| HS Code | 272049 |
| Density | 1.34 g/cm³ |
| Melt Flow Rate | 15 g/10 min at 230°C/2.16 kg |
| Tensile Strength At Break | 50 MPa |
| Elongation At Break | 150% |
| Flexural Modulus | 2200 MPa |
| Flexural Strength | 80 MPa |
| Notched Izod Impact Strength | 60 J/m |
| Heat Deflection Temperature | 85°C at 0.45 MPa |
| Vicat Softening Temperature | 105°C |
| Glass Transition Temperature | 110°C |
| Light Transmittance | 88% |
| Haze | 1% |
| Mold Shrinkage | 0.5% |
As an accredited SK Chemicals ECOTRIA® PEN/PETG Blend R102 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | SK Chemicals ECOTRIA® PEN/PETG Blend R102 is supplied in 25 kg moisture-resistant bags, palletized and labeled for industrial storage and transport. |
| Container Loading (20′ FCL) | SK Chemicals ECOTRIA® PEN/PETG Blend R102 is loaded into a 20-foot FCL container, palletized and secured for export shipment. |
| Shipping | SK Chemicals ECOTRIA® PEN/PETG Blend R102 is supplied as non-hazardous copolyester resin pellets in moisture-proof bags, fiber drums, or octabins on pallets. Transport in closed, dry vehicles; protect from moisture, direct sunlight, and physical damage. No UN hazard class or special transport label is required. |
| Storage | Store `SK Chemicals ECOTRIA® PEN/PETG Blend R102` in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed to prevent moisture pickup and contamination. Avoid dust generation and accumulation; use grounding/bonding to control static. Separate from strong oxidizers and follow SDS/local regulations. |
| Shelf Life | Typically two years when stored dry in unopened original packaging at ambient temperature, away from direct sunlight and moisture. |
Competitive SK Chemicals ECOTRIA® PEN/PETG Blend R102 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Among melt-processable barrier resins used in cosmetic, personal-care, and fragrance-contact packaging, SK Chemicals ECOTRIA® R102 is formulated as an amorphous polyethylene naphthalate/glycol-modified polyethylene terephthalate blend. The naphthalene dicarboxylate unit increases chain stiffness and interchain cohesion relative to unmodified PETG, while the glycol-modified terephthalate fraction retains melt processability, toughness, and optical transparency. R102 is supplied as natural pellets for injection molding and sheet extrusion where standard PETG fails by environmental stress cracking or excessive oxygen ingress. The naphthalate-derived absorption in the 320–380 nm region also provides partial UV screening. Published data for the exact R102 grade in peer-reviewed literature is limited; performance is therefore verified using the relevant ISO or ASTM methods on production-representative specimens.
Thermal and rheological comparison begins with the glass transition. Standard PETG grades generally exhibit a glass transition temperature by ISO 11357-2:2020 in the range 78–82°C, whereas PEN homopolymer is typically near 120–125°C. PEN/PETG blends develop a single composition-dependent glass transition when transesterification is sufficient; R102 is positioned in the intermediate region. The glass transition elevation reduces deformation under warm-fill conditions and allows short-cycle hot filling up to a temperature that must be confirmed on the final part geometry. In parallel, oxygen permeability measured by ASTM D3985 on 300 µm compression-molded sheet or 500 µm injection-molded plaques is lower than PETG. Published class-level data for naphthalate-containing blends show oxygen transmission coefficients roughly 2–4 times below PETG at 23°C and 0% RH, but not as low as PEN homopolymer. Water vapor transmission follows a smaller reduction because the naphthalate unit is not a polar barrier; WVTR is controlled primarily by thickness and degree of orientation.
Mechanical response is also shifted. Tensile yield strength under ISO 527-2:2012 at 50 mm/min remains close to the PETG baseline, while elongation at break typically decreases when the naphthalate fraction exceeds 20 wt%. Notched Izod impact under ISO 180/A is generally between 20 and 60 J/m, but the exact value depends on processing history and moisture content. The amorphous structure limits mold shrinkage to isotropic values; shrinkage classification is made under ISO 294-4 after 48 h at 23°C and 50% RH.
Differences from other products are most visible in chemical resistance and UV exposure. Compared with standard PETG, R102 exhibits slower solvent uptake and a higher critical strain for craze initiation in terpene-containing fragrances. Compared with PCTG, the naphthalate-containing backbone provides a denser aromatic packing and stronger UV absorption; however, the melt processing window is narrower than PCTG when temperatures approach 270°C. Compared with PEN homopolymer, R102 requires lower melt temperature and a shorter residence time, shows reduced screw torque in a 25 mm single-screw extruder at 80 rpm, and avoids the rapid crystallization of PEN at low mold temperatures.
Dehumidified-air drying is mandatory before melt processing. The pellets should be dried in a desiccant-bed hopper fed with air at dew point ≤ -30°C and temperature 65–80°C for 4–6 h to reach residual moisture below 0.01% by ISO 15512:2019 Method A. Drying beyond 8 h at the upper temperature is not advisable because surface tack and acetaldehyde generation can increase. On a reciprocating-screw injection molding machine with a 20:1–24:1 L/D barrel, a low-compression screw and free-flow ring valve are preferred. Initial barrel settings of 220–240°C at the rear zone, 235–250°C at the center, and 245–255°C at the nozzle are common practice, with melt temperature measured by infrared thermometry held below 265°C. Melt residence time should be kept under 5 min at maximum temperature; in hot-runner systems, externally heated manifolds should use low-mass torpedo tips and avoid dead spots where naphthalate degradation forms yellow bodies. Holding pressure 40–70 MPa, back pressure 0.5–1.5 MPa, and screw speed 50–120 rpm are appropriate starting values. Mold temperature is maintained at 15–30°C for surface gloss and dimensional stability; higher mold temperatures up to 45°C reduce residual stress but increase cooling time by approximately 15–25% for a 2 mm wall.
The blend is specified where PETG closures, bottles, and trays fail by craze initiation at molded-in stress concentrators such as gate vestiges, weld lines, or sharp corner radii. Fragrance compounds with log P values above 2.5, including d-limonene, linalool, and methyl salicylate, plasticize PETG surfaces and reduce critical strain. In ECOTRIA R102, the naphthalene unit lowers equilibrium solvent uptake and raises the critical strain for environmental stress cracking. A ranking test using ASTM D543, Method A, with cotton-swab or bent-strip contact at 0.5% strain for 30 min at 23°C can be used to qualify incoming lots; published data for this specific blend configuration is limited, but class-level results place R102 above PETG and below PEN homopolymer in ethanol/water and limonene resistance. Continuous immersion in methylene chloride, acetone, or N-methylpyrrolidone is outside the operational window because these solvents can produce haze and stress cracking within 24 h at 23°C. Similarly, aqueous systems above pH 10 at temperatures above 50°C accelerate ester hydrolysis and should be avoided in continuous service.
Compliance statements are application-specific and must be confirmed with the grade-specific certificate. The following table records the primary regulatory touchpoints for food-contact, packaging, and electrical/electronic uses where a PEN/PETG blend is submitted for qualification.
| Area | Standard or clause | Threshold / condition |
|---|---|---|
| EU food-contact plastics | Commission Regulation (EU) No 10/2011 as amended | Overall migration ≤ 10 mg/dm² in food simulants A, B, C, D1, D2, E depending on final article |
| US food-contact polymers | FDA 21 CFR 177.1630 where applicable to PET-type base polymers; verify grade-specific Food Contact Notification for naphthalate-containing articles | Extractive limits per applicable regulation |
| Packaging heavy metals | EU 94/62/EC Article 11 | Sum of Pb, Cd, Hg, Cr(VI) ≤ 100 mg/kg |
| RoHS | Directive 2011/65/EU Annex II | Pb ≤ 0.1 wt%, Cd ≤ 0.01 wt%, Hg ≤ 0.1 wt%, Cr(VI) ≤ 0.1 wt% |
| REACH SVHC | Regulation (EC) No 1907/2006, Article 33 | No intentional SVHC above 0.1 wt% per article |
| Residual moisture | ISO 15512:2019 Method A | ≤ 0.01 wt% before melt processing |
When the melt is injected into multi-cavity closures with wall sections exceeding 3 mm, the lower melt viscosity of R102 permits filling at lower packing pressure than PEN homopolymer. Gate design should minimize shear heating because the naphthalene segment is prone to shear-induced yellowing in small sprues and hot-runner drops. In a 40 mm, 20:1 L/D single-throat hot-runner system with valve gates, sequential valve opening can reduce weld-line formation in oval caps. Part shrinkage is measured under ISO 294-4 after 24 h at 23°C and 50% RH; the amorphous phase yields isotropic shrinkage, but gate area can show slightly higher shrinkage due to orientation. Dimensional capability for a 25 mm closure should be verified by coordinate measuring machine after 24 h moisture equilibration. If cracking occurs during capping torque testing, the failure is usually initiated at the top of the cap at the cold weld line; increasing mold temperature from 20°C to 35°C and reducing second-stage packing time can lower internal stress.
Sheet extrusion for formed cosmetic trays and inserts uses a process window that differs from injection molding. The amorphous melt exhibits higher melt stiffness and edge stability, allowing 300–600 µm sheet to be run on a 30:1 L/D single-screw extruder with a barrier screw and a 40/60/80 screen pack. Melt pumps are recommended to reduce surging; roll-stack temperature settings of 40°C upper roll, 50°C middle roll, and 40°C lower roll are typical starting conditions for 350 µm sheet. Thermoforming should be performed at a sheet surface temperature 10–25 K above the glass transition of the grade; actual values are to be confirmed by dynamic mechanical analysis under ISO 6721-11. Plug-assisted forming reduces corner thinning but introduces contact marks if the plug temperature exceeds 80°C. Scrap regrind is acceptable up to 20 wt% when dried with virgin pellets; higher regrind fractions shift haze and lower notched Izod under ISO 180/A. Published data for this specific R102 configuration is limited for regrind levels above 20 wt%; process validation is required.