight distribution

    The density value of 0.955 g/cm³ is lower than typical fully linear unimodal HDPE grades in the 0.960–0.965 g/cm³ range, indicating controlled short-chain branching from an alpha-olefin comonomer. This branching disrupts crystalline packing and lowers flexural modulus while increasing environmental stress crack resistance measured according to ASTM D1693 in 10% Igepal CO-630 at 50 °C; the F50 value is typically >30 h. The high-load melt index to melt flow rate ratio of 25.7:1 is the principal rheological indicator for converters because it correlates with shear-induced thinning in die tooling and with sag resistance after parison extrusion. At apparent shear rates typical of extrusion blow molding dies, 100–500 s⁻¹, the material exhibits pronounced shear thinning, while the low-shear melt viscosity remains sufficient to limit parison drawdown on tooling with die diameters from 70 mm to 150 mm. A density of 0.955 g/cm³ corresponds to a crystalline fraction of approximately 68–70% when calculated against the commonly used two-phase model of 1.000 g/cm³ crystalline and 0.855 g/cm³ amorphous polyethylene. Grade-specific molecular-weight averages such as Mw, Mn, and Mz are not consistently disclosed in current SSTPC technical data sheets; published data for this specific configuration is limited, and converters should rely on flow rate ratio, die swell, and melt strength measurements rather than inferred GPC values.

    Additive packages in 5502XA include primary and secondary antioxidants sufficient to protect melt during multiple extrusion heats, but the detailed stabilization chemistry is not disclosed in standard technical literature. No intentionally added plasticizer or slip agent is identified in commercially available documentation. As with all HDPE blow molding grades, the incorporation of post-consumer recyclate alters flow rate ratio and ESCR; processors should validate each formulated blend by ASTM D1238, ASTM D1693, and ASTM D638 before production qualification.

    PropertyTypical ValueTest Method
    Density0.955 g/cm³ASTM D1505
    Melt flow rate at 190 °C/2.16 kg0.35 g/10 minASTM D1238
    High-load melt index at 190 °C/21.6 kg9.0 g/10 minASTM D1238
    Tensile stress at yield27 MPaASTM D638, Type IV, 50 mm/min
    Elongation at break>600%ASTM D638
    Flexural modulus1200 MPaASTM D790
    Notched Izod impact at 23 °C6 kJ/m²ISO 180/A
    ESCR, 10% Igepal CO-630, 50 °C, F50>30 hASTM D1693
    Vicat softening temperature127 °CASTM D1525
    Brittleness temperature<-70 °CASTM D746

    Why does back pressure during extrusion blow molding affect melt integrity?

    In continuous extrusion blow molding, back pressure is generated by the die head, mandrel, and parison programming tooling rather than by a shut-off nozzle as in injection molding. A back pressure of 10–20 MPa upstream of the die head is typical for HDPE 5502XA on a 90 mm single-screw extruder with 30:1 L/D, a barrier feed section, and a Maddock mixer. Barrel set points of 170–200 °C, adapter and head set points of 200–210 °C, and a melt temperature of 200–225 °C maintain homogeneous melt without exceeding the oxidative threshold near 230 °C. At melt temperatures above 230 °C, residence times must be kept below 5 min; otherwise chain scission manifests as reduced parison hang, increased die-lip deposit, and reduced notched Izod impact measured at 23 °C by ISO 180/A.

    The low standard melt flow rate of 0.35 g/10 min means that intensive shear in the screw compression zone is required to avoid unmelted gel particles. Screw speed on a 90 mm extruder is commonly set at 45–70 min⁻¹, with head pressure 18–25 MPa. Die swell for this grade is typically 25–35% under these conditions, requiring tooling with a die gap from 1.5 mm to 2.5 mm for wall thicknesses between 1.2 mm and 3.0 mm. Pre-drying is not required for virgin pellets at relative humidity below 60%; at higher humidity or with hygroscopic regrind, surface moisture can generate splay and melt-pressure fluctuation. Regrind addition up to 30 wt% is generally tolerated when sieved to 8 mm and metered separately, but blend melt index must be revalidated according to ASTM D1238.

    When surface moisture is suspected, a desiccant hopper dryer set to 70–80 °C for 2–4 h can restore consistent extrusion, but drying must not exceed 90 °C to avoid pellet agglomeration. Processing with a grooved feed section increases throughput and melt pressure stability, but barrel temperature in the feed zone must remain below 80–90 °C to prevent premature melting and feed angle slip.

    When HDPE 5502XA replaces lower-molecular-weight injection-molding grades

    When a converter considers HDPE 5502XA as a replacement for a lower-molecular-weight injection-molding HDPE with a melt flow rate of 8–20 g/10 min (ASTM D1238, 190 °C/2.16 kg), the process boundary changes from injection molding to extrusion blow molding. The low melt flow rate of 0.35 g/10 min precludes short filling of thin-wall injection cavities with flow-length-to-wall-thickness ratios above 150:1. Instead, the product is processed on accumulator-head or continuous shuttle blow molding machines with clamp force typically 250–350 kN for 20–30 L containers.

    Property differences are not limited to rheology. Typical tensile stress at yield is 27 MPa (ASTM D638, Type IV, 50 mm/min), compared with approximately 30–32 MPa for some 0.960 g/cm³ injection-grade HDPE resins. The flexural modulus of 1200 MPa (ASTM D790) is lower than high-density injection grades exceeding 1500 MPa, while ESCR values are significantly higher: >30 h by ASTM D1693 versus values below 10 h often reported for lower-molecular-weight, narrow-MWD injection grades. These differences favor 5502XA for aggressive chemical packaging, but top-load stiffness is reduced and must be compensated by increased wall thickness or container ribbing.

    Compared to higher-density unimodal blow-molding HDPE at 0.960–0.965 g/cm³, the density of 0.955 g/cm³ provides a larger tie-molecule population and improved stress-crack resistance under ASTM D1693, but lower tensile yield and lower Vicat softening temperature of 127 °C (ASTM D1525). The grade is therefore preferred when stackability and continuous chemical contact dominate; it is less appropriate for hot-fill packaging above 90 °C or for applications requiring continuous service temperatures above 70 °C under load.

    Food-contact and packaging compliance is governed by extraction, migration, and heavy-metal standards

    Regulatory compliance for completed packaging depends on the finished article, not solely on the resin. Typical certificates for HDPE 5502XA reference polyolefin food-contact status under 21 CFR 177.1520(c), pending end-use extraction testing with the actual container geometry and barrier layer configuration. In the European Union, compliance is assessed under Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm². Chinese food-contact evaluation under GB 4806.7-2016 applies total migration limits of 10 mg/dm², potassium permanganate consumption of 10 mg/kg, and heavy metal as lead of 1 mg/kg.

    For non-food industrial packaging, REACH Regulation (EC) No 1907/2006 requires communication of substances of very high concern above 0.1 wt% in the article; no SVHC is identified for the standard pellet form in available safety data sheets. RoHS Directive 2011/65/EU Annex II is not a primary packaging regulation but applies when HDPE packaging is incorporated into electrical and electronic equipment. Standards cited in qualification protocols commonly include ASTM D1505 for density, ASTM D1238 for melt flow rate, ISO 180/A for notched Izod impact, and ASTM D1693 for environmental stress crack resistance.

    Regulatory DomainStandard or RequirementApplication Condition
    U.S. FDA21 CFR 177.1520(c)Olefin polymer food-contact base resin; finished article extraction validation required
    European Union(EU) No 10/2011Overall migration ≤ 10 mg/dm²; specific migration limits by food simulant
    ChinaGB 4806.7-2016Total migration ≤ 10 mg/dm²; potassium permanganate consumption ≤ 10 mg/kg; heavy metal as Pb ≤ 1 mg/kg
    EU chemicalsREACH (EC) No 1907/2006SVHC notification above 0.1 wt%; standard grade data sheet indicates no intentionally added SVHC
    Electrical/electronic equipmentRoHS Directive 2011/65/EU Annex IIRestricted substances relevant when packaging is integrated into EEE

    Production of 20–30 L jerry cans for detergent and solvent packaging on a long-stroke accumulator blow molding machine illustrates the operational limits of HDPE 5502XA. A typical configuration uses a 60 mm extruder with 30:1 L/D, a 1.5 kg accumulator head, a 70 mm die, and a mold closing force of 250–300 kN. Barrel profile from feed to metering is 160/175/190/200 °C, head and die zones at 200 °C, and melt temperature measured by infrared pyrometer at 210–220 °C. Cycle time for a 1.8–2.2 mm nominal sidewall is 45–60 s, including parison programming, mold close, blow, exhaust, and part removal. Under these conditions, the high-load melt index of 9.0 g/10 min provides sufficient extrusion throughput while the low standard melt flow rate of 0.35 g/10 min prevents parison drawdown before mold closing.

    Drop impact at -18 °C and stress-crack resistance under ASTM D1693 are the principal release tests for detergent and agrochemical containers. Finished containers must also be evaluated for top-load strength according to ASTM D2659 and for leakage according to ASTM D4991 or the applicable UN packing group test protocol. Processing constraints include avoiding melt temperatures above 230 °C for more than 5 min, maintaining regrind below 30 wt% unless ESCR is revalidated, and excluding copper-based heat stabilizers if the container is intended for chlorinated solvents because metallic residues can accelerate oxidative degradation.