| HS Code | 635788 |
| Density | 0.955 g/cm³ |
| Meltflowrate | 0.20 g/10 min (190°C/2.16 kg) |
| Tensilestrengthatyield | 26 MPa |
| Elongationatbreak | ≥500% |
| Flexuralmodulus | 1100 MPa |
| Vicatsofteningtemperature | 125 °C |
| Brittlenesstemperature | ≤-70 °C |
| Hardnessshored | 65 |
| Notchedizodimpactstrength | 20 kJ/m² |
| Environmentalstresscrackingresistance | >1000 h |
| Waterabsorption | <0.01% |
| Thermalconductivity | 0.44 W/m·K |
| Dielectricconstant | 2.3 |
| Volumeresistivity | >10^16 Ω·cm |
As an accredited Sinopec Zhenhai HDPE ZH5502HP factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Zhenhai HDPE ZH5502HP is packaged in 25 kg PP woven bags, suitable for industrial handling and bulk transport. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Sinopec Zhenhai HDPE ZH5502HP, approximately 17–18 MT, typically packed in 25kg bags per container. |
| Shipping | Sinopec Zhenhai HDPE ZH5502HP is shipped as non-hazardous polymer pellets, typically in 25 kg bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped in FCL/LCL containers. Transport by sea or land; keep dry and avoid direct sunlight, excessive heat, and contamination. No dangerous goods classification applies. |
| Storage | Store Sinopec Zhenhai HDPE ZH5502HP under roof in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, and moisture. Keep original packaging sealed and palletized; prevent contamination by dust, oils, chemicals, or moisture. Avoid excessive stacking pressure and sharp objects. Maintain good housekeeping; clean spills promptly, as pellets can create slipping hazards. Observe normal fire precautions. |
| Shelf Life | Shelf life is 24 months when stored in a cool, dry, ventilated place, away from direct sunlight and ignition sources. |
Sinopec Zhenhai HDPE ZH5502HP is processed in thin-wall dairy packaging cells at a nominal melt flow rate of 5.0–6.0 g/10 min when measured under ISO 1133-1:2022 at 190 °C with a 2.16 kg load. The grade enters 128-cavity stack moulds for yogurt cups, dairy dessert cups, and ice cream tubs with wall stock of 0.45–0.60 mm and flow lengths of 110–140 mm. Barrel temperature profiling is set from 190 °C at the feed section to 225 °C at the nozzle, while hot runner valve gates are held at 260–280 °C to avoid premature skin freeze. Injection pressure typically falls between 80 and 100 MPa on this tooling class, with clamp force between 300 and 450 tonnes depending on projected area and cavity count. Mould coolant temperature is controlled between 18 and 30 °C; excursions above 32 °C increase sidewall ovality beyond 0.8 mm after 24 h. Mould shrinkage is recorded at 24 h after demoulding under ISO 294-4; values are 1.4–1.8% in the flow direction and 1.2–1.6% in the transverse direction. Differential shrinkage above 0.3 percentage points between axes produces rim ovality that can reduce stacking fit in dairy cup filling lines. The finished cup must comply with European food-contact legislation when certified lots are used: overall migration under Regulation (EU) 10/2011 Annex III and Annex V is assessed with simulant A and simulant D2, and the limit is <10 mg/dm². For North America, compliance is demonstrated under FDA 21 CFR 177.1520(c) clause 3.1a or 3.1b, depending on final article density and extractable fraction. For the domestic Chinese market, GB 4806.7-2016 total migration and potassium permanganate consumption requirements are applied. In-mould label grade polypropylene requires a melt stock temperature of at least 225 °C for fibre tear adhesion; below this value label edge lift appears within 48 h of filling. Regrind from trim and rejected cups is metered into virgin material at 10–15 wt%; higher regrind fractions above 20 wt% can increase gel speck density and odour because the stabiliser package is designed for low residence time. Screw retraction after plastication is limited to 2–4 mm of suck-back, not above 5 mm, because excessive decompression pulls air into the melt cushion and produces gate stringing on valve-gated hot runners. Nozzle contact force is kept between 1.5 and 2.0 kN. Mill certificate values for lot density, melt flow rate, and tensile yield should be used for process capability indexing.
Beverage closures from ZH5502HP are moulded at cap body weights of 1.8–3.2 g with tamper-evident band hinge thickness between 0.25 and 0.35 mm. Gate freeze time is the primary throughput constraint in 96-cavity and 192-cavity valve-gated hot runner tools. The gate orifice diameter is specified at 0.6–0.9 mm; a smaller gate generates high shear heating and acetaldehyde-like off-notes in some additive packages, while a larger gate extends hold-pressure time and increases cycle time by 0.8–1.5 s. Plasticating units of 35–45 mm screw diameter and L/D ratio 22:1 to 24:1 are used on clamp units from 150 to 250 tonnes. Cavity temperature for carbonated soft drink closures is held at 10–15 °C to control knurl ovality and bridge flatness, while hot-fill aseptic closure tools operate at 20–25 °C to reduce moulded-in stress. Melt temperature is set between 230 and 240 °C; above 245 °C the stabiliser can generate volatile degradation products that fail sensory thresholds in mineral water applications. High-speed injection of 100–150 mm/s and stepped hold pressures of 45/35/20 MPa are typical. Condensation-induced splay occurs when cavity surface temperature falls below the dew point of the moulding hall; dehumidification to 40–50% RH or closed-loop mould temperature control is required. The closure must pass venting performance and stress-crack resistance tests: ESCR is monitored under ASTM D1693 condition B in 100% Igepal CO-630 at 50 °C, with F50 values in the 30–60 h range for the high-flow HDPE closure class, but exact acceptance is lot-specific. Notched impact strength at 23 °C under ISO 179-1:2010/1eA is maintained above 4 kJ/m²; at -20 °C the Charpy value is typically 15–25% lower. Closure thread profiles are held to minimum tolerances of ±0.05 mm and verified by optical scanners at 100% inspection cells.
| Parameter | Reference standard or regulation | Typical acceptance window |
|---|---|---|
| Melt flow rate at 190 °C/2.16 kg | ISO 1133-1:2022 | 5.0–6.0 g/10 min |
| Density | ISO 1183-1:2019 | 0.953–0.957 g/cm³ |
| Overall migration in beverage simulant | Regulation (EU) 10/2011 | <10 mg/dm² |
| US food-contact status | FDA 21 CFR 177.1520(c) | End-use condition E–G |
| China food-contact migration | GB 4806.7-2016 | <10 mg/dm² |
| Stress-crack resistance | ASTM D1693 condition B | F50 ≥ lot-specific minimum |
Pressure drops in valve-gated hot runners above 30 MPa reduce gate icing but can damage the bridge fibres in thin tamper-evident slits. The part design therefore balances gate orifice diameter, cavity count, and nozzle bush temperature. The finished closures are suitable for still water, carbonated soft drink, and aseptic dairy bottles, provided the specific additive package is approved for the target food type.
Returnable transit packaging moulded from ZH5502HP includes stackable crates, euro containers, and lightweight pallet feet with gate-to-edge distances above 450 mm. The principal process conflict is that the 5.0–6.0 g/10 min melt flow rate enables filling long flow paths at moderate pressure, but the same flow class produces higher orientation gradients along the melt front. On 800–1200 tonne injection moulding machines with shot weights above 1 kg, flatness deviation on a 600 mm × 400 mm crate base exceeds 3 mm when packing pressure drops below 35 MPa before gate freeze. A stepped hold profile of 70 MPa for 2 s, 45 MPa for 5 s, and 25 MPa for 2 s is used to compensate volumetric shrinkage without overpacking the gate area. Melt temperature between 200 and 215 °C and cooling water at 12–18 °C in drilled circuits are typical. Gate design for large-area crates avoids pinpoint gates; fan or tab gates of 1.5–2.0 mm thickness are preferred to prevent jetting at flow-length-to-thickness ratios above 200:1. The mould filling pattern is validated by short-shot series and ultrasonic wall thickness mapping; weld lines around handle openings are moved by changing gate location, not by increasing temperature alone. Impact resistance at cold storage temperature is checked under ISO 179-1:2010/1eA at -20 °C. Elevated zinc stearate or stearic acid residues above 0.1 wt% can plate out on vent surfaces after prolonged cycles, causing gas burn at handle ends; periodic vent cleaning at intervals of 5,000–10,000 cycles is standard on production lines. Regrind usage is limited to 20 wt% because repeated shear history lowers low-temperature impact strength by 10–15% per pass and increases melt viscosity variability. Chemical exposure in logistics chains includes diluted organic acids from fruit and vegetable juice, alkaline cleaning solutions at pH 9–11, and occasional fuel residues. ESCR evaluation under ASTM D1693 condition B is supplemented with in-house exposed-strip tests under constant strain. Flammability classification under UL 94 HB at 3.0 mm is accepted for warehousing because no flame-retardant additives are used. Published data for ZH5502HP in crate geometries with high regrind content is limited; production plants typically validate a three-lot capability study before start of a new tool. Finished crates and pallet elements must comply with the general safety requirements of the EU Packaging and Packaging Waste Directive 94/62/EC, but the directive does not prescribe material-specific concentration limits for polyethylene.
Cosmetic overcaps and closure shells made from ZH5502HP are produced in 32-cavity to 64-cavity tools with polished or photo-etched cavity surfaces. The application is more sensitive to volatile carbonyl compounds than food-contact packaging because fragranced personal care products can mask or amplify off-odours. Melt temperature is capped at 235 °C, and residence time is limited to 6 min because polyolefin thermal degradation products, particularly hexanal, nonanal, and heptanal, rise sharply above that threshold in high-flow HDPE without additional antioxidant boosting. A masterbatch with acid scavenger and secondary antioxidant is added at 0.5–1.0 wt% only when lot certificates show high residual acidity or peroxide index; unnecessary additive loading beyond 1.5 wt% reduces stress-crack resistance. Hot runner systems are purged with low-viscosity HDPE after colour changes or after running acetal and PET in the same cell; purge volume of 1.5–2.0 times barrel capacity is used. Screw speed is held below 120 rpm on 40 mm plasticating units to minimise shear heating. Mould temperature is set at 15–25 °C for gloss control; matte photo-etch surfaces require the upper end of this range to replicate texture depth above 25 µm. The finished cap dimensions are checked against thread profiles using vision systems and plug gauges; mould shrinkage of 1.5–2.0% under ISO 294-4 affects screw thread pitch and the snap-fit undercut diameter. If the overcap is intended for child-resistant packaging, the complete closure system must pass ISO 8317:2015 sequential opening tests, not just the HDPE shell. Cosmetic packaging compliance is governed by Regulation (EC) 1223/2009 for safety of cosmetic products, but the plastic article itself is not covered by a single global migration standard; suppliers often use EU 10/2011 test methods as a proxy for skin-contact extractables, supplemented by GB 4806.7-2016 for export to China. Dimensional stability after 48 h is assessed by conditioning at 23 °C and 50% RH, with diameter changes above 0.4% indicating excessive post-mould crystallisation due to rapid cooling. The end product range includes serum bottle overcaps, fragrance pump ferrules, and cream jar outer shells.
Household totes, under-bed storage bins, and modular storage containers in ZH5502HP are moulded with wall thickness between 1.5 and 3.0 mm and stack heights up to 600 mm. Stacking load tests are carried out at 23 °C and 40 °C; a column of three loaded containers with 10 kg distributed load must not show creep deflection above 5 mm after 24 h. The resin’s tensile modulus under ISO 527-2:2012 is typically below 1,200 MPa, so vertical rib geometry is thickened to 1.8–2.5 mm at the base rather than increasing wall stock uniformly. Mould cooling near the base is designed with bubblers and conformal channels to extract heat from rib intersections; sink marks deeper than 0.05 mm are visible on textured surfaces. Integral living hinges are a known weak point in high-flow HDPE. Repeated flexing beyond 10,000 cycles at 23 °C leads to stress whitening and crack initiation; a loose snap-lid or discrete steel hinge is preferred over an integral polypropylene-style hinge because polyethylene does not self-hinge with the same fibrillar morphology as polypropylene. The process uses melt temperature of 210–230 °C, injection pressure of 70–90 MPa, and screw back pressure of 0.5–1.0 MPa. Mould temperature control between 20 and 35 °C is adjusted upward for textured surfaces to reduce flow marks but must not exceed 40 °C, since cooling time increases nonlinearly. Notched Izod impact under ISO 180/A at 23 °C is maintained above 4 kJ/m² for incoming resin. Detergent contact and dishwasher exposure impose the main environmental stress-cracking risk. Hot water above 70 °C under detergent load can cause distortion and stress whitening; repeated exposure to alkaline solutions at pH 10–12 combined with external stress may initiate ESCR. The resin should be tested under ASTM D1693 condition B; values below 20 h for the finished article are considered unacceptable for export to high-humidity climates. Colors are compounded with high-density polyethylene carrier masterbatch at 2–4 wt%; pigment loading above 5 wt% can reduce Charpy impact strength by 15–20% and should be revalidated per color. The articles are not intended for microwave reheating above 100 °C or for oven use; HDPE’s deflection temperature under 0.455 MPa is in the 70–85 °C range under ISO 75-2. Published data for this specific geometry is limited, and stack-load deflection should be validated on a prototype tool before full production.
At 0.8 mm wall thickness in 100 mL graduated specimen containers, ZH5502HP is processed in cleanroom injection moulding cells with 90–110 tonne clamp force and 32-cavity cold runner tools. The tool is cleaned and neutralised to remove residual processing aids from previous resins because the finished container may contact diagnostic fluids or pharmaceutical samples. Melt temperature is held at 215–230 °C and hold pressure at 40–50 MPa; the cold runner size is balanced to limit cavity-to-cavity weight variation below 0.5%. Low-temperature impact resistance is evaluated by drop tests from 1.0 m at -20 °C; a notched Izod value above 3 kJ/m² under ISO 180/A at 23 °C is used as incoming resin control. Sterilisation dose is controlled at 25 kGy gamma or electron beam; dose mapping must cover the thread root and base corners because local under-dose can leave bioburden. Post-sterilisation dimensional change is measured by coordinate measuring machine and is accepted within 0.5% of the pre-sterilisation diameter; beyond this the cap seal interference is compromised. Cytotoxicity is tested under ISO 10993-5:2009 and skin irritation under ISO 10993-10:2010 when patient-contact claims exist. The resin must meet pharmacopoeial requirements for polyolefins under Ph. Eur. 3.1.3 and extractables screening under USP <661.1> and USP <661.2>. Particulate contamination from pellet dust is reduced by closed-loop conveying and dedusting to below 0.5 wt% fines. Pre-drying at 80 °C for 2 h is used when storage humidity exceeds 60%; HDPE is not hygroscopic but surface condensation on pellets causes splay. Additive levels are not modified without requalification because slip agents and antioxidants migrate into aqueous media and affect leachables profiles. Published data for gamma-sterilised ZH5502HP in this container geometry is limited; dose mapping, post-sterilisation dimensional change, and leachables should be validated per lot before release to regulated markets.
Competitive Sinopec Zhenhai HDPE ZH5502HP prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Zhenhai HDPE ZH5502HP is a high-density polyethylene resin produced at the Sinopec Zhenhai Refining & Chemical complex. The grade designation is a commercial product identifier, not an ISO material classification, and must be read with the mill certificate or technical datasheet before any process qualification. The material is supplied in pellet form for extrusion, blow molding, and selected injection molding applications where high melt strength and environmental stress crack resistance are relevant. Density is verified according to ISO 1183-1:2019, melt mass-flow rate according to ISO 1133-1:2022 at 190 °C/2.16 kg and 190 °C/5.0 kg, tensile properties according to ISO 527-2:2012, and notched Charpy impact according to ISO 179-1:2023. Because lot-specific values for ZH5502HP vary with the production campaign, no single density or melt flow figure should be treated as fixed without reference to the certificate of analysis.
The suffix "HP" is a manufacturer-controlled performance modifier and does not replace the formal designation system for polyethylene under ISO 1873-1:1993 or the corresponding Chinese national system. In buyer-side quality practice, the useful lot-certificate parameters are not limited to a single MFR point. The melt flow rate ratio, calculated from ISO 1133-1:2022 as MFR under 21.6 kg divided by MFR under 2.16 kg, provides a practical indication of molecular weight distribution. High-molecular-weight HDPE grades used for blow molding and thick-wall extrusion commonly exhibit melt flow ratios between 15 and 35. A shift of more than 10% between lots can indicate a change in molecular architecture, with consequences for die swell, parison sag, melt fracture, and slow crack growth. The certificate of analysis should also report density, tensile yield stress, elongation at break, and notched Charpy impact. A lot release based only on nominal density and MFR is insufficient for load-bearing or long-lifetime components.
Rheological screening for lot acceptance uses capillary or rotational rheometry because the melt flow rate ratio alone does not resolve shear-thinning behavior. Capillary rheometry at 190 °C over shear rates from 10 s⁻¹ to 1000 s⁻¹ can reveal the degree of shear thinning. Broad-molecular-weight HDPE typically shows a power-law index between 0.45 and 0.60 in the processing shear-rate region, while narrow-molecular-weight HDPE may show an index closer to 0.70. These differences affect die swell and the onset of melt fracture. High-molecular-weight HDPE with a low melt flow rate and broad molecular weight distribution can show die swell above 50% at shear rates above 500 s⁻¹. Narrow-molecular-weight injection grades commonly show die swell below 20% under the same conditions. These values are class-level data and must be requalified on the ZH5502HP lot rather than assumed from generic literature.
Accumulator-head blow molding imposes long melt residence times because the melt accumulates under low shear before being forced through the die. For high-molecular-weight HDPE, oxidation induction time measured by ISO 11357-6:2018 at 210 °C should remain above 20 min for parts intended for extended outdoor or hot-fluid service. A drop in oxidation induction time below 10 min is a processing warning and may indicate stabilizer consumption during compounding or melt residence above 220 °C. On accumulator machines, melt residence time should be held below 60 min at melt temperatures below 210 °C. If the molding cycle is interrupted, the accumulator should be purged rather than held at temperature. The first mechanical indicator of thermal degradation is usually a reduction in elongation at break under ISO 527-2:2012. A loss of more than 20% from virgin lot tensile data after the addition of regrind suggests that the recycle fraction is too high or thermally damaged. In extrusion blow molding, regrind addition is normally restricted to 15–30% by mass with clean internal scrap, but this bound must be validated for ZH5502HP through a specific process capability study.
On general-purpose single-screw extruders with 24:1 to 30:1 L/D and compression ratios from 2.5:1 to 3.5:1, processing is generally compatible with HDPE of this molecular weight band. The feed throat should remain below 40 °C to prevent pellet bridging. Barrel zone settings between 170 °C and 210 °C are commonly used for high-molecular-weight HDPE. Melt temperature measured at the die should not exceed 230 °C for extended periods because thermo-oxidative chain scission shifts the molecular weight distribution and reduces melt strength. If the line uses a screen pack, a pressure rise above 25–30 MPa across a 20/40/60/100 mesh pack commonly indicates gel accumulation or insufficient pre-filtration. Published data for this specific configuration is limited; these values are class-level HDPE extrusion parameters and should be verified on the ZH5502HP lot certificate and machine capability study.
Mechanical property requirements are typically governed by the end-product standard rather than the resin catalogue value. For rigid industrial packaging and thick-wall components, tensile yield stress is tested at 23 °C under ISO 527-2:2012. Class-level HDPE results commonly fall between 22 MPa and 32 MPa, but the ZH5502HP value must be read from the certificate of analysis. Elongation at break above 600% is common for HDPE at 23 °C. Notched Charpy impact under ISO 179-1:2023 is a sharper discriminator for molecular architecture. High-molecular-weight HDPE grades can show notched Charpy values from 8 kJ/m² to above 30 kJ/m² at 23 °C. A lot with density at the upper 0.960 g/cm³ limit may show lower impact resistance than a lot at 0.948 g/cm³, even if both meet the commercial specification. If impact resistance at −30 °C is required, low-temperature notched Charpy results should be requested; room-temperature data do not substitute for low-temperature performance.
Slow crack growth is the critical failure mode in pressurized water and chlorinated water service. HDPE piping and industrial ducting require either a validated minimum required strength classification under ISO 9080:2012 and ISO 12162:2011, or long-term hydrostatic test data on the finished product. A resin datasheet that lists only density and MFR is insufficient for this service. For polyethylene with high environmental stress crack resistance, screening methods include the notched constant ligament stress test under ISO 16770:2004 or the bent strip test under ASTM D1693-15b. If ZH5502HP is proposed for chlorinated water at 60 °C, specific ESCR data must be obtained because published data for this specific configuration is limited. In the absence of such data, the material should not be substituted for a certified PE100-RC or PE4710 pipe compound. PE100 materials are associated with a minimum required strength of 10 MPa under ISO 12162:2011; design stress is further reduced by temperature and oxidant factors. For potable hot water with chlorine residual above 0.5 mg/L, the hydrostatic design basis may need to be derated below 8 MPa unless the resin has demonstrated resistance through chlorine-specific protocols.
Against a high-flow injection-molding HDPE with MFR 190 °C/2.16 kg in the 10–30 g/10 min range, the high-molecular-weight profile associated with ZH5502HP reduces melt flow length and increases injection pressure. On a hydraulic injection machine with clamp force of 1500 kN, the same mold may require an increase in holding pressure from 35 MPa to more than 60 MPa when switching from a 20 g/10 min HDPE to a 0.30 g/10 min grade. This is a processing difference rather than a defect. Higher injection pressures are associated with improved impact toughness and ESCR. Conversely, compared with a high-molecular-weight film grade with broad molecular weight distribution, ZH5502HP may show lower bubble stability if used in blown film because its molecular design and additive package are not optimized for film stretching. A 0.2–0.3 g/10 min film grade typically shows higher melt strength at 190 °C and a lower gel count. These comparisons should be used for allocation decisions only after confirming the ZH5502HP certificate values.
| HDPE family | Typical MFR at 190 °C/2.16 kg | Melt flow rate ratio 21.6/2.16 kg | Primary processing method | Qualitative failure signature |
|---|---|---|---|---|
| ZH5502HP high-molecular-weight band | 0.20–0.60 g/10 min; verify certificate | 15–35 | Thick-wall extrusion blow molding, sheet, large-part injection | Melt fracture at low temperature, parison sag, pressure-limited filling |
| High-flow injection HDPE | 10–30 g/10 min | 7–12 | Injection molding | Weld-line brittleness, lower ESCR |
| Blown film HDPE | 0.20–0.30 g/10 min | 18–35 | Blown film extrusion | Bubble instability, gel streaks, low dart impact |
| Bimodal PE100 pipe compound | 0.20–0.50 g/10 min at 190 °C/5.0 kg | >30 | Pipe extrusion | Slow crack growth, hydrostatic failure below design life |
Regulatory conformance for food-contact use must be established under a specified jurisdiction. In the United States, HDPE resin used in food-contact articles is generally subject to FDA 21 CFR 177.1520, which covers olefin polymers with density limits and extractable fraction limits depending on use conditions. In the European Union, compliance is determined under Regulation (EU) 10/2011 for plastic food-contact materials, with an overall migration limit of 10 mg/dm² and specific migration limits for additives. These are not automatically met by the base resin designation. The converter must obtain a compliance statement from Sinopec for ZH5502HP and verify that the complete formulation, including color masterbatch and processing aids, does not exceed migration thresholds. For industrial non-food applications, REACH SVHC screening should be available in the safety data sheet, and RoHS Directive 2011/65/EU restricts cadmium, lead, mercury, and hexavalent chromium in electrical equipment housings.
Storage below 40 °C and protection from UV exposure are standard. Pre-drying is not generally required for HDPE unless the resin has been exposed to condensation or relative humidity above 60%; if free moisture is visible, hot-air drying at 70–80 °C for 2–4 hours should be used. ZH5502HP should not be combined with amine-based flame retardant additives without compatibility testing because amine chemistry can interact with the phenolic stabilizer package and shift the onset of oxidative degradation. Masterbatch carriers should be HDPE or compatible polyethylene; low-molecular-weight carriers can reduce melt strength. Pigment systems containing copper phthalocyanine should be assessed for long-term oxidative stability under ISO 11357-6:2018, particularly in hot-water service. The material should not be processed above 250 °C melt temperature because rapid degradation and volatilization occur; this is the operational boundary.