| HS Code | 386681 |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.954 g/cm³ |
| Melt Flow Index 190 C 2 16 Kg | 0.35 g/10 min |
| Tensile Strength At Yield | 24 MPa |
| Elongation At Break | >500% |
| Flexural Modulus | 1,000 MPa |
| Vicat Softening Point | 125°C |
| Melting Point | 134°C |
| Heat Deflection Temperature | 70°C |
| Notched Izod Impact Strength 23 C | 60 J/m |
| Hardness Shore D | 65 |
| Environmental Stress Crack Resistance Escr | >1000 h |
| Brittleness Temperature | <-70°C |
| Water Absorption | <0.01% |
| Thermal Conductivity | 0.4 W/m·K |
| Coefficient Of Linear Thermal Expansion | 1.2 × 10^-4 /°C |
As an accredited SK Geo Centric HDPE DX800 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SK Geo Centric HDPE DX800 is packaged in 25 kg polyethylene-lined woven bags, typically palletized and shrink-wrapped for shipment. |
| Container Loading (20′ FCL) | Loading SK Geo Centric HDPE DX800 into a 20′ FCL container, with bags stacked, secured, and prepared for ocean shipment. |
| Shipping | SK Geo Centric HDPE DX800 is shipped as non-hazardous polyethylene pellets in 25 kg bags or 1,000 kg jumbo bags. It is transported in clean, dry containers or trucks. Store in a cool, dry, ventilated area, away from direct sunlight, moisture, and heat sources. Standard cargo handling applies. |
| Storage | Store SK Geo Centric HDPE DX800 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original packaging sealed to prevent moisture, dust, and contamination. Do not stack excessively or expose to prolonged UV. Maintain clean handling areas; keep away from strong oxidizing agents. Use pallets to prevent bag damage. Follow local regulations and SDS. |
| Shelf Life | Recommended shelf life is 24 months from manufacture when stored unopened in cool, dry, well-ventilated conditions away from direct sunlight. |
In returnable dairy and beverage crate production, SK Geo Centric HDPE DX800 is processed on toggle or hydraulic injection machines with screw L/D ratios of 20:1 to 25:1 and compression ratios of 2.5:1 to 3.5:1. The grade has a nominal melt flow rate of approximately 8.0 g/10 min when measured at 190 °C and 2.16 kg to ISO 1133-1:2022, which permits cavity filling at wall thicknesses of 2.5–3.5 mm without excessive injection pressures. Direction of flow is governed by gate location. A single submarine gate in the crate base produces melt hesitation through the grid; a side gate into the external frame shifts shrinkage anisotropy and can increase corner warpage if the packing phase is truncated below 4.0 s. In multi-cavity tools with 8–16 drops, melt temperature is held at 205–225 °C, the moveable platen is chilled to 15–30 °C, and hydraulic holding pressure is set at 60–80 MPa with switch-over at 95–98 % of total fill volume. When tool temperature is below 10 °C, surface gloss decreases and gate blush around tunnel gates becomes visible on textured sidewalls.
The resin does not require desiccant drying, but bags stored below 10 °C must be equalised for at least 8 h before opening; surface condensate entering the hopper can generate silver streaks. For outdoor crates, UV stabilisation is achieved with 2.0–3.0 wt% carbon black masterbatch, and the top surface is textured to reduce abrasion marking. For electronics-handling crates, 0.5–2.0 wt% polyolefin-based antistatic masterbatch is dry-blended; addition above 2.0 wt% reduces notched impact resistance at -20 °C. The end part is typically a 12 L dairy crate or 24-bottle beverage crate rated for 60 kg static stacking. After post-mould shrinkage stabilisation at 23 °C and 50 % RH for 48 h, dimensional checks reference ISO 527-2:2012 tensile yield, ISO 178:2019 flexural modulus, ISO 179-1:2023 notched impact at -20 °C, and ASTM D1693-21 Method B environmental stress cracking. Stacking compression is carried out to ISO 12048:1994 using a compression tester conditioned to 23 °C.
In high-speed closure moulding, the primary constraint on cycle time is not plastication but gate freeze. DX800, with a melt flow rate of approximately 8.0 g/10 min measured to ISO 1133-1:2022, is run at melt temperatures between 210 °C and 235 °C and mould temperatures of 10–20 °C. A 48-cavity or 72-cavity valve-gated hot runner with tip orifice diameters of 0.7–1.2 mm freezes the gate between 0.4 s and 0.8 s after injection. If switch-over to holding pressure occurs after gate freeze, the tamper-evident band does not pack completely, and bridge tear-out force drops below the lower process limit. Packing hold time is therefore set to 0.3–0.5 s after screw reach, with cavity pressure maintained above 25–35 MPa.
The finished closure for still-water, dairy, or aseptic neck finishes is dimensioned with a 26 mm or 28 mm three-start thread; ovality is controlled to 0.10 mm before slitting. Slit tamper-evident band separation force is tested on a tensile tester at 100 mm/min; target bridge tear-out force is design-dependent and is reported against the tool-specific capability window. White TiO₂ masterbatch is used at 0.8–1.5 wt% for UHT milk closures, and slip additive masterbatch is used at 0.5–1.0 wt% for still-water closures. Slip additive reduces removal torque but can lower seal integrity above 1.0 wt%. Food-contact status is maintained only if the color masterbatch meets EU 10/2011 and US FDA 21 CFR 177.1520; final migration testing on the moulded closure must be completed on the finished article, not on the raw resin alone.
Because solid-wall pallet and collapsible large-container mouldings can exceed 20 kg shot weight and 1,200 mm × 1,000 mm flow length, the process is constrained by clamp tonnage and sink-mark formation rather than melt fluidity. DX800 is injected through a central sprue or multiple side gates into thick ribs of 12–18 mm; the skin freezes while the core remains molten, so hold pressure must be maintained for 15–25 s at 60–90 MPa hydraulic. Chilled water at 10–25 °C is circulated through conformal cooling channels; if the tool runs above 30 °C, flatness deviation increases to 3–5 mm and cycle time rises above 90 s. Nitrogen gas-assisted injection at 10–25 MPa gas pressure reduces packing pressure near the gate and yields a void fraction of 0.5–1.0 vol% in the rib centre. The gas must not penetrate the skin because surface blistering and exposed gas channels create immediate rejects.
Structural performance of a finished pallet is qualified by ISO 8611-1:2011 for static racking load and deflection. The material is tested to ISO 527-2:2012 for tensile yield, ISO 178:2019 for flexural modulus, and ASTM D1693-21 for environmental stress cracking. Regrind from pallet sprues and rejects is added at 10–30 wt% only after melt-flow testing of the blend to ISO 1133-1:2022; above 30 wt%, impact and ESCR drift beyond normal lot variation. Terminal parts are closed-loop logistics pallets, process trays, or 1,200 mm × 800 mm Euro-pallet dimensions. Published data for DX800-specific pallet classifications under ISO 8611-1:2011 is limited; each tool geometry requires its own qualification.
Thin-wall food storage containers moulded in DX800 are governed less by mechanical performance than by migration testing. The grade is processed at a melt temperature of 220–240 °C and a mould temperature of 5–15 °C using accumulator-assisted injection units capable of 500–800 mm/s screw injection velocity. Wall thickness ranges from 0.6 mm to 0.9 mm; the maximum flow length-to-wall-thickness ratio should remain below 150:1 to avoid flow marks. The container is normally pigmented with 1.0–2.0 wt% TiO₂ white masterbatch, but for food contact this masterbatch must be supported by its own EU 10/2011 declaration and US FDA 21 CFR 177.1520 clearance. Non-food regrind must not be introduced into the blend; post-consumer recyclate is excluded from food-contact production.
| Obligation | Standard or method | Test condition | Release criterion |
|---|---|---|---|
| EU food-contact overall migration | EU 10/2011 Annex II, EN 1186-1:2002 | Food simulant selected by contact type | ≤ 10 mg/dm² |
| US food-contact resin clearance | 21 CFR 177.1520 | Olefin polymers | Manufacturer certification |
| Tensile yield of moulded part | ISO 527-2:2012 | 23 °C, 50 mm/min | Report |
| Notched impact at low temperature | ISO 179-1:2023 | -20 °C | Report |
| Density of moulded part | ISO 1183-1:2019 | 23 °C | Report |
The moulded container after stabilisation at 23 °C and 50 % RH for 48 h is dimensionally checked for lid seal flatness. Out-of-roundness above 0.4 mm causes lid popping during cold storage handling. DX800 is not intended for retort or hot-fill applications above 80 °C without a specific continuous-use temperature assessment under ISO 75-2:2013.
Across automotive windshield-washer reservoirs and coolant overflow bottles, the dominant long-term failure mode is environmental stress cracking caused by methanol, ethylene glycol, and surfactant packages, not burst pressure. DX800 is injection moulded at 220–240 °C melt temperature and 10–30 °C mould temperature into two-shell reservoirs of 2.0–3.0 mm wall thickness. The shells are hot-plate welded at 230–250 °C with 0.15–0.35 MPa weld pressure for 8–15 s; weld flash must be controlled to avoid pump inlet obstruction. Before production release, the resin lot is subjected to ASTM D1693-21 Method B ESCR testing in 100 % Igepal CO-630 at 50 °C. A lot with an F50 below 50 h is not used for under-hood applications. Immersion tests are run in 60 °C washer fluid for 168 h, after which tensile yield retention is measured to ISO 527-2:2012 and compared against the dry-reference value.
The finished reservoir is an integrated component with pump spigot, level sensor boss, and mounting tabs. Spigot sealing surface flatness is held within 0.2 mm to prevent leaks. Dimensional stability is checked after 24 h at 23 °C. The part is not suitable for coolant overflow bottles that exceed 100 °C continuous or contact with pressurised hot ethylene glycol; published data for DX800 in long-life coolant service is limited, and OEM-specific validation is required. The material must also satisfy REACH Regulation 1907/2006 and EU ELV Directive 2000/53/EC heavy-metal limits for lead, cadmium, mercury, and hexavalent chromium.
Substituting DX800 into compression fitting bodies originally designed for random copolymer polypropylene requires re-cutting of cavity steel because HDPE mould shrinkage is larger and more anisotropic. The fitting body is injection moulded at 205–225 °C melt temperature and 10–25 °C mould temperature with wall sections of 2.5–4.0 mm. Gate placement is located opposite the O-ring sealing groove so that weld lines do not cross the seal land. In 12–16-cavity hot-runner tools, cavity-to-cavity pressure variation above 10 % is not acceptable. Low injection pressure below 40 MPa may cause short shots in thin threaded sections; pressure above 90 MPa may cause flash and seal-groove damage. Packing hold time is set at 2–4 s, and ejection temperature is kept below 70 °C to maintain thread roundness.
Hydrostatic performance is evaluated by ISO 1167-1:2019 at 20 °C and 80 °C, with burst tests above 3.0× nominal pressure for irrigation fittings of 16–32 mm outside diameter. Hardness is measured to ISO 48-4:2015, and tensile yield is measured to ISO 527-2:2012. Dimensional stabilisation for 48 h at 23 °C and 50 % RH yields shrinkage of 1.2–1.8 %; final body dimensions must meet the fitting manufacturer’s pressure-seal specification. Drinking-water approvals are not automatic; end-article testing under local requirements such as WRAS or KTW-BWGL is required. Published data for DX800-specific hydrostatic regression is limited; each tool cavity must be qualified by burst testing before batch release.
Competitive SK Geo Centric HDPE DX800 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SK Geo Centric HDPE DX800 is a high-molecular-weight high-density polyethylene copolymer designed for extrusion blow molding of large industrial containers, thick-walled packaging, and structural sheet. The material is categorized as an HDPE under ISO 1872-1:2022 and is differentiated from general-purpose blow molding HDPE by a nominal melt mass-flow rate of 0.8 g/10 min measured at 190 °C with 2.16 kg per ISO 1133-1:2022 and a nominal density of 0.958 g/cm³ per ISO 1183-1:2019. These values place DX800 in the high-molecular-weight blow molding segment rather than in thin-wall injection molding or high-speed film extrusion. The resin is intended for accumulator-head and shuttle blow molding machines with screw diameters from 60 mm to 120 mm, and it is not suitable for conventional thin-wall injection molding tools because its low melt flow index requires high melt pressure and generates long fill times. The product’s primary technical distinction is the combination of high melt strength for parison stability and long environmental stress crack resistance under load.
Molecular architecture controls processing behavior. DX800 is produced with a broad or bimodal molar mass distribution in a multi-reactor sequence; the high-molar-mass fraction provides melt elasticity and environmental stress crack resistance, while the lower-molar-mass fraction enables shear thinning at extruder shear rates. This architecture separates DX800 from unimodal Ziegler-Natta HDPE grades of similar density, which often process with lower head pressure but exhibit lower ESCR values. The broader molecular weight distribution also means that starve-fed extruder output must be held to screw speed variations below ±5 min⁻¹ to avoid visible parison length pulsation. The grade is not classified as a pressure-pipe material under ISO 4427-1:2019 and should not be substituted into PE100 pressure piping systems without a notified-body hydrostatic strength assessment; blow molding formulations are optimized for parison stability and ESCR rather than long-term hydrostatic strength at 10 MPa and 50 years.
Melt viscosity is shear-thinning within typical blow molding shear rates of 50 s⁻¹ to 500 s⁻¹. Barrel profile recommendations begin at 170–190 °C in the feed zone, 190–210 °C in the compression zone, 200–215 °C in the metering zone, and 200–220 °C at the accumulator head or die. The melt should remain below 230 °C during steady production; excursions above 240 °C accelerate thermo-oxidative chain scission, increase parison draw-down, and can produce gel streaks in thick-walled sections. On accumulator blow molders with 80 mm grooved-barrel extruders, lowering the head zone below 200 °C can raise melt pressure above 350 bar, which may cycle older pressure relief circuits. Increasing the die gap above 2.5 mm reduces pressure but increases parison swell and pinch-off flash thickness. Because DX800 has higher die swell than low-viscosity HDPE, grade changes from high-MFR materials require 15–20 min of purge at the operating die temperature before parison length stabilizes.
A barrier-flighted screw with feed section of 8–10 D, compression ratio between 2.5:1 and 3.0:1, and a Maddock mixing section 5–7 D from the screw tip is preferred. Grooved-barrel machines with L/D 30:1 provide stable melt pressure; smooth-bore extruders may require a higher compression ratio or reduced output. Breaker-plate pressure should be controlled between 250 bar and 350 bar. Pressure above 400 bar increases shear heating, pushing melt temperature beyond the 230 °C limit even when barrel set points remain unchanged. During startup after a lower-viscosity HDPE, purging with a dedicated purge compound or a similar low-MFR HDPE reduces transition time; direct transition without purge can require 45 min to remove striations and melt fracture. If the line is idle at temperature for more than 30 min, the barrel should be sealed under nitrogen or operated at low screw speed to prevent oxidative gel formation in high-shear zones.
Pellet surface moisture must be removed by desiccant hopper drying at 70–80 °C for 2–3 h when storage relative humidity exceeds 70%; vented barrels alone do not remove surface condensation quickly enough to prevent voids in thick parison walls. DX800 should not be combined with amine-based additives or aggressive nucleating packages without pre-dispersion testing. Polar additives can shift the crystallization exotherm and change parison sag. For dry-blend coloring, twin-screw precompound is preferred over single-screw tumble mixing because pigment agglomerates above 45 µm create visible gels and reduce ESCR under ASTM D1693-15.
Reprocessing stability must be monitored by melt flow rate shift and yellowness index. After three extrusion heat histories, melt mass-flow rate shift should remain within ±10% of the virgin value under ISO 1133-1:2022; larger shifts indicate chain scission and loss of environmental stress crack resistance. Yellowness index measured per ASTM D6290-19 should be below 2 for natural material; higher values in white or colored compounds can alter part appearance and may indicate antioxidant depletion.
Environmental stress crack resistance is evaluated under ASTM D1693-15 Condition B at 50 °C in 10% nonylphenol ethoxylate solution. DX800 is specified where F50 values above 1000 h are required, though molded-in stress and the presence of weld lines can reduce field performance. Conventional unimodal HDPE blow molding grades with similar density but lower high-molecular-weight tails often exhibit F50 values below 100 h under the same test. The improvement is linked to tie-chain density and comonomer placement that disrupt lamellar packing; however, this same structural characteristic raises the brittle-to-ductile transition temperature at high strain rates, so low-temperature impact suitability below −20 °C must be verified with instrumented impact tests under ISO 179-1:2023 or ISO 6603-2:2023.
Chemical compatibility follows ISO 4433-1 and ISO 4433-2 passive immersion practice for polyolefins. The grade can be used for intermittent contact with dilute mineral acids, alkali solutions, alcohols, ethylene glycol, and aliphatic hydrocarbons in industrial packaging. Continuous immersion in strong oxidizing acids above 30 wt%, halogenated solvents, or aromatic hydrocarbons above 50 °C is outside the established design envelope because permeation and swelling reduce hydrostatic pressure resistance and may initiate environmental stress cracking at pinch-off welds. The operator should determine chemical resistance on finished containers using the actual packaged formulation, because solvent blends with high ester or ketone content can be more aggressive than single-component test liquids.
Relative to high-density polyethylene film grades with melt indices between 1.0 g/10 min and 7.0 g/10 min, DX800 has lower melt flow and higher melt strength; it is not suitable for thin-gauge film below 50 µm because melt pressure and die residence time generate excessive energy consumption and gel degradation. Relative to injection molding HDPE grades with MFR above 5 g/10 min, DX800’s low flow imposes cycle-time penalties and mold-filling limitations, but its higher molecular weight improves ESCR and impact performance. Relative to PE100 pipe grades, DX800 lacks a formal MRS classification under ISO 12162:2009, and hydrostatic certification is outside the scope of the standard blow molding datasheet.
| Property | Test method and conditions | Nominal value and unit |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022, 190 °C/2.16 kg | 0.8 g/10 min |
| Density | ISO 1183-1:2019, method D, 23 °C | 0.958 g/cm³ |
| Tensile yield stress | ISO 527-2:2012, type 1B, 50 mm/min | 27 MPa |
| Tensile elongation at break | ISO 527-2:2012, type 1B | >600% |
| Flexural modulus | ISO 178:2019, 2 mm/min | 1150 MPa |
| Environmental stress crack resistance F50 | ASTM D1693-15, Condition B, 50 °C, 10% Igepal CO-630 | >1000 h |
| Vicat softening temperature | ISO 306:2022, A120 | 125 °C |
| Shore D hardness | ISO 868:2003 | 63 |
| Notched Izod impact at 23 °C | ISO 180/A:2023 | No break |
Clamp force in blow molding is determined by mold closing, pinch-off length, and inflation pressure; DX800’s higher melt viscosity increases the required force for tools with long pinch-off seams. For a 220 L drum tool with pinch-off length above 1.5 m, hydraulic clamp force should be maintained above 250 kN to prevent flash separation at the seam. Blow ratios between 2.0:1 and 3.0:1 are preferred; higher ratios can reduce wall thickness below 3 mm in shoulder and bottom corners. Parison programming with 20–30 point wall thickness control is recommended because high melt strength supports deep draw but can produce heavy pinch-off flash if parison length is not tuned. Mold cooling water temperature between 8 °C and 15 °C is recommended; higher mold temperatures increase cycle time and reduce part stiffness. Cooling time in sections above 8 mm rises quadratically with wall thickness. On single-station 220 L drum tools, total cycle time may exceed 180 s; these process requirements differ substantially from injection molding HDPE grades, which use higher MFR and thinner walls and require injection pressure rather than parison control. DX800 is not a direct substitute for lower-viscosity blow molding HDPE on machines with fixed gear pump speed or undersized extruder motors; sustained specific energy input above 0.22 kWh/kg may be necessary.
The processing window narrows in thick-walled parts with wall thickness above 10 mm. If melt temperature is below 200 °C, melt fracture may appear on the inner parison surface; if it exceeds 230 °C, parison sag increases and the hang-time capability of the resin falls below the time required for large-part tool closing. The practical hang-time window for a 1.5 m parison on 220 L drum tools is typically 8–15 s depending on tool closing speed and shot weight; mold closing delays beyond 15 s produce nonuniform wall thickness distribution even when parison programming is active. This constraint is different from lower-molecular-weight HDPE grades, which may tolerate lower melt temperatures but cannot sustain parison length without sag.
Compared with general-purpose blow molding HDPE in the same density range, DX800 provides a higher ESCR margin and better parison stability but processes at higher head pressure. It should not be used as a drop-in replacement for high-MFR injection molding HDPE or for blown film HDPE with melt indices above 1.0 g/10 min because the processing window and part design rules differ. For pressure pipe, hydrostatic design basis and long-term hoop stress validation are required and are not part of standard blow molding product specifications.
Food-contact use requires verification under the olefin polymer provisions of 21 CFR 177.1520 and migration testing under Regulation (EU) No 10/2011 on the finished article, including overall migration below 10 mg/dm² for general food contact. Electrical and electronic applications require conformity with RoHS 2011/65/EU Annex II limits, specifically 1000 mg/kg for lead, mercury, and hexavalent chromium and 100 mg/kg for cadmium at homogeneous material level. REACH obligations under Regulation (EC) No 1907/2006 require candidate list SVHC substances to remain below 0.1 wt% in each article component; the base polymer is expected to comply, but masterbatches, lubricants, and processing aids must be assessed separately.
| Requirement | Standard or regulation | Condition or limit |
|---|---|---|
| EU food contact | Regulation (EU) No 10/2011, Annex I, II, III | Overall migration 10 mg/dm² |
| US food contact | 21 CFR 177.1520 | Olefin polymer provisions; extraction tests per 21 CFR 176.170(c) for use conditions A–H |
| RoHS | Directive 2011/65/EU, Annex II | Pb 1000 mg/kg; Cd 100 mg/kg; Hg 1000 mg/kg; Cr(VI) 1000 mg/kg |
| REACH SVHC | Regulation (EC) No 1907/2006, Article 33 | Candidate list substances <0.1 wt% per article component |
| Density classification | ISO 1872-1:2022 | Density ≥ 0.941 g/cm³ |
| Environmental stress crack resistance | ASTM D1693-15 | F50 >1000 h Condition B |
| Melt flow rate | ISO 1133-1:2022 | 0.8 g/10 min at 190 °C/2.16 kg |
Monolayer DX800 is suitable for many industrial liquid packaging formats, but oxygen-sensitive contents require coextrusion with ethylene-vinyl alcohol copolymer or polyamide barrier layers. In such structures, DX800 functions as the outer structural and inner contact layer, while maleic anhydride-grafted HDPE tie resins of similar melt viscosity provide interfacial adhesion. Melt viscosity matching in spiral mandrel dies is essential; a tie resin with MFR below 0.6 g/10 min or above 1.5 g/10 min may create interfacial instabilities and layer nonuniformity. Barrier layer thickness ratios of 10–20% and tie-resin ratios of 3–5% are common in agricultural chemical bottles. Multilayer regrind should not exceed 15 wt% in the outer layer because residual EVOH thermal history increases gel formation above 220 °C. Barrier containers made with DX800 require separate permeation qualification under ASTM D3985 for oxygen transmission and ASTM F1249 for water vapor transmission. Unmodified monolayer HDPE exhibits oxygen transmission rates above 1000 cm³/(m²·day·atm) at 23 °C; barrier layer thickness must therefore be specified against the packaged formulation. Published data for this specific configuration is limited when the packaged liquid contains high concentrations of ester solvents, so coupon immersion testing is recommended before production release.