Sinopec Yanshan HDPE 1620J is a high-density polyethylene injection-moulding grade produced by Sinopec Beijing Yanshan Company. The product is specified for thin-wall packaging, caps and closures, housewares, toys, and open-top crates. Its nominal melt mass-flow rate is 16 g/10 min at 190 °C/2.16 kg when tested to ISO 1133-1:2022, and its nominal density is 0.962 g/cm³ when tested to ISO 1183-1:2019. These two values place 1620J in the high-flow, medium-density segment of the Yanshan HDPE range, where spiral-flow length, stiffness, and cooling-limited cycle time govern manufacturing economics.
The grade is supplied as pellets and is typically pigmented or compounded downstream. Published data for the exact additive package of 1620J is limited; certificates of analysis for each production lot should be obtained before running colour-critical or hot-runner multi-cavity tools. Surface moisture on pellets stored above 60% RH can produce splay or silver streaks in moulded parts. Desiccant predrying at 70 °C for 1 h to 2 h with a dew point not higher than -20 °C is applied where surface appearance is critical.
Moisture absorption of HDPE is below 0.01% by weight after 24 h immersion at 23 °C according to ISO 62:2008; therefore, predrying is required only for surface moisture, not for bulk hydrolysis. This distinguishes HDPE from polyesters and polyamides, where drying is driven by hydrolysis kinetics.
What Are the Nominal Property and Test Standard Matrix for HDPE 1620J?
The following characterisation matrix summarises nominal release values and test methods used for HDPE 1620J. Values are not design minima; they represent typical production data and are subject to lot-to-lot variation.
| Property | Nominal value | Test method |
|---|---|---|
| Melt mass-flow rate, 190 °C/2.16 kg | 16 g/10 min | ISO 1133-1:2022 |
| Density | 0.962 g/cm³ | ISO 1183-1:2019 |
| Tensile yield stress | 26 MPa | ISO 527-2:2012 |
| Tensile elongation at break | ≥80% | ISO 527-2:2012 |
| Flexural modulus | 1,100 MPa | ISO 178:2019 |
| Notched Izod impact strength at 23 °C | 3.5 kJ/m² | ISO 180:2019 |
| Vicat softening temperature, A50 | 124 °C | ISO 306:2022 |
| Shore D hardness | 65 | ISO 868:2003 |
| Linear mould shrinkage | 1.5% to 2.5% | ISO 294-4:2018 |
Lot-to-lot melt-flow variation is typically controlled within ±1 g/10 min, and density variation is typically controlled within ±0.002 g/cm³. Converters running narrow-gate hot-runner tools below 0.8 mm gate diameter should evaluate each lot because small melt-viscosity shifts can alter gate freeze-off time and part mass.
Injection Moulding Parameters, Melt Temperature Limits, and Short-Shot Prevention on Injection Lines
On general-purpose injection moulding machines with screw L/D ratios of 20:1 to 24:1 and compression ratios of 2.5:1 to 3.0:1, the melt temperature for 1620J is typically set between 190 °C and 230 °C. A practical melt-temperature control window of ±5 °C around 210 °C is used on thin-wall production lines because larger excursions alter fill viscosity and cushion stability. Below 180 °C, incomplete homogenisation has been observed as flow-line visibility in sections thinner than 0.8 mm. Above 240 °C, oxidative degradation may occur when melt residence time exceeds 5 min, producing yellowing and an acrid odour.
Hydraulic injection pressures of 60 MPa to 90 MPa are typical for single-cavity moulds with 1.5 mm nominal wall thickness. For 0.6 mm thin-wall containers, peak pressures up to 120 MPa may be required depending on gate geometry and flow length. Mould temperature is generally held between 20 °C and 50 °C. The lower bound shortens cooling time but increases shrinkage anisotropy; the upper bound reduces warpage in flat lids and shallow containers at the cost of longer cycle time.
Back pressure is normally set between 0.5 MPa and 1.0 MPa, with screw surface speeds of 0.3 m/s to 0.5 m/s. Back pressure above 1.5 MPa increases melt temperature and can reduce the cycle-time advantage of the high-flow grade. Screw recovery should be completed within the cooling phase; a cushion of 3 mm to 6 mm is typically maintained to stabilise hold pressure. In machines with shot size below 25% of barrel capacity, residence-time distribution broadens and degradation risk increases; a smaller barrel or higher utilisation is preferred.
Rheometer measurements show pseudoplastic behaviour: apparent viscosity falls as shear rate increases from 100 s⁻¹ to 1,000 s⁻¹. Melt pressure sensors in the nozzle are more reliable than barrel set points for detecting viscosity shifts because actual melt temperature is influenced by screw speed, back pressure, and residence time. For semicrystalline HDPE, gate diameter should be 50% to 75% of the part wall thickness; tunnel gates below 0.6 mm can cause premature gate freeze-off and require excessive packing pressure.
Linear mould shrinkage for 1620J is reported in the range 1.5% to 2.5%, measured according to ISO 294-4:2018. Thin sections cooled rapidly at low mould temperatures tend to shrink less in the flow direction and more in the transverse direction, producing warpage in rectangular lids. Raising mould temperature towards 50 °C reduces this anisotropy but increases cooling time. For bosses with thickness above 3 mm, short surface solidification can trap sink marks; gas counterpressure or longer pack time is used when surface flatness is critical.
Weld-line strength in high-flow injection grades is generally lower than in lower-flow grades because rapid quenching reduces interdiffusion at the melt front. For HDPE, weld-line strength retention of 60% to 80% relative to the unwelded value is commonly cited in ISO 527-2 tensile tests. Parts with structural bosses or snap-fit features should be gated so that weld lines are placed away from high-stress regions.
For hot-runner multi-cavity production with valve gates, the low melt viscosity at shear rates above 1,000 s⁻¹ means that gate freeze-off time, not melt temperature alone, controls part mass. In a 32-cavity hot-runner mould with part mass below 15 g, short-shot prevention requires balanced gate diameters and an injection velocity profile with a controlled fast-fill phase followed by a low-velocity pack. Published data for this specific configuration is limited, but production-scale trials indicate that fill-time variation above 0.1 s across cavities can produce part-mass variation above 1.5%.
How Does 1620J Differ From Other Sinopec Yanshan HDPE Grades?
1620J differs from film and blow-moulding grades in the Yanshan HDPE range primarily in melt-flow rate and molecular weight distribution. A film grade such as 5000S is typically reported at 0.9 g/10 min with density of 0.954 g/cm³; its higher melt strength is required for bubble stability in blown film. If 1620J were processed on blown-film equipment, low melt strength would produce bubble instability and unacceptable gauge variation. Similarly, large-part blow-moulding grades such as 7600M have lower melt flow and higher melt strength to limit parison sag; 1620J is not a direct substitute.
Within injection-moulding grades, 2200J is typically cited at 5.5 g/10 min with density of 0.968 g/cm³. The lower melt flow of 2200J gives higher melt pressure and may be selected for thicker-wall crates requiring greater stiffness and impact resistance, whereas 1620J is selected for thin-wall articles where fill pressure and cycle time are limiting. The grade 1600J is often listed with similar nominal melt flow and density to 1620J; direct comparative data in public literature is limited, and converter trials are used to distinguish lot-to-lot additive behaviour, colour shift, and warpage in flat lids.
Because the published nominal melt flow of 1600J and 1620J can overlap, selection between the two should not be made solely from melt-flow index. Differential scanning calorimetry, flexural modulus, and moulded-part shrinkage at 50 °C mould temperature provide a more useful basis. High-flow injection grades generally have narrower molecular weight distribution and lower weight-average molecular weight than blow-moulding grades, producing lower zero-shear viscosity and lower melt strength.
During start-up and material changeover, 1620J should not be processed after PVC residues without thorough purging. At processing temperatures, PVC can liberate hydrogen chloride and catalyse polyethylene chain scission. The grade is incompatible with strong oxidising agents and should not be stored in direct sunlight for prolonged periods. Machine shutdown procedures should avoid holding the melt above 230 °C for more than 10 min. Purging with a low-density polyethylene or a dedicated purging compound is used to remove degraded material from barrel and hot-runner dead spots.
When Food-Contact and Hazardous-Substance Compliance Govern Material Selection
Food-contact status for HDPE 1620J is evaluated under GB 4806.7-2016 for plastic materials and articles in contact with foodstuffs, FDA 21 CFR 177.1520 for olefin polymers, and EU Regulation (EU) No 10/2011 as amended. Compliance is formulation-specific: the base resin may meet the relevant framework, but converters must verify overall migration, specific migration of additives, and sensory properties on the finished article. A compliance matrix for common regulatory instruments is provided below.
| Regulatory instrument | Assessment scope | Typical converter verification |
|---|---|---|
| GB 4806.7-2016 | Food-contact plastic materials and articles | Overall migration, potassium permanganate consumption, heavy metals as specified |
| FDA 21 CFR 177.1520 | Olefin polymers | Density ≥ 0.94 g/cm³ and extractables limits per subpart B |
| EU Regulation (EU) No 10/2011 | Plastic materials in contact with food | Overall migration limit 10 mg/dm²; specific migration limits per Annex I |
| REACH Regulation (EC) No 1907/2006 | Substances of very high concern | Candidate List concentration threshold 0.1% w/w |
| RoHS Directive 2011/65/EU | Electrical and electronic equipment | Pb 0.1%, Hg 0.1%, Cd 0.01%, Cr(VI) 0.1%, PBB 0.1%, PBDE 0.1% |
RoHS and REACH compliance are not automatic for all colourants and processing aids added downstream. The final article may require separate testing under the specific packaging material category. Published data for the highly specific migration behaviour of 1620J in fatty food simulants is limited; for fatty food contact, the converter should commission migration testing under the intended time-temperature conditions.
At the end of processing, regrind from 1620J can be re-introduced into injection moulding at controlled levels; the maximum acceptable regrind fraction depends on part thickness, impact requirements, and food-contact status. Post-consumer recycled HDPE is not a direct substitute for virgin 1620J without re-qualification of density, melt-flow rate, and contamination under ISO 1133-1:2022 and ISO 1183-1:2019.