| HS Code | 253104 |
| Density | 0.954 g/cm³ |
| Meltflowrate | 0.35 g/10 min (190°C/2.16 kg) |
| Tensileyieldstrength | ≥25 MPa |
| Tensilebreakstrength | ≥30 MPa |
| Elongationatbreak | ≥600% |
| Flexuralmodulus | ≥1000 MPa |
| Impactstrength | ≥200 J/m |
| Vicatsofteningtemperature | ≥120°C |
| Brittlenesstemperature | ≤-60°C |
| Meltingpoint | 130°C |
| Hardnessshored | 65 |
| Environmentalstresscrackresistance | ≥1000 h |
| Waterabsorption | ≤0.01% |
| Volumeresistivity | ≥10^16 Ω·cm |
| Dielectricconstant | 2.3 |
| Crystallinity | 80-90% |
As an accredited Sinopec Zhenhai HDPE ZH5502H factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Zhenhai HDPE ZH5502H is packaged in 25 kg polyethylene-lined woven bags, typically 40 bags per 1000 kg pallet. |
| Container Loading (20′ FCL) | Sinopec Zhenhai HDPE ZH5502H loaded in a 20′ FCL, typically in 25kg bags, securely stowed for ocean export. |
| Shipping | Sinopec Zhenhai HDPE ZH5502H is shipped as non-hazardous solid pellets in 25 kg PP woven bags, 500/1000 kg jumbo bags, or bulk bags, palletized and stretch-wrapped. Transport in clean, dry containers/trucks; keep away from moisture, direct sunlight, heat, and contaminants. Store in a ventilated warehouse. Handle with standard industrial precautions. |
| Storage | Store Sinopec Zhenhai HDPE ZH5502H in a cool, dry, well-ventilated warehouse. Keep original bags closed, on pallets, off the floor, away from direct sunlight, moisture, heat, and ignition sources. Avoid contamination with oils, dust, or chemicals. Protect from prolonged high temperatures and ultraviolet exposure. Use first-in, first-out rotation, maintain clear labeling, avoid excessive stacking, and keep away from strong oxidizers. |
| Shelf Life | Shelf life is 24 months from production date when stored in original packaging, cool, dry, ventilated area, away from sunlight. |
Sinopec Zhenhai HDPE ZH5502H is evaluated on production-scale accumulator-head extrusion blow moulding lines where single-station machines process 20–30 L jerry cans through 200 L tight-head drums. The polymer is charged at the feed throat through a gravimetric metering unit, and screw zone set points are typically maintained between 190 °C and 210 °C, with the extrusion head held at 200–215 °C. Melt temperature measured at the die is normally kept in the 205–215 °C band; excursions above 225 °C are associated with oxidative gel formation and detectable odour in the blown article. The accumulator head is programmed with a 10–20 point parison wall-thickness curve for 200 L drums, and the die gap is adjusted from 0.8 mm to 2.5 mm along the stroke to compensate for parison sag and die swell. Density is determined by ISO 1183-1 or ASTM D1505; melt mass-flow rate is measured according to ISO 1133-1 at 190 °C under 2.16 kg. High-density polyethylene grades in this viscosity band are commonly specified with a melt flow rate from 0.25 g/10 min to 0.40 g/10 min and a density from 0.953 g/cm³ to 0.957 g/cm³, but lot acceptance must be based on the producer certificate for ZH5502H.
For UN-certified 1H1 dangerous goods drums, stack testing is conducted for 28 days at 40 °C, drop testing follows conditioning at -18 °C, and hydraulic pressure testing is performed on the assembled drum body. ZH5502H can be considered for such applications only when the converter has qualified wall-thickness distribution, pinch-off geometry and closure torque retention with the specific drum design. A wall-thickness scan across the drum circumference should be taken at 12–16 points; variation exceeding ±0.4 mm in the lower sidewall is frequently linked to top-load buckling. Top-load resistance is evaluated according to ASTM D2659 after conditioning at 50 °C for 4 h. The grade is not intrinsically UV-stabilised; outdoor storage of drums therefore requires 2.0–3.0 wt% carbon black masterbatch or an approved hindered amine light stabiliser package, with carbon black dispersion verified by ISO 18553.
| Assessment | Standard or reference | Common production qualification condition |
|---|---|---|
| Density | ISO 1183-1 / ASTM D1505 | Reported at 23 °C on conditioned compression-moulded plaques |
| Melt mass-flow rate | ISO 1133-1 | 190 °C, 2.16 kg nominal load |
| Environmental stress crack resistance | ASTM D1693 Condition B | 100% Igepal CO-630 at 50 °C |
| Notched Charpy impact | ISO 179-1/1eA | Conditioned at -30 °C for low-temperature transport qualification |
| Food contact packaging | FDA 21 CFR 177.1520 / EU Regulation 10/2011 | Migration testing per EN 1186-1 and EN 13130-1 |
| UN dangerous goods packaging | UN Model Regulations Chapter 6.1 | 1H1 drum stack, drop and hydraulic pressure tests |
| Restricted substances | REACH Regulation 1907/2006, RoHS Directive 2011/65/EU | Supplier declaration with lot traceability |
The limiting unit operation is not extrusion throughput but cooling of the flashed pinch-off region and the lower sidewall. Mould cooling channels are typically spaced at 25–40 mm pitch with chilled water supplied at 8–12 °C; this configuration reduces part ejection temperature below 60 °C for a 25 L container with a nominal wall of 1.8–2.4 mm. On production-scale shuttle machines, cycle times from 55 s to 80 s are regularly observed for such containers depending on pinch-off design and blow-air time. For a 200 L drum with a sidewall of 2.5–3.5 mm, cycle time may extend from 150 s to 240 s. Published cycle-time data for this specific configuration are limited; the cited ranges are observed for high-molecular-weight HDPE grades within the same melt flow band and should be confirmed on the target line. If mould temperature is lowered below 6 °C, condensation in humid production halls causes splay and micro-pitting of the surface; if it exceeds 20 °C, cooling time increases non-linearly because the part remains above the HDPE crystalline plateau longer than acceptable.
Parison hang time is governed by zero-shear viscosity and molecular weight distribution. A broad distribution permits sag resistance for part lengths above 1,000 mm, but excessive die swell can pinch the needle blow point and produce an eccentric bottom flash. Tooling for ZH5502H should allow a die swell factor from 1.25 to 1.45; if the parison diameter is too close to the cavity minimum diameter, the lower weld line is thickened and trim force increases. A screw L/D ratio from 25:1 to 30:1 with a decompression zone and a Maddock dispersive mixer has been found to reduce gel breakdown when regrind is incorporated at 10–25 wt%. Melt temperature set points below 190 °C increase screw torque and may cause unplastisized particles to appear as surface gels, while temperatures above 220 °C shorten the induction time for thermo-oxidative degradation in the accumulator head. The process window at the die is therefore narrow in comparison with general-purpose blow moulding grades; converters should log melt temperature, head pressure and parison sag ratio for each lot.
In monolayer detergent bottles, the limiting degradation mode is environmental stress cracking at the pinch-off weld, not tensile yield or top-load collapse. Bottles filled with 10–30% nonionic surfactant formulations are stored at 40–50 °C for stability testing. ASTM D1693 Condition B is applied using 100% Igepal CO-630 at 50 °C; the acceptance threshold is not universal and is set by the filling brand, with qualification ranges commonly from 30 h to 100 h for notched bars depending on wall thickness and filler concentration. For ZH5502H, published ESCR values for specific commercial detergent packages are limited, so each bottle geometry must be qualified with the actual fill liquid. In coextruded structures, ZH5502H serves as the structural layer against an EVOH or polyamide barrier layer. The layer distribution is normally 55–70% virgin HDPE, 20–30% post-consumer recycled HDPE, and 10–15% tie and barrier layers; however, the exact ratio must be established by bottle drop and ESCR testing because recycled high-density polyethylene contains branching and polar contaminants that alter weld-line strength.
Pinch-off temperature is the main process variable controlling weld-line quality. A flash temperature above 180 °C increases oxidative degradation at the weld, while below 160 °C the two parison walls may not consolidate into a coherent seam. For a 1 mm sidewall bottle, the mould flash gap is generally set from 0.1 mm to 0.3 mm; wider gaps produce heavy flash but insufficient weld compression. Ethoxylated amine antistatic additives should be avoided for bottles containing high-pH laundry cleaners because crack initiation at the neck finish may occur during prolonged storage. If such additive packages are required, the filled bottle should be re-qualified by ASTM D1693 after at least 30 days of storage at 50 °C. The absence of a specific published data set for ZH5502H with amine-based antistats means that compatibility cannot be assumed without this confirmatory step.
Extrusion blow moulding lines producing 100–1,000 mL containers for veterinary pharmaceuticals and crop-protection concentrates qualify ZH5502H because the high-molecular-weight portion of the distribution limits parison drawdown and permits neck calibration without excessive ovality. The parison is blown with dried air at 6–8 bar through a calibrated blow pin; calibration time is held for 8–15 s before exhaust to keep neck concentricity within ±0.2 mm. Lot-to-lot melt flow variation should be monitored by ISO 1133-1 at 190 °C/2.16 kg. A shift of even 0.05 g/10 min can alter parison sag and wall distribution if blow-air pressure and mould close speed are not adjusted, and this effect is more pronounced in small bottles with thin sidewalls below 0.8 mm. In high humidity, surface moisture on pellets can create splay or pin holes; drying at 70–80 °C for 1–2 h is recommended when pellets have been stored in unheated silos at relative humidity above 70%. Colour masterbatch carriers should be HDPE-compatible; use of LDPE-carrier masterbatches at loadings above 3% may reduce ESCR by introducing short-chain branching at the weld line, although published data for ZH5502H under this specific masterbatch combination are limited.
Container designs with handle pinch-off, pour spouts and drainage sumps develop multiple weld lines that act as mechanical weak points during transport. In agrochemical containers, UV stabilisation is achieved with 2.0–3.0 wt% carbon black masterbatch or an approved hindered amine light stabiliser package. Dispersion is assessed according to ISO 18553; poor carbon black dispersion creates brittle zones at the pinch-off, and notched Izod per ASTM D256 can decline when undispersed particles exceed 20 µm. Low-temperature impact at -20 °C and -30 °C is evaluated by ISO 179-1/1eA. For small containers subjected to drop testing, the base and handle regions should show no crack propagation after drops from 1.8 m at -18 °C for Packing Group II liquids; the drop height changes with packing group and container density. Flash trim knives should be maintained sharp; a dull trim blade leaves micro-nicks that act as crack initiators and can cause failure even when the polymer itself retains adequate impact strength. The pinch-off flash should be trimmed while still slightly warm, because cold trimming below ambient temperature increases the incidence of notch formation along the weld flash boundary.
Diesel exhaust fluid packaging in 10 L and 20 L containers is tested under cold-climate logistics conditions. The HDPE layer must retain impact strength after 24 h conditioning at -40 °C. Testing per ISO 179-1/1eA at -30 °C provides a conservative indication of low-temperature embrittlement. Parison programming must increase the corner wall thickness to at least 25–35% above the nominal sidewall; if the wall at the bottom chimb is thinner than 1.5 mm, drop failure propagates from the pinch-off region. Accumulator-head tooling with a 10-point programming function is normally used so that the chimb, shoulder and handle zones receive additional material without over-thickening the panel centre, which would increase cooling time and distort the container.
ZH5502H is not a barrier resin; for long-term diesel exhaust fluid shelf life above 12 months, a multilayer structure with EVOH is used. In this structure, ZH5502H is used as the inside and outside HDPE layers, while tie layers and EVOH account for 8–15% of total wall thickness. The HDPE outer layer is compounded with 2.0–2.5 wt% carbon black concentrate if outdoor storage is expected. Amine-based processing stabilisers or antistats should not be introduced without re-qualifying low-temperature impact; some amines can promote environmental stress cracking in high-density polyethylene exposed to urea-based diesel exhaust fluid. At mould temperatures below 5 °C, surface condensation may produce micro-pits; at melt temperatures above 220 °C, oxidative gels create weak points that fail in -40 °C drop tests. The combination of low mould temperature, high melt temperature and excessive regrind above 25 wt% is particularly detrimental in this application because the gel nuclei concentrate at the pinch-off line and reduce crack propagation resistance after cold impact.
Competitive Sinopec Zhenhai HDPE ZH5502H prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Zhenhai HDPE ZH5502H is a bimodal high-density polyethylene supplied in pellet form for blown-film conversion. Manufacturer trade literature identifies the nominal density as 0.955 g/cm³ when measured to ISO 1183-1 and the melt mass-flow rate as 0.22 g/10 min at 190 °C under 2.16 kg load to ISO 1133-1:2022. The molecular weight distribution comprises a low-molecular-weight component that lowers die-lip shear stress and a high-molecular-weight component that increases extensional melt strength and bubble stability. Primary applications documented in trade literature are high-stiffness grocery sacks, refuse liners, and thin industrial packaging where downgauging and moisture barrier are specified. This product is not a high-flow injection moulding resin; injection grades typically show MFR values above 5 g/10 min and cannot sustain a stable blown-film bubble at comparable blow-up ratios.
Detailed datasheet values vary with additive package and pelletising conditions. The most frequently cited set of nominal properties appears in Table 1. Published lot-to-lot variation for film-grade HDPE is typically tighter for density than for dart impact because dart impact is influenced by film thickness, frost-line height, and blow-up ratio.
In capillary rheometry at 190 °C, bimodal HDPE with melt flow rates near 0.2 g/10 min tends to show lower apparent viscosity at die-shear rates above 500 s⁻¹ than a unimodal resin of identical melt flow rate. The low-molecular-weight mode acts as an internal processing aid, while the high-molecular-weight mode raises zero-shear viscosity and melt strength. This combination permits the use of narrower die gaps from 1.4 mm to 2.0 mm without inducing heavy melt fracture and allows blow-up ratios from 3.5:1 to 4.5:1. By contrast, conventional unimodal HDPE film grades often must be run at wider die gaps or lower output to avoid bubble instability at the same film density.
Compared with chromium-catalyzed HDPE of similar density, ZH5502H may show lower catalyst residue and more neutral color, but direct comparison on the same blown-film line is required because comonomer type, additive type, and molecular weight distribution shape influence dart impact and tear resistance more than density alone. Compared with metallocene-catalyzed HDPE film grades, the resin normally exhibits higher stiffness and lower puncture and tear at equivalent gauge; the difference in heat-seal initiation temperature is also relevant for vertical form-fill-seal operations.
On a blown-film line with a 50 mm spiral mandrel die and 1.2 mm die gap, a switch from a unimodal HDPE of equivalent melt index to a bimodal grade such as ZH5502H can permit an output increase of 10–20 % before melt fracture onset, all else equal. The gain is driven by a lower power-law index in the die-shear region; for HDPE blown-film extrusion, the power-law index between 100 s⁻¹ and 1000 s⁻¹ is often between 0.25 and 0.40. Published rheological data for ZH5502H on a specific production line are limited; converter-specific capillary studies are required to confirm the output gain.
For high-output blown-film conversion, the processing envelope is set by melt pressure, die-lip build-up, and bubble stability rather than by melt temperature alone. On grooved-feed single-screw extruders of 55–75 mm screw diameter with L/D 30:1 and barrier screws, melt temperature is typically controlled at 190–210 °C. Die gap is usually set from 1.4 mm to 2.0 mm, and the bubble is operated at a blow-up ratio of 3.5:1 to 4.5:1. At screw speeds above 100 rpm, melt pressure on a 75 mm grooved-feed extruder can approach 350 bar, depending on die diameter, spiral channel depth, and screen-pack fouling. If die-lip shear stress exceeds the critical melt-fracture threshold, which for typical HDPE occurs in the order of 0.2 MPa, the die gap must be widened or melt temperature raised.
Batch-to-batch melt flow rate variation of ±0.02 g/10 min may be visible as bubble diameter drift on automatic air-ring systems, particularly when combined with recycled material. Incoming resin acceptance should include melt flow rate per ISO 1133-1:2022 and density per ISO 1183-1 before start-up. The resin should not be mixed with high-flow HDPE grades or with polypropylene-contaminated regrind above 2 wt%, because the resulting melt viscosity heterogeneity reduces bubble stability and increases gauge scatter.
| Property | Test standard | Range |
|---|---|---|
| Density | ISO 1183-1 | 0.954–0.956 g/cm³ |
| Melt flow rate | ISO 1133-1:2022, 190 °C, 2.16 kg | 0.20–0.24 g/10 min |
| Tensile yield stress | ISO 527-2 | 27–29 MPa |
| Elongation at break | ISO 527-2 | 600–800 % |
| Dart impact F50 | ASTM D1709A | 140–180 g |
The table is a comparative screening set, not a guaranteed specification. Product qualification for critical film structures should include capillary rheometry over a shear-rate sweep from 10 s⁻¹ to 1000 s⁻¹ and blown-film trials at the intended blow-up ratio, frost-line height, and take-up speed.
Dart impact measured under ASTM D1709A is especially sensitive to frost-line height. Raising the frost-line height from 4 die diameters to 8 die diameters can increase dart impact by a factor of 1.5 or more in high-molecular-weight HDPE, while lowering machine-direction tear resistance measured under ASTM D1922. The reverse change improves optical clarity at the expense of impact toughness. This property trade-off is the principal reason the grade is run at intermediate frost-line heights in grocery-sack and liner applications.
In blown film, orientation alters the balance between machine-direction and transverse-direction properties. For HDPE film with a blow-up ratio of 4:1, tensile yield stress is generally higher in the machine direction than in the transverse direction by 10–20 %, and Elmendorf tear strength measured under ASTM D1922 is usually higher in the transverse direction. For ZH5502H, trade literature highlights machine-direction tear retention as a downgauging advantage over conventional unimodal resin. This claim should be verified on the target film line because air-ring design, frost-line height, and die gap influence orientation more than resin density.
Differences in seal initiation and hot-tack performance are governed by comonomer type and additive package. The grade may require corona treatment to raise surface energy above 40 dyn/cm for printing; after corona treatment, surface energy may decay below 38 dyn/cm within 72 h if migratory slip additives dominate. For side-seal grocery sacks, seal-bar temperature is commonly set between 135 °C and 150 °C with cooling water at 20 °C; beyond 150 °C, seal-edge deformation and film shrinkage increase.
When downgauging below 12 µm is attempted, bubble stability and dart impact retention become the controlling variables. The high-molecular-weight fraction supports bubble stability at thin gauge, but stalk stability degrades if frost-line height is below 4 die diameters. Maintain frost-line height at 4–8 die diameters and use a dual-lip air ring with chilled air at 8–12 °C to improve gauge uniformity. Pre-drying is not normally required; if pellet surface condensation occurs at warehouse humidity above 60 % RH, dry for 2 h at 80 °C in a desiccant-air hopper dryer to prevent surface defects and pinholes. Avoid addition of peroxide masterbatch; chain scission in the high-molecular-weight fraction can reduce dart impact to 60 % or less of the original value and produce film with insufficient creep resistance.
Additive selection in thin HDPE film is limited by plate-out and migration. Slip agents based on erucamide or oleamide require time to bloom to the surface; at 1000–1500 ppm, coefficient of friction measured under ISO 8295 typically decreases from 0.35–0.45 to 0.10–0.20 after 24–48 h. Antiblock agents such as synthetic silica at 2000–5000 ppm reduce blocking but raise haze. For ZH5502H, the film producer should verify additive concentration limits with the supplier because the high-molecular-weight fraction can delay additive bloom and change sealing performance.
Pigment masterbatches based on titanium dioxide can shift bubble emissivity and complicate infrared thickness measurement. When white film is produced on the same line, machine-direction gauge variability may increase because the auto-gauge sensor must be recalibrated for the pigment concentration. A precompounded white masterbatch at 5–8 wt% with polyolefin carrier is common, but black speck dispersion must be monitored by film inspection under ASTM D6290 or an equivalent camera system.
Finished film can be evaluated for food-contact status under FDA 21 CFR 177.1520 for olefin polymers, provided that the final article meets end-use extraction limitations and all additives are authorized. In the European Union, compliance is assessed under EU No 10/2011 through migration testing of the finished film, because overall migration and specific migration limits depend on thickness, additive package, and food simulant. The resin as supplied is not intended for medical implants or long-term structural load-bearing parts; creep, fatigue, and biocompatibility data are not established for those service conditions.
Do not dry-blend with amine-based antistatic additives at high concentrations because amine migration can interfere with printing primers and reduce heat-seal strength at sealing temperatures of 135–150 °C. Regrind levels above 20 wt% can narrow the bubble-stability window if the recycled fraction contains degraded gel, polypropylene, or high-viscosity foreign resin. Under REACH, the downstream user must verify substances of very high concern in the final article; under RoHS, HDPE is not restricted for cadmium, lead, mercury, or chromium VI unless contaminated by recycled feedstock.