Sinopec Yangzi Hdpe 5301b

Sinopec Yangzi HDPE 5301B

    • Product Name: Sinopec Yangzi HDPE 5301B
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 330719
    Density 0.954 g/cm³
    Melt Flow Rate 0.35 g/10 min
    Tensile Yield Strength ≥26 MPa
    Elongation At Break ≥500%
    Flexural Modulus ≥1100 MPa
    Notched Izod Impact Strength ≥25 kJ/m²
    Vicat Softening Temperature ≥125 °C
    Brittleness Temperature ≤-70 °C
    Shore D Hardness 65
    Environmental Stress Cracking Resistance ≥1000 h
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >1×10^16 Ω·cm
    Thermal Conductivity 0.42 W/m·K
    Melting Point 130-135 °C

    As an accredited Sinopec Yangzi HDPE 5301B factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Yangzi HDPE 5301B is supplied in 25 kg net polyethylene-lined woven bags, palletized for transport and storage.
    Container Loading (20′ FCL) Sinopec Yangzi HDPE 5301B in 20′ FCL: 25 kg bags, palletized or floor-loaded, shrink-wrapped, secured for ocean transport.
    Shipping Sinopec Yangzi HDPE 5301B is a non-hazardous high-density polyethylene resin. It is normally shipped in 25 kg bags or 500–1000 kg jumbo bags on pallets, inside containers. Not regulated as dangerous goods. Store dry, away from heat, moisture, and direct sunlight.
    Storage Store Sinopec Yangzi HDPE 5301B in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Place on pallets, not directly on floors. Avoid prolonged UV exposure and static accumulation. Maintain good housekeeping and comply with local regulations.
    Shelf Life Typical shelf life is 24 months when stored in a cool, dry, ventilated warehouse, away from direct sunlight and moisture.
    Application of Sinopec Yangzi HDPE 5301B

    In food-contact dairy and juice bottle production, Sinopec Yangzi HDPE 5301B is processed at a melt flow index of 0.30 g/10 min under ISO 1133-1:2022 and density 0.953 g/cm³ under ISO 1183-1:2019. Barrel temperatures are set from 170°C to 205°C, die head temperature is held at 185–205°C, and blow air pressure is controlled at 0.55–0.75 MPa; mould cooling circuits operate with water at 8–15°C to stabilise pinch-off and neck-trim geometry. Compliance is evaluated under FDA 21 CFR 177.1520(c) for direct-contact olefin polymers, Commission Regulation (EU) No 10/2011 Annex I with an overall migration limit of 10 mg/dm², and China’s GB 4806.6-2016 for food-contact plastic materials. The formulation ratio requires 100 wt% virgin 5301B; where a colorant is specified, a PE-based food-contact masterbatch is limited to ≤2 wt% and must be referenced against GB 9685-2016. Downstream processing uses continuous parison extrusion through a die gap of 1.5–2.5 mm with parison programming for wall-thickness control on handled bottles. Finished articles are 200 mL–1 L milk and juice bottles, 500 mL edible-oil bottles with 38 mm neck finishes, and light-scale food-service portion containers.

    How does environmental stress crack resistance influence detergent bottle formulations with HDPE 5301B?

    Household detergent, bleach, and fabric-softener containers produced from 5301B require environmental stress crack resistance because nonionic surfactants and hypochlorite act as stress-cracking agents at pinch-off seams and handle weld lines. Compliance for non-food household packaging rests on REACH Regulation (EC) No 1907/2006 Article 33, CLP Regulation (EC) No 1272/2008 for classified mixtures, and EC No 648/2004 for the detergent product itself; the polymer article is not subject to food-contact clearance but must not destabilise the filled formulation through component migration. The compound is charged at 95–98 wt% virgin 5301B with 2–5 wt% PE-based pigment masterbatch; post-consumer recyclate may be incorporated at ≤15 wt% only after ESCR requalification under ASTM D1693 condition B shows F₅₀ not less than 80% of the virgin datum. Extrusion blow moulding is carried out on continuous shuttle machines with screws of L/D 24:1–30:1 and compression ratio 3.0–3.5; melt temperature is capped at 210°C because higher temperatures accelerate oxidative chain scission and reduce ESCR. The parison is blown at 0.70–0.85 MPa into aluminium moulds at 9–14°C. A recognised production failure mode is vertical body cracking after 3–6 weeks of warehouse storage under 1.5 m top load when regrind exceeds 15 wt%; top-load verification is run under ISO 12048-2001. Terminal product types are 500 mL–5 L detergent bottles, 750 mL bleach bottles, and trigger-spray bottles for surface cleaning fluids.

    Pharmaceutical bottle parison control, extractables testing, and compendial polymer monographs

    Pharmaceutical oral solid and syrup bottles moulded from 5301B are produced by injection blow moulding and extrusion blow moulding with post-mould washing. Compendial compliance is demonstrated under USP <661.1> plastic packaging systems, Ph. Eur. 3.1.3 polyolefins, FDA 21 CFR 177.1520(c) for direct aqueous contact, and ICH Q3D for elemental impurity risk assessment from closure-to-bottle migration. The resin is charged at 100 wt% virgin 5301B without antistatic or slip additives; if a processing aid is necessary for thin-wall parison control, ≤0.5 wt% fluoropolymer masterbatch is used and documented under the pharmaceutical packaging change-control dossier. Injection blow moulding preforms are injected at 185–205°C, core rod temperature is set at 7±1°C, and blow mould temperature is controlled at 8–12°C; extrusion blow moulded tablet bottles are fabricated on shuttle machines with needle blow at 0.45–0.65 MPa. Wall thickness for 100 mL tablet bottles is specified at 0.8–1.2 mm with thread ovality below 0.3 mm for child-resistant closure engagement. Production-scale deviation in core rod temperature above 15°C yields wall thickness variation exceeding 0.15 mm and cap thread ovality failures above 2%; closed-loop chiller control is required to maintain process capability. Terminal formats are 20–500 mL tablet bottles, 500 mL–1 L syrup bottles, and dropper bodies for oral liquid dosing.

    UN-rated jerrycan production from 5301B for agrochemical and industrial chemical filling requires validation against the UN Model Regulations 21st rev Chapter 6.1.5, ADR/RID 6.1.5 packaging provisions, and IMDG Code 6.1.5 for marine consignments. Formulation ratio for hazardous-liquid jerrycans is 88–93 wt% 5301B blended with 4–8 wt% LLDPE and 3–5 wt% carbon black HDPE masterbatch; the LLDPE addition increases drop-impact elongation but reduces top-load rigidity, so the ratio is fixed by UN drop test at 1.2 m and hydraulic leakage test at 250 kPa for 30 min. Accumulator-head blow moulding with 50–100 point parison programming controls wall thickness between handle pinch-off and bottom chime; die head temperature is 190–205°C, mould temperature 10–16°C, and blow pressure 0.80–0.90 MPa. A documented field failure mode in 20 L jerrycans is handle pinch-off flash thickness above 1.8 mm causing localised low-stress drop fracture at −18°C; the corrective is flash-trim die tuning and mould venting slot depth of 0.03 mm. Terminal pack types are 5 L, 10 L, 20 L, and 25 L HDPE jerrycans marked UN 3H1 for non-removable head and 3H2 for removable-head configurations, used for pesticides, industrial solvents, and oilfield chemicals.

    When 5301B replaces glass in 100–500 mL cosmetic and personal care bottles, what tooling and surface finish controls apply?

    Cosmetic and personal care bottle production with 5301B targets glass replacement in lotion, shampoo, body wash, and skin care applications where drop resistance and pack weight reduction are specified but optical transmission is not required. Compliance is assessed under EC No 1223/2009 Article 17 for cosmetic product compatibility; FDA 21 CFR 177.1520(c) may apply when the same bottle platform is shared with oral-care products. The ratio is 93–97 wt% 5301B with 3–7 wt% PE-based colorant masterbatch and no filler; silicone-based mould release is avoided because it reduces hot-stamp and screen-printing adhesion. Shuttle extrusion blow moulding is used with pre-blow pressure 0.5–0.6 MPa, final blow pressure 0.65–0.75 MPa, and mould temperature 12–18°C. High-gloss tooling with P20 aluminium cavities and venting slot depth 0.03 mm is required to reach surface gloss above 85 GU at 60° per ISO 2813. A recurring production defect is flow mark formation at pre-blow pressure below 0.5 MPa, generating cosmetic surface reject rates above 4%; raising pre-blow pressure to 0.55–0.60 MPa removes the defect but narrows the operating window for thin-wall bottles below 0.6 mm. Finished articles are 100–500 mL lotion bottles, pump bottles, and cream jars with neck finishes from 24/410 to 28/410.

    Industrial lubricant and car care bottle dimensioning against compression and vibration standards

    Industrial lubricant and car care containers moulded from 5301B are dimensioned for vertical compression in pallet stacks, vibration during truck transport, and long-term contact with formulated engine oils and automotive care fluids. Standards include ASTM D4169-22 for distribution simulation, ISO 12048-2001 for compression testing of packages, and ASTM D1693 condition A for environmental stress crack resistance where hydrocarbon formulations contain ester or detergent additives. The compound is blended at 90–95 wt% 5301B with 5–10 wt% in-house regrind generated from the same production line and 2–4 wt% carbon black masterbatch for opacity and UV shielding. The use of in-house regrind is limited to 10 wt% if the bottle is loaded in the bottom layer of a pallet stack greater than 1.5 m. Process equipment is screw accumulator blow moulding with barrel temperature 190–210°C, die head temperature 195–205°C, and blow pressure 0.75–0.85 MPa. After moulding, each container is leak-tested by pressure decay at 35 kPa for 5 s; cycle time for a 5 L bottle is typically 35–45 s depending on cooling air temperature. Terminal products are 1 L, 2 L, and 5 L engine oil bottles with side-viewing strips, 500 mL–1 L car-care additive bottles, and windshield washer fluid containers with internal membrane seals.

    Free Quote

    Competitive Sinopec Yangzi HDPE 5301B prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Yangzi HDPE 5301B is a pelletized high-density polyethylene produced at the Yangzi Petrochemical complex and supplied primarily for continuous extrusion blow moulding of small to medium hollow articles. The grade is distinguished within the Yangzi HDPE portfolio by a combination of moderate melt flow and controlled die swell that permits stable parison formation on shuttle and reciprocating-screw machines. Density measured in accordance with ISO 1183-1:2019 on compression-moulded specimens is reported as 0.953 g/cm³, with a production-release window of 0.950–0.956 g/cm³. Melt mass-flow rate under ISO 1133-1:2022 at 190°C/2.16 kg is reported as 0.5 g/10 min, with production-release material typically spanning 0.40–0.60 g/10 min. The base stabilization package is designed for closed-loop regrind addition up to 20 wt% without marked loss of oxidation induction time, provided the regrind is dry and free of mixed resin contamination. The resin is not intended for pipe-grade long-term hydrostatic design basis under ISO 9080, nor for high-speed injection moulding; those service regimes require other Yangzi HDPE grades.

    What Are the Principal Specification Boundaries for Sinopec Yangzi HDPE 5301B?

    Table 1 summarizes the release data used for incoming inspection on extrusion blow-moulding lines. Values are not purchase specifications; lot-specific certificates of analysis take precedence.

    Table 1. Reported resin property release profile for Sinopec Yangzi HDPE 5301B
    PropertyTest methodUnitReported value or range
    DensityISO 1183-1:2019g/cm³0.950–0.956
    Melt mass-flow rateISO 1133-1:2022g/10 min0.40–0.60
    Tensile stress at yieldISO 527-2MPa22–26
    Tensile strain at breakISO 527-2%>600
    Flexural modulusISO 178:2019MPa900–1000
    Charpy notched impact strength at 23°CISO 179-1:2010kJ/m²5–8
    Environmental stress-cracking resistance, F50ASTM D1693 condition Bh>600
    Vicat softening temperature, A50ISO 306:2022°C123–126

    Because these values are generated on compression-moulded or injection-moulded laboratory specimens, they do not transfer directly to blow-moulded side walls; process-induced crystallinity and orientation produce local differences in yield stress and ESCR.

    On shuttle blow-moulding machines with screw diameters of 25–45 mm and L/D ratios of 20–25:1, set temperatures from feed to die are 175–185°C, 190–200°C, 200–210°C, and 205–215°C. Blow pressure between 0.6 MPa and 0.8 MPa is applied, with mould temperatures of 10–30°C to balance cycle time against surface gloss. Clamp force normally falls between 50 kN and 200 kN for articles below 2 L. No predrying is required if hopper inlet relative humidity remains below 60%; above that threshold, 2 h at 80°C in a desiccant tray dryer removes surface moisture and prevents splay. Die land length is maintained at 10–15× the die gap to suppress melt fracture, and the mandrel diameter is undersized relative to the container neck finish by 15–25% to account for parison swell and post-moulding shrinkage. Blow-up ratios between 2.5:1 and 4:1 are preferred; outside this range, wall thickness uniformity and top-load performance can deteriorate.

    Rheological and Thermal Response Across the Processing Window

    Capillary rheometry at 190°C shows shear-thinning behaviour, with apparent viscosity decreasing from approximately 3,500 Pa·s at 100 s⁻¹ to 800 Pa·s at 1,000 s⁻¹. Melt strength measured by a haul-off rheometer at 190°C is reported between 0.15 N and 0.25 N at draw ratios below 6:1. Die swell at 210°C lies between 40% and 60%, requiring the die and mandrel to be undersized relative to the finished neck finish. Differential scanning calorimetry at 10°C/min heating gives a peak melting temperature of 131–135°C and crystallization temperature of 112–116°C. On blow-moulded walls of 1.0–2.0 mm, mould temperatures below 20°C lower bulk crystallinity by 2–5% relative to slower-cooled compression mouldings, shifting low-temperature impact response and reducing post-moulding shrinkage. These thermal transitions place 5301B within the typical HDPE envelope, not in the elevated-temperature service class of silane-crosslinkable or PE-RT grades.

    Parison sag, melt fracture, and die-lip drool are the three conversion faults most often recorded for 5301B on shuttle blow-moulding equipment. Sag becomes significant when shot weight exceeds 1.5 kg or when the melt temperature at the die exceeds 220°C; a parison programmer with divergent pinch points is then used to maintain wall thickness within ±5%. Melt fracture appears at shear rates above 1,500 s⁻¹ in conventional dies with land lengths below 10×die gap; raising the die temperature to 215°C or reducing screw speed usually clears the sharkskin pattern. Die-lip drool is controlled by maintaining the die land at 205–215°C and by cleaning the lip with copper-free brass tools at 8 h intervals on high-output lines. Splay and delamination are observed when pellet moisture exceeds 0.05% by weight; such lots require drying before processing.

    When 5301B Is Benchmarked Against Other Yangzi HDPE Grades

    Table 2 compares commercially reported grade profiles. The primary difference is melt flow rate and molecular weight distribution, which control processing route.

    Table 2. Comparative grade profiles within the Sinopec Yangzi HDPE range
    GradeMelt flow rate at 190°C/2.16 kgDensityPrimary conversion routeApplication focus
    5301B0.40–0.60 g/10 min0.953 g/cm³Extrusion blow mouldingSmall to medium hollow articles
    5000S0.25–0.35 g/10 min0.954 g/cm³Extrusion blow moulding, blown filmLarge containers, carrier film
    5306J5.5–6.5 g/10 min0.957 g/cm³Injection mouldingThin-wall housewares, caps
    6100M0.13–0.17 g/10 min0.949 g/cm³Pipe extrusionPressure pipe

    The lower MFR of 5000S provides greater melt strength for large parisons but requires higher torque and melt temperature. 5301B permits faster screw recovery on 45 mm extruders when wall thickness is less than 2 mm. Compared with 5306J, 5301B cannot be processed on injection machines with clamp force below 1,000 kN without excessive pressure drop and short shots. Pipe grade 6100M has lower MFR and higher hydrostatic design stress under ISO 9080, but 5301B is not intended for long-term internal pressure service. Published data for thin-wall injection moulding of 5301B is limited; it should not be substituted for 5306J without tool trial.

    Food-contact compliance for the natural resin should be confirmed against 21 CFR 177.1520, which covers olefin polymers, and against EU 10/2011 where applicable. The base grade does not require intentionally added perfluorinated processing aids; however, masterbatch and lubricant packages must be disclosed by downstream compounders. Storage below 30°C and 60% relative humidity for less than 12 months is recommended. Natural 5301B is not UV-stabilized for outdoor service; if exposure under ISO 4892-2 is required, 2.0–3.0 wt% of carbon black or hindered amine light stabilizer masterbatch should be incorporated during extrusion. The resin is not classified as a hazardous substance under REACH in the supplied pellet form, but workplace exposure limits for polymer dust apply during regrind operations.

    Incoming inspection on blow-moulding lines samples each delivery for melt flow rate, density, and oxidation induction time because batch-to-batch variation in density of ±0.005 g/cm³ is small but can shift top-load performance. Fourier-transform infrared spectroscopy is used to screen for mixed LLDPE, which appears as an additional 1,375 cm⁻¹ methyl band. Lots with melt flow rate below 0.35 g/10 min are directed to heavier parison tools, while lots above 0.65 g/10 min require lower die temperatures to avoid sag.

    Assessing Environmental Stress-Cracking Resistance Under Igepal CO-630 and Chemical Exposure Boundaries

    ESCR under ASTM D1693 condition B in 100% Igepal CO-630 at 50°C exceeds 600 h for compression-moulded plaques. Blow-moulded parts with weld lines and pinch-off zones can exhibit F50 values reduced by 30–50%. The resin resists dilute mineral acids, aqueous alkalis, and aliphatic alcohols below 40°C. Continuous exposure to aromatic hydrocarbons, chlorinated solvents, or strong oxidizing acids above 40°C causes swelling and stress cracking. Nonylphenol ethoxylate-based cleaning agents at concentrations above 5% should be avoided at weld lines because localized orientation accelerates crack propagation. Oxidative stability measured by ISO 11357-6 at 200°C normally exceeds 20 min for virgin pellets, but amine-based slip/antistatic additives can reduce this to below 20 min and should be evaluated before use.

    During grade transitions on single-screw extrusion blow-moulding lines, purging with a similar-melt-flow HDPE is required until melt pressure deviation is less than 5% of steady state. On 65 mm extruders at 40 rpm, purge times of 20–30 min are used after LLDPE or fractional-melt HDPE. Regrind flake ground to 8 mm or less and blended at 10–20 wt% with virgin pellets maintains parison diameter variability within ±3% on production lines. The grade is incompatible with amine-based slip/antistatic additives that lower oxidation induction time below 20 min at 200°C under ISO 11357-6.

    Top