    • Product Name: SK Geo Centric HDPE JK910
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 354146
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.35 g/10 min
    Tensile Strength At Yield 29 MPa
    Tensile Elongation At Break >500 %
    Flexural Modulus 1,200 MPa
    Vicat Softening Temperature 125 °C
    Heat Deflection Temperature 0 45 Mpa 70 °C
    Shore D Hardness 65
    Notched Izod Impact Strength 23 C 60 J/m
    Environmental Stress Crack Resistance F50 >1000 h
    Melting Point 134 °C
    Brittleness Temperature < -70 °C

    As an accredited SK Geo Centric HDPE JK910 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing SK Geo Centric HDPE JK910 is supplied in 25 kg bags, stacked on pallets, or in 1,000 kg jumbo bags.
    Container Loading (20′ FCL) SK Geo Centric HDPE JK910 bags are palletized, securely stowed, and lashed inside a 20-foot FCL container for ocean export.
    Shipping SK Geo Centric HDPE JK910 is generally shipped at ambient temperature as non-hazardous polyethylene pellets in 25 kg woven bags, 500–1,000 kg jumbo bags, or bulk trucks/containers. It requires no UN number, hazard class, or transport label. Keep packages dry, closed, and away from ignition sources. Standard industrial transport applies.
    Storage Store SK Geo Centric HDPE JK910 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, and ignition sources. Keep original bags or containers closed, clean, and palletized to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers. Maintain stable ambient temperature, do not overstack, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is typically 24 months when stored cool, dry, sealed, and away from direct sunlight in unopened packaging.
    Application of SK Geo Centric HDPE JK910
    During high-cavitation production of thin-walled dairy spread tubs, frozen-food containers, and food service lids, process stability is governed more by gate freeze-off and mould cooling behaviour than by plastication capacity. SK Geo Centric JK910 is specified as an injection moulding high-density polyethylene with a typical melt mass-flow rate of 9 g/10 min under ASTM D1238 at 190°C and 2.16 kg, and a nominal density of 0.954 g/cm³ under ASTM D1505. This flow range permits filling of wall thicknesses between 0.6 mm and 1.5 mm on accumulator-assisted injection machines of 1,500 kN to 4,500 kN clamp force when injection time is held below 0.5 s per cavity, although the practical flow-length-to-thickness ratio depends on gate location and cavity layout. Melt temperature at the nozzle is normally maintained between 210°C and 250°C; lower settings reduce the risk of heat-accelerated off-flavour compounds but raise injection pressure by approximately 15% to 25% relative to a higher-flow polypropylene alternative. Mould surface temperature is typically set between 10°C and 30°C, with lower temperatures reducing cycle time but increasing frozen-layer thickness and in-plane orientation in round tubs. Excessive orientation produces post-mould ovality; parts moulded at 10°C may exhibit warpage values two to three times greater than parts moulded at 30°C when measured by a flatness gauge over a 200 mm chord. On automatic filling lines, out-of-roundness above 0.5 mm across a 150 mm diameter is sufficient to disrupt heat-seal lidding film geometry and produce leakers.
    ParameterTest methodRepresentative range for high-flow HDPE injection grade
    Melt mass-flow rateASTM D1238, 190°C/2.16 kg8.5 g/10 min to 9.5 g/10 min
    DensityASTM D1505, 23°C0.952 g/cm³ to 0.956 g/cm³
    Tensile yield stressASTM D638, 50 mm/min22 MPa to 26 MPa
    Flexural modulusASTM D790, 1% secant850 MPa to 1,000 MPa
    Notched Izod impactASTM D256, 23°CNo break or >25 kJ/m²
    Deflection temperatureASTM D648, 0.455 MPa65°C to 75°C
    Mould shrinkageASTM D955, 2.0 mm plaque1.5% to 2.5%
    Direct food contact applications must use the grade only within the supplier’s regulatory position. In the United States, olefin polymers are evaluated under FDA 21 CFR 177.1520(c); in the European Union, plastic food contact materials must comply with EU Regulation No 10/2011, including the overall migration limit of 10 mg/dm² for non-fatty foods and 60 mg/kg for fatty food simulants, unless Annex I-specific migration limits for each pigment and stabiliser are lower. Organoleptic acceptance for low-odour applications is commonly tested by EN 1230-2; HDPE can absorb volatile residues from previous barrel residence, so purging with a low-odour HDPE or talc-filled purge compound before food-contact production is required. Pre-drying is not generally required for HDPE because absorbed moisture does not cause hydrolytic chain scission; however, surface condensation on cold pellets moved into a warm mezzanine can generate splay. If relative humidity exceeds 60%, pellets should be passed through a hopper dryer at 60°C to 70°C for 1 h to 2 h. The use of regrind in food contact is permitted only when the material is derived from the same food-contact production line, and the resulting granulate is tested for migration and sensory performance.

    What Limits Fast-Cycle Production of 20 L Pails in Multi-Cavity Tooling?

    The primary constraint in industrial pail moulding is not plastication rate but the ability to pack the gate boss, handle bridge, and stacking rim before the gate freezes. On a single-cavity 20 L pail tool with a projected area of 0.18 m² to 0.22 m², documented hydraulic cavity-pressure levels of 350 bar to 450 bar produce clamp force demand between 650 kN and 950 kN; multi-cavity pail tools therefore require toggle or two-platen clamping units of 2,000 kN to 5,000 kN. Barrier screws with diameters of 90 mm to 110 mm and L/D ratios of 20:1 to 24:1 deliver the required shot weight of 0.7 kg to 1.1 kg without excessive residence time or melt-temperature overshoot. Cycle time is normally 18 s to 30 s for wall thicknesses of 1.5 mm to 2.5 mm, with a chilled mould at 10°C to 25°C and a cooling-water temperature differential of 2°C to 4°C. If the gate boss is not packed, a visible gate void appears and the stacking-rim height can vary by 0.3 mm to 0.8 mm, which is sufficient to cause unstable pallet stacking. During mould trials on high-flow HDPE grades of this density class, reject rates from handle webbing cracks and out-of-round rims increase sharply when mould temperature exceeds 25°C or when demoulding is attempted before cooling-water outlet temperature drops below 35°C.Detergent-containing pails require ESCR screening. Moulded-in stress at the gate boss and handle roots can reduce effective ESCR relative to compression-moulded test plaques by 30% to 50%; for this reason, an ASTM D1693 condition B plaque F50 value above 50 h does not guarantee a pail will survive stack-load stress cracking. The handle bridge should be designed with a minimum radius of 3 mm, and the sidewall thickness at the stacking rim should transition with a draft angle of at least 1.5° per side. HDPE grades in this density and melt-flow class are not recommended for continuous service with strong hydrocarbon solvents, aromatic cleaners, or oxidising acids; permeation and environmental stress cracking under stack stress are the limiting mechanisms.Closure production differs from pail moulding because dimensional tolerance at the tamper-evident band and gate vestige height determine performance in continuous-thread caps. For 28 mm PCO 1810 or PCO 1881 caps, the shell wall thickness is normally 1.8 mm to 2.5 mm; JK910-class material at 9 g/10 min fills 32-cavity to 48-cavity hot-runner tools with valve gates of 0.8 mm to 1.2 mm diameter. The advantage of a valve gate is a gate vestige below 0.2 mm; edge-gated cold-runner tools may leave a vestige that interferes with torque-controlled capping. Application torque for 28 mm PET or HDPE bottles commonly ranges from 1.8 N·m to 2.5 N·m; strip torque should exceed 3.5 N·m, and torque retention after 24 h at 50°C should remain above 70% of the application value. There is no single ASTM closure torque-retention method covering all geometries; the applicable standard is the bottler’s internal protocol or ASTM D3198 for application and removal torque of continuous-thread closures. Induction-sealed closures made from HDPE are limited by liner support stiffness; if the cap shell softens during sealing at 200°C to 250°C board temperature, the rim can warp and lose roundness. For aggressive oxygen bleach or terpene-containing cleaning products, the closure sidewalls must be screened for stress cracking using ASTM D1693; low ESCR grades with a bent strip F50 below 30 h may develop visible cracking within weeks when moulded-in stress is high. For pharmaceutical closures, composition must comply with USP 661.1 and Ph. Eur. 3.1.3 where applicable; extractables and leachables data are required. Slip agents and colourants must not exceed the additive limitations in FDA 21 CFR 177.1520(c).

    Returnable Dairy Crates and Agricultural Tote Bodies: Ribbing, Impact, and Outdoor Weathering

    The structural design of returnable dairy crates made from HDPE depends on flexural stiffness and bottom drop impact at low temperature. For JK910-class material with a flexural modulus tested by ASTM D790 in the range of 850 MPa to 1,000 MPa, rib depth on crate sidewalls is typically 5 mm to 12 mm, with rib thickness no more than 50% to 60% of the nominal wall to avoid sink marks. Stacking lugs and rib intersections should have radii no smaller than 2 mm; sharp internal corners produce notch stress that reduces impact performance. Drop-impact testing at -20°C is a common release criterion for dairy crate trials; HDPE grades of this density generally retain ductile impact at low temperature, but moulded-in stress and frozen-in orientation can shift the failure mode to brittle fracture if the melt temperature at the nozzle falls below 200°C or if the mould is overpacked. Outdoor agricultural tote bodies require weatherability. Carbon black loading of 2.0% to 2.5% by weight and a hindered-amine light stabiliser masterbatch at 0.2% to 0.5% are common for multi-year outdoor service; accelerated weathering is evaluated by ISO 4892-2 cycle 1 at 1,000 h or by ASTM G154 cycle 1, with acceptance defined as no surface cracking and a Charpy impact retention above 70% of the unaged value. Up to 30% clean in-house regrind can typically be introduced without marked loss of impact strength if the material is melt filtered through a 600 µm screen pack and the regrind particle size remains below 8 mm. Higher regrind fractions increase the risk of black specks, silver streaks, and lot-to-lot melt flow drift; the melt flow rate should be rechecked by ASTM D1238 after every regrind addition.
    ApplicationStandard or regulationCritical test or criterion
    Thin-wall food contact articlesFDA 21 CFR 177.1520(c), EU 10/2011, GB 4806.6Overall migration 10 mg/dm² or 60 mg/kg; sensory EN 1230-2
    Industrial pails and detergent packagingASTM D1693 condition BEnvironmental stress-crack resistance; stack-load simulation
    Continuous-thread closuresASTM D3198, USP 661.1, Ph. Eur. 3.1.3Application torque 1.8 N·m to 2.5 N·m; strip torque >3.5 N·m
    Outdoor crates and agricultural totesISO 4892-2, ASTM G1541,000 h weathering; impact retention >70%
    Freezer-grade storage bins and cold-room totes present a different set of constraints because the primary mechanical risk is brittle impact after prolonged cold storage, not short-term tensile failure. High-density polyethylene with a density of 0.954 g/cm³ and a notched Izod impact at 23°C generally above 25 kJ/m² under ASTM D256 remains ductile at -20°C, but the mode of loading changes when storage bins are handled with fork tines or thrown onto concrete. The drop test is therefore performed at -20°C with a minimum wall thickness of 2.0 mm; corner radii below 3 mm are not recommended because the notched impact strength of semi-crystalline HDPE is more sensitive to radius than ABS or polypropylene. For cold-room cleaning, the bins are exposed to quaternary ammonium disinfectants and alkaline detergents; under continuous bending stress, these fluids can produce environmental stress cracking. ESCR screening by ASTM D1693 condition A is commonly specified at 100 h or 200 h for stressed applications, although published data for this specific JK910 configuration are limited. The acceptable service temperature for continuous load is determined by deflection temperature under load and creep modulus; the ASTM D648 value at 0.455 MPa for this class is typically 65°C to 75°C, but stacked bins at 40°C can creep and deform under sustained static loads above 0.9 MPa. Loads should therefore be distributed by interlocking stacking lugs rather than point contact.

    When Creep Load Limits Long-Term Stacking of Automated Warehouse Bins

    Automated storage and retrieval systems require bins that maintain dimensional stability under vertical dead load and lateral acceleration. For HDPE, the relevant property is not short-term tensile modulus but creep modulus at warehouse temperature; high-flow injection grades with a flexural modulus of 900 MPa may show apparent creep modulus below 400 MPa after 1,000 h under 4 MPa load at 23°C. This means a bin sidewall deflecting more than 2 mm can interfere with shuttle forks or barcode readers. High-density polyethylene expands at approximately 1.5 × 10⁻⁴ m/m°C to 2.0 × 10⁻⁴ m/m°C; a temperature swing from 10°C to 40°C across a 600 mm bin length produces length changes of 2.7 mm to 3.6 mm, which must be accommodated by the rack design. JK910-class material is preferable to lower-density polyethylene because the higher density increases stiffness and lowers mould shrinkage; however, higher density also reduces environmental stress-cracking resistance. The processing window for low-warp bins requires a melt temperature of 210°C to 240°C, a mould temperature of 15°C to 35°C, and an injection speed profile that avoids hesitation marks. Gate location for a rectangular bin should be offset from the centre to prevent jetting; a fan gate with a land length of 1.0 mm to 1.5 mm is typical. In automated warehouse service, plastic bins are not recommended for static stack loads above 200 kg per stack unless the base is reinforced with steel or a structural foam core.
    Free Quote

    Competitive SK Geo Centric HDPE JK910 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    SK Geo Centric HDPE JK910 is an injection-moulding high-density polyethylene with a nominal melt flow index of 10 g/10 min at 190 °C under a 2.16 kg load as determined by ASTM D1238, and a nominal density of 0.956 g/cm³ under ASTM D1505. The resin is supplied as pellets and is intended for rigid injection-moulded articles such as industrial crates, stacking pallets, household containers, and closures. Its position within the SK Geo Centric HDPE slate is defined by higher fluidity than extrusion and blow-moulding grades and by lower molecular weight than pipe or large-part blow-moulding resins. That molecular difference reduces injection pressure and cooling time in multi-cavity tools but also lowers environmental stress crack resistance relative to high-molecular-weight HDPE.

    For closure applications, JK910 lies below high-flow HDPE grades of 20 g/10 min or higher. The lower throughput per cavity is offset by higher notched impact and greater stiffness. Closures with a 2 mm wall and internal thread typically require a melt temperature of 220–240 °C and a minimum injection pressure determined by short-shot analysis. Published comparative data for JK910 against a 20 g/10 min closure grade is limited; thin-wall closures with flow path ratios above 150:1 should be evaluated in the tool under actual mould temperature and gate geometry.

    Does the 10 g/10 min Melt Flow Index Constrain Weld-Line Strength in Thick Crate Sections?

    The melt flow index is not a direct viscosity measurement but is used as an inverse average-molecular-weight marker. A 10 g/10 min HDPE under ASTM D1238 has a shorter average chain length than a 0.3–0.7 g/10 min blow-moulding HDPE, which reduces pressure loss in runners and permits filling of ribs that drop below 1.5 mm wall thickness. Capillary rheometry on generic high-flow HDPE at 220 °C shows an apparent viscosity between 600 and 900 Pa·s at 100 s⁻¹, falling to 150–300 Pa·s at 1,000 s⁻¹. Published JK910-specific capillary rheometry should be read from the current lot certificate. Melt temperatures of 200–240 °C are used, with the upper limit of 240 °C protecting against oxidative chain scission during extended residence time.

    Weld-line strength is governed by interdiffusion at the flow front. The lower molecular weight of JK910 accelerates re-entanglement at a given melt temperature, but it also reduces tensile strength at the weld. When a crate tool uses multiple gates, weld-line tensile strength under ISO 527-2 commonly retains 50–70 % of the unwelded value for this class of HDPE; JK910-specific lot verification is required. Raising melt temperature within the 200–240 °C window and extending packing time improve molecular contact at the weld, while mould temperatures above 60 °C can prolong cycle time without proportional strength gain.

    Plastication on a standard injection screw requires attention to screw recovery and melt homogeneity. A 50 mm diameter screw with 20:1 L/D and a 2.5:1 compression ratio can plasticate HDPE at 30–60 rpm with a back pressure of 0.5–1.0 MPa. Screw speeds above 120 rpm may introduce unmelted pellets at low back pressure. The shot volume should be kept between 20 % and 80 % of barrel capacity. If a masterbatch is used, a 2–4 % letdown is typical for colour or stabiliser concentrates, and the mixture must be tumble-blended before entering the hopper to avoid concentration variation.

    Shrinkage behaviour in a production crate tool is dominated by packing pressure and cooling asymmetry rather than melt flow alone. On a 2,800 kN hydraulic injection moulding machine with a 22:1 L/D general-purpose screw and a 2.6:1 compression ratio, mould shrinkage of 1.4–2.2 % is observed under ASTM D955 on 3.2 mm plaque specimens. When holding pressure is reduced below 35 MPa, voids and sink marks develop at rib intersections. Above 70 MPa, flash may appear along the parting line if the clamp force is marginal. In a 600 mm-long crate side panel, asymmetric cooling can generate warpage of 2–4 mm. Turbulent-flow bubblers in core inserts and a mould temperature of 20–40 °C reduce this deviation. Hot-runner systems should maintain a gate temperature below 240 °C and use valve-gate sequencing to prevent flow-front stall behind deep ribs.

    When a Stacking Pallet Is Moulded from JK910 Instead of a High-Molecular-Weight Blow-Moulding HDPE

    For pallet moulding, the shorter chain population in JK910 lowers the injection pressure requirement and shortens plastication time. A 1,200 mm-long pallet deck with wall thickness 5 mm can be filled at a melt temperature of 230 °C on a 6,000 kN clamping-force machine. A 0.4 g/10 min blow-moulding HDPE would require an estimated 15–25 % higher injection pressure or a hotter melt. The trade-off appears in environmental stress crack resistance: under ASTM D1693 Condition B, 10 % Igepal, high-flow homopolymer HDPE often exhibits F50 below 50 h, whereas lower-flow HDPE can exceed 100 h. JK910 is therefore selected for pallets with high stiffness and fast cycle demands, but returnable pallets exposed to aggressive detergents in cold storage should be tested under loaded flexure at 50 °C in the relevant cleaning solution.

    Comparative property envelope: JK910 versus low-flow HDPE extrusion grade
    PropertyTest methodJK910 injection gradeLow-flow extrusion HDPE
    Melt flow indexASTM D1238, 190 °C, 2.16 kg10 g/10 min0.3–0.7 g/10 min
    DensityASTM D15050.956 g/cm³0.955 g/cm³
    Flexural modulusASTM D7901,150–1,250 MPa950–1,100 MPa
    Tensile yield strengthASTM D63827–29 MPa25–27 MPa
    Notched Izod impact, 23 °CASTM D25650–70 J/m100–200 J/m
    ESCR, Condition B, 10 % IgepalASTM D1693<50 h50–300 h

    The 10 g/10 min flow class reduces injection pressure but narrows the operating window for heavy-wall structural parts because the lower melt strength can produce jetting in thick sections if injection speed is too high. Jetting is controlled by using a sprue or gate geometry that promotes a spreading flow front and by setting injection speed below 100 mm/s at the screw for a 50 mm screw diameter. Published data for JK910 in thick pallet tools is limited; process development should include short-shot studies at 230 °C and 40 °C mould temperature.

    Mechanical Failure Modes in Cold-Climate Pallets Are Governed by No-Notch Impact More Than Density

    At service temperatures below -20 °C, high-density polyethylene loses ductility. Notched Izod results at 23 °C under ASTM D256 do not predict low-temperature fracture in thick sections because the notch radius and loading speed differ from field impacts. Pallets and crates used in frozen logistics should be evaluated with ISO 179-1/1eA at -30 °C or with a Gardner falling-weight test per ASTM D5420 at the specified service temperature. JK910 has lower molecular weight than high-molecular-weight injection grades with 3–5 g/10 min MFR; as a result, its low-temperature impact retention is generally lower. When drop impact at -30 °C is required, a higher-molecular-weight HDPE grade should be evaluated rather than relying on density or room-temperature flexural modulus.

    Chemical Resistance, Environmental Stress Cracking Resistance, and Permeation Boundaries

    JK910 is a non-polar semicrystalline polyolefin with typical HDPE resistance to dilute acids, aqueous alkalis, and polar solvents, but it is incompatible with strong oxidizers, aromatic hydrocarbons, chlorinated solvents, and ketones under continuous stress. The material should not be specified for gasoline or aggressive solvent packaging without barrier testing. Hydrocarbons permeate HDPE and can swell the part by more than 1–3 % mass increase after extended immersion, depending on wall thickness and temperature. Environmental stress cracking is the limiting failure mode in detergent packaging and pressurised containers. HDPE of this flow class usually exhibits lower ESCR than lower-MFR HDPE, as shown in the preceding comparative table. Any new application should include a full-part ESCR exposure at 50 °C in the intended chemical environment per ASTM D1693 or a notched constant-strain test mapped to service loading.

    Before a food-contact declaration is issued for a JK910 article, the converter must verify the pellet formulation against the supplier’s regulatory statement. The base HDPE is generally designated as an olefin polymer under FDA 21 CFR 177.1520 when the additive package meets extraction limits. Under EU 10/2011, overall migration must not exceed 10 mg/dm² for the finished article under the food-contact test conditions appropriate to the pack type. JK910 is not inherently medical-grade, and no USP Class VI or ISO 10993 claim should be made without explicit qualification. Addition of masterbatch, regrind, or processing aids alters the regulatory position. Regrind of the same resin can be used at proportions up to 20 % in non-food industrial parts, but food-contact use of regrind must be validated for migration.

    Compliance verification matrix for JK910 in rigid packaging and industrial mouldings
    RequirementStandard or clauseTypical verification limit
    Food-contact olefin polymer, USFDA 21 CFR 177.1520Supplier compositional statement required
    Plastic food-contact material, EUEU 10/2011Overall migration 10 mg/dm²
    SVHC screeningREACH 1907/2006/ECArticle 0.1 % w/w per SVHC
    Heavy metals in electrical/electronic articlesRoHS 2011/65/EUCd 100 ppm; Pb, Hg, Cr(VI) 1,000 ppm each
    US packaging heavy metalsCONEG TPCHSum of Pb, Cd, Hg, Cr(VI) 100 ppm

    Compliance must be re-evaluated after any additive change because stabiliser packages, colourants, and processing aids can shift the overall migration profile and cause a previously compliant article to fail under EU 10/2011 or FDA 21 CFR 177.1520. A lot-specific supplier certificate and, where required, an independent laboratory migration report should be retained as part of the conformity file.

    When bulk bags are stored outdoors, condensation can carry surface moisture into the hopper. Pre-drying is not needed below 50 % relative humidity, but during humid weather the pellets should be dried at 70–80 °C for 2 h in a desiccant or hopper dryer. Moisture above 0.05 % can generate splay, silver streaks, and surface roughness. Contamination with PP, PET, or PVC must be kept below 0.5 % because immiscible domains cause delamination and gas marks. After processing, the barrel should be purged with low-MFR HDPE or a commercial purging compound before shutdown, particularly if a prior resin was processed above 260 °C.