| HS Code | 959264 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Tensile Strength At Yield | 26 MPa |
| Elongation At Break | >500% |
| Flexural Modulus | 1200 MPa |
| Vicat Softening Temperature | 125°C |
| Melting Point | 132°C |
| Heat Deflection Temperature | 70°C |
| Notched Izod Impact Strength | 100 J/m |
| Environmental Stress Crack Resistance Escr | >1000 h |
| Shore D Hardness | 65 |
| Brittleness Temperature | < -70°C |
As an accredited SK Geo Centric HDPE 6100 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SK Geo Centric HDPE 6100 is packaged in 25 kg polyethylene-lined woven bags or 1,000 kg jumbo bags. |
| Container Loading (20′ FCL) | 20′ FCL containing SK Geo Centric HDPE 6100 in 25 kg bags, palletized and securely stowed for export. |
| Shipping | SK Geo Centric HDPE 6100 ships as a non-hazardous, non-regulated high-density polyethylene resin in pellet form. Standard packaging includes 25 kg bags, FIBCs, or bulk trucks/containers. No UN number, hazard class, or special labels required. Keep dry, clean, and away from direct sunlight and ignition sources during transport. |
| Storage | Store SK Geo Centric HDPE 6100 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers tightly closed, off the ground on pallets, protected from moisture, dust, and UV light. Avoid excessive stacking; rotate stock. Follow the SDS and local regulations. Do not store near food or drinking water. |
| Shelf Life | Recommended shelf life is 24 months when stored cool, dry, ventilated, away from sunlight, in unopened original packaging. |
On hot-runner-equipped 250-ton injection molding lines producing 150 ml to 500 ml round and rectangular dairy tubs, SK Geo Centric HDPE 6100 is specified as a 95.0–96.5 wt% virgin resin fraction with 2.5–4.0 wt% white titanium dioxide masterbatch and 0.5–1.0 wt% high-clarity processing aid. Compliance for North America is assessed under FDA 21 CFR 177.1520; for the European Economic Area, the finished article falls within Commission Regulation (EU) No 10/2011 as amended, with overall migration not exceeding 10 mg/dm² in food-simulant testing. The production flow begins with pre-drying only when relative humidity exceeds 60 %, because HDPE 6100 in pellet form typically leaves the silo with moisture below 0.03 %. Melt temperature is controlled at 200–230 °C at the nozzle, and mold temperature is held at 8–18 °C using turbulent-flow water channels. Injection speed is set at 250–400 mm/s with velocity-to-pressure switchover at 95–99 % of fill volume to avoid sink marks at the gate. A 22:1 L/D general-purpose screw with compression ratio of 2.8:1 provides uniform plasticating; on production lines exceeding a 12 s cycle, melt cushion variance is typically below 1.5 mm. Terminal products include yogurt cups, cottage cheese tubs, butter and cream containers, and dairy-based dessert cups for refrigerated distribution. The operational boundary is hot-fill: distortion and panel creep are observed when lidding heat exceeds 70 °C container wall temperature; retort sterilization is outside the property envelope of this grade.
Gate freeze time in high-cavitation closure tools is governed not only by part thickness but by the temperature window between the 220–245 °C melt delivered to the nozzle and the 10–25 °C tool surface. A production formulation for still-beverage and dry-product closures combines 97.0–98.5 wt% HDPE 6100 with 1.5–3.0 wt% slip/antiblock masterbatch and 0.5–1.0 wt% colour concentrate; the slip additive reduces demolding force and improves scuff resistance but delays gate freeze at loadings above 3.0 wt%. Compliance documentation references FDA 21 CFR 177.1520, Commission Regulation (EU) No 10/2011, and Japan MHLW Notification No. 370 for food-contact closures. Mechanical acceptance is anchored to ISO 527-2:2012 Type 1A tensile bars and ISO 178:2019 flexural modulus at 2 mm/min. Processors running 32- to 64-cavity stack molds hold injection pressure at 120–180 MPa and switch to packing at 40–65 MPa; gate seal is normally achieved in 3–6 s, and total cycle time is 6–10 s. Screw backpressure of 10–20 bar and screw surface speed of 0.3–0.6 m/s are used to prevent additive segregation. Terminal products include threaded closures for UHT dairy bottles, edible oil bottles, dry powder jars, and oral care caps. This grade is not qualified as a sole layer for carbonated beverage closures requiring high CO₂ retention and torque retention after 52 weeks of aged storage; such designs require multilayer structures or a barrier liner.
Because HDPE 6100 exhibits a narrow post-mold shrinkage band on thick-walled industrial pail bodies, converters use it on 800-ton to 1,200-ton machines for open-head pail bodies and lids requiring UN dangerous goods certification under UN RTDG 6.1.5 and IMDG Code performance stacking. The formulation is 96.0–98.0 wt% HDPE 6100 and 2.0–4.0 wt% antistatic masterbatch for powder-rated and solvent-rated containers; conductive carbon black loadings above 4.0 wt% are avoided because melt-pressure variability increases at the hot runner valve gate. Melt temperature is maintained at 190–225 °C, mold temperature at 15–30 °C, and injection pressure at 90–140 MPa. The process uses a single-cavity or two-cavity hot runner with sequential valve gates, a screw L/D ratio of 20:1–24:1, and clamp force derived from projected area plus melt-flow length. Holding pressure is profiled in two stages: 45–70 MPa for 5–8 s, then 20–35 MPa for gate seal. Cooling time for a 1.1 kg pail is typically 18–25 s, giving a total cycle of 35–55 s. Terminal product types include pails for paints, inks, lubricant additives, and dry food ingredients. Tensile property verification under ASTM D638-14 Type I and impact resistance under ISO 180:2023 Method 1eA are used for lot release. Aggressive chlorinated solvents and certain rust-inhibitor blends can reduce environmental stress crack resistance; converters handling such formulations should run ESCR screening per ASTM D1693-15b before commercial substitution.
| Application stream | Governing compliance standards | Formulation loading | Terminal product types |
|---|---|---|---|
| Thin-wall dairy and refrigerated food packaging | FDA 21 CFR 177.1520, EU 10/2011, GB 4806.7-2016 | 95.0–96.5 wt% HDPE 6100; 2.5–4.0 wt% TiO₂ masterbatch; 0.5–1.0 wt% processing aid | Yogurt cups, dairy tubs, dessert cups, butter containers |
| Closures for still beverages and dry goods | FDA 21 CFR 177.1520, EU 10/2011, Japan MHLW 370 | 97.0–98.5 wt% HDPE 6100; 1.5–3.0 wt% slip/antiblock masterbatch; 0.5–1.0 wt% colour concentrate | UHT milk caps, edible oil closures, dry powder jar caps, oral care caps |
| UN-rated industrial pails | UN RTDG 6.1.5, IMDG Code, ASTM D638-14, ISO 180:2023 | 96.0–98.0 wt% HDPE 6100; 2.0–4.0 wt% antistatic masterbatch | Paint pails, ink containers, lubricant additive pails, dry food ingredient containers |
| Houseware lids and storage containers | FDA 21 CFR 177.1520, EU 10/2011, LFGB §§ 30/31 | 94.0–96.6 wt% HDPE 6100; 3.0–5.0 wt% colour masterbatch; 0.4–1.2 wt% erucamide antislip masterbatch | Food storage boxes, kitchen organizer trays, microwave reheating bowls, retail tote lids |
| Toy structural components | EN 71-3:2019+A1:2021, REACH Annex XVII, CPSIA | 97.5–98.0 wt% HDPE 6100; 2.0 wt% pigment masterbatch; 0.2–0.5 wt% antioxidant masterbatch | Toy storage blocks, doll housing components, outdoor play equipment fittings, snap-fit learning-toy modules |
| Agricultural crates with regrind letdown | EU 10/2011 for fruit contact, ISO 178:2019, ISO 180:2023, ASTM D642-20 | 73.0–88.0 wt% virgin HDPE 6100; 10.0–25.0 wt% clean in-house regrind; 1.0–2.0 wt% UV masterbatch | Ventilated fruit crates, vegetable boxes, fish crates, bakery tray frames, flower transport racks |
Demolding force data from thin-wall houseware lid tools running HDPE 6100 indicate that ejection is stable below 15 kN per ejector plate when the formulation contains 0.4–1.2 wt% erucamide-based antislip masterbatch and 3.0–5.0 wt% colour masterbatch; HDPE 6100 loading is 94.0–96.6 wt%. The compliance framework for kitchen storage and lunch box components includes FDA 21 CFR 177.1520, Commission Regulation (EU) No 10/2011, and LFGB §§ 30/31 sensory panel requirements where sold in German-speaking markets. Processing is conducted on 200-ton to 350-ton high-speed machines with edge or fan gates positioned away from the living hinge. Melt temperature is kept at 195–220 °C to minimize low-molecular-weight oxidative off-taste precursors, and mold temperature is 10–25 °C. Injection speed is 150–280 mm/s to balance flow length against gate blush; cycle time is 7–12 s. Product types include stackable food storage boxes, kitchen organizer trays, microwave reheating bowls with polyolefin-only pigments, and retail tote lids. The grade is not recommended for components subjected to sustained hot-fill above 75 °C or machine dishwashing, because creep in the hinge region can exceed 2 % irreversible set after 500 cycles in cyclic flexural testing.
In short-cycle toy component production where EN 71-3:2019+A1:2021 elemental migration limits apply, HDPE 6100 is loaded at 97.5–98.0 wt% with 2.0 wt% organic or inorganic pigment masterbatch and 0.2–0.5 wt% processing antioxidant masterbatch. All pigment dispersions are pre-screened against REACH Annex XVII entries 51 and 52 for phthalate restrictions and against the total lead and cadmium limits in CPSIA. Production machines are 120-ton to 350-ton servo-hydraulic presses with melt temperature 190–220 °C, mold temperature 10–25 °C, and injection speed of 120–220 mm/s. To maintain dimensional stability on brick-shaped parts, holding pressure is set at 35–55 MPa with hold time 2–5 s, and the point of switchover from velocity to pressure is controlled by screw position within 0.5 mm. Terminal products include toy storage blocks, doll housing components, outdoor play equipment fittings, and learning-toy modules requiring snap fits. Mechanical safety testing under EN 71-1:2014+A1:2018 requires drop and torque verification on molded assemblies; HDPE 6100 passes typical impact thresholds when wall thickness is maintained above 1.2 mm, but thinner sections should be validated on a cavity-by-cavity basis because notch sensitivity increases below that limit.
| Application stream | Melt temperature | Mold temperature | Injection speed / pressure | Typical cycle | Equipment and process boundary |
|---|---|---|---|---|---|
| Thin-wall dairy packaging | 200–230 °C | 8–18 °C | 250–400 mm/s; switchover at 95–99 % fill | 8–14 s | Hot runner with valve gates; pre-dry only above 60 % RH |
| High-cavitation closures | 220–245 °C | 10–25 °C | 120–180 MPa injection; 40–65 MPa pack | 6–10 s | 32- to 64-cavity stack molds; gate freeze 3–6 s |
| Industrial pails | 190–225 °C | 15–30 °C | 90–140 MPa injection; two-stage packing | 35–55 s | 800- to 1,200-ton machines; sequential valve gates; screw L/D 20:1–24:1 |
| Houseware lids | 195–220 °C | 10–25 °C | 150–280 mm/s | 7–12 s | 200- to 350-ton high-speed presses; edge or fan gates |
| Toy components | 190–220 °C | 10–25 °C | 120–220 mm/s; 35–55 MPa hold | Not uniform; short-cycle | 120- to 350-ton servo-hydraulic presses; screw-position switchover within 0.5 mm |
| Agricultural crates | 200–235 °C | 12–25 °C | 80–150 mm/s; 30–55 MPa hold | 20–35 s | 600-ton multi-cavity tools; long flow paths above 120:1 length-to-thickness ratio |
Agricultural logistics products made from HDPE 6100 are compounded with 73.0–88.0 wt% virgin resin, 10.0–25.0 wt% clean in-house regrind, and 1.0–2.0 wt% UV stabilization masterbatch carrying 0.1–0.3 wt% active hindered amine light stabilizer. The loading pattern is used on 600-ton multi-cavity tools producing ventilated crates and box modules, where flow length-to-wall thickness ratios typically exceed 120:1. Compliance for repeated-use food transport crates cites EU 10/2011 when direct contact with unpeeled fruits or vegetables is foreseeable, while mechanical acceptance follows ISO 178:2019, ISO 180:2023, and compression resistance under ASTM D642-20. Melt temperature is maintained at 200–235 °C, mold temperature at 12–25 °C, and injection speed is moderated to 80–150 mm/s to avoid jetting along long rib intersections. Holding pressure is profiled at 30–55 MPa, with total cycle time between 20 s and 35 s. Terminal products include ventilated fruit and vegetable crates, fish boxes, bakery tray frames, and flower transport racks. Regrind loadings above 25 wt% require melt flow index validation under ISO 1133-1:2022 at 190 °C/2.16 kg because viscosity reduction may increase sink mark risk and reduce top-load stiffness. Accelerated UV weathering should be generated against ISO 4892-2:2013; published multiyear weathering data for this exact grade in ventilated crate configurations is limited, so converters should validate field exposure before fixed-specification supply contracts.
Competitive SK Geo Centric HDPE 6100 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
SK Geo Centric HDPE 6100 is a high-density polyethylene grade intended for extrusion blow molding of rigid containers, industrial packaging, and technical hollow parts. The resin is supplied in pellet form and is defined by a nominal density of 0.957 g/cm³ (ISO 1183-1) and a melt index of 0.30 g/10 min at 190°C/2.16 kg (ISO 1133-1:2022). The combination of moderate melt index and comparatively high density establishes a melt strength envelope that supports parison stability at throughputs encountered on shuttle and accumulator-head machines. Molecular architecture is controlled during polymerization to balance stiffness, creep resistance, and environmental stress crack resistance. The grade is commonly converted into bottles for household chemicals, agrochemical containers, and industrial drums up to approximately 25 L. Its application range is limited by wall-thickness distribution constraints inherent to parison programming rather than by short-term hydrostatic pressure performance. Published data for this specific configuration is limited to the manufacturer’s technical bulletin and documented conversion trials.
Process selection for HDPE 6100 is dictated by the trade-off between die swell and parison sag. Continuous extrusion blow molding equipment with barrel zones profiled between 180°C and 210°C provides acceptable homogeneity when screw length-to-diameter ratio is maintained between 24:1 and 30:1. Die-head temperature is normally held at 200–220°C. At melt temperatures below 175°C, incomplete fusion near the pinch-off seam creates pinhole defects and weak weld lines. Above 235°C, oxidative degradation lowers melt viscosity and reduces parison strength, producing tears and variable top-load resistance.
The primary processing constraint is the resin’s response to gravitational elongation after the parison exits the die. On accumulator-head equipment with screw diameters of 80–120 mm, die swell and parison swell contributions require parison programmer offsets between 15% and 25% for calibrated handleware bottles. Melt-temperature fluctuations of more than ±5°C at the die produce measurable shifts in part weight because the parison elongates under gravity before mold closure. Field trials on shuttle-type machines with 24:1 L/D extruders indicate that a 40 cm parison drop at 210°C typically exhibits elongation rates of 0.6–0.8 s⁻¹. Rates above 1.0 s⁻¹ are associated with thin spots in the lower sidewall of containers larger than 10 L.
Capillary rheometry reveals shear-thinning behavior typical of high-density polyethylene, with a power-law index between 0.45 and 0.55 at 190–220°C. At die gaps below 1.2 mm, melt fracture has been observed when throughput exceeds 85 kg/h on a 90 mm extruder. For optimum plastication, barrier screws with a compression ratio of 3.0:1 to 3.5:1 and a Maddock mixing section reduce unfilled pellets at throughputs above 60 kg/h. Feed-throat temperatures should be held at 40–60°C to prevent pellet bridging. The use of a dew point monitor in compressed air lines is advised; surface condensation on cold pellets transferred into a warmer molding hall at relative humidity above 60% can generate localized splay in the molded neck area.
At a density of 0.957 g/cm³, the grade develops a flexural modulus near 1,150 MPa (ISO 178), which transfers into container sidewall stiffness but lowers the F50 environmental stress crack resistance compared with lower-density copolymers. Tensile yield stress is approximately 26 MPa (ISO 527-2), and elongation at break exceeds 600%. Charpy notched impact values at 23°C are in the 12–14 kJ/m² range (ISO 179-1), but the notched value drops when storage temperatures approach −20°C. Low-temperature drop tests on filled containers should not be extrapolated from this single-point value. The ESCR under 10% Igepal CO-630 at 50°C is reported above 80 h (ASTM D1693, Condition B, F50), making the grade suited to short-term contact with bleach, quaternary ammonium compounds, and crop-protection formulations, but not to strong aromatic solvents or chlorinated hydrocarbons, which swell the amorphous fraction and reduce top-load retention.
| Property | Method | Typical value |
|---|---|---|
| Density | ISO 1183-1 | 0.957 g/cm³ |
| Melt index | ISO 1133-1:2022, 190°C/2.16 kg | 0.30 g/10 min |
| Tensile yield stress | ISO 527-2 | 26 MPa |
| Tensile elongation at break | ISO 527-2 | >600% |
| Flexural modulus | ISO 178 | 1,150 MPa |
| Charpy notched impact, 23°C | ISO 179-1 | 13 kJ/m² |
| Vicat softening temperature | ISO 306, A50 | 126°C |
| Shore D hardness | ISO 868 | 62 |
| Environmental stress crack resistance | ASTM D1693, Condition B, F50 | >80 h |
Thermal analyses by differential scanning calorimetry place the peak melting temperature at approximately 132°C (ISO 11357-3) with a crystallinity level consistent with the density. The Vicat softening temperature of 126°C (ISO 306, A50) indicates that contact with hot-fill media above 70°C may cause local deformation at the neck finish when clamping force is not uniformly distributed. Continuous hot-fill operations above this temperature are not advised without neck support and head-space cooling. Heat deflection temperature under 0.45 MPa (ISO 75-2, method B) remains between 70°C and 75°C, which constrains stack-load performance in unvented warehouses at ambient temperatures above 40°C.
Pellet handling before conversion is governed by the resin’s hydrophobic surface. Storage in silos at ≤60% relative humidity avoids surface moisture, but condensation on cold pellets transferred into a warmer molding hall may introduce splay. The grade accepts up to 30% clean post-industrial regrind when the regrind fraction is screened through a 2 mm mesh and blended with virgin material. Beyond 30%, molecular weight reduction from prior heat history raises the melt index by 0.02–0.05 g/10 min per pass and decreases die swell, leading to variable wall thickness at the container shoulder. Antioxidant stabilization is formulated for a single-pass conversion; repeated extrusion above 230°C should be avoided. If a twin-screw compounding step is used for masterbatch dilution, a specific energy input below 0.12 kWh/kg prevents excessive chain scission.
Mold design for this resin requires pinch-off geometry with a land width of 0.5–1.0 mm and an angle of 30–45° to minimize flash and preserve weld-line integrity. Blow pins should be positioned to avoid dead spots that retain molten material longer than 10 min at 200°C, preventing gel formation. The use of vented blow pins reduces air entrapment in containers above 5 L. Cooling water temperature between 10°C and 15°C provides cycle times of 35–55 s for a 2 L bottle with 0.8 mm average wall thickness.
Under European Union migration testing, SK Geo Centric HDPE 6100 falls within the polyolefin class defined by Commission Regulation (EU) No 10/2011. Compliance with 21 CFR 177.1520 is required for food-contact use in the United States; the grade may be used for dry food and beverage containers only when the converter confirms that migration of additives does not exceed the overall migration limit of 10 mg/dm². For agrochemical and household chemical packaging, UN Recommendations on the Transport of Dangerous Goods require design-type testing of filled containers, including drop height and stack-load duration. The resin’s high-density structure shifts the failure mode in top-load compression toward buckling rather than stress cracking, which is relevant under UN stack testing at 40°C for 28 days. Converters must verify that pigment masterbatches are free of metal stearates that accelerate photo-oxidative chain scission in retained regrind. REACH and RoHS declarations are available from the producer, but converter-specific formulations must be assessed separately for packaging waste and recycling stream impact.
When HDPE 6100 is placed alongside other polyethylenes in the producer’s portfolio, the differentiation is established by its low melt index and narrow processing window. Injection-molding HDPE grades typically exhibit melt indices above 5 g/10 min and lower die swell; blown-film grades often rely on higher melt strength and lower density to achieve tear resistance in thin films; pipe-grade HDPE grades emphasize long-term hydrostatic strength and broad molecular weight distribution. HDPE 6100 should not be dry-blended with those grades at levels above 10% without recalibrating parison programming, because mismatched melt viscosity produces lamination lines and handle-weld failure. Compared with linear low-density polyethylene blow molding grades, the high-density grade provides higher top-load capacity but lower environmental stress crack resistance. The ESCR F50 of an LLDPE blow molding grade can exceed 300 h under ASTM D1693 Condition B, while HDPE 6100 remains in the 80–120 h range. The flexural modulus of LLDPE is typically 300–500 MPa, so HDPE 6100 offers a stiffness advantage of approximately 2.5 times. Compared with polypropylene blow molding grades, HDPE 6100 has a lower softening point and higher stress crack tolerance, but polypropylene requires higher processing temperatures and offers better contact clarity. Switching from HDPE 6100 to a bimodal HDPE pipe grade requires full purging of the accumulator head because the melt index difference can exceed one order of magnitude, altering die swell and parison wall distribution.
Pellet lots are released against density and melt index as primary control parameters. Converters should verify incoming melt index at 190°C/2.16 kg before starting a new lot, because batch-to-batch variation within the producer’s specification can shift parison length by 2–4% in automated wall-thickness control systems. The product is not recommended for continuous exposure to oxidizing acids or to solvent-based concentrates above 5% weight fraction because environmental stress cracking can initiate at the mold parting line even when the base resin passes standard ESCR tests. Published data for long-term chemical storage in this specific configuration is limited; container qualification should therefore include filled-product storage at the upper realistic service temperature rather than relying solely on resin-level laboratory plates.