Sinopec Yanshan Hdpe 5200b

Sinopec Yanshan HDPE 5200B

    • Product Name: Sinopec Yanshan HDPE 5200B
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 237224
    Productname Sinopec Yanshan HDPE 5200B
    Manufacturer Sinopec Beijing Yanshan Petrochemical Company
    Materialtype High Density Polyethylene (HDPE)
    Grade 5200B
    Density 0.954 g/cm³
    Meltflowrate 0.35 g/10 min (190°C/2.16 kg)
    Meltingpoint 131 °C
    Vicatsofteningtemperature 125 °C
    Tensilestrengthatyield 24 MPa
    Elongationatbreak >600 %
    Flexuralmodulus 1000 MPa
    Notchedizodimpactstrength 80 J/m
    Environmentalstresscrackresistance >1000 h
    Hardnessshored 65
    Waterabsorption <0.01 %
    Thermalexpansioncoefficient 1.2e-4 /°C
    Dielectricstrength 20 kV/mm
    Volumeresistivity >1e16 ohm·cm
    Processingtemperature 170–220 °C
    Moldshrinkage 1.5–3.0 %
    Moisturecontent <0.05 %
    Ashcontent <0.1 %
    Bulkdensity 0.55 g/cm³
    Chemicalresistance Good to acids, alkalis, and salts; poor to hydrocarbons
    Appearance White pellets
    Odor Odorless

    As an accredited Sinopec Yanshan HDPE 5200B factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Yanshan HDPE 5200B is packaged in 25 kg polyethylene-lined woven bags, or 1000 kg jumbo bags for bulk shipment.
    Container Loading (20′ FCL) Sinopec Yanshan HDPE 5200B resin is packed in 25kg bags and loaded into 20-foot FCL containers for secure ocean export.
    Shipping Sinopec Yanshan HDPE 5200B is shipped as a non-hazardous solid thermoplastic resin in 25 kg woven bags or 1000 kg jumbo bags, palletized and stretch-wrapped. Typically transported in 20'/40' containers by sea, truck, or rail under normal conditions, away from moisture, heat, and contamination.
    Storage Store Sinopec Yanshan HDPE 5200B in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and strong oxidizers. Keep original bags or containers tightly closed to prevent moisture, dust, and contamination. Stack pallets safely within load limits to avoid deformation. Maintain good housekeeping; avoid prolonged UV exposure. Follow local regulations and manufacturer’s safety data sheet.
    Shelf Life Shelf life for Sinopec Yanshan HDPE 5200B is typically 24 months when stored unopened in cool, dry, ventilated conditions, away from sunlight.
    Application of Sinopec Yanshan HDPE 5200B

    Sinopec Yanshan HDPE 5200B enters extrusion blow molding lines as a high-molecular-weight grade with a nominal density of 0.952 g/cm³ under ISO 1183-1:2019 and a melt flow index of 0.30 g/10 min under ISO 1133-1:2022. In 220 L L-ring drum manufacturing, the material is processed on accumulator head machines with grooved-feed single-screw extruders having length-to-diameter ratios from 24:1 to 30:1. The barrel temperature profile is typically set from 180 °C near the feed throat to 230 °C in the metering zone, and the die head is held at 215 °C to 225 °C to produce a melt temperature of 200 °C to 210 °C at parison exit. The parison weight for a 220 L L-ring drum ranges from 9.5 kg to 11 kg, and the parison drop length is 1.2 m to 1.6 m before mold closure. Melt strength is sufficient to limit sag to less than 8 % of initial parison length when the die gap and die swell are calibrated with a 20-point to 50-point servo-hydraulic parison programmer. The die swell of high-molecular-weight HDPE in drum applications is commonly observed at 25 % to 40 %; therefore the die gap must be set narrower than the target parison wall thickness by the measured swell ratio on the specific machine. The blow-up ratio is set between 2.2:1 and 3.0:1, and pre-blow pressure is staged from 0.2 MPa to 0.5 MPa before final blow at 0.7 MPa to 1.0 MPa. The mold is maintained at 10 °C to 18 °C, and the clamp force on a single-station drum machine is maintained above 1,200 kN to avoid widening the pinch-off zone.

    The bottom pinch-off seam is inspected by cutting 20 mm flash strips and conducting a room-temperature folding test; flash that cracks before reaching 180 ° bend indicates insufficient melt fusion at the weld. For UN-certified packaging, the finished drum is subjected to the UN 6.1.5.3 drop test at -18 °C, the UN 6.1.5.6 stacking test, and the UN 6.1.5.4 leakproofness test at 30 kPa internal pressure. ESCR is the primary chemical resistance screen under ASTM D1693-15 Condition B at 50 °C; typical high-molecular-weight drum grades in this density class can range from 150 h to 600 h depending on lot comonomer distribution and cooling-induced internal stress. For 5200B, published data for this specific configuration is limited, so incoming lot testing is required and the pinch-off zone must be sampled separately from the sidewall. Continuous contact with concentrated nitric acid, oleum, or strong oxidizing sodium hypochlorite above 60 °C is outside the operational boundary of this polyethylene grade. For open-yard storage, a UV stabilizer package is required and periodic re-certification under ISO 4892-3:2016 is used to detect embrittlement after 24 months of exposure.

    Processing parameter comparisons for Sinopec Yanshan HDPE 5200B blow molding at three downstream scales
    Parameter25 L jerrican220 L L-ring drum1,000 L IBC inner bottle
    Melt temperature195–215 °C200–210 °C205–220 °C
    Die head temperature200–215 °C215–225 °C215–230 °C
    Mold temperature10–15 °C10–18 °C10–16 °C
    Blow-up ratio2.0–2.8:12.2–3.0:12.4–3.0:1
    Blow pressure0.6–0.9 MPa0.7–1.0 MPa0.6–1.0 MPa
    Clamp force350–500 kN1,200–1,800 kN1,500–2,200 kN

    Can 5200B Maintain IBC Inner Bottle Wall Thickness Distribution Under Programmed Parison Blow-Up Ratios of 2.8:1?

    In 1,000 L IBC inner bottle production, the limiting variable shifts to corner-thinning control. The parison for an IBC bottle is typically inflated to a blow-up ratio of 2.4:1 to 3.0:1, and a square cage geometry creates a wall thickness reduction of 20 % to 30 % at the shoulder and bottom chime compared with the sidewall midpoint when a linear parison programmer is used. Production lines therefore use 64-point to 128-point servo-hydraulic die gap controllers and stage the blow pressure from 0.6 MPa pre-blow to 1.0 MPa final blow. The die head temperature is increased to 215 °C to 230 °C, and mold temperature is held at 10 °C to 16 °C. Wall thickness is measured with an ultrasonic gauge over a 50 mm grid; the minimum acceptable thickness at any load-bearing point is 1.5 mm for general chemical service. The bottle is then inserted into a steel frame and subjected to the applicable UN IBC drop test and bottom lift test. Failure in this configuration most often occurs at the top-cap weld perimeter under excessive closing torque or at the pinch-off line if the parison melt temperature falls below 190 °C. Published data for 5200B in 1,000 L IBC inner bottles is limited; validation trials must correlate molded-in stress at the cap area with ESCR results obtained under ASTM D1693-15.

    Monolayer off-road fuel tank production requires permeation resistance to be decided before mechanical loading. A 4 mm nominal wall of 5200B does not satisfy SAE J1737 hydrocarbon permeation limits without a barrier step; therefore inline fluorination or post-mold fluorine passivation is applied to create a fluorinated polyethylene layer of 1 μm to 5 μm on the inner surface. The fluorination reactor temperature is kept below 80 °C to avoid excessive surface oxidation and weld-line elongation loss. On an accumulator head machine, 5200B is parison-formed at die temperatures of 210 °C to 230 °C and blown into a cast aluminum mold kept at 12 °C to 18 °C. The formed tank is subjected to a fuel soak test with Fuel C at 40 °C for 20 weeks, followed by a 25 kPa pressurization leak check; wall thickness at the fuel tank corners is specified at no less than 3 mm. For coextruded structures with EVOH or polyamide barrier layers, published data for 5200B is limited, and tie resin compatibility must be verified at die lip shear rates of 100 s⁻¹ to 1,000 s⁻¹ to prevent interfacial instability. The grade is not recommended for pressurized fuel systems above 0.3 MPa continuous operating pressure without a structural support frame.

    When 5200B Is Blown into 25 L Agrochemical Jerricans, Closure Torque and Seam Fusion Set the Lot Release Boundary

    Shuttle blow molding machines with one to four parison heads process 5200B at melt temperatures of 195 °C to 215 °C and mold temperatures of 10 °C to 15 °C. Closure torque retention after filling and after thermal cycling from -10 °C to 40 °C is measured with a digital torque wrench; the release limit is a torque decay of less than 15 % from the original capping torque. For UN-certified jerricans, the complete package is validated by the applicable UN drop test, stacking test, and leakproofness test. Weld-line integrity is tested according to ASTM D638-14 on specimens cut perpendicular to the handle pinch-off seam; the yield stress at the weld should reach at least 80 % of the parent wall value. Values below 60 % are traced to insufficient melt temperature, excessive clamping dwell, or contamination at the pinch edge. The operational limitation is that 5200B is not used with diketonitrile-containing formulations having high free acidity unless an internal barrier or fluorination is applied. A non-standard but widely used screening method stores filled containers at 50 °C for 30 days with a 10 % nonionic surfactant solution; this test detects environmental stress cracking earlier than standard ESCR coupons.

    Marine floats and sectional water tank liners made from Sinopec Yanshan HDPE 5200B are evaluated by long-term hydrostatic stress, not by short-term tensile flow. A cylindrical float with a nominal wall thickness of 3 mm to 5 mm is blown at a blow-up ratio of 1.8:1 to 2.4:1, which preserves hoop-direction wall uniformity. Long-term hydrostatic design basis is determined under ISO 9080:2022 on compression-molded or extruded plaques, and the design stress is held below the 10,000 h extrapolated creep rupture value by a safety factor of 1.6 to 2.0. Outdoor exposure demands carbon black content of 2.0 % to 2.5 % by mass, verified by ISO 6964:2019, because unstabilized high-density polyethylene can embrittle within 18 to 24 months in subtropical UV environments. When potable water contact is required, compliance with FDA 21 CFR 177.1520 and NSF/ANSI 61 is verified on the finished article. The flange weld line is an operational limitation: molded-in stress at the flash removal region has led to crack initiation in continuous wave loading after approximately 5,000 cycles when the rib radius is below 2 mm. Published data for 5200B in marine float service is limited, so a design verification test using ASTM D1693-15 on stressed compression-molded sheets is applied as a conservative material screen.

    Battery Acid Container Wall Thickness and Pinch Weld Integrity in 35 % Sulfuric Acid

    Containers blown for 35 % sulfuric acid service use 5200B because the grade resists mineral acid at ambient temperature. For a container with 35 % sulfuric acid at specific gravity 1.26, the minimum wall thickness is set at 1.2 mm at the sidewall and 2.0 mm at the bottom corners, providing a safety factor against drop impact and internal pressure at 40 °C. Short-term chemical resistance is screened by ASTM D543-20 Method B, but long-term compatibility is better correlated with ASTM D1693-15 because the stressed surface accelerates oxidative and acid-induced crack growth. The bottom pinch-off weld is the dominant failure site if parison melt temperature falls below 190 °C, because high-molecular-weight HDPE does not fuse adequately at low temperature. The blow pin is purged with dry air to avoid condensation of sulfuric acid fog, and the mold is vented at the parting line to prevent trapped gas from generating microporosity in the weld. Containers with visible weld-line roughness should not be filled. Concentrated nitric acid, hydrogen peroxide blends, and acid service above 60 °C are outside the compatibility range of this grade. Published data for 5200B in battery acid container service is limited, so each mold lot is tested by a 1 m drop after filling and by a 30 kPa internal leak test.

    Compliance checklist for 220 L L-ring drums blown from Sinopec Yanshan HDPE 5200B
    Test or propertyStandardResult criterion
    Melt flow indexISO 1133-1:20220.25–0.35 g/10 min at 190 °C, 2.16 kg
    DensityISO 1183-1:20190.950–0.954 g/cm³
    ESCRASTM D1693-15 Condition BLot-dependent; verify against specified minimum
    Drop testUN 6.1.5.3No leakage after -18 °C drop
    Stacking testUN 6.1.5.6No rupture after 28 days at 40 °C
    LeakproofnessUN 6.1.5.4No leak at 30 kPa internal air pressure
    Free Quote

    Competitive Sinopec Yanshan HDPE 5200B prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Yanshan HDPE 5200B is a high-density polyethylene extrusion blow-molding grade supplied in pellet form. The material is positioned in the low-MFR, high-density class used for rigid containers and industrial bottles. Density measured at 23 °C according to ISO 1183-1 is typically reported in the 0.949–0.953 g/cm³ interval. Melt mass-flow rate at 190 °C and 2.16 kg according to ISO 1133-1 is generally below 0.50 g/10 min, with many certificate-of-analysis values near 0.30 g/10 min. These values describe the product class and are not a substitute for the supplier certificate of analysis.

    The designation 5200B is commonly referenced in extrusion blow-molding feasibility studies because the melt-flow class balances processability with end-use rigidity. The low melt index indicates elevated molecular weight and higher zero-shear viscosity compared with general-purpose injection-molding HDPE grades. This viscosity characteristic supports a melt that can sustain its own weight during parison formation. Containers with relatively deep draw and large sidewall surfaces can therefore be molded with acceptable average wall thickness when blow pressure, pre-blow delay, and mold venting are matched to the resin.

    The resin is polymerized to produce high melt strength and a controlled molecular weight distribution for extrusion blow molding. It is not intended for blown film extrusion or thin-wall injection molding. In injection tools, the low melt index increases filling pressure and limits flow length. In blown film lines, it can reduce bubble stability and throughput. The product is therefore positioned as a dedicated blow-molding grade within the Yanshan HDPE family.

    Typical applications include blow-molded containers for industrial chemicals, detergents, lubricants, agricultural formulations, and certain household products. Container capacities are commonly below 30 L. The grade is suited to applications where parison hang time, pinch-off integrity, and uniform wall thickness are production-critical. It is not recommended for small-mouth bottles requiring high-speed reciprocating screw injection-blow molding, or for thin-film packaging.

    Service conditions influence selection. Continuous contact with strong oxidizing acids, aromatic hydrocarbons, or chlorinated solvents should be avoided unless compatibility testing is completed. HDPE environmental stress-cracking resistance can be reduced by polar wetting agents and certain detergents; design stress and service temperature should be validated using an ESCR test such as ASTM D1693.

    What limits parison hang time when 5200B is processed on accumulator-head machines?

    Melt temperature is the primary control variable. On accumulator-head machines with screw L/D ratios of 24:1 to 30:1, processing is commonly established at melt-temperature set points between 180 °C and 210 °C. The lower boundary maintains viscosity and reduces parison sag, but raises screw torque, backpressure, and die-head pressure. The upper boundary lowers viscosity and may increase parison length variation. Process-capability data from production-scale lines indicate that wall-thickness uniformity can degrade if melt-temperature variation exceeds ±5 °C. Operators often adjust the temperature profile in 5 °C steps while measuring die-head pressure and parison length.

    Die geometry is equally significant. For containers below 30 L, the die gap is typically set between 0.8 mm and 1.5 mm. Wider gaps reduce shear heating but increase shot weight per stroke and can reduce surface finish. Narrower gaps improve surface quality but raise the risk of melt fracture and excessive shear. Multi-point parison programming is used to compensate for sag and to increase pinch-off thickness at the bottom of the container. If the die gap exceeds 2.0 mm, programming can become insufficient for shot volumes above 5 L. Published data for this specific configuration is limited; the admissible die gap should be confirmed on the target blow-molding line.

    Pre-drying of 5200B is not normally required for material stored in closed bags at ambient humidity. If pellets are exposed to relative humidity above 60% or condensation, surface moisture can enter the feed throat and cause splay or small bubbles in the molded surface. A desiccant hopper dryer at 80 °C for 2 h is usually sufficient. Drying above 90 °C should be avoided because pellet agglomeration can occur in hopper dryers and disrupt feed.

    Accumulator-head machines processing 5200B are generally operated with barrel profile temperatures rising from 170 °C near the feed throat to 200 °C at the metering section, with the head and die maintained at 190–210 °C. These values are starting points, not specifications. Screw speed is set to avoid shear heating above 10 °C over the melt set point. If actual melt temperature exceeds the setpoint by more than 10 °C, screw speed or backpressure should be reduced. The melt cushion in the accumulator should be kept stable, and shot size should be controlled so that first-in-first-out melt displacement is not disturbed.

    Mold design for 5200B follows HDPE extrusion blow-molding practice. Pinch-off lands should be sharp enough to produce a clean weld; excessive radius can create a weak tail and increased regrind. Blow-pin and neck-finish dimensions must follow applicable finish standards. Production experience on shuttle machines shows that insufficient clamp force at the parting line generates flash and uneven bottom welds. Containers below 5 L are commonly blown with clamp forces of 5–15 tons; larger jerry cans may require clamp forces above 25 tons. Mold temperatures between 10 °C and 25 °C are typical; chilled-water control reduces cycle time but may increase visible flow lines if the mold surface is not polished or textured to the correct depth.

    Lot-Release Property Verification and Standardized Test Methods

    The following matrix lists physical and mechanical properties commonly requested for 5200B when qualifying material for a blow-molded application. The table does not constitute a specification; each lot must be verified against the current supplier certificate of analysis.

    PropertyTest methodTypical class range or condition
    DensityISO 1183-10.949–0.953 g/cm³ at 23 °C
    Melt mass-flow rateISO 1133-1<0.50 g/10 min at 190 °C/2.16 kg; lot average near 0.30 g/10 min
    Tensile yield stressISO 527-224–28 MPa at 50 mm/min
    Nominal tensile elongation at breakISO 527-2>500%
    Flexural modulusISO 178850–1100 MPa at 2 mm/min
    Charpy notched impact strengthISO 179-1/1eA>20 kJ/m² at 23 °C
    Environmental stress-cracking resistanceASTM D169310% Igepal CO-630, 50 °C; failure time is condition-dependent

    The tensile and flexural intervals are representative of the melt-flow class and are not guaranteed lot-average values. Lot-release certificates for 5200B may report density, MFR, tensile yield stress, and optionally ESCR; flexural modulus and impact strength are frequently type-test values rather than lot-release tests. Users should request the full technical datasheet and specify the test method revision when comparing suppliers.

    Mechanical property verification should be performed on compression-molded plaques or cut specimens from molded containers, depending on the failure mode under investigation. The ISO 527-2 tensile test is usually run at 50 mm/min with specimen type 1A. Flexural modulus per ISO 178 is measured at 2 mm/min on 4 mm thick specimens. Charpy impact tests per ISO 179-1/1eA use a V-notch. Environmental stress-cracking resistance is typically evaluated by ASTM D1693 under 10% Igepal CO-630 at 50 °C; failure times are strongly dependent on specimen thickness, molding history, and internal stress. For that reason, ESCR data should not be compared across laboratories unless the complete test condition is reported.

    For food-contact applications, the base olefin polymer may meet the compositional requirements of FDA 21 CFR 177.1520 and EU Regulation 10/2011; however, food-contact compliance is not an inherent property of the product. The molded container must be tested under the intended food simulant, time, and temperature conditions. Users should obtain written lot-specific compliance statements from the supplier before commercial food use.

    For industrial packaging, material safety data and regulatory declarations should be supplied with each shipment. The base HDPE grade is expected to be compliant with the substance restrictions in EU RoHS Directive 2011/65/EU and with the registration requirements of REACH; however, these declarations must be verified for the specific production site and grade. When packaging is intended for export, the user should confirm food-contact or product-contact compliance under the destination market’s national regulations.

    When regrind from 5200B is reprocessed in a closed-loop container line

    Regrind utilization is standard in extrusion blow molding. For 5200B, closed-loop regrind from trimmed tails, flash, and defective bottles can be re-introduced at levels commonly up to 30 wt%; higher levels may require validation because the melt index can shift due to thermal history and contamination. Granulators with screen-hole diameters of 6–8 mm are often used to limit fines. Dust and fines below 1 mm should be minimized because they melt unevenly and can form visible specks in the molded surface.

    The melt flow of recycled 5200B should be monitored against the virgin lot by ISO 1133-1 or ASTM D1238. A shift greater than 0.05 g/10 min from the virgin lot average indicates the need to reduce regrind ratio, adjust melt temperature, or inspect contamination. In production-scale equipment, barrel pressure is also monitored as a surrogate for viscosity; a sustained pressure drop at constant screw speed and temperature suggests molecular-weight reduction or contamination.

    Mixing 5200B regrind with high-MFR HDPE injection grades, impact copolymers, polypropylene, or barrier polymers such as EVOH or nylon should not be performed without a defined end-use specification and compatibility testing. Incompatible barrier-layer scrap can produce parison delamination, reduced weld strength, and variable wall-thickness distribution.

    During shutdown, the extruder should be purged with a low-MFR HDPE to remove degraded material from the head and die. Restart procedures include a 15–30 min heat soak and slow screw rotation at 5–10 rpm before production speed is resumed. These practices reduce black specks and dimensional variation on start-up.

    Differences between 5200B and a high-MFR HDPE film or injection resin can be screened by melt-flow measurement. Film-extrusion grades in the Yanshan family often have MFR values near 0.8–1.2 g/10 min to promote bubble stability and drawdown; injection grades commonly exceed 4 g/10 min to fill molds. Substituting 5200B into a blown film line generally raises melt pressure and reduces output. Substituting a film grade into a blow molder reduces parison hang time and may increase sidewall thinning. Therefore, a comparative trial on the target line remains the only reliable method when changing melt-flow class.

    Some high-density blow-molding grades are optimized for ESCR by increasing comonomer content or broadening molecular weight distribution. These changes can reduce density and flexural modulus. 5200B is typically specified where the balance of stiffness and melt strength is acceptable for industrial containers. If the product must withstand aggressive surfactant solutions, a dedicated ESCR-optimized grade may be required; ASTM D1693 data should be used for comparison.

    The user should verify the current technical datasheet and certificate of analysis before designing molds or specifying equipment. The processing window should be confirmed with the actual lot, particularly for containers with wall thickness below 0.6 mm, large flat panels, or capacities above 30 L. Operation outside the validated melt-temperature band or regrind ratio may increase rejects from wall-thickness variation, weld-line weakness, and stress-cracking at the pinch-off.