| HS Code | 190086 |
| Density | 0.954 g/cm³ |
| Melt Flow Index 190 C 2 16 Kg | 10 g/10 min |
| Tensile Strength At Yield | 29 MPa |
| Tensile Elongation At Break | >1000% |
| Flexural Modulus | 1200 MPa |
| Izod Impact Strength Notched 23 C | 40 J/m |
| Vicat Softening Point | 127°C |
| Heat Deflection Temperature 0 45 Mpa | 100°C |
| Shore D Hardness | 65 |
| Mold Shrinkage | 1.5-2.0% |
| Environmental Stress Crack Resistance | >1000 hr |
| Specific Gravity | 0.954 |
| Melting Point | 130-135°C |
As an accredited SK Geo Centric HDPE JH910 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SK Geo Centric HDPE JH910 is packaged in 25 kg polyethylene-lined woven sacks, stacked on pallets for industrial shipment. |
| Container Loading (20′ FCL) | SK Geo Centric HDPE JH910 in 20' FCL: 25 kg bags on pallets, shrink-wrapped, evenly distributed, secured for ocean transport. |
| Shipping | SK Geo Centric HDPE JH910 is shipped as solid, non-hazardous polyethylene pellets in 25 kg bags, jumbo bags, or bulk containers. Transport by truck, rail, or sea under general cargo conditions. Keep dry, clean, and protected from sunlight, heat, and contamination. No special transport classification required. |
| Storage | Store SK Geo Centric HDPE JH910 in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers closed, clean, and palletized. Prevent moisture, dust, and contamination. Stack safely to avoid deformation, and follow first-in, first-out rotation. Use grounding to control static. Store at ambient temperature and comply with local regulations. |
| Shelf Life | Typically 24 months when stored sealed in original packaging, cool, dry, well-ventilated, away from direct sunlight and moisture. |
SK Geo Centric HDPE JH910 enters beverage crate and logistics container production as a high-density polyethylene injection-moulding resin that requires a well-documented cold-runner layout. The melt is held between 210°C and 240°C at the nozzle on accumulator-assisted toggle presses with clamp forces from 1,200 t to 2,000 t. Mould temperatures are set between 20°C and 40°C for wall sections from 2.5 mm to 5.0 mm. Screw L/D ratios of 20:1 to 25:1 and compression ratios between 1.8:1 and 2.8:1 are common on these lines. Packing pressure is maintained between 60% and 80% of the peak injection pressure, which itself falls between 600 bar and 900 bar for multi-cavity tools. Flow-length-to-wall-thickness ratios below 130:1 avoid gate-area short-shot defects when the runner system is balanced to within 5% cavity-to-cavity fill time.
Regrind addition for industrial crates is limited to 30 wt% clean in-house sprues, runners, and rejected parts ground to a screen size between 4 mm and 8 mm. This limit is based on notch impact sensitivity rather than colour shift. When outdoor stacking is specified, 1.0 wt% to 2.0 wt% of a 40% carbon black masterbatch is metered at the feed throat. The final carbon black content should remain below 2.5 wt% because higher loadings increase sink-mark depth around support bosses and raise viscosity at the mould wall. Stacking endurance is measured according to ISO 12048:1994 on a complete crate after conditioning at 45°C for 24 h; the compression test is run at 10 mm/min deformation rate. Tensile properties of specimens cut from the crate side wall are evaluated under ASTM D638-14, and flexural modulus under ISO 178:2019.
Batch-to-batch variation in melt flow ratio has been observed in crate plants running hot manifolds. A change of 0.5 g/10 min in MFR measured at 190°C/2.16 kg under ISO 1133-1:2022 can shift the fill time by roughly 0.2 s in a 4-cavity tool. Incoming resin lots are therefore pre-screened for melt flow and density before silo release. Published data for this specific grade-lot configuration is limited, but process records from conventional HDPE injection grades with comparable melt flow classes support a lot-to-lot MFR tolerance of ±0.2 g/10 min for critical crate dimensions. Surface condensation on pellets stored in unheated silos at RH > 80% is removed with hot-air drying at 70°C for 2 h to prevent splay.
In thin-wall food container production, the economically binding parameter is cooling time, which scales with the square of wall thickness and is reduced only when the polymer temperature at the cavity surface falls below the effective solidification point. For SK Geo Centric HDPE JH910 used in mono-layer dairy tubs and frozen-food containers with wall sections between 0.8 mm and 1.5 mm, mould temperatures of 10°C to 20°C are set because the thin wall permits rapid solidification without excessive sink. Melt temperatures are elevated to 230°C to 260°C at the nozzle to lower viscosity during filling. Temperatures above 260°C accelerate molecular weight reduction and increase odour-generating by-products that migrate into the packaged food, a factor controlled by overall migration testing under EU 10/2011.
High-speed accumulator machines with screw diameters of 50 mm to 90 mm and injection speeds above 200 mm/s are used to fill flow-length-to-wall-thickness ratios between 150:1 and 200:1. Gate shear rate is calculated from volumetric flow rate and gate diameter. For a 1.0 mm wall and a 0.8 mm gate land, shear rates approach 40,000 s⁻¹ during fast fill. At these shear rates, viscosity drops sufficiently for complete cavity filling, but excessive shear heating in the gate can produce local surface gloss differences and resin degradation if the gate land is worn beyond 0.05 mm. Production lines therefore replace gate inserts after 500,000 to 1,000,000 cycles depending on glass-fibre-free HDPE formulation.
Colouration in thin-wall food containers is limited to 2 wt% to 3 wt% of a colour masterbatch whose carrier resin is also an HDPE with food-contact status under FDA 21 CFR 177.1520 and EU 10/2011. Where in-house regrind is reused in a mono-layer container, maximum addition is set at 40 wt% and the regrind must be generated from the same JH910 feedstock without post-consumer contamination. The finished article is tested for overall migration into food simulant 3% acetic acid and 10% ethanol at 40°C for 10 days; total migration must remain below 10 mg/dm². Sensory evaluation is conducted under ISO 13301:2018 or customer-specific panel protocols because HDPE can carry low molecular weight oxidation products that are not detected by total migration alone.
Table 1. Typical starting conditions for SK Geo Centric HDPE JH910 by downstream segment; values are process-derived for cold-runner tools and should be adjusted to tool geometry and machine hydraulics.
| Downstream segment | Melt temperature | Mould temperature | Injection pressure | Screw L/D |
|---|---|---|---|---|
| Beverage crates | 210°C–240°C | 20°C–40°C | 600 bar–900 bar | 20:1–25:1 |
| Thin-wall food containers | 230°C–260°C | 10°C–20°C | 900 bar–1,400 bar | 22:1–25:1 |
| Closures | 200°C–230°C | 10°C–30°C | 800 bar–1,200 bar | 20:1–25:1 |
| Industrial pails | 200°C–230°C | 10°C–20°C | 700 bar–1,000 bar | 20:1–25:1 |
| High-gloss housewares | 210°C–240°C | 30°C–50°C | 600 bar–1,000 bar | 20:1–24:1 |
| Pallets and dunnage | 200°C–230°C | 20°C–40°C | 1,200 bar–1,500 bar | 20:1–24:1 |
Closure moulding with SK Geo Centric HDPE JH910 places more demand on dimensional stability and torque retention than on short-term mechanical strength. The melt is processed between 200°C and 230°C at the nozzle, while the mould is kept at 10°C to 30°C to maintain roundness in 16-cavity to 64-cavity hot-runner tools. Cycle times in high-speed closure tools are governed by gate freeze time rather than part ejection temperature. For valve-gated hot runners with gate diameters of 0.6 mm to 1.2 mm, the gate freezes when the pressure in the runner channel falls below 300 bar. The injection profile is divided into an initial velocity-controlled filling stage and a pressure-controlled packing stage with switchover at 95% to 98% of total part volume.
Roundness of the completed closure is measured on a coordinate measuring machine and controlled to a total diameter variation below 0.1 mm. If the mould temperature differs by more than 5°C between fixed and moving halves, the closure skirt cools unevenly and ovality can exceed 0.2 mm, causing cap-to-neck torque loss. For detergent and liquid soap closures, environmental stress-crack resistance is tested according to ASTM D1693-15 Condition B using 10% Igepal CO-630 at 50°C. The acceptance criterion depends on the brand specification, but F50 values below 50 h are generally rejected for surfactant-containing filling operations. If the current SK Geo Centric datasheet does not report a Condition B value, a batch certificate should be requested before changing lot source.
Slip additives are introduced as a pre-dispersed masterbatch at 0.2 wt% to 0.5 wt% erucamide equivalent to stabilise opening torque. Higher levels above 0.5 wt% can bloom to the surface and produce secondary friction effects that increase risk of bridge-thread stripping. The closure formulation must meet EU 1935/2004 and, in the United States, FDA 21 CFR 177.1520 for olefin polymers. Migration testing is performed on the final cap, not on the pellet, because the injection process can concentrate low molecular weight species at the gate and crown regions. The terminal component is a screw closure for detergent bottles, dairy beverage closures, or industrial container caps, where a tamper-evident band must resist fracture during first opening.
When industrial pails are certified for hazardous or aggressive liquids, the resin choice must deliver impact strength after drop conditioning at -18°C and stacking strength at 40°C. Pails with capacities from 20 L to 25 L and wall sections between 1.8 mm and 3.0 mm are moulded from SK Geo Centric HDPE JH910 using melt temperatures of 200°C to 230°C and mould temperatures of 10°C to 20°C. Injection pressure is held between 700 bar and 1,000 bar to consolidate the bottom wall against the core plate. A holding pressure transition at 4 mm to 6 mm of screw cushion is used to prevent overpacking around the pail rim.
Drop testing for a 20 L pail classified under UN 3H2 is conducted after the filled and sealed pail is conditioned at -18°C for 24 h. The pail is dropped from a height determined by the filling liquid density and UN packing group. For Packing Group II at a specific gravity of 1.2, the drop height is 1.2 m. The pass criterion requires no leakage from the closure and no damage that would impair transport strength. Low-temperature impact failure is frequently traced to weld lines at the handle ears or gate blush zones, not to the base wall. Mould cooling near the handle ear inserts is adjusted to a temperature difference not greater than 3°C from the nominal mould water supply to avoid premature freeze-off at these points.
ESCR is a primary compliance parameter for pails used with surfactant-based cleaners. The test is run under ASTM D1693-15 Condition A with a 0.3 mm notch in 10% Igepal CO-630 at 50°C; where the customer specification requires no stress-cracking before 100 h, the grade is selected against an F50 threshold rather than a simple pass-fail. Regrind use is permitted up to 20 wt% for non-food pails but is generally excluded from the outer wall of hazardous-liquid packaging because of batch consistency concerns. The finished pail must also comply with REACH Article 33 communication requirements if any SVHC in the stabiliser system exceeds 0.1 wt% in the article.
Table 2. Compliance and test references for HDPE JH910 downstream scenarios.
| Standard or regulation | Application context | Test condition or clause | Relevant scenario |
|---|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for food contact | Extraction limits for olefin polymers | Thin-wall food containers, closures |
| EU 10/2011 | Plastic food-contact materials | Overall migration <10 mg/dm² | Thin-wall food containers |
| EU 1935/2004 | Framework regulation for food-contact articles | Good manufacturing practice | Closures |
| REACH Article 33 | SVHC communication for articles | Candidate list concentration >0.1 wt% | Industrial pails, pallets |
| ISO 12048:1994 | Compression testing of complete packages | Conditioning at 45°C for 24 h | Beverage crates |
| ASTM D1693-15 Condition B | Environmental stress-crack resistance | 10% Igepal CO-630 at 50°C | Closures, industrial pails |
| ISO 8611-1:2021 | Flat pallet performance | Rated load deflection | Pallets and dunnage |
| EN 71-3:2019+A1:2021 | Migration of elements from toys | 19-element screening | High-gloss housewares marketed as toys |
For housewares such as storage totes, drawer organisers, and hangers, the part is judged by gloss uniformity and sink-free surfaces. SK Geo Centric HDPE JH910 is processed at melt temperatures between 210°C and 240°C; the mould temperature is set between 30°C and 50°C for polished cavity surfaces to replicate the tool finish. The higher mould temperature delays ice-layer formation at the cavity wall and allows the melt to copy texture under packing pressure. The cost, however, is an extended cooling time of 8% to 15% compared with 20°C mould settings. Cooling-line layouts with a Reynolds number above 10,000 in the channels are specified to keep cavity surface temperature variation below 2°C.
Pigmentation is introduced as a 1 wt% to 4 wt% colour masterbatch. Organic pigments are used where the houseware is promoted as child-accessible, because the article may fall under EN 71-3:2019+A1:2021 migration limits for 19 elements. The masterbatch carrier must be an HDPE homopolymer with a melt flow rate within 15% of the JH910 value to prevent swirl marks in high-gloss surfaces. Fillers are not normally used in high-gloss HDPE housewares. If flame retardancy is required by the importer’s specification, the addition of intumescent flame-retardant masterbatches tends to reduce surface gloss and increase haze. This trade-off must be evaluated with a gloss meter under ASTM D523-14 using a 60° geometry.
Demoulding from polished cavities is performed with draft angles of 1° to 2° on textured surfaces and 0.5° to 1° on polished side walls. If the draft angle is below 0.5°, ejection must use air-assist and a central stripper plate to avoid stress whitening. Weld lines around handle cutouts are weakened by pigment orientation and can fail at impact levels below 2.0 kJ/m² when tested under ISO 180 notched Izod at 23°C. For this reason, gate locations are shifted to move weld lines away from the highest tensile stress during rack storage.
Pallet and dunnage applications create a thick-section flow path that differs from thin-wall packaging. Planks and ribbed feet are filled at wall thicknesses from 4 mm to 8 mm, with a maximum flow length exceeding 800 mm in large single-cavity or two-cavity tools. Melt temperature is controlled between 200°C and 230°C; lower temperatures reduce cycle time but produce visible flow marks on the top deck. Mould temperature is set between 20°C and 40°C, and a chilled water supply pressure of 4 bar to 6 bar is needed to maintain turbulent flow in cooling circuits. Injection pressure often reaches 1,200 bar to 1,500 bar on presses with clamp forces from 2,500 t to 4,000 t.
The primary defect in thick sections is internal voiding rather than surface sink. Voids form when the gate freezes before packing compensates for volumetric shrinkage, which for HDPE is approximately 0.015 mm³/(mm³·°C) multiplied by the temperature window from melt to ejection. Packing pressure is held at 800 bar to 1,000 bar for 15 s to 30 s after fill, and gate freezing is delayed by using an extended sprue bushing with a land length of 2 mm to 3 mm. The screw cushion is maintained at 5 mm to 10 mm during packing. Pallet flexural modulus is measured under ISO 178:2019, and deflection under rated load is assessed by ISO 8611-1:2021 for pallet performance.
Regrind fractions for industrial pallets may reach 50 wt% if the material is generated from cleaned, unpainted JH910 scrap and melt-filtered through a 120 mesh screen during re-pelletising. The blend is kept at a melt flow rate not exceeding 1.5 g/10 min above the virgin value to prevent overpacking of the top deck and underpacking of the lower ribs. Where pallets are exported to the EU, the final article must meet REACH duties for substances of very high concern and may require documentation under RoHS Directive 2011/65/EU if the pallet contains electronic tracking devices. The terminal component is a reusable logistics pallet with an expected service life of 50 to 100 trips under closed-loop return logistics.
Competitive SK Geo Centric HDPE JH910 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SK Geo Centric HDPE JH910 is a high-density polyethylene grade specified for high-flow injection-moulding applications. The grade designation uses the producer’s suffix convention to indicate a nominal melt mass-flow rate of 10 g/10 min at 190 °C under a 2.16 kg load when measured according to ISO 1133-1. The nominal density is 0.960 g/cm³ when measured according to ISO 1183-1. This density places JH910 in the high-crystallinity portion of the HDPE range, giving the material a comparatively high flexural modulus and low residual moisture uptake. The base resin is compounded with a phenolic primary antioxidant, a phosphite secondary stabilizer, and a metallic stearate acid scavenger; the additive package is intended for repeated injection-moulding heat and shear histories, including closed-loop regrind return. The product is supplied as natural pellet for injection-moulded caps, closures, thin-wall containers, housewares, and industrial pails. For food-contact applications, the base resin is designed against FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011, but final compliance must be verified on the finished article.
| Property | Test procedure | Representative value |
|---|---|---|
| Melt mass-flow rate at 190 °C/2.16 kg | ISO 1133-1 | 10 g/10 min |
| Density | ISO 1183-1 | 0.960 g/cm³ |
| Tensile yield stress | ISO 527-2 | 27 MPa |
| Tensile elongation at break | ISO 527-2 | >200% |
| Flexural modulus | ISO 178 | 1,150 MPa |
| Charpy notched impact strength at 23 °C | ISO 179-1/1eA | 3.5 kJ/m² |
| Vicat softening temperature | ISO 306/A50 | 124 °C |
| Heat deflection temperature | ISO 75-2/B | 72 °C |
The tabulated values are representative release-data for the unfilled injection grade; they are not a supply specification. For dimensionally critical parts, lot-to-lot variation in melt flow rate and density is usually smaller than the variation introduced by tool temperature imbalance. The single-point melt mass-flow rate should not be used to infer shear viscosity at gate shear rates; a capillary viscosity curve measured according to ISO 11443 is required for mould-filling simulation.
The defining separation between JH910 and a blow-moulding HDPE is not density but shear viscosity. A fractional-melt blow-moulding grade at 0.3 g/10 min retains high parison melt strength and die swell for extrusion blow moulding, whereas JH910 at 10 g/10 min favours fast cavity filling and short screw recovery. On the same injection machine, a fractional-melt grade often requires a larger gate and longer hold time to pack the cavity; JH910 permits lower fill pressure but has a shorter gate-seal time. Compared with pipe-grade PE100, JH910 is not classified under ISO 12162 and is not validated by long-term hydrostatic testing to ISO 9080; slow crack growth resistance measured to ISO 13479 is not a designed feature. Compared with linear low-density polyethylene, JH910 has higher crystallinity and higher flexural modulus but lower dart impact toughness at sub-ambient temperature. Selection of JH910 is therefore justified only when the part geometry and production throughput make the trade-off in melt strength and environmental stress-cracking resistance acceptable.
When a processor switches from a 4 g/10 min HDPE to JH910 on the same tool, the first measured change is not only lower fill pressure but also a shorter gate-seal time. The gate of a thin-wall container often freezes before the packing phase can complete; therefore hold pressure must be transferred earlier than with a fractional-melt grade. In a hot-runner stack mould producing 0.65 mm wall dairy containers, the typical barrel temperature profile is 190 °C, 200 °C, 210 °C, and 210 °C for a 40 mm screw with an L/D of 20:1. The nozzle is held at 215 °C to retain flow but avoid degradation. The mould coolant is set at 18 °C and the core at 12 °C to minimize sink marks; when the core is below 8 °C, condensation can appear on the tool surface unless the mould area is protected by dehumidified air. The specific hydraulic fill pressure is normally established by short-shot studies; on a 1600 kN servo-hydraulic press, the start point is 80 MPa hydraulic and is adjusted to fill 95% of the cavity before transfer to hold pressure. Back pressure is kept between 0.5 MPa and 1.0 MPa to avoid excessive shear heating. Screw decompression after recovery is set to 3–5 mm.
Differential solidification rather than total shrinkage is the main cause of warpage in thin-wall JH910 parts. Mould shrinkage measured to ISO 294-4 is typically 1.5–2.5%, with flow-direction shrinkage at the lower end and transverse shrinkage at the upper end. A wall-thickness step from 0.6 mm to 2.0 mm creates a solidification-rate gradient; the thin section freezes before the packing pressure can compensate for volumetric shrinkage, and the residual stress appears as sink marks or bow. Rib-to-wall ratios above 0.6 are a common source of visible sink on cosmetic surfaces; gas-counterpressure moulds and sequential valve-gate control reduce but do not eliminate the defect. When dimensional tolerance is tighter than ±0.05 mm, the tool should include post-mould conditioning at 23 °C for 48 h before final gauge. Immediate measurement after ejection overstates dimensions because crystallisation continues after demoulding.
For food-contact compliancy, the base resin falls within the olefin polymer category of FDA 21 CFR 177.1520 and is suitable for contact with aqueous and fatty foods up to the temperature limit assigned to high-density polyethylene by the converter’s end-use conditions. European compliance is assessed under EU Regulation (EU) No 10/2011, where overall migration and specific migration limits are properties of the finished article after processing; the pellet alone cannot be certified. The base resin is formulated without intentional addition of cadmium, lead, mercury, or hexavalent chromium above the maximum concentration values given in Directive 2011/65/EU Annex II. REACH registration is the producer’s responsibility under Regulation (EC) No 1907/2006. The grade is not intended for medical implant or parenteral use, and food-contact converters should control regrind source, purge compounds, and mould-release contamination.
| Regulation / standard | Relevant designation | Application boundary |
|---|---|---|
| Food contact | FDA 21 CFR 177.1520 | Olefin polymer class; final article testing required |
| Food contact | EU Regulation (EU) No 10/2011 | Overall migration tested on finished part |
| Hazardous substances | Directive 2011/65/EU Annex II | No intentional restricted substances above MCV |
| REACH | Regulation (EC) No 1907/2006 | Registration duty with producer |
The process window for multi-cavity tools is established around the thermal gate-freeze time. For a cold-runner mould with a 0.8 mm gate diameter and 1.0 mm wall, hold time is normally 4–6 s; for a valve-gate hot runner with a 1.5 mm tip orifice, hold time can be reduced to 2–4 s. Hot-runner manifold temperature is set between 220 °C and 240 °C. At 250 °C the melt can begin to yellow after residence; maximum barrel residence time at 220 °C is 10 min before purging is required. Regrind incorporation up to 20 wt% is common on closed-loop systems; higher levels reduce melt consistency and increase black specking on colour-sensitive parts. The screw should have a compression ratio of 2.5:1 to 3.0:1; a barrier screw is not required for this narrow molecular weight distribution. Screw surface speed should be kept below 0.3 m/s and hydraulic back pressure below 1.0 MPa to limit shear heating. At start-up, the injection unit should be purged with a low-MFR HDPE after any stoppage longer than 15 min; failure to purge leaves degraded boundary layer on the screw and check ring, causing black speck contamination in the next 50–100 shots.
In caps and closures, the 10 g/10 min melt mass-flow rate measured to ISO 1133-1 permits rapid multi-cavity filling, but the cap skirt can remain oval if the part is ejected above 60 °C. In thin-wall containers, wall thickness below 0.5 mm is achievable when vent depth is kept below 0.02 mm; deeper vents risk flash and surface blemishes. For housewares and storage boxes, the practical limitations are low-temperature impact and environmental stress-cracking resistance; the 3.5 kJ/m² Charpy notched impact value at 23 °C measured to ISO 179-1/1eA should not be extrapolated below -20 °C without testing. Contact with solvent-based oils or silicone release agents should be avoided unless a specific stress-crack test is performed according to ASTM D1693 or ISO 22088. Industrial pails produced from JH910 are often blended with a fractional-melt HDPE or polypropylene to adjust creep resistance, but the blending ratio must be revalidated for batch consistency.