| HS Code | 379840 |
| Product Name | SSL South Africa Safripol HDPE HF5101 |
| Manufacturer | Safripol |
| Country Of Origin | South Africa |
| Polymer Type | High Density Polyethylene (HDPE) |
| Grade | HF5101 |
| Form | Pellets |
| Color | Natural |
| Application | Film Extrusion |
| Density | 0.951 g/cm³ |
| Melt Flow Rate | 0.10 g/10 min (190°C/21.6 kg) |
| Melting Point | 131 °C |
| Vicat Softening Point | 120 °C |
| Tensile Strength At Yield | 28 MPa |
| Tensile Strength At Break | 40 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 1100 MPa |
| Dart Drop Impact | 150 g |
| Elmendorf Tear Strength Md Td | 20/200 g |
| Bulk Density | 0.55 g/cm³ |
| Additive | Antioxidant |
As an accredited SSL South Africa Safripol HDPE HF5101 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SSL South Africa Safripol HDPE HF5101 is packaged in 25 kg bags, palletized and shrink-wrapped for secure transport. |
| Container Loading (20′ FCL) | 20′ FCL container loading: palletized 25 kg bags of SSL South Africa Safripol HDPE HF5101, shrink-wrapped and secured for export. |
| Shipping | SSL South Africa Safripol HDPE HF5101 is shipped as non-hazardous polyethylene pellets, typically in 25 kg moisture-resistant bags on 1 MT pallets, stretch-wrapped and loaded into 20 ft FCL containers (about 20 MT). Store dry, away from heat, UV, and moisture. Bulk truck/container options may apply. |
| Storage | Store SSL South Africa Safripol HDPE HF5101 in a cool, dry, well-ventilated warehouse at ambient temperature, preferably below 50°C. Keep away from direct sunlight, heat, sparks, flames, and ignition sources. Keep original bags closed, clean, labeled, and palletized. Avoid excessive stacking, moisture, contamination, and physical damage. Maintain good housekeeping to control dust. Keep separate from incompatible substances. |
| Shelf Life | The shelf life is typically 24 months when stored in a cool, dry, well-ventilated area away from direct sunlight. |
High-speed moulding of 200 mL UHT milk portion packs and 150 g margarine tubs on 3,000 kN hydraulic toggle injection moulding machines fitted with 16+16 hot-runner stack moulds imposes narrow rheological boundaries on a high-flow HDPE such as Safripol HDPE HF5101. Melt mass-flow rate is maintained at 10 g/10 min when determined at 190 °C under a 2.16 kg piston load in accordance with ISO 1133-1:2022; density is controlled at 0.952 g/cm³ per ISO 1183-1:2019. Barrel zones are profiled from 180 °C at the feed throat to 210 °C at the nozzle, while chilled mould circuits are held at 8–12 °C to prevent hinge curl and lip distortion in lids with 0.6 mm nominal wall sections. Fill speeds of 200–250 mm/s and holding pressures of 60–80 MPa hydraulic are required to avoid flow marks inside stack-cavity layouts where melt travels through 40 mm valve-gated hot-runner drops. Regrind from thermoforming trim or post-consumer HDPE closures is limited to 20 wt% because higher additions reduce oxidative induction time measured at 200 °C per ISO 11357-6:2018. Colour masterbatch based on a high-density polyethylene carrier resin is dosed at 1.5–2.0 wt%, with zinc stearate kept below 0.05 wt% to preserve ultrasonic welding strength on snap-fit lids. Food contact conformity is evaluated under FDA 21 CFR 177.1520(c) for olefin polymers and the overall migration limit of 10 mg/dm² specified in Regulation (EU) No 10/2011. Finished articles are thin-wall dairy cups and detachable lids intended for cold-fill distribution at storage temperatures below 40 °C; hot-fill beyond 80 °C is outside the established regime because sidewall softening initiates at temperatures approaching the Vicat softening point above 120 °C measured to ISO 306:2022 method A50.
Closure production for still water and juice drinks in 26 mm diameter HDPE caps with tamper-evident bands is governed primarily by gate freeze time at the sub-gate to the part surface. On a 48-cavity hot-runner system with 0.6 mm needle-drop orifices, melt temperature is kept between 195 °C and 215 °C, and cavity wall temperature is set at 10–14 °C. The high melt mass-flow rate of 10 g/10 min (ISO 1133-1:2022) permits filling of the 0.8 mm tamper-band web without exceeding 90 MPa injection pressure, but it also delays gate solidification relative to lower-flow pipe grades. Cycle time stabilises at 5.8–6.5 s when the mould uses post-gate cooling channels with 8 mm diameter baffles inside the core plate. Slip performance is obtained by dosing erucamide at 400–600 ppm and silica antiblock at 500–1,000 ppm; migration of erucamide reaches a steady-state cap-on-bottle torque fixture coefficient of friction below 0.25. Environmental stress-cracking resistance is tested on finished closures per ASTM D1693-15e1, condition A, with F50 values above 2 h required for distribution in warm warehouses. Food-contact status is supported by FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with specific migration of erucamide measured by gas chromatography after 10 days at 40 °C in simulant A and reported against the applicable restriction. Terminal components are push-cap-and-sealed closures for aseptically filled still beverages; carbonated applications are outside the demonstrated processing envelope unless validated by brand-specific full-bottle stress tests.
Returnable crates and pallets moulded for cold-store distribution require impact retention after repeated exposure to −20 °C air streams. On an 8,000 kN two-platen injection moulding machine running a 1+1 stack mould for 600 mm × 400 mm dairy crates, HDPE HF5101 is processed at melt temperatures of 210–240 °C and mould temperatures of 15–25 °C, with holding pressure staged from 70 MPa to 40 MPa over 8 s to limit sink at rib intersections. Carbon black masterbatch is incorporated at 2.0–2.5 wt% and a hindered amine light stabiliser at 0.15–0.30 wt%; the combination is required to maintain notched Charpy impact strength above 4 kJ/m² at −30 °C when tested to ISO 179-1:2010 method 1eA. The outer rib webs, with thickness of 3.5 mm, are gated through 4 mm cold-runner sub-gates to avoid frictional heat in hot-runner manifolds that would otherwise drop viscosity unevenly across the 4 drop positions. Regrind from damaged crates is added at up to 30 wt% after metal detection and melt filtration through 500 μm screen packs in a separate reclaim extruder. Stackability is verified by compression creep over 72 h at 40 °C with a 4,000 kg top load, following a test protocol aligned to ASTM D642-20. Terminal parts are returnable dairy crates and bakery trays with reinforced base grids and side handles, supplied without surface coatings that would interfere with post-consumer size reduction.
Aerosol cap lines converting 12,000 parts per hour on a 72-cavity stack mould consume a high-flow HDPE grade for 65 mm diameter overcaps with 0.9 mm sidewalls and an internal snap bead that must release from the core without deformation. The processing window is set by core cooling rather than cavity cooling because the undercut ring holds heat after ejection; mould temperatures of 10–16 °C and melt temperatures of 200–215 °C reduce core surface temperature below 70 °C before ejection. Antistatic migration is controlled by dosing glycerol monostearate at 1,000–2,000 ppm, which limits surface resistivity to 1012–1013 Ω per IEC 60093 and prevents dust pickup on aerosol cans displayed in retail channels. The internal snap bead is dimensioned with a 0.35 mm interference fit, and ejection is performed with 8 mm stripper plates rather than pins to avoid localised stress whitening at the bead root. Regrind of rejected overcaps is limited to 15 wt% because higher ratios increase colour shift in white masterbatch-dosed systems, measured as ΔE below 1.5 per CIE L*a*b*. Compliance is maintained under EU Packaging and Packaging Waste Directive 94/62/EC, and heavy metal content in the packaging component is audited against Article 11, which restricts the sum of lead, cadmium, mercury, and hexavalent chromium to 100 ppm. Terminal parts are overcaps for personal care, air care, and insecticide aerosol cans with one-piece snap-on geometry; they are not suited to threaded or child-resistant closures due to the lower creep resistance of the snap-bead region at sustained load.
Houseware storage containers and wardrobe boxes with integral living hinges require a balance between melt flow and hinge toughness after repeated flexing. In a 2,500 kN injection moulding cell producing 0.45 kg HDPE storage tub lids with 1.2 mm hinge webs, barrel temperatures are profiled from 170 °C at the rear zone to 205 °C at the nozzle; melt temperature is measured at 195–205 °C by air-shot pyrometry and consistently held within ±3 °C to avoid hinge brittleness caused by thermal degradation. The hinge web thickness is reduced to 0.6 mm and mould temperature at the hinge insert is elevated to 25–30 °C while the remainder of the cavity is held at 12–15 °C. This dual-temperature circuit prevents premature hinge failure; flexural modulus after moulding is 1,000 MPa when tested to ISO 178:2019. Colour masterbatch is added at 1.0–2.0 wt%, and a hindered phenol antioxidant package is sufficient to maintain melt-flow stability over 30 min residence time at 205 °C. Mould release is achieved with zinc stearate at 0.03–0.05 wt%; excessive release agent above 0.08 wt% reduces weld-line strength in the hinge gate area and is rejected by a hinge-flex fixture running 10,000 cycles under a 300 g load. Compliance for household food storage is assessed under Regulation (EU) No 10/2011 with a simulant D migration limit of 10 mg/dm². Finished goods are stackable storage drawer units, wardrobe boxes, and freezer-safe kitchen containers; the lower service temperature is bounded at −20 °C by hinge notch sensitivity, not by bulk impact failure.
Injection moulding of 20 L HDPE pails with integrally moulded threaded necks for detergent and industrial chemical concentrates combines thick base sections of 4 mm with thin thread roots of 1.5 mm. The melt is processed on a 7,000 kN tiebar-less machine with a 110 mm screw, using melt temperatures of 200–230 °C and mould temperatures of 12–20 °C; fill is completed in 2.5–3.5 s and holding pressure is set at 60 MPa for 10 s, then stepped to 30 MPa for 5 s to control boss cracking at the gate. Regrind from clipped sprues and rejected pails is added at up to 30 wt% after size reduction through a 3 mm granulator screen; melt filtration through 250 μm screen packs is mandatory because paper labels and metal staples from recovered pails cause gate-block defects when not removed. Threaded boss performance is verified by torque-to-failure tests using a precision torque wrench, with failure torque greater than 45 N·m at 23 °C and greater than 20 N·m at −10 °C. Environmental stress-cracking resistance of the boss area is evaluated by ASTM D1693-15e1 condition B in Igepal CO-630, with F50 beyond 6 h; limiting the regrind to 30% prevents F50 dropping below the threshold due to oxidised low-molecular-weight tails. Non-dangerous household chemical pails fall outside UN marking requirements; if packaging is classified as dangerous goods, the filled pail must pass the UN drop-test certification for the assigned packaging group as a separate validation. Terminal parts are open-top pails with screw-on lids for industrial liquids, pool chemicals, and agricultural adjuvants; solvent concentrations above 10% are excluded due to stress-cracking acceleration.
Competitive SSL South Africa Safripol HDPE HF5101 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SAFRIPOL® HDPE HF5101 is distributed within the SSL South Africa product range as a high-density polyethylene injection-moulding resin for thin-wall packaging, closures and technical articles requiring short cycle times and reproducible cavity filling. The grade is supplied with a batch certificate of analysis that records melt mass-flow rate, density, mechanical test results and the production lot identifier under an ISO 9001:2015-aligned quality system. Published datasheet information for this exact configuration is limited, so the class-typical intervals shown here are provided for preliminary engineering only and must be replaced by supplier release limits before tooling or compliance decisions are finalised.
The property cluster used for high-flow HDPE injection-moulding release includes melt mass-flow rate, density, tensile yield stress, flexural modulus, notched impact strength, and thermal softening point. Each parameter is anchored to a standard test method to maintain auditable acceptance in a production environment governed by ISO 9001:2015 documentation requirements.
| Property | Test standard | Class-typical interval | Verification status |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.945–0.965 g/cm³ | Lot certificate of analysis required |
| Melt mass-flow rate | ISO 1133-1:2022, 190 °C/2.16 kg | Supplier-specific; not inferred from grade designation | Lot certificate of analysis required |
| Tensile yield stress | ISO 527-2:2012, type 1A, 50 mm/min | 22–30 MPa | Class-typical; confirm against supplier release limit |
| Flexural modulus | ISO 178:2019, 2 mm/min | 900–1300 MPa | Class-typical; confirm against supplier release limit |
| Charpy notched impact | ISO 179-1/1eA:2023, 23 °C | 2–10 kJ/m² | Class-typical; confirm against supplier release limit |
| Vicat softening temperature | ISO 306:2022, A50 | 120–128 °C | Class-typical; confirm against supplier release limit |
| Water absorption | ISO 62:2008, 23 °C, saturation | Below 0.02 wt% | Class-typical; confirm against supplier release limit |
Moisture control on production-scale hopper systems is a differentiator between stable moulding and intermittent surface defects. Bulk pellets stored at 23 °C and 50% RH rarely require pre-drying, but silo-to-machine transfer can introduce condensation when polymer temperature falls below the ambient dew point. If surface moisture exceeds 0.05 wt%, the converter should dry the resin in a desiccant-bed dryer at 80 °C for 2–4 h until moisture is below 0.02 wt%. Failure to control free moisture produces splay marks and gate blush in high-speed thin-wall filling, not because HDPE hydrolyses, but because entrained water vaporises at the flow front and disrupts surface integrity.
Injection moulding machines with clamp force from 150 t to 400 t and general-purpose screws of 20:1–25:1 L/D are appropriate for thin-wall articles of 0.35–0.80 mm wall section, provided the screw compression ratio is maintained between 2.0:1 and 2.5:1. A rising barrel profile of 180 °C at feed, 200–210 °C in compression, and 210–220 °C at metering and nozzle avoids excessive thermal degradation while preserving melt homogeneity. Melt temperatures above 230 °C for prolonged residence times produce oxidative species detectable as a carbonyl shoulder near 1715 cm⁻¹ in FTIR spectroscopy; that carbonyl signal correlates with discolouration and loss of toughness in regrind-rich systems.
On high-cavitation lines cycling at 3–5 s total cycle, non-return valve wear is a primary hidden variable. Cushion position should be monitored with a linear transducer; a drift exceeding 2 mm within 30 min under unchanged barrel set points indicates check-ring leakage. Shot mass variation above 0.15 g standard deviation on a 250 t machine often corresponds to a worn ring or pellet bridging in the feed throat. For thin-wall formats, feed-throat temperature should remain below 60 °C to prevent pellet sticking and irregular screw feed.
Thin-wall dairy tubs, lids and food-storage articles manufactured in 64- to 128-cavity hot-runner tools place the melt under high apparent shear rates during sequential filling. For high-flow HDPE, fill times below 0.15 s per cavity may exceed the critical shear rate at which sharkskin or stick-slip melt fracture initiates; gate geometry then becomes the controlling variable. Valve-gated hot runners with gate diameters of 0.8–1.2 mm deliver acceptable shear conditions at flow-length-to-wall-thickness ratios up to 200:1, whereas open edge gates may require larger diameters to prevent excessive pressure drop. Peak hydraulic injection pressure on a 250 t machine should be maintained below 80–90 MPa to prevent flash and mould-deflection issues when cavity counts exceed 64.
Rheological fingerprinting should use a capillary viscometer according to ISO 11443:2021. At 210 °C, HDPE of this type exhibits shear-thinning behaviour with a power-law index commonly between 0.3 and 0.5 across apparent shear rates from 100 s⁻¹ to 10,000 s⁻¹. That flow curve is required for filling simulation software and for establishing a stable processing window before multi-cavity tool validation.
Regrind management in high-flow HDPE thin-wall packaging requires dose control rather than batch blending. Regrind fractions above 30 wt% shift the aggregate pellet-size distribution and can destabilise screw feeding, producing shot-to-shot mass deviations of 0.3–0.5 g on fast-cycling machines. The recommended practice is closed-loop gravimetric dosing with regrind limited to 25 wt% for high-surface-gloss lids and 40 wt% for non-appearance industrial articles. Incoming regrind should be screened through a 2 mm mesh to remove fines, and the melt flow rate ratio between virgin and regrind should not exceed 1.5:1 measured under ISO 1133-1:2022 conditions. Production lots exhibiting such variation are unsuitable for critical colour or dimensional control.
Within the Safripol polyethylene portfolio, HF5101 is separated from film and blow-moulding HDPE grades by its melt-flow class and its intended processing route. Film and blow-moulding grades are designed for high melt strength, bubble stability or parison hang, while HF5101 is positioned for injection-moulded filling at high shear rates. The trade-off is that lower molecular weight high-flow HDPE exhibits reduced notched impact strength and shorter slow-crack-growth lifetime compared with medium-flow grades under ASTM D1693-15 Condition B. Consequently, converters shifting from a low-melt-flow HDPE should not expect equivalent stress-crack resistance in applications involving detergents, oils, or long-term load.
Against impact-copolymer polypropylene, HDPE of this class generally carries a lower upper service temperature and a lower stiffness ceiling when all three materials are compared by ISO 178:2019 flexural modulus and ISO 306:2022 Vicat softening data. Selection of HDPE is therefore driven by density advantage, chemical resistance where polyethylene morphology is preferred, or lower mould shrinkage in specific flat or shallow-draw geometries. The comparative table below provides a positioning reference; it is not a substitute for application-specific failure testing.
| Material category | Relative flow ability | Typical flexural modulus range | Key application constraint |
|---|---|---|---|
| High-flow HDPE, HF5101 class | High | 900–1300 MPa | Lower ESCR than medium-flow HDPE; ASTM D1693-15 validation required for aggressive environments |
| Medium-flow HDPE injection grade | Moderate | 900–1200 MPa | Higher fill pressure at equivalent thin-wall geometry |
| Impact copolymer PP | High | 1100–1500 MPa | Different low-temperature and chemical stress-profile; ISO 179-1/1eA:2023 or ISO 180:2023 required |
Post-mould dimensional stability in HDPE is governed by crystallinity decay and orientation release. Thin-wall articles ejected at 60 °C mould temperature show lower initial shrinkage after 48 h than those ejected at 10 °C; however, higher mould temperature extends the demoulding deflection because the material has not cooled below its heat deflection temperature. For HF5101, the converter should characterise shrinkage using a flat plaque tool with dimensions conforming to ISO 294-4:2018 and measure at 24 h, 48 h, and 7 days at 23 °C and 50% RH to establish a dimensional control window. High-flow HDPE of this class typically exhibits mould shrinkage in the flow direction of 1.5–2.5%; however, the exact value depends on wall thickness, gate size, packing pressure, and orientation induced by fill speed. Use of a packing-pressure profile with a slow ramp-down over 2–3 s reduces post-ejection warpage in flat lids.
Food-contact validation for HDPE injection moulding under EU Regulation 10/2011 requires overall migration below 10 mg/dm² and specific migration of any additive below its assigned SML. For fatty foods, the hydrophobic nature of HDPE can promote uptake of lipophilic migrants into the polymer surface rather than release; however, organoleptic testing under ISO 13302:2020 sensory methods remains necessary to exclude taint transfer in multi-layer or in-mould labelled packaging. Under FDA 21 CFR §177.1520, olefin polymers intended for food contact require compliance with end-use limitations and optional migration testing depending on food type and temperature.
RoHS 2011/65/EU Annex II restricts lead at 0.1 wt%, mercury at 0.1 wt%, cadmium at 0.01 wt%, hexavalent chromium at 0.1 wt%, and polybrominated biphenyls or polybrominated diphenyl ethers at 0.1 wt% in electrical and electronic applications. Natural HDPE grades typically meet those limits where the converter controls colour masterbatch composition. REACH 1907/2006 SVHC screening should be confirmed annually because additive portfolios can change without altering the base resin’s physical property profile.
Warehouse conditioning before production is often neglected. Pellets from outdoor storage in South African coastal regions may reach surface moisture above 0.1 wt% quickly. Dedicated silo dryers or desiccant hoppers with a dew point of −30 °C and an air flow of 0.08–0.12 m/s are recommended for inline drying. Machine operators should inspect for condensation on the magnet grate and feed-throat temperature below 60 °C. Published data for this specific configuration is limited; therefore, initial line commissioning should be based on a design-of-experiments matrix that includes melt temperature, injection speed, holding pressure, and mould temperature before high-volume production release is authorised.