| HS Code | 872384 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate | 0.04 g/10 min |
| Tensile Strength At Yield | ≥28 MPa |
| Elongation At Break | ≥600% |
| Vicat Softening Point | ≥125°C |
| Melting Point | 130-135°C |
| Brittleness Temperature | ≤-70°C |
| Environmental Stress Cracking Resistance | >1000 h |
| Ash Content | ≤0.03% |
| Moisture Content | ≤0.1% |
| Haze | ≤12% |
| Dart Impact Strength | ≥200 g |
As an accredited Sinopec Yangzi HDPE 7000F factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Yangzi HDPE 7000F is packaged in 25 kg polyethylene-lined woven bags, 1000 kg per pallet for industrial use. |
| Container Loading (20′ FCL) | Sinopec Yangzi HDPE 7000F loaded in 20′ FCL containers, typically 25MT in 25kg bags, palletized or loose, secure dry transport. |
| Shipping | Sinopec Yangzi HDPE 7000F is a non-hazardous, film-grade high-density polyethylene resin. It is usually shipped by sea or truck in 25 kg PP woven bags or jumbo bags, palletized and stretch-wrapped. Standard 20'FCL loads about 18–20 MT. Store/transport cool, dry, ventilated, away from moisture, sunlight, heat, and ignition sources. |
| Storage | Store Sinopec Yangzi HDPE 7000F in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, moisture, heat, and ignition sources. Keep original bags sealed on pallets, off the floor, and protect from sharp objects, heavy stacking, oils, chemicals, and strong oxidizers. Do not expose to UV or excessive temperatures. Maintain good housekeeping and follow first-in, first-out stock rotation. |
| Shelf Life | Typically 24 months from production when stored in original unopened packaging, dry, cool, and protected from direct sunlight. |
Mono-layer blown film lines converting Sinopec Yangzi HDPE 7000F into thin-gauge retail carrier bag film are typically operated with melt temperatures of 190°C to 215°C, a spiral mandrel die gap of 1.2 mm to 1.8 mm, and blow-up ratios between 3.5:1 and 5.0:1; these settings affect machine-direction tear resistance and bubble stability in final film thicknesses of 8 µm to 18 µm. Lot release criteria for the resin include nominal density of 0.956 g/cm³ and melt flow rate of 0.04 g/10 min at 190°C under 2.16 kg load, measured by ISO 1183-1:2019 and ISO 1133-1:2022. Where direct food contact is intended, the converter is responsible for demonstrating conformity under FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 Annex I; otherwise, retail packaging and dry indirect contact are assessed through the same conformity framework on a lot-specific basis. In industrial formulations, HDPE 7000F is charged at 92 wt% to 100 wt% of the polymer phase, with the remaining 0 wt% to 8 wt% comprising a slip/antiblock masterbatch based on a compatible HDPE or LLDPE carrier; exact masterbatch loading is confirmed by coefficient of friction under ASTM D1894 and blocking load under ASTM D3354, not by nominal supplier recommendation alone. The downstream production process is single-stage blown film extrusion followed by inline conversion consisting of sealing, cutting, and handle die-cutting; no post-extrusion curing or conditioning step is required. Production-scale grooved-feed extruders with L/D 30:1 to 36:1 and screw speeds above 60 rpm exhibit bubble flutter when the frost line is moved beyond 5% of the stable operating height, and die-lip deposit formation accelerates when melt temperature exceeds 220°C at prolonged residence. Terminal finished product types are vest-style retail carrier bags, produce bags, and thin-gauge promotional sacks.
In PCR-rich refuse sack film production, post-consumer recycled high-density polyethylene streams from rigid bottle and film recovery introduce molecular weight degradation, residual polyolefin immiscibility, and non-melt contamination that broadens molecular weight distribution and increases melt fracture sensitivity. Sinopec Yangzi HDPE 7000F is metered into PCR-rich formulations at 25 wt% to 45 wt% to raise melt strength and stabilize bubble geometry, although published data for this exact grade and PCR configuration is limited; the precise ratio is therefore determined by measuring the PCR melt flow rate drift according to ISO 1133-1:2022 and by monitoring bubble lay-flat width variation. Compliance for recycled-content refuse sacks and bin liners is governed by REACH Article 33 communication obligations for substances of very high concern, EU Packaging and Packaging Waste Directive 94/62/EC Annex II heavy metal concentration limits, and EU Regulation 2022/1616 when recycled materials are used in food-contact exterior applications. The production process combines a co-rotating twin-screw compounding extruder with L/D 40:1, vacuum venting at −0.08 MPa, and melt temperature control at 200°C to 215°C; HDPE 7000F is added through a separate gravimetric feed at the selected ratio to avoid pre-mix contamination. Compounded pellets are then converted on a blown film line with a 200 mm die, 1.2 mm die gap, and screen packs of 80/100/80 mesh; pre-drying of PCR flake at 80°C for 2 h is applied only when moisture content exceeds 0.1 wt% to prevent steam-surface defects caused by incidental PET or cellulosic contamination. Terminal finished product types are post-consumer recycled refuse sacks, bin liners, and heavy-gauge shopping bags carrying PCR content claims.
Three-layer coextruded structures for dry food pouches position HDPE 7000F as the core layer at 60 wt% to 75 wt% of total film weight, while LLDPE or LDPE skin layers supply heat sealing and hot-tack performance. Where direct food contact is intended, conformity is assigned to EU Regulation 10/2011 Annex II overall migration limit of 10 mg/dm² and FDA 21 CFR 177.1520(c) 2.1 for dry and aqueous food types; additive migration must be evaluated under EU Regulation 10/2011 Annex III food simulant assignments rather than assumed from resin compliance alone. The production process uses three extruders feeding a multi-layer spiral mandrel die, with the core extruder configured with L/D 30:1 and barrier mixing elements at 190°C to 220°C, while skin extruders operate at 180°C to 210°C to limit viscosity mismatch at the die exit. Interlayer stability is preserved when the skin/core viscosity ratio remains below 1.8:1 under high-shear conditions; line audits record bubble breaks when adapter-to-die temperature differentials exceed 8°C. The core layer addition of HDPE 7000F at 60 wt% to 75 wt% supports tensile modulus performance measurable under ISO 527-3, while the skin layers are maintained at 25 wt% to 40 wt% to permit jaw sealing at 120°C to 160°C and 0.3 MPa to 0.6 MPa sealing pressure. Terminal finished product types are dry-food pouches, cereal liner films, and institutional folding-pack overwrap.
At production speeds above 80 cycles/min, high-speed form-fill-seal and automatic bagging lines evaluate HDPE 7000F through film-to-metal coefficient of friction and blocking resistance because any slip failure appears as seal jaw sticking or web tracking loss. Sinopec Yangzi HDPE 7000F is formulated at 95 wt% to 99 wt% with a synthetic silica or calcium carbonate masterbatch at 1 wt% to 5 wt% to reduce blocking; the addition ratio is validated by ASTM D3354 blocking load and ASTM D1894 kinetic COF, with industrial targets normally below 0.30 coefficient of friction, although published data for this exact resin grade under specific masterbatch chemistries is limited. Regulatory compliance for packaging of non-food consumer goods follows REACH Annex XVII substance restrictions and EU Packaging Directive 94/62/EC Article 11 limits for cadmium, mercury, lead, and hexavalent chromium. The downstream production process is blown film extrusion followed by in-line slitting and corona discharge at 38 mN/m to 44 mN/m to ensure print adhesion for automated barcode scanning; process settings include a dual-lip air ring and internal bubble cooling to hold frost line height within 2 to 3 die diameters. Production-scale failure modes include gauge bands when oscillating haul-off calibration drifts and seal contamination when slip additive migration exceeds film surface saturation. Terminal finished product types are automatic packaging wrap for non-woven goods, mail-order garment bags, and high-speed magazine overwrap.
| Downstream scenario | Primary regulatory/standard anchor | Process verification method | HDPE 7000F addition ratio | Finished product type |
|---|---|---|---|---|
| Mono-layer retail carrier bag film | ISO 1183-1:2019; ISO 1133-1:2022; FDA 21 CFR 177.1520(c); EU 10/2011 | ASTM D1894; ASTM D3354 | 92–100 wt% | Vest carrier bags, produce bags |
| PCR-rich refuse sack film | REACH Article 33; EU 94/62/EC Annex II; EU 2022/1616 | ISO 1133-1:2022; bubble stability audit | 25–45 wt% | PCR refuse sacks, bin liners |
| Three-layer dry-food pouch core | EU 10/2011 Annex II; FDA 21 CFR 177.1520(c) 2.1 | ISO 527-3; seal strength testing | 60–75 wt% | Dry-food pouches, cereal liners |
| High-speed automatic packaging film | REACH Annex XVII; EU 94/62/EC Article 11 | ASTM D1894; ASTM D3354 | 95–99 wt% | Garment bags, magazine overwrap |
| Flexible intermediate bulk container liner | ISO 21898; EU 10/2011 | Gauge profile; seal integrity test | 98–100 wt% | FIBC liners, drum liners |
For flexible intermediate bulk container liner film, thick-gauge blow film tubes of 50 µm to 100 µm are produced from Sinopec Yangzi HDPE 7000F at blow-up ratios of 1.5:1 to 2.5:1; the lower blow-up ratio reduces machine-direction/cross-direction shrinkage anisotropy relative to retail carrier bag film, but requires a wider die gap of 1.8 mm to 2.2 mm and haul-off tension below 6 N/mm to compensate for higher machine-direction orientation. Compliance is set by ISO 21898 for flexible intermediate bulk containers for non-dangerous goods, with additional food-contact conformity under EU Regulation 10/2011 when the liner contacts dry food ingredients; dangerous goods applications require UN performance certification on the complete filled container, not on the liner film alone. The formulation addition ratio is 98 wt% to 100 wt% HDPE 7000F with 0 wt% to 2 wt% antioxidant/processing stabilizer masterbatch; slip and antiblock additives are omitted because their migration to the film surface can reduce heat-seal seam integrity at the liner bottom. The production process uses blown film extrusion with internal bubble cooling, gusseting in-line, and optional corona treatment of 36 mN/m to 40 mN/m only when surface printing is required; production-scale observations record film-blocking defects when line speed is increased without corresponding adjustment of cooling air temperature and internal bubble pressure. Terminal finished product types are FIBC inner liners, drum liners, and pallet containment tubes.
Competitive Sinopec Yangzi HDPE 7000F prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Yangzi HDPE 7000F is a high-density polyethylene resin produced by Sinopec Yangzi Petrochemical Company Limited. The grade is supplied as white translucent pellets and is intended primarily for high-strength blown film extrusion. Typical melt mass-flow rate, determined according to ISO 1133-1:2022 at 190 °C under 2.16 kg, is 0.04 g/10 min. Typical density, determined according to ISO 1183-1:2019, is 0.956 g/cm³. The product is differentiated from general-purpose HDPE film grades by its bimodal molecular weight distribution and high molecular weight fraction, which increase melt strength, bubble stability, and finished film tensile properties at thin gauges. Primary downstream usage includes T-shirt carrier bags, refuse sacks, liners, and industrial packaging films; it is also used in multilayer coextruded films where the HDPE layer contributes stiffness, moisture barrier, and down-gauging potential relative to low-density polyethylene and linear low-density polyethylene layers.
Typical resin-fixed characteristics reported for Sinopec Yangzi HDPE 7000F are listed below. Film property values remain dependent on processing conditions, gauge, blow-up ratio, and additive masterbatches.
| Property | Test method | Reported typical value |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022, 190 °C/2.16 kg | 0.04 g/10 min |
| Density | ISO 1183-1:2019 | 0.956 g/cm³ |
| Tensile strength at yield | ISO 527-2:2012 | 24 MPa |
| Elongation at break | ISO 527-2:2012 | >600% |
Processing of Sinopec Yangzi HDPE 7000F requires blown film equipment capable of managing high melt viscosity and high extrusion pressures. Single-screw extruders with grooved feed sections and screw lengths of 25:1 to 30:1 L/D are typically specified. Barrel temperature profiles are usually set from 180 °C to 210 °C, with melt temperature maintained between 190 °C and 230 °C. Operation below 190 °C increases the risk of melt fracture and die-pressure instability, while sustained operation above 230 °C can initiate oxidation, gel formation, and discoloration. The die gap for high molecular weight HDPE film is generally wider than that used for LLDPE; die gaps of 1.2 mm to 1.8 mm are typical. Blow-up ratio is commonly held between 3:1 and 5:1. Frost line height is normally set at 5 to 9 die diameters, depending on gauge and bubble stability requirements. Head pressure on a 90 mm grooved-feed extruder can reach 30–50 MPa depending on screw speed, screen pack configuration, and melt temperature. Because of the low melt flow rate, backpressure and motor load are higher than with conventional film HDPE grades with melt flow rates of 0.3–1.0 g/10 min. Screen packs using 80–120 mesh breaker plates reduce gel-related pinholes but increase pressure and residence time.
Melt temperature should be confirmed using a calibrated melt thermocouple in the adapter or die, not inferred from barrel set points alone. Screw cooling is often required to control frictional heat in the feed zone. Output rates are governed by torque, motor capacity, and melt pressure limits; a 90 mm extruder with a 30:1 L/D grooved-feed screw may operate in a 180–260 kg/h range depending on die diameter, frost line height, and downstream conversion requirements. Published data for output on smaller lines is limited, and converter trials are required to determine specific throughput windows.
No pre-drying is required for HDPE 7000F under normal warehouse conditions. If pellets are stored at relative humidity above 60% and transferred into a warm production area, surface condensation can occur. Surface moisture is not absorbed into the polymer matrix but can produce pinholes and bubble instability. Pellets exposed to condensation should be air-purged at ambient temperature or passed through a dehumidified hopper before extrusion. Avoid halogenated cleaning agents and strong oxidizing cleaners in contact with the pellet feed system.
Differences from lower-viscosity HDPE film grades are most evident in pressure, torque, and bubble cooling. 7000F does not process as a drop-in replacement on lines optimized for LLDPE because the neck height and bubble shape differ. Higher melt strength allows a taller bubble and higher blow-up ratios without collapse, but air-ring cooling must be sufficient to stabilize the high molecular weight film. Internal bubble cooling is advisable at outputs above 200 kg/h for gauge control and frost line consistency.
The bimodal molecular weight distribution of Sinopec Yangzi HDPE 7000F contributes to high melt strength and environmental stress crack resistance. The low molecular weight fraction improves processability, while the high molecular weight fraction increases toughness and tear resistance. This architecture produces a shear-thinning response that is more pronounced than in unimodal HDPE grades. Gel count and film appearance are sensitive to extrusion temperature, residence time, and screen pack condition. Gels arising from excessive residence time or dead spots in the die can appear as undispersed fish-eye defects in thin film. Extruder and die design should minimize stagnation zones. Periodic purging with a HDPE purge compound or a commercial polyolefin purging agent is recommended after prolonged residence above 230 °C.
Film appearance is also influenced by die lip cleanliness and die gap uniformity. Die lines from damaged or worn lips cannot be corrected by temperature adjustment. Die gap should be verified with feeler gauges to ensure concentricity within ±0.05 mm across the circumference. Melt fracture at the die exit can be reduced by increasing die gap, raising melt temperature, or lowering output. Excessive melt temperature above 230 °C is not recommended because it may increase oxidation gel and reduce film toughness. The oxidation induction time of the as-supplied resin is typically determined by ISO 11357-6, but the specific value should be confirmed from the current product datasheet.
Comparative gel count testing can be conducted using ASTM D3596 or internal camera-based gel counters on cast or blown film samples. Published data for gel count on this specific grade is limited, and converters should establish statistical process control limits based on their own extrusion line and re-grind fraction. Re-grind addition of 10–20 wt% from edge trim or start-up film is generally feasible if the re-grind is clean and not degraded. Higher re-grind levels reduce bubble stability and increase gel risk.
When 7000F is blended with LLDPE or LDPE, the blend morphology and film properties depend on screw mixing intensity and melt temperature. Low-shear screws may produce poor blend homogenization, leading to visible haze bands and inconsistent tear properties. Distributive mixing sections such as Maddock or pineapple mixers improve dispersion. Blend ratios must be verified against desired modulus, dart impact, and sealing performance; a 70/30 7000F/LLDPE blend may increase dart impact but reduce modulus and barrier properties compared with neat 7000F.
Blown film produced from 7000F typically exhibits higher stiffness and lower elongation than LLDPE film at equivalent gauge. The difference is measurable by tensile modulus using ISO 527-2:2012 or ASTM D882. Water vapour transmission rate is generally lower than for LDPE and many LLDPE films, but exact values should be measured using ASTM F1249 or ISO 15106-2. The coefficient of friction of 7000F film without slip additives is usually high; slip agent masterbatch is required for bag-making operations requiring low friction. Coefficient of friction is measured using ISO 8295 or ASTM D1894. Antiblock masterbatch addition is commonly required at 2–5 wt% to control blocking in wound film rolls, depending on film gauge and storage temperature.
Dart impact, Elmendorf tear, and puncture resistance are gauge-dependent and are strongly influenced by blow-up ratio and frost line height. Higher blow-up ratios tend to balance machine-direction and transverse-direction tear strength. A blow-up ratio of 4:1 to 5:1 is often used for refuse sacks and heavy-duty liners to improve TD tear. Dart drop impact can be tested according to ASTM D1709 Method A or ISO 7765-1. For film below 15 µm, pin-hole resistance and gel dispersion become more critical than resin-fixed mechanical properties. Published data for dart impact on this specific grade at very thin gauges is limited; converter-level film testing is required.
Replacement of a conventional unimodal HDPE film grade with Sinopec Yangzi HDPE 7000F typically requires machine-setting changes rather than a simple pellet substitution. Because the melt flow rate is lower, barrel temperature settings may need to be increased by 10–20 °C in the compression and metering zones. The die gap should be widened from typical LLDPE gaps of 0.8–1.2 mm to 1.4–1.8 mm. The blow-up ratio may need to be increased from 2.5:1–3:1 to 3.5:1–5:1 to maintain tear balance. The frost line height should be raised to provide additional melt relaxation and bubble stability. Motor load and die pressure usually increase by 20–40% relative to a 0.5–1.0 g/10 min HDPE film grade, depending on screw design and output.
Extruders with low-torque drives or shallow metering sections may not achieve acceptable output without excessive melt pressure. A grooved-feed extruder with a 25:1 L/D or longer screw and a high-torque gearbox is preferred. Barrier screws with spiral or cross-hole mixing sections improve thermal homogeneity and reduce gel-related defects. Conventional three-zone screws may be adequate for narrow processing windows but are less forgiving at high output.
The substitution is not appropriate for all film structures. In applications requiring high dart impact at freezer temperatures, an LLDPE-rich blend or a LLDPE/HDPE coextruded structure may be preferable. 7000F contributes stiffness, tensile strength, and moisture barrier but does not provide the low-temperature toughness of linear low-density polyethylene produced with metallocene catalysts. For frozen food packaging, the finished film must be tested for low-temperature dart impact and seal integrity using ASTM D1709 and ASTM F88 or ISO 527-3 as applicable.
Differences from other high-density polyethylene grades are also evident in sealing behaviour. HDPE 7000F has a higher melting temperature range than LDPE and lower hot-tack strength than many LLDPE grades. Heat-seal temperature settings on bag machines must be recalibrated. The heat-seal initiation temperature typically increases relative to LLDPE and LDPE. Seal strength testing should follow ASTM F88 or ISO 527-3. A pneumatic jaw sealer with controlled temperature and dwell time is required to obtain reproducible seal strength data.
For refuse sacks and liners, 7000F can permit down-gauging while maintaining tensile load capacity. However, down-gauging must be validated against puncture and tear requirements. A 20 µm film from 7000F may replace a 25 µm film from a lower modulus grade in stiffness-limited applications, but tear resistance and puncture resistance must be tested to ASTM D1922, ASTM D5748, or ISO equivalents before commercial substitution. Puncture resistance is particularly sensitive to film gauge and stress concentration at fold lines.
In coextruded structures, 7000F is commonly used as the core or outer layer for stiffness and moisture barrier. The die gap and extruder temperature profile for the HDPE layer must be independent of the LLDPE or LDPE layers. Coextrusion feedblocks and dies should be designed for viscosity mismatch; high-viscosity HDPE adjacent to low-viscosity LLDPE can produce interfacial instability if layer ratios or die geometry are not optimised. Melt temperature difference between adjacent layers should be controlled to avoid warpage and interfacial distortion.
Storage life of unconverted pellets is generally 12–24 months from production when stored in unopened original packaging at temperatures below 40 °C and away from direct sunlight. Prolonged exposure to ultraviolet light and heat can reduce the stabiliser package and shift the melt flow rate. Regrind must be kept free of paper, metal, and moisture. A metal detector and magnetic separator upstream of the extruder are recommended for high-speed bag lines to protect the screw and die from tramp metal damage.
Regulatory documentation for food-contact packaging should be obtained from the resin supplier and the final film converter. HDPE 7000F may be suitable for food-contact applications when the finished article complies with FDA 21 CFR 177.1520 for olefin polymers and EU Regulation (EU) No 10/2011 on plastic materials intended for food contact. Suitability depends on migration testing under the intended food simulants and temperature conditions. Compliance of the resin alone does not guarantee compliance of the final film, because additives, masterbatches, processing aids, and printing inks may also migrate. Downstream converters are responsible for verifying overall migration limits using EN 1186-1 and specific migration methods listed in Annex III of EU 10/2011. REACH and RoHS documentation should be obtained through the supply chain. The polymer itself is exempt from REACH registration as a polymer under Article 6(2) of Regulation (EC) No 1907/2006, but monomers and impurities used in its manufacture are subject to registration and supply-chain communication requirements.