| HS Code | 252588 |
| Density | 0.954 g/cm3 |
| Melt Flow Rate 190 C 2 16 Kg | 0.08 g/10 min |
| Tensile Yield Strength | 25 MPa |
| Elongation At Break | >=600% |
| Flexural Modulus | 1000 MPa |
| Notched Izod Impact Strength | 30 kJ/m2 |
| Vicat Softening Temperature | 125 °C |
| Brittleness Temperature | <=-70 °C |
| Environmental Stress Cracking Resistance | >=1000 h |
| Shore D Hardness | 60 |
| Water Absorption | <=0.01% |
| Dielectric Constant | 2.3 |
| Thermal Conductivity | 0.4 W/m·K |
| Melting Point | 130 °C |
As an accredited Sinopec Zhenhai HDPE ZH6098 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Zhenhai HDPE ZH6098 is packaged in 25 kg PP woven bags, palletized and wrapped for industrial shipment. |
| Container Loading (20′ FCL) | Sinopec Zhenhai HDPE ZH6098 container loading: 20′ FCL, palletized bags, dry, secured, standard industrial packaging for safe transport. |
| Shipping | Sinopec Zhenhai HDPE ZH6098 is a non-hazardous polyethylene resin, typically shipped in 25 kg PP woven bags or 1000 kg jumbo bags. Transport by truck, rail, or sea in clean, dry containers. Store under cover, away from moisture, direct sunlight, heat, and contamination. Avoid hooking or tearing packaging. |
| Storage | Store Sinopec Zhenhai HDPE ZH6098 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags sealed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and sharp objects. Maintain good housekeeping; no smoking. Recommended ambient storage temperature, protect from weather. Store in accordance with local regulations and manufacturer's instructions. |
| Shelf Life | Sinopec Zhenhai HDPE ZH6098 typically has a 24-month shelf life from production when stored cool, dry, ventilated, sealed, and away from sunlight. |
Sinopec Zhenhai HDPE ZH6098 is processed as a high molecular weight PE100-class pipe resin with a nominal melt flow rate of 0.23 g/10 min at 190 °C / 5 kg (ISO 1133-1, condition T) and a density of 0.949 g/cm³ (ISO 1183-1). In potable water main production, the industry compliance route is ISO 4427-2 for PE100 pipes and ISO 12162 for the MRS 10.0 MPa classification, with GB/T 13663.2 applied in Chinese domestic potable water certification. Batch release hydrostatic testing uses ISO 1167-1 specimens cut from the finished pipe, requiring no ductile or brittle failure at 20 °C, 12.4 MPa, 100 h and at 80 °C, 5.4 MPa, 165 h for water-service formulations. The formulation addition ratio for UV-stable black pipe is 5.8–6.2 wt% of 40% carbon black masterbatch added to natural ZH6098 pellets, yielding 2.3–2.5 mass% carbon black in the final pipe wall; loadings below 2.0 mass% fail long-term UV integrity and loadings above 2.5 mass% are rejected because pigment agglomerates reduce slow crack growth resistance by acting as stress concentrators. The downstream production process uses a grooved-barrel single-screw extruder with L/D 33:1 to 36:1, barrier screw geometry, and a screened melt stream at 210–235 °C; the melt temperature must remain below 240 °C because oxidative chain scission accelerates above that threshold and shifts the molecular-weight distribution toward lower melt strength. Vacuum calibration follows with tank water at 16–22 °C, and multi-zone spray cooling is sequenced from 40 °C to 15 °C to control frozen-in residual stress in thick walls. Terminal products include SDR 11 and SDR 17 PE100 mains from DN 20 to DN 1200, coiled service lines up to DN 63, and electrofusion fittings moulded from the same stabilised base resin.
Gas distribution networks impose rapid crack propagation and slow crack growth requirements that are not part of the standard potable water acceptance path. The governing conformity framework is ISO 4437 for PE100 gas pipes, supported by ISO 13477 for rapid crack propagation at 0 °C and ISO 13479 for notched pipe slow crack growth; in China, GB 15558.1 adds mandatory batch release criteria. The formulation addition ratio depends on the pipe colour pathway. Yellow gas pipe produced from natural ZH6098 typically uses 2.0–4.0 wt% yellow pigmented masterbatch; black gas pipe with yellow identification stripes uses 2.0–2.5 mass% carbon black in the wall and a co-extruded yellow stripe layer compounded at 3–5 wt% pigment masterbatch. The downstream extrusion process for gas pipe leverages the same high-torque single-screw platform as water pipe, but barrel set-points are reduced to 200–220 °C and cooling gradients are extended to reduce residual stress, which directly affects RCP resistance. To preserve slow crack growth performance, reclaim addition is limited to clean in-house pipe regrind at or below 10 wt%, and any external recycled material is excluded under ISO 4437 quality plans. Terminal product types include DN 20–630 gas mains, coiled service pipes, and directional drilling strings where fusion joining under ISO 21307 is used.
| Compliance parameter | Standard/Method | Acceptance window |
|---|---|---|
| Carbon black content in black PE100 pipe | ISO 6964 | 2.0–2.5 mass% |
| Hydrostatic strength at 20 °C, 100 h | ISO 1167-1 | 12.4 MPa no failure |
| Hydrostatic strength at 80 °C, 165 h | ISO 1167-1 | 5.4 MPa no failure |
| Oxidative induction time at 200 °C | ISO 11357-6 | ≥20 min |
Slurry transport in mineral processing rejects steel on sites where acidic mill water, chloride-bearing process water, or high-solids tailings accelerate erosion-corrosion. The applicable compliance standard for industrial HDPE piping is ISO 15494, with PE100 material classification under ISO 12162; many mining specifications additionally require the pipe compound to meet the PE4710/PE100 equivalence under ASTM D3350 and the fusion-joint qualification procedure of ISO 21307. The formulation addition ratio for surface tailings lines exposed to UV is 5.8–6.2 wt% of 40% carbon black masterbatch, producing 2.3–2.5 mass% carbon black; buried slurry piping may be run in natural unpigmented PE100 compound with 0 wt% carbon black only where UV exposure is absent. Production of thick-wall slurry pipe reaches wall thicknesses of 50–80 mm on extrusion lines equipped with internal air or internal water cooling; without internal cooling, gravitationally driven melt sag creates wall-thickness eccentricity greater than ±10%, and the resulting thin spots fail hydrostatic revalidation. Melt temperatures in thick-wall production are capped near 215 °C to prevent sag and to protect the high molecular weight tail; output rates drop to 150–400 kg/h depending on diameter, which is below thin-wall water pipe throughput. Terminal products include tailings transport lines, dredge discharge pipes, and heap-leach process water distribution headers.
Ground-source heat pump loop production with ZH6098 exploits the same slow crack growth resistance that qualifies PE100 for pressure service, but the product geometry and joining requirements are different. The pipe material is typically specified to ISO 4427 for PE100 and dimensionally to ASTM F714, while closed-loop borehole installations may follow local geotechnical codes; published data for ZH6098 in this specific configuration is limited, so batch qualification should be based on ISO 1167-1 hydrostatic testing rather than extrapolation from water-mains performance. The formulation addition ratio for buried closed-loop pipes is 0 wt% carbon black when the pipe is installed below frost depth and not exposed to UV during storage; for surface pond loops and header manifolds exposed to sunlight, 5.8–6.2 wt% of 40% carbon black masterbatch is used. Downstream production involves extrusion of small-DN pipe from DN 20 to DN 63 with rapid vacuum sizing and coil winding; coil memory must be controlled by maintaining winding diameter above 20× pipe diameter to prevent kinking during uncoiling in borehole insertion. Terminal product types include geothermal U-bend loops, pond loops, and manifold headers joined by socket fusion to ISO 21307.
Marine intake and outfall lines specified for long-run submerged service are produced only where submerged pipelines must tolerate wave-induced cyclic loading, saltwater, and long lay lengths. Compliance is commonly anchored to ISO 4427 for material and AWWA C906 or ASTM F714 for dimension and hydrostatic design in water service; subsea joints are butt-fused to ISO 21307 with weld bead removal and independent NDT. The formulation addition ratio for black marine line pipe is 5.8–6.2 wt% of 40% carbon black masterbatch to reach 2.3–2.5 mass% carbon black, because surface exposure during staging and tow-out requires UV protection; no flame-retardant or mineral filler is added, as any increase in density beyond the product specification would reduce buoyancy control in marine installation. Wall-thickness control is the critical production bottleneck: for wall thicknesses above 60 mm, the residual heat in the melt core cannot be extracted quickly enough through the outer pipe surface without internal cooling. Production lines use internal air cooling or water mist cooling inside the pipe bore to balance shrink rates; otherwise, a differential temperature of 15–25 °C between the inner and outer surfaces creates residual stress that can cause centreline voiding or poor fusion weld alignment. Output is deliberately slowed to maintain a melt temperature below 230 °C and to hold outer wall thickness variation within ±8%. Terminal product types include desalination plant intake and discharge lines, power plant cooling-water outfalls, and temporary effluent bypass pipelines.
In buried electrical and fibre-optic infrastructure, cable protection ducts derived from ZH6098 represent a lower-pressure application in which the high molecular weight PE100 rheology is used more for crush resistance and slow crack growth than for hydrostatic design. The applicable conformity route is EN 61386-24 for buried underground conduit systems and ASTM F2160 for solid-wall HDPE conduit; electrical installation codes may require additional flame-spread evaluation because HDPE is not inherently flame-retardant. The formulation addition ratio is 5.8–6.2 wt% of 40% carbon black masterbatch for above-ground and UV-exposed ducts, yielding 2.3–2.5 mass% carbon black; indoor conduits may be unpigmented natural or tinted with non-conductive masterbatch below 2.0 wt%. Downstream production runs on either smooth solid-wall pipe lines or corrugated pipe extruders with vacuum corrugators; for corrugated duct, the melt is formed continuously against moving mould blocks at line speeds up to 25 m/min, and wall thickness is controlled at the corrugation valley rather than the peak. Terminal product types include power cable conduits, telecom duct bundles, and fibre-optic protection pipes for direct burial.
Competitive Sinopec Zhenhai HDPE ZH6098 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Zhenhai HDPE ZH6098 is an injection moulding grade of high-density polyethylene produced by Sinopec Zhenhai Refining & Chemical Company. In the producer’s commercial nomenclature, the ZH prefix identifies the Zhenhai manufacturing site, and the numeric suffix 6098 differentiates the grade within the high-flow HDPE injection portfolio. Published technical data sheets list a nominal melt flow index of 9.8 g/10 min at 190 °C/2.16 kg under ISO 1133-1 and a nominal density of 0.960 g/cm³ under ISO 1183-1. These values place ZH6098 in the high-flow segment of HDPE injection moulding resins, where cavity fill is rapid but melt strength is proportionally reduced.
Lot-specific certificates of analysis control the full specification. The values stated in technical data sheets are typical published values, not universal acceptance criteria. Where a final part is covered by regulatory requirements, the certificate of analysis, safety data sheet, and finished-article test reports are the controlling documents.
High-flow HDPE is strongly shear-thinning. On a capillary rheometer at 190 °C, the apparent viscosity of a 9.8 g/10 min HDPE at 1,000 s⁻¹ is typically below 200 Pa·s, while a 0.4 g/10 min PE100 pipe grade remains higher by more than an order of magnitude. The practical result is lower injection pressure in thin-wall gates, but also reduced melt elasticity and an increased tendency to drool from open nozzles. The melt temperature range recommended in conversion trials is 190–230 °C. Below 180 °C, unmelted particles and flow lines appear in thick sections; above 240 °C, oxidative chain scission reduces notched impact strength. Mould temperature is normally 30–70 °C, with 35–45 °C used for fast cycling of parts below 2.0 mm wall thickness.
The shear rate at the gate during thin-wall moulding can exceed 10,000 s⁻¹. At such shear rates, HDPE melt enters a pseudo-plastic regime in which pressure drop becomes less than proportional to flow rate. This permits small gate diameters with ZH6098. However, excessive shear heating at gates smaller than 0.8 mm can cause gate blush, stringing, and local molecular degradation.
Differential scanning calorimetry under ISO 11357-3 shows a melting peak near 130–135 °C for high-density polyethylene; the exact onset and peak depend on thermal history and additive package. The density of 0.960 g/cm³ corresponds to a crystallinity level of approximately 65–75 % when calculated from a two-phase density model. This crystallinity contributes to flexural modulus and surface hardness but reduces low-temperature impact and environmental stress-crack resistance relative to medium-density and linear-low-density grades.
Published technical data sheets for Sinopec Zhenhai HDPE ZH6098 report the following typical property ranges. These ranges are not specification limits.
| Property | Test standard | Typical published range |
|---|---|---|
| Melt flow index, 190 °C/2.16 kg | ISO 1133-1 | 9.0–10.0 g/10 min |
| Density | ISO 1183-1 | 0.959–0.961 g/cm³ |
| Tensile yield stress | ISO 527-2 | 26–28 MPa |
| Nominal tensile strain at break | ISO 527-2 | >500 % |
| Flexural modulus | ISO 178 | 1,100–1,300 MPa |
| Notched Izod impact strength, 23 °C | ISO 180/A | 4–6 kJ/m² |
| Vicat softening temperature, A50 | ISO 306/A50 | 125–129 °C |
| Mould shrinkage | ISO 294-4 | 1.5–2.5 % |
For comparison with lower-flow HDPE injection grades, the melt flow index is the primary selector. Medium-flow HDPE injection grades commonly exhibit 3–5 g/10 min, whereas ZH6098 approaches 9.8 g/10 min. In production trials on comparable high-flow HDPE, the change can reduce injection pressure by approximately 15–30 % in similar part geometries, but the exact reduction depends on wall thickness, gate dimensions, and mould temperature. Because melt strength is reduced, the melt cushion should be controlled within 3–6 mm on reciprocating-screw machines to avoid nozzle drool and cushion depletion.
Tooling configuration for ZH6098 must account for its low melt viscosity. In cold-runner systems, round runner diameters of 6–10 mm are typical. Submarine gates below 0.8 mm increase shear heating and may cause gate blush or stringing. For open containers, direct or edge gates with land lengths of 0.5–1.5 mm reduce jetting. Hot-runner systems with valve gates are common in high-cavitation closures; manifold temperatures should be held within 5–10 °C above the nozzle melt temperature to prevent cold slugs without promoting degradation.
In thin-wall containers with wall thickness between 1.2 mm and 2.5 mm, the low melt viscosity allows filling at moderate injection velocities of 80–150 mm/s; however, the resulting orientation and cooling-rate gradients produce non-uniform shrinkage. Parts moulded from ZH6098 require positive ejection features and adequate draft angles, typically 0.5–1.0° on core surfaces and 1.0–2.0° on textured cavity surfaces. Ejector pins must be positioned over ribs and gussets. Otherwise high ejection force at short cooling times produces sink marks or white stress-whitening around the pin faces.
On reciprocating-screw injection moulding machines of 1,200–4,000 kN clamp force and 40–60 mm screw diameter, ZH6098 is processed with a general-purpose polyolefin screw of 20:1–25:1 L/D and compression ratio 2.5:1–3.5:1. Back pressure is set in the range 0.5–1.5 MPa to homogenise the melt without excessive temperature rise. Screw speed is typically 50–150 rpm. Shot size should be kept between 30 % and 70 % of barrel capacity to limit residence time.
Clamp force requirements can be approximated from cavity pressure. In thin-wall containers moulded from high-flow HDPE, peak cavity pressure is typically 30–60 MPa. For a projected part area of 1,000 cm², this corresponds to 3.0–6.0 kN/cm²; therefore a 4,000 kN machine is suited to projected areas around 700–1,300 cm². Flash-free sealing requires flat mould faces and sufficient clamp force, because the high flow of ZH6098 makes flash more likely under inadequate clamping.
Common production failure modes recorded during start-up of ZH6098 moulds include flash at the parting line when clamp force is insufficient, burn marks at rib ends when venting is inadequate, and sink marks above thick bosses when holding pressure is not profiled. These failure modes are not unique to ZH6098 but are amplified by high flow and fast solidification. Vent depths at the parting line for HDPE should be 0.02–0.03 mm; deeper vents may allow flash.
Published injection-moulding studies on high-flow HDPE report that increasing melt temperature from 200 °C to 220 °C improves weld-line tensile strength by 8–15 % when test specimens are cut from moulded plaques under ISO 527-2. The improvement is not linear and should be confirmed on the actual part. Venting of weld-line areas is necessary to prevent trapped air from weakening the bond.
The principal differences between ZH6098 and other HDPE grades emerge from molecular mass distribution and melt flow index. Pipe-grade HDPE, including PE100 compounds, has a melt flow index below 0.5 g/10 min under ISO 1133-1 and is formulated for long-term hydrostatic strength evaluated under ISO 9080. ZH6098 cannot be substituted into pressure piping because the high melt flow correlates with lower long-term creep resistance and lower slow crack growth resistance. Blow-moulding HDPE grades typically maintain a melt flow index of 0.3–1.0 g/10 min or are high-molecular-weight grades with substantial shear-thinning; their parison sag resistance is not present in ZH6098. Film-grade HDPE with melt flow indices below 1.0 g/10 min provides greater dart impact and tear strength in film form. Relative to these extrusion and blow-moulding grades, ZH6098 is optimised for injection moulding productivity, not for melt strength or long-term hydrostatic durability.
Table 2 summarises typical class-level differences. The ranges are representative of commercial HDPE types and are not direct producer specifications for every grade in the class.
| Grade class | MFR under ISO 1133-1 | Density under ISO 1183-1 | Representative performance limitation |
|---|---|---|---|
| ZH6098 high-flow injection | 9.0–10.0 g/10 min | 0.959–0.961 g/cm³ | reduced melt strength; moderate impact |
| PE100 pipe | 0.2–0.5 g/10 min | 0.950–0.960 g/cm³ | long-term hydrostatic strength required |
| HDPE blow moulding | 0.3–1.0 g/10 min | 0.945–0.955 g/cm³ | parison sag resistance required |
| HDPE film | 0.2–1.0 g/10 min | 0.945–0.955 g/cm³ | dart impact and tear strength required |
The comparison is not purely compositional. Pipe grades are often bimodal and contain carbon black or stabiliser packages, whereas ZH6098 is designed for high-speed injection moulding with minimal melt strength. Replacing a pipe grade with ZH6098 in pressure service would violate the long-term hydrostatic design basis of ISO 9080. Conversely, using a pipe grade in thin-wall injection would require melt temperatures approaching or exceeding 260 °C and would still produce short shots and high clamp force because the MFR is lower by roughly 20-fold.
The grade is used in rigid injection-moulded articles where high flow, moderate stiffness, and adequate room-temperature impact strength are required. Typical application categories include stackable crates, small-to-medium storage containers, buckets, caps and closures with tamper-evident bands, household articles, and industrial pails for non-hazardous contents. In caps and closures, the high melt flow permits filling of small gates and long flow paths; however, closure sealing performance is determined by the moulded dimensions and creep resistance of the material, not by MFR alone. Top-load compression of containers can be evaluated under ISO 12048, and drop-test performance is evaluated under the relevant distribution-test standard selected by the end user.
Regrind of ZH6098 from sprues and reject parts can be re-introduced at 20–40 wt% without significant loss of flow, provided it is dry and free of contamination. Higher regrind fractions reduce impact strength and increase variability in melt flow index. Closed-loop recycling should therefore be validated by measuring MFR after repeated extrusion cycles.
Outdoor grades need stabilisation. Unpigmented or non-UV-stabilised parts exposed to solar radiation develop surface microcracks and embrittlement. Carbon black content of 2.0–2.5 wt% is common for weatherable HDPE parts, with weathering assessment under ISO 4892-2 or ISO 4892-3. Food-contact suitability must be established on the finished article under GB 4806.6-2016 or EU Regulation 10/2011, because additives and colourants in the final compound influence migration. Pre-drying is not usually required for HDPE, but if the resin is stored at relative humidity above 60 %, surface moisture should be removed by drying at 80 °C for 2–4 h using a desiccant dryer to prevent surface splay.
The material is not intended for continuous hot-water pressure pipe service, and published data for ZH6098 in such configurations is limited. Processing above 250 °C should be avoided because oxidative degradation can cause discoloration, odour, and loss of impact strength. Environmental stress-crack resistance is not normally guaranteed for ZH6098 and is not equivalent to pipe-grade HDPE. For aggressive liquid packaging or detergent containers, ESCR should be tested under ISO 22088-3 or ISO 16770. For low-temperature impact applications below −20 °C, Charpy notched impact under ISO 179-1/1eA or tensile impact under ISO 8256 is required, because the room-temperature notched Izod value alone does not guarantee ductile behaviour at freezer temperatures.