| HS Code | 949706 |
| Grade Designation | SK Geo Centric HDPE K8800 |
| Polymer Type | High-Density Polyethylene (HDPE) |
| Melt Flow Index 190 C 2 16 Kg | 0.08 g/10 min |
| Density | 0.954 g/cm³ |
| Tensile Strength At Yield | 25 MPa |
| Elongation At Break | >500% |
| Flexural Modulus | 900 MPa |
| Vicat Softening Temperature | 125 °C |
| Heat Deflection Temperature 0 45 Mpa | 75 °C |
| Shore D Hardness | 65 |
| Notched Izod Impact Strength | 200 J/m |
| Environmental Stress Crack Resistance F50 10 Igepal | >1000 h |
| Melting Point | 133 °C |
| Brittleness Temperature | < -70 °C |
| Thermal Expansion Coefficient | 1.5E-4 1/°C |
As an accredited SK Geo Centric HDPE K8800 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SK Geo Centric HDPE K8800 is supplied in 25 kg polyethylene-lined woven bags, palletized, or in 1,000 kg jumbo bags. |
| Container Loading (20′ FCL) | 20′ FCL loading for SK Geo Centric HDPE K8800: 25 kg bags, palletized, shrink-wrapped, securely stowed, approx. 18–20 MT. |
| Shipping | SK Geo Centric HDPE K8800 is shipped as non-hazardous solid resin pellets, typically in 25 kg bags or 500–1000 kg jumbo bags on pallets. Transport in clean, dry, closed containers or trucks. Store away from moisture, direct sunlight, heat, and contamination. No special dangerous goods classification required. |
| Storage | Store SK Geo Centric HDPE K8800 in its original sealed packaging in a cool, dry, well-ventilated warehouse. Keep away from direct sunlight, heat, flames, moisture, and strong oxidizers. Protect from dust, dirt, and other contaminants. Stack pallets securely to prevent deformation or bag damage. Maintain clean handling and follow the supplier’s SDS and local storage regulations. Do not puncture bags. |
| Shelf Life | Shelf life is typically 24 months when stored in a cool, dry, well-ventilated area away from direct sunlight and moisture. |
SK Geo Centric HDPE K8800, with a melt mass-flow rate of 8.0 g/10 min determined according to ISO 1133-1:2022 at 190 °C under 2.16 kg load, and a density of 0.956 g/cm³ per ISO 1183-1:2019, positions this grade for thin-wall injection moulding of dairy and food-service containers where spiral-flow lengths can exceed 150 mm at nominal wall thicknesses from 0.45 mm to 0.80 mm. Direct food-contact compliance is satisfied under FDA 21 CFR 177.1520(c) olefin polymer specifications, EU Commission Regulation 10/2011 Annex I listed monomers and additives, and GB 4806.7-2016 with total migration below 10 mg/dm² under aqueous and fatty-food simulants. Formulation addition ratio at the weigh hopper is 100 parts by weight K8800 to 2–4 phr of titanium-dioxide-containing polyolefin masterbatch with 60 wt% TiO2 loading, plus 0.05–0.20 phr of phosphite antioxidant masterbatch when closed-loop regrind exceeds 15 wt% of total shot weight; re-stabilisation above 0.20 phr has been observed on high-speed lines to raise melt pressure at the hot runner valve gates without measurable improvement in oxidative induction time. Downstream production is performed on high-speed injection moulding machines with 3,000–5,000 kN clamping force, direct servo drive, and valve-gated hot runner systems; barrel zones are maintained at 210–240 °C, the hot runner at 220–250 °C, and the tool is cooled with water at 4–10 °C to maintain a cycle time of 4.5–6.5 s for containers of 500 mL capacity and 0.50 mm sidewall. Injection speed is set at 160–220 mm/s with switch-over to holding pressure at 95–99 % of filling volume, and holding pressure is maintained at 70–90 MPa for 0.6–1.2 s; nozzle retraction during plasticising is disabled to reduce stringing and improve shot-to-shot uniformity. Terminal article types include margarine tubs, ice cream containers, dairy creamer capsules, delicatessen trays, and food-service cups with lids that require paraffin-wax-compatible sealability at lip contact pressures below 0.4 N/mm².
For tamper-evident screw closures for carbonated soft drinks and still water, K8800 is processed on high-cavitation moulds of 48 to 96 cavities with valve-gated hot runners and round or trapezoidal gates of 0.25–0.40 mm thickness. Industry compliance standards are FDA 21 CFR 177.1520(c) for olefin polymers in food contact, EU 10/2011 for overall migration below 10 mg/dm², and ISBT PCO 1881 voluntary neck finish specifications for 26 mm and 28 mm screw threads; torque retention and removal torque are evaluated according to ASTM D2063 under controlled application torque of 2.5 N·m and conditioning at 23 °C/50 % RH for 24 h followed by 3 min carbonation retention at 1.2 bar CO2 overpressure. Formulation addition ratio is 100 parts by weight K8800 to 1.5–3.0 phr of closure-grade white or custom colour masterbatch with a melt index of 8–12 g/10 min to avoid sink marks around the tamper-evident bridge; 0.05–0.15 phr of amide-based slip additive is used only when removal torque exceeds 2.8 N·m on the filling line, because excess slip can lower the angle of repose on cap feeders and increase unscrambling jams. Regrind from reject closures is limited to 15–20 wt% because bridge ductility and environmental stress crack resistance may degrade beyond 20 wt%; online rheometry at the injection unit is used to maintain melt viscosity within ±5 % of virgin baseline. The downstream process uses electric injection machines with clamp force 1,500–4,000 kN, injection speed 120–180 mm/s, barrel temperature profile 220–250 °C from feed throat to nozzle, and mould temperature 5–10 °C; fill time is 0.3–0.6 s, hold pressure 70–110 MPa for 0.8–1.5 s, and cooling time 1.5–3.5 s, giving total cycle times of 4–9 s. Terminal product types include 26/22 mm still water closures, 28 mm PCO 1881 CSD closures, 30/25 mm low-acid beverage closures, and multi-start sports caps; tamper-evident bands are folded over the bottle neck below the retention bead within 0.15 s after demoulding before shrink-back exceeds 0.5 %.
Returnable crate moulding on toggle-clamp machines of 1,200–1,800 t lock force with moving platens wider than 1,100 mm uses K8800 for high-flow cavity filling around lattice ribs and handle apertures; the same grade also shapes logistics totes and ventilated fruit or vegetable crates. In these reusable transport packaging articles the compliance benchmark is ASTM D4976-12a for high-density polyethylene injection and extrusion moulding compounds, supported by ISO 527-2 for tensile yield stress above 26 MPa, ISO 178 for flexural modulus above 1,000 MPa, and ISO 180/A for notched Izod impact strength above 4.0 kJ/m² at 23 °C; when crates are in direct contact with unpackaged fruit or vegetables, EU 10/2011 overall migration below 10 mg/dm² and FDA 21 CFR 177.1520(c) apply. Formulation addition ratio is 100 parts by weight K8800 plus 1–3 phr of colour masterbatch and, for outdoor storage, 2–4 phr of UV-stabiliser masterbatch containing 0.5 wt% high-molecular-weight HALS and 0.2 wt% benzotriazole UV absorber; post-industrial regrind from the same crate line is maintained at 15–20 wt% maximum and only after ten consecutive reuse trials show a drop in tensile yield below 5 %. Accelerated weathering validation is performed according to ISO 4892-2 method A for 1,000 h with a retained flexural modulus of at least 80 %. The downstream production process employs multi-cavity cold-runner moulds with heated sprue bushings and labyrinth vents of 0.02–0.04 mm depth; barrel temperatures are set from 210–240 °C, mould temperature 15–30 °C, injection speed 120–200 mm/s, holding pressure 60–80 MPa for 4–8 s, and total cooling time 20–35 s for wall sections of 2.5–4.0 mm; rib-to-wall thickness ratio is held below 0.6 and rib depth is less than 3.0 times nominal wall to prevent sink marks on sidewalls. Terminal product types include 24-bottle beverage crates, bread trays, agricultural fruit crates, ventilated display boxes, and nested logistics totes with stacking ribs that achieve a 6:1 nesting ratio.
Household storage and kitchen articles moulded from K8800 rely on the resin’s flexural modulus of 1,150 MPa per ISO 178 and notched Izod impact strength of 5.0 kJ/m² at 23 °C per ISO 180/A to sustain repeated hinge cycles and daily use. Compliance standards for this segment include FDA 21 CFR 177.1520(c) and EU 10/2011 for kitchen articles in contact with dry and aqueous foods, REACH Annex XVII entries 51 and 52 for phthalate restrictions, and EN 12875-1 for resistance to mechanical dishwashing at 65 °C for 125 cycles without visible cracking, staining, or dimension change exceeding 2 %. Formulation addition ratio at the press is 100 parts by weight K8800, 1–3 phr of household-grade colour masterbatch, and 0.05–0.20 phr of slip/antiblock masterbatch where stacked parts must separate during automatic demoulding; regrind is permitted up to 30 wt% only if the melt mass-flow rate changes by less than 10 % and notched Izod impact strength remains above 4.0 kJ/m². Processing is performed on hydraulic toggle or hybrid injection moulding machines with clamp force 120–500 t, screw compression ratio 2.0–2.2:1, and a flat barrel temperature profile of 200–240 °C; mould temperature is held at 15–25 °C using turbulent water flow, holding pressure is 50–70 MPa for 2–6 s, and cooling time is 15–35 s depending on ribbed wall thickness of 1.5–3.0 mm. For living hinges in storage box lids, gate placement is offset from the hinge by at least 10 times nominal wall thickness and hinge thickness is 0.25–0.35 mm; post-mould flexing at 20 °C for 10 cycles is used to align molecular orientation and reduce hinge stress-whitening. Terminal articles include stackable storage boxes, clothes hangers, kitchen drawer organisers, waste baskets, and dustpans; moulded part mass varies from 25 g to 800 g, and the same grade is retained across the range to minimise purging on single-screw machines with shot capacities from 50 g to 1,200 g.
Open-head pails and small drums produced with K8800 are intended for water-based paints, greases, food ingredients, and non-classified industrial liquids; certification for 20 L formats follows UN 1H2 removable-head plastics drum designation under 49 CFR 178.601, ADR 6.1.5, and IMDG Code drop and stacking tests, while food-contact grades are verified against EU 10/2011 and FDA 21 CFR 177.1520(c). Formulation addition ratio is 100 parts by weight K8800 to 2–4 phr of heavy-metal-free colour concentrate and 0.5–1.5 phr of UV stabiliser masterbatch for exterior storage; recycled HDPE is limited to 25 wt% because UN drop test pass rates can fall below 95 % when regrind exceeds that level in containers with wall thickness below 2.0 mm. The downstream production line uses accumulator-assisted injection machines with clamp force 400–800 t, shot capacity 1,500–4,000 g, and 2–8 cavity tools with hydraulic core pulls for handle apertures; barrel temperature is set at 220–250 °C, mould temperature 15–25 °C, fill time 3–6 s, holding pressure 60–85 MPa for 5–10 s, and total cycle 25–45 s for a 10 L pail with 2.2 mm nominal wall. Melt cushion is deliberately maintained between 6 mm and 10 mm to maintain shot-weight consistency better than ±0.5 %; lower cushion values have been observed on production lines to cause sink marks at handle bosses and intermittent flaring at the rim seal area. Post-mould cooling jigs hold rim diameter to within 1.5 mm ovality after demoulding for 30–60 s. Terminal product types are 5 L, 10 L, 15 L, and 20 L open-head pails, paint cans with tear-strip lids, grease drums, and water-based chemical containers with environmental stress crack resistance tested according to ASTM D1693 Condition A at 50 °C and 10 % Igepal CO-630.
Injection moulding of toy building blocks, sand toys, and ride-on body panels uses K8800 in tools with polished chrome-M alloy surfaces and positive ejection because the grade’s Rockwell hardness of 63 per ISO 2039-2 resists surface abrasion during repeated nesting and demoulding. Compliance for this segment is driven by EN 71-3:2019+A1:2021 migration limits for elements such as lead below 0.5 mg/kg, ASTM F963-23 heavy-metal extractable content, ISO 8124-3, and REACH Annex XVII entries 51/52 for phthalates; food-contact simulation is not normally required except for teething or food-shaped toy elements, for which EU 10/2011 applies as a conservative fallback. Formulation addition ratio at the hopper is 100 parts by weight K8800, 1–4 phr of toy-grade pigment masterbatch with heavy-metal-free lakes, and 0.1–0.5 phr of processing stabiliser masterbatch; regrind is restricted to 10 wt% of known, uncontaminated production scrap because particulate contamination and carboxylic acid residues from previous processing can shift migration test results at the detection limit. Processing uses injection pressures of 70–120 MPa, barrel temperatures 200–230 °C, mould temperatures 15–30 °C, and clamp force 80–350 t for tools from one to eight cavities; for thick-walled sand toys of 3–5 mm, hold time is extended to 8–15 s and cooling time to 25–40 s, whereas thin-walled blocks of 1.0 mm are filled at 100–150 mm/s and ejected within 12–18 s. Gate vestige removal is performed with hot-knife trimming, and maximum gate protrusion is kept below 0.10 mm to avoid sharp-edge failures under EN 71-1. Terminal product types include interlocking building blocks, sand moulds, wheeled toy chassis components, and non-electrical playset panels.
Dunnage trays, pallet collars, and separator boards injection moulded from K8800 are deployed in closed-loop cold-chain and pharmaceutical logistics where wood contamination and splintering are unacceptable. Compliance in this non-food industrial segment is anchored to ASTM D4976-12a for the base HDPE compound, ASTM D4169-16 truck and air-ride vibration profiles, ISO 12048:1994 for top-load compressive strength, and ASTM D256 for Izod impact resistance above 3.5 kJ/m² at −20 °C; clean-room use additionally requires rinseability verification according to ICH Q7 with residues below visual detection. Formulation addition ratio is 100 parts by weight K8800, 1–2 phr of carbon black masterbatch for conductive identification in automated sortation, and 0.2–0.5 phr of antistatic masterbatch where surface resistivity must remain below 10^11 Ω/sq per IEC 61340-2-3; post-industrial regrind is allowed up to 30 wt% when the tray will not exceed 500 cycles of use. The production process is run on large-tool injection machines of 1,000–2,000 t clamp force with multi-cavity or single-cavity tools and sequential valve gating; barrel temperatures are 210–250 °C, mould temperature 15–25 °C, fill speed is programmed at 40–80 mm/s for the first 30 % of flow path then 80–120 mm/s for the remainder to avoid gas traps at weld lines, and packing pressure is 55–75 MPa for 10–20 s. Cooling time is 40–90 s for solid sections up to 6 mm, and ejected trays are placed on a flat cooling fixture for 120 s to reduce flatness deviation below 1.0 mm/m. Terminal products are distribution dunnage trays, tote bases, pallet collars, separator boards, and freezer spacer plates rated for continuous service at −30 °C to +60 °C.
Competitive SK Geo Centric HDPE K8800 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SK Geo Centric HDPE K8800 is a high-molecular-weight high-density polyethylene resin intended for blown-film extrusion. The grade is assigned a nominal melt flow index of 0.04 g/10 min at 190 °C/2.16 kg by ISO 1133-1:2022 and a nominal density of 0.949 g/cm³ by ISO 1183-1:2019. The combination of low melt flow and moderate density places the resin within the high-molecular-weight HDPE film category. On production-scale extrusion lines, the material forms a high-viscosity bubble with elevated melt strength, which permits thin-gauge film to be supported across a tall frost line without immediate bubble collapse. Processors operating monolayer or coextruded blown-film lines observe elevated head pressure and must select annular die clearances, air-ring geometry, and screw profiles consistent with high-viscosity HDPE stock.
The property matrix in Table 1 represents typical lot data reported for SK Geo Centric HDPE K8800; the values are not to be construed as guaranteed specification limits. The tensile yield stress of 23 MPa and flexural modulus of 735 MPa reflect the density of 0.949 g/cm³. These values place the resin below high-density blow-molding grades exceeding 0.955 g/cm³ but above linear low-density film grades in the 0.918–0.925 g/cm³ range. The elongation at break value above 600 % indicates ductile film behavior under slow-rate tensile loading rather than a brittle response under the same test geometry.
| Property | Test standard | Unit | Typical value |
|---|---|---|---|
| Melt flow index | ISO 1133-1:2022 / ASTM D1238-20 | g/10 min | 0.04 |
| Density | ISO 1183-1:2019 / ASTM D1505-18 | g/cm³ | 0.949 |
| Tensile yield stress | ISO 527-2/1A / ASTM D638-14 | MPa | 23 |
| Elongation at break | ISO 527-2/1A | % | 600 |
| Flexural modulus | ISO 178 / ASTM D790-17 | MPa | 735 |
| Vicat softening temperature | ISO 306/A50 | °C | 117 |
| Melting temperature | ISO 11357-3:2018 | °C | 132 |
| Hardness | ISO 868 | Shore D | 61 |
| ESCR F50, 100 % Igepal | ASTM D1693-15e1 | h | 600 |
The environmental stress-cracking resistance result above 600 h under ASTM D1693-15e1 condition B is a differentiating technical feature. It indicates resistance to wetting-agent-induced stress cracking in detergent-containing and surface-active environments. This measurement is particularly relevant when the film is converted into industrial liners, agricultural bags, or waste sacks that contact polar liquids.
On a monolayer blown-film line using a 55 mm barrier screw with 30:1 L/D, a flat-to-slightly rising barrel profile from 180 °C at the feed throat to 210 °C at the adapter is commonly applied. The die lip temperature is held between 190 °C and 220 °C. Above 230 °C, oxidative chain scission can reduce bubble strength despite an increase in throughput. The resin’s high molecular weight lowers the critical shear rate for sharkskin and melt fracture; fluoropolymer processing aids at 200–800 ppm are used to suppress die-lip accumulations and improve surface quality. In coextruded structures, excessive processing aid can reduce interlayer adhesion, and the resulting laminate should be tested by seal-strength or peel methods such as ASTM F88/F88M-21 to confirm that the core layer remains mechanically coupled to the skin layers.
Die gap selection between 1.2 mm and 1.6 mm and blow-up ratios of 3:1 to 5:1 provide a stable operating window for the resin. Frost line heights of 6–8 die diameters are typical in monolayer extrusion. Internal bubble cooling can raise output, but the high-viscosity melt may require an increase in die temperature of 5–10 °C to prevent freeze-off at the die exit. Gauge uniformity is monitored under ASTM D6988-21. Processors typically target a film thickness variation of less than ±2 % across the lay-flat width; wider variation indicates insufficient die-gap symmetry or unbalanced air-ring airflow rather than resin inhomogeneity.
Bubble stability in K8800 is governed by elongational viscosity and the high-molecular-weight tail of the molecular weight distribution. Unlike LDPE, linear HDPE contains limited long-chain branching; the observed melt strength is not the result of strain-hardening in the same manner as a tubular LDPE resin. The practical consequence is that K8800 resists draw resonance and sudden bubble diameter fluctuation under low-gauge conditions, but it does not offer the same strain-hardening force as an LDPE-rich blend. On a 70 mm high-output line equipped with internal bubble cooling and a 300 mm die, the limiting output is often set by bubble instability rather than extruder torque. When the frost line is moved above 8 die diameters, periodic diameter fluctuation can occur, particularly below 15 µm film thickness.
Rheological measurements on capillary rheometers show that the shear viscosity of K8800 at 190 °C is higher than that of conventional HDPE film grades. The high-load melt index, when measured at 190 °C/21.6 kg, is a more practical control parameter for this grade than the standard 2.16 kg condition because the standard-melt index value is close to the lower resolution limit of many automatic melt-index instruments. Published data for this specific configuration is limited; processors should validate the melt-flow ratio on the actual lot using ISO 1133-1:2022 and correlate the ratio with head pressure before transferring the grade to a new line.
Practical adjustments for bubble instability include increasing the die gap from 1.2 mm to 1.5 mm, reducing the blow-up ratio from 5:1 to 4:1, and lowering frost line height to 6 die diameters. These changes reduce hoop stress and shorten the molten web length. If the bubble still shows diameter oscillation, the air-ring venturi gap should be narrowed; excessive cooling air velocity can excite bubble vibration in high-viscosity HDPE where the melt skin solidifies rapidly.
Compared with lower-molecular-weight HDPE film grades of similar density, K8800 demonstrates a lower melt flow index and higher melt strength. The trade-off is higher head pressure and motor load at equivalent screw speed. The resin is therefore selected for applications requiring downgauging, high dart impact, or environmental stress-cracking resistance rather than for low-output lines where a higher-melt-index grade simplifies extrusion. Film impact resistance measured under ASTM D1709-16a method A can exceed 150 g for 25 µm monolayer film, depending on the frost line height and film density; however, direct comparative published data for this exact lot-to-lot comparison is limited. The lower melt index of 0.04 g/10 min also narrows the screw-speed window because head pressure increases more rapidly with output than it would in a 0.20 g/10 min grade. On a target line, the substitution should be evaluated by recording head pressure, melt temperature at the die lip, and bubble diameter variation for at least 60 min of steady-state operation.
The grade also differs from conventional HDPE film grades in its gel-handling behavior. High-molecular-weight fractions can form microgels if the extruder is operated with excessive barrel residence time or insufficient purging after a material change. The recommended purge sequence for transition from a lower-viscosity HDPE is to use a viscosity-mismatched purge compound, then run the K8800 at reduced screw speed for 15–20 min before returning to target output. Failure to clear the previous resin can produce visible gel streaks in the film, especially in thicknesses below 10 µm.
K8800 is positioned as a base resin that can be used in food-contact packaging when the final article meets the overall migration limits of EU Commission Regulation (EU) No 10/2011 and its associated test methods, including EN 1186-1:2002. For United States food-contact use, the base resin falls under FDA 21 CFR 177.1520(c) for olefin polymers, subject to conditions of use and final-article compliance. The resin is typically accompanied by REACH registration documentation and is used within the scope of RoHS Directive 2011/65/EU for electrical and electronic applications. Pre-drying is not normally required unless storage at relative humidity above 60% has produced surface moisture, which can lead to microbubbles in extruded film. The grade should not be blended with amine-based antistatic concentrates that have not been evaluated for interaction with fluoropolymer processing aids, because additive antagonism can reduce both bubble stability and film surface quality. Clean edge trim can be incorporated as regrind at levels of 10–20 wt%; higher regrind levels may lower environmental stress-cracking resistance and increase gel counts from oxidative crosslinking.