Sinopec Yanshan Hdpe 7600m

Sinopec Yanshan HDPE 7600M

    • Product Name: Sinopec Yanshan HDPE 7600M
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 561448
    Melt Flow Rate 7.0 g/10 min
    Density 0.960 g/cm³
    Tensile Strength At Yield 30 MPa
    Elongation At Break 500%
    Flexural Modulus 1200 MPa
    Notched Izod Impact Strength 50 J/m
    Vicat Softening Temperature 125 °C
    Heat Deflection Temperature 75 °C
    Shore D Hardness 65
    Water Absorption 0.01%
    Mold Shrinkage 1.5-2.5%
    Melting Point 130-135 °C
    Thermal Conductivity 0.4 W/m·K
    Dielectric Constant 2.3
    Volume Resistivity >10^16 Ω·cm
    Dielectric Strength >20 kV/mm

    As an accredited Sinopec Yanshan HDPE 7600M factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Yanshan HDPE 7600M packaging: 25 kg PE-lined woven bags, also available in 1000 kg jumbo bags, palletized for transport.
    Container Loading (20′ FCL) 20′ FCL loading: Sinopec Yanshan HDPE 7600M, 25 kg bags; about 17–18 MT palletized or 22 MT loose per container.
    Shipping Sinopec Yanshan HDPE 7600M ships as non-hazardous polyethylene pellets, typically in 25 kg PP woven bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers, avoiding moisture, direct sunlight, heat, and contamination. No special dangerous goods handling is required.
    Storage Store Sinopec Yanshan HDPE 7600M in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep original bags or containers tightly closed, off the floor, and protected from moisture, dust, oils, and contaminants. Avoid prolonged UV exposure. Maintain clean, dry handling conditions and good industrial hygiene. Use first-in, first-out stock rotation.
    Shelf Life Stable for 24 months when stored in original packaging under cool, dry, ventilated conditions, away from direct sunlight and heat.
    Application of Sinopec Yanshan HDPE 7600M

    Sinopec Yanshan HDPE 7600M is a high-density polyethylene blow-moulding grade specified for closed-die extrusion-blow moulding where low melt index, high melt strength, and environmental stress-crack resistance are controlling. The grade is characterised by a melt flow rate below 1.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 and a nominal density of 0.950 g/cm³ under ISO 1183-1:2019. These two boundaries define parison hang time, drop impact, pinch-off weld integrity, and long-term chemical containment performance. The downstream scenarios below are restricted to industrial applications in which HDPE 7600M is used as a base resin; no high-flow injection-moulding or film-extrusion claims are made. Lot-specific melt rheology, density, and additive package should be obtained from the supplier certificate of analysis before setting accumulator-head parameters. HDPE 7600M does not require pre-drying unless surface condensation is present from humid storage; hopper inlet temperature should be kept above 20 °C and residual moisture below 200 ppm to avoid surface splay.

    Downstream boundaryPrimary standard / test methodTypical 7600M loadingTerminal article
    200 L UN drumUN Model Regulations Chapter 6.1; ASTM D1693-15100 phr200 L 1H1 tight-head drum
    1000 L IBC inner bottleADR 6.5.4; UN 31H1100 phr1000 L IBC inner container
    Automotive fuel tankECE R34 Annex 5; GB 18352.6-2016100 phr skin layers40–80 L fuel tank system
    Agrochemical barrier containerUN Model Regulations Chapter 6.1; UN 3H190–95 wt% of wall mass1–20 L pesticide bottle
    Vertical water storage tankASTM D1998-21; NSF/ANSI 61100 phr500–5000 L storage tank
    Underhood reservoirISO 527-2:2012; ISO 179-1:2010100 phr4–7 L washer reservoir
    Flotation / secondary containmentISO 178:2019; ASTM D1693-15100 phrBuoyancy module

    UN 1H1 Drum Wall Thickness and ESCR Limits

    For 200 L tight-head drums, the primary manufacturing risk is not short-term burst but environmental stress-crack growth along the pinch-off weld, which is why HDPE 7600M is selected over lower molecular weight grades. The drum body is extrusion-blow-moulded on an accumulator-head machine with a grooved-barrel extruder diameter of 80–120 mm and L/D ratio of 25:1–30:1; barrel temperatures are profiled from 170 °C at the feed throat to 210–230 °C at the die head. The compliance envelope is set by UN Model Regulations Chapter 6.1 for Packing Group II and III liquids, which requires a drop test, leakproofness test, hydraulic pressure test, and stacking test on 1H1 non-removable-head plastics drums. The batch recipe is 100 phr HDPE 7600M, carbon black masterbatch at 1.5–3.0 wt% for ultraviolet opacity, phenolic/phosphite antioxidant package at 0.15–0.30 wt%, and polymer processing aid at 0.02–0.06 wt%. Regrind from own drum trims is limited to 25 wt% because higher levels reduce ESCR measured under ASTM D1693-15 and decrease drop impact tested under ASTM D2463-15. Parison weight for a 200 L body is in the 3.5–5.5 kg range depending on top and bottom chime geometry; blow pressure is held at 0.6–0.9 MPa, and mould closing speed is reduced in the final 20 mm of travel to avoid pinch-off flash fracture. Finished articles are 200 L 1H1 tight-head drums and 220 L open-head 1H2 containers for solvent, lubricant, and chemical distribution.

    What Determines Parison Stability in 1000 L IBC Inner Bottle Moulding?

    A 1000 L IBC inner bottle imposes a parison length above 2,000 mm; parison sag must be controlled within ±1.5 mm wall variation along the vertical sidewall, otherwise the bottle fails the 31H1 composite IBC hydraulic pressure sequence under ADR 6.5.4 and UN Model Regulations Chapter 6.5. The type-approved floor in chemical distribution is the 31H1 rigid plastics inner receptacle inside a steel cage, with top discharge closure. Formulation input is 100 phr HDPE 7600M, UV stabilizer masterbatch at 0.4–1.2 wt%, processing aid at 0.02–0.05 wt%, and colourant masterbatch not exceeding 0.3 wt% to limit screw-slip variability. If fluorinated IBC bottles are reground, the fluorinated regrind stream is held below 15 wt% because fluorine-containing surface layers increase melt-pressure variation at the die head by more than 2 MPa on 100 mm extruders. The process uses a large accumulator blow moulder with 100–150 mm screw diameter, 25:1–30:1 L/D, die gap of 2.0–3.5 mm, and a 100-point parison programmer; bottle mass for a 1000 L inner container is 13–17 kg, and cooling time is 250–400 s depending on mould temperature, which is held at 20–40 °C. In-mould closure of the top filling port is followed by flange trimming and leak testing at 0.3 bar gauge. Finished products are 1000 L inner bottles, 31H1 composite IBCs, and 600 L variants for specialty solvents.

    Across multilayer fuel tank production, the narrowest parison programming window among blow-moulded automotive components is defined by the interaction of HDPE 7600M skins and an EVOH barrier core. Regulatory acceptance is referenced to ECE R34 Annex 5 fire resistance for plastic fuel tanks and to GB 18352.6-2016 evaporative emission requirements in China, while export programmes may additionally apply EPA 40 CFR Part 86 evaporative emission certification. The wall distribution is expressed by layer split rather than additive weight: HDPE 7600M outer and inner skins each account for 15–20 wt% of total wall thickness, regrind 35–45 wt%, maleic anhydride grafted polyethylene tie layers 5–10 wt%, and EVOH barrier 3–6 wt%. The HDPE skins are compounded with carbon black masterbatch at 2.0–3.0 wt% and antioxidant at 0.15–0.30 wt%. The main process conflict is thermal: EVOH must be kept below 230 °C to avoid gel formation, while HDPE 7600M requires 200–230 °C for low melt fracture and stable parison diameter; therefore the coextrusion feed block is designed with separate temperature zones and the tie resin is selected with melt temperature 190–220 °C. Parison programming uses 128–256 points because the tank’s pinch-off seam and top-wall corners are the highest permeation and burst-risk zones. Cycle time for a 40–80 L fuel tank system ranges from 120–180 s, followed by blowout monitoring, burst testing, and hydrocarbon permeation measurement under OEM-specific procedures. Terminal parts are passenger vehicle fuel tanks and diesel fuel reservoirs.

    When EVOH Coextrusion Replaces In-Mould Fluorination for Agrochemical Containers

    Mono-layer HDPE containers for solvent-borne agrochemicals fail package-permeation screening unless in-mould fluorination is performed; where fluorination is rejected for downstream recyclability reasons, the line is configured for three-layer coextrusion with HDPE 7600M skins and an EVOH barrier core. Packaging certification is referenced to UN Model Regulations Chapter 6.1, Packing Group III for concentrated pesticide formulations, and the 3H1 tight-head plastics jerrican code; the barrier bottle is also evaluated for stack loading and closure torque retention after storage at 50 °C for 28 days. The layer split is HDPE 7600M at 90–95 wt% of total wall mass, EVOH core at 4–8 wt%, and maleic anhydride grafted polyethylene tie at 2–4 wt%; the HDPE layer includes UV stabilizer masterbatch at 0.3–1.0 wt% and colourant below 0.5 wt%. The blow-moulding line is a continuous shuttle or long-stroke machine with 6–20 cavities for 1–20 L bottles; melt temperature is held at 180–220 °C, die head at 180–210 °C, blow pressure at 0.5–0.8 MPa, and cycle time at 7–20 s depending on cavity count. The limiting defect is layer redistribution in the bottom pinch-off zone, where EVOH thinning below 1.5 wt% of local wall mass creates solvent permeation hot spots; programmers therefore set a local wall thickening of 15–30% at the pinch-off ledge. Finished goods are 1–20 L pesticide bottles, crop-protection chemical containers, and solvent maintenance cans.

    In vertical water storage tanks blown from HDPE 7600M, wall-section programming is biased toward the bottom knuckle radius and the top dome weld, where hydrostatic pressure and moulded-in stress intersect. Compliance for non-food process water uses ASTM D1998-21 for polyethylene upright storage tanks, while potable-water contact requires NSF/ANSI 61 certification of the finished tank rather than the pellet alone; formulations used for dark-coloured outdoor tanks are 100 phr HDPE 7600M with UV stabilizer masterbatch at 0.5–2.0 wt%, antioxidant at 0.15–0.35 wt%, and carbon black at 0.3–1.0 wt%. White or light-coloured grades substitute titanium dioxide masterbatch at 1.0–3.0 wt% to reduce surface temperature; the accompanying carrier resin should be HDPE with low melt index to preserve parison hang time. The process uses an accumulator blow moulder with shot size between 3 kg and 9 kg, die gap 2.0–3.5 mm, and mould temperature 20–40 °C; base-wall programming is 8–15 mm, sidewall 4–8 mm, and cooling time 300–600 s. The main process failure is warpage after demoulding when the part is stripped before core cooling below 70 °C, causing ovality at the top flange. Finished products are 500–5000 L vertical water storage tanks, rainwater harvesting tanks, and process-fluid holding tanks.

    Windshield Washer Reservoirs, Coolant Surge Tanks, and Underhood Blow-Moulded Reservoirs

    Underhood reservoirs are produced on multi-cavity shuttle or accumulator blow-moulding lines where cycle time is governed by pinch-off flash thickness and insert loading. The material acceptance basis for these parts typically references ISO 527-2:2012 tensile yield and ISO 179-1:2010 Charpy notched impact at -30 °C; engine-compartment flammability is evaluated under ISO 3795:1989, and the part is accepted only below the customer’s burn-rate limit. The formulation is 100 phr HDPE 7600M, long-term heat-stabilizer masterbatch at 0.3–0.8 wt%, carbon black masterbatch at 0.2–1.0 wt%, and processing aid at 0.02–0.05 wt%; no plasticizer is added because migration would embrittle the weld and increase stress-crack sensitivity. The process uses barrel temperatures from 180 °C to 220 °C, blow pressure 0.5–0.8 MPa, mould temperature 15–35 °C, and cycle time 30–70 s; filler necks and mounting bosses are hot-plate welded or insert-moulded, requiring a wall thickness at the weld land of at least 2.0 mm. The primary plant-observed failure is coolant-surge tank cracking at the internal return-line boss when the moulded-in stress exceeds 5 MPa after ageing; residual stress is therefore checked by immersion in a 0.5 wt% detergent solution at 80 °C for 24 h. Finished articles are 4–7 L windshield washer reservoirs, coolant surge tanks, and auxiliary fluid reservoirs for commercial vehicles.

    At the high-wall-thickness end of HDPE 7600M processing are large blow-moulded flotation hulls and chemical process secondary containment liners. Acceptance testing for these parts is usually customer-specific but invokes ISO 178:2019 flexural modulus, ISO 527-2:2012 tensile properties, and ASTM D1693-15 ESCR after surface oxidation. The formulation is 100 phr HDPE 7600M, UV stabilizer masterbatch at 1.0–2.0 wt% for outdoor exposure, antioxidant at 0.15–0.30 wt%, and carbon black at 2.0–3.0 wt% where ultraviolet resistance is the controlling requirement. The blow-moulding route uses an accumulator head with shot weights up to 40 kg and die diameters above 200 mm; parison programming is set for wall thickness from 5 mm to 15 mm, and mould temperature is held at 20–35 °C to control crystallinity and shrinkage anisotropy. Cooling time ranges from 600 s to 1200 s depending on section thickness; forced-air internal cooling is used to reduce cycle time but increases the risk of surface haze if airflow is not dried to a dew point below -20 °C. Published data for this specific configuration with HDPE 7600M is limited, so pilot trials with the actual wall thickness and UV formulation are required before full-rate production. Finished parts include flotation buoys, secondary containment basins, and industrial immersion floats.

    Free Quote

    Competitive Sinopec Yanshan HDPE 7600M prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Yanshan HDPE 7600M is a high-molecular-weight high-density polyethylene blow molding resin produced by Sinopec Beijing Yanshan Company. The grade is supplied as pellets, and typical lot data place density in the range 0.952 g/cm³ to 0.956 g/cm³ under ISO 1183-1:2019. High-load melt flow index measured at 190 °C with a 21.6 kg load under ISO 1133-1:2022 is generally between 6.0 g/10 min and 9.0 g/10 min. These values place the resin in the large-part extrusion blow molding segment rather than in low-load injection molding flow regimes. Primary application areas include industrial containers, 200 L tight-head drums, intermediate bulk container liners, and multilayer automotive fuel tank shells in which high melt strength, parison hang stability, impact resistance, and environmental stress crack resistance control part performance. In contrast to general-purpose injection molding HDPE grades whose melt flow index at 2.16 kg is commonly between 8 g/10 min and 20 g/10 min, 7600M does not show meaningful low-load flow; the high molecular weight and long-chain entanglement density require high-load rheology and accumulator-head processing.

    Environmental stress crack resistance is the most consequential property separating 7600M from unimodal blow molding HDPE resins of similar density. Under ASTM D1693 condition B, with 10% Igepal CO-630 at 50 °C, high-molecular-weight broad-distribution resins in this density class commonly fail only after 500 h or more, whereas lower-molecular-weight blow molding grades may show brittle failure between 30 h and 100 h under identical loading. The difference is attributed to tie-molecule concentration and slow crack growth resistance in the higher-molecular-weight fraction. Published lot data for this specific grade should be interpreted with attention to test plaque thickness, notching direction, and conditioning protocol; ESCR values are not intrinsic constants and can be degraded by rapid cooling, excessive orientation, or insufficient homogenization of regrind. In multi-pass production, residual stress from blow molding can reduce field ESCR relative to compression-molded laboratory plaques.

    What Melt Rheology and Die Performance Distinguish 7600M from Lower-Molecular-Weight Blow Molding Resins?

    On production-scale single-screw extruders, 7600M processes with a pronounced shear-thinning viscosity profile but requires higher motor torque and more aggressive screw cooling than injection molding grades. Typical extrusion blow molding lines use screws with 24:1 to 30:1 L/D ratios, compression ratios of 2.5:1 to 3.0:1, and barrier or Maddock mixing sections. Barrel set points from feed zone to metering zone are commonly 170 °C to 200 °C, with the die head held between 190 °C and 210 °C to limit parison sag. Melt temperature at the accumulator or die entry should remain below 220 °C to limit antioxidant consumption and gel formation. Because the resin exhibits elevated melt elasticity, parison diameter swell can be significantly greater than that of lower-molecular-weight HDPE grades; die gap settings and parison programming must compensate for this response, particularly on large drums where wall thickness distribution is controlled by servo-hydraulic parison programming. Published data for exact die swell values across all industrial die geometries is limited, but equipment suppliers recommend wall-thickness control programs with at least 100 to 200 axial programming points for parts exceeding 20 L volume. Compared with a general-purpose blow molding HDPE with high-load melt flow index between 12 g/10 min and 25 g/10 min, 7600M requires wider die gaps, lower shear rates, or both to avoid sharkskin and melt fracture.

    Parison sag and melt strength comparisons are operationally useful in selecting this grade. A common industrial method extrudes a constant-length parison and records the time to reach 10% elongation under gravity at a fixed die temperature. High-molecular-weight HDPE grades with high-load melt flow index near 7 g/10 min show longer sag times than grades with high-load melt flow index above 12 g/10 min at the same melt temperature. This difference permits the use of larger parison lengths and more complex three-dimensional blow mold geometries without excessive wall thinning. The trade-off is increased extruder backpressure and higher energy input per kilogram of melt.

    Tensile, Flexural, and Impact Responses Under Laboratory Conditioning

    Mechanical property data for 7600M are typically generated on 2 mm compression-molded plaques conditioned at 23 °C and 50% relative humidity for 48 h. Tensile yield stress under ISO 527-2 at 50 mm/min is generally reported between 25 MPa and 28 MPa. Tensile modulus falls near 950 MPa, while flexural modulus under ISO 178 is commonly between 900 MPa and 1100 MPa. Notched Izod impact strength under ISO 179-1/1eA at 23 °C exceeds 20 kJ/m², and the resin often does not exhibit complete brittle failure at 0 °C. These values are not lot-release guarantees but representative ranges for high-molecular-weight HDPE blow molding resins of this density. The property profile differs from that of lower-viscosity blow molding grades, where higher high-load melt flow index improves flow but lowers ESCR and low-temperature impact.

    Comparative property ranges for high-molecular-weight blow molding, conventional blow molding, and injection molding HDPE
    ParameterTest method7600M typicalConventional blow molding HDPEInjection molding HDPE
    DensityISO 1183-10.952–0.956 g/cm³0.945–0.952 g/cm³0.950–0.960 g/cm³
    High-load melt flow indexISO 1133-1, 190 °C, 21.6 kg6.0–9.0 g/10 min12–25 g/10 minnot applicable
    Tensile yield stressISO 527-2, 50 mm/min25–28 MPa21–26 MPa24–30 MPa
    Flexural modulusISO 178900–1100 MPa850–1000 MPa1100–1400 MPa
    ESCR, condition BASTM D1693> 500 h typical30–100 hnot applicable

    Compared with general-purpose blow molding HDPE of lower density, 7600M typically exhibits lower shrinkage at demolding and higher melt strength. The higher density also contributes to greater stiffness and reduced permeation of aqueous chemicals, but can reduce low-temperature impact in thick-wall configurations. The high-load melt flow index range of 6.0–9.0 g/10 min is selected to balance processability on accumulator-head machines against end-use ESCR. Grades with high-load melt flow index below 4 g/10 min can provide additional ESCR improvement but often require higher melt temperatures and may exceed the torque capacity of older extruders. Grades with high-load melt flow index above 12 g/10 min show easier flow and shorter cycle times but lose parison melt strength and long-term crack resistance.

    If Coextruded Fuel Tank Shells Contain EVOH Barrier Layers, Then Viscosity Matching and Die Gap Control Govern Process Stability

    Multilayer blow molding of fuel tank shells uses 7600M as the inner and outer HDPE skins because the high melt strength supports parison formation at large diameters. A representative six-layer structure is HDPE outer, regrind, tie layer, EVOH barrier, tie layer, and HDPE inner. EVOH layer mass fraction is commonly held at 2% to 4% of the total wall thickness; adhesive tie layers occupy 2% to 5%, and the regrind layer is typically limited to 20% to 30% of total mass unless extensive production validation supports higher levels. Viscosity matching at the layer interfaces is a critical processing requirement. If the high-load viscosity difference between adjacent layers exceeds approximately 20% at the local shear rate, interfacial instability, layer thickness variation, and barrier defects can occur. Coextruded die heads for six-layer structures commonly use spiral mandrel distributors and require uniform melt temperature across the die; HDPE melt temperatures are maintained at 200 °C to 220 °C, while EVOH streams are kept below 230 °C to avoid degradation. Die gap settings on large fuel tank lines are typically between 1.8 mm and 3.0 mm; narrowing the die gap below 1.5 mm increases wall shear stress and can initiate melt fracture in the high-molecular-weight HDPE skins. Published data for a specific coextrusion line arrangement is limited, and the permitted layer proportions must be established on the production equipment with barrier permeation testing under ISO 15105-2 or an equivalent oxygen transmission method.

    Clamp force and mold cooling also differ from small-container blow molding. Fuel tank shells with wall thickness between 3 mm and 10 mm require low mold surface temperatures and extended blowing pressure after pinch-off to control shrinkage and minimize warpage. Pressure hold times are set by part mass and wall thickness distribution, and cycle-time reductions without thickness verification can increase internal stress. Ultrasonic wall-thickness mapping across the pinch-off zone is used on production lines because thickness bands below 2 mm near the pinch-off are a recurring failure site in 200 L drum and fuel tank applications.

    Regrind Ratio, Stabilizer Depletion, and Moisture Uptake Boundaries

    Production-scale blow molding generates significant regrind from flash, tops, and tails. For 7600M, in-plant regrind addition is typically accepted up to 30% by weight, but higher fractions require monitoring of residual stabilizer concentration because each heat history consumes phenolic and phosphite antioxidants. Under high ambient humidity above 60%, pellets and regrind should be dried at 80 °C for 4 h before extrusion to keep moisture below 0.05 wt%; otherwise surface splay, reduced melt strength, and parison pinholes may result. Residual antioxidant levels can be checked by ASTM D6810; if the hindered phenolic antioxidant content falls below the supplier’s recommended minimum, regrind ratio must be reduced or a masterbatch replenishment strategy implemented. The resin is not recommended for long-term contact with strong oxidizing acids above 40 °C or with low-viscosity aromatic hydrocarbons that cause rapid environmental stress cracking. Published data for prolonged exposure to aggressive chlorinated solvents in blow-molded parts is limited; each container design must be validated using the target chemical and actual wall-thickness distribution.

    Routine quality control for 7600M often includes apparent density and pellet size consistency because pellet bridging in hopper feed can cause screw surging. Pellet dimensions commonly range from 2 mm to 4 mm in diameter and 2.5 mm to 4 mm in length; deviations can alter feed angle and throughput stability on single-screw blow molding machines. On high-output lines, gravimetric feed control and hopper vibration are used to limit bridging when pellet size distribution shifts between lots.

    Lot acceptance and technical data sheets for 7600M typically list density, high-load melt flow index, tensile yield stress, flexural modulus, notched Izod impact, and ESCR with method designations specified by ISO 1183-1, ISO 1133-1, ISO 527-2, ISO 178, ISO 179-1, and ASTM D1693. Food-contact and potable-water suitability are determined on the finished article rather than on raw resin alone; suppliers may reference FDA 21 CFR 177.1520 and EU Regulation 10/2011 for the base polymer composition. RoHS 2011/65/EU applies to electrical and electronic equipment and does not by itself certify packaging resins. For industrial container certification, the blow-molded article must pass the applicable UN performance test for dangerous goods packaging, not the resin lot.

    Top