Sinopec Yangzi Hdpe 4902t

Sinopec Yangzi HDPE 4902T

    • Product Name: Sinopec Yangzi HDPE 4902T
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 473870
    Density 0.949 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.20 g/10 min
    Tensile Yield Strength ≥26 MPa
    Tensile Strength At Break ≥30 MPa
    Elongation At Break ≥500%
    Flexural Modulus ≥1000 MPa
    Vicat Softening Temperature ≥120°C
    Melting Point 130-135°C
    Notched Izod Impact Strength ≥40 kJ/m²
    Environmental Stress Cracking Resistance ≥1000 h
    Hardness Shore D 60-65
    Brittleness Temperature ≤-70°C
    Water Absorption <0.01%
    Dielectric Strength ≥20 MV/m

    As an accredited Sinopec Yangzi HDPE 4902T factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Yangzi HDPE 4902T is supplied in 25 kg woven polypropylene bags, available in 1,000 kg jumbo bags for bulk handling.
    Container Loading (20′ FCL) 20′ FCL container loading: Sinopec Yangzi HDPE 4902T in 25 kg bags, palletized or floor-loaded, secure stowage for sea freight.
    Shipping Sinopec Yangzi HDPE 4902T is a non-hazardous high-density polyethylene resin. It ships in 25 kg woven bags, jumbo bags, or bulk containers. Store dry, cool, and ventilated; avoid moisture, heat, sunlight, and contamination. Not classified as dangerous goods for transport. Standard MSDS provided.
    Storage Sinopec Yangzi HDPE 4902T should be stored indoors in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original bags sealed on pallets to prevent moisture, dust, and contamination. Protect from rain and water. Avoid prolonged UV exposure, sharp objects, and stacking damage. Use first-in, first-out rotation.
    Shelf Life Shelf life is typically 24 months when stored in original, unopened packaging, dry, ventilated, away from direct sunlight.
    Application of Sinopec Yangzi HDPE 4902T

    Sinopec Yangzi HDPE 4902T enters potable water pressure pipe extrusion as a bimodal, high-density polyethylene resin classified under ISO 12162 as PE100. The finished pipe is governed by ISO 4427-2:2019, with parallel market requirements under EN 12201-2:2011+A1:2018 and GB/T 13663.2-2018; material qualification requires long-term hydrostatic strength regression according to ISO 9080:2012 with a minimum required strength of 10 MPa at 20 °C/50 years and sustained pressure testing under ISO 1167-1:2006. Black potable water pipe is formulated from 100 phr base resin with 5.0–6.25 phr of a 40% carbon black masterbatch, producing a final carbon black content of 2.0–2.5 wt%; carbon black dispersion is controlled to ISO 18553 grade ≤3. Where blue water service pipe is produced, a phthalocyanine blue masterbatch is metered at 0.5–1.5 wt%, but only after potable-water migration certification under AS/NZS 4020 or the relevant national positive list. Production equipment for water pipe typically consists of a grooved-feed single-screw extruder with L/D 30–36 and a barrier screw feeding a spiral mandrel die of 16–630 mm diameter. Barrel temperatures are maintained at 190–210 °C and melt temperature at 200–220 °C; on a 60 mm grooved-feed extruder, die head pressure commonly ranges from 25–35 MPa. Vacuum calibration at −0.3 to −0.8 bar and two-stage spray cooling with water at 15–25 °C stabilize outside diameter, ovality, and residual stress. Terminal products include SDR 11/PN16 and SDR 17/PN10 potable water mains, distribution laterals, service risers, and connection spigots from 20 mm to 1200 mm outside diameter. Sustained melt temperature above 230 °C lowers oxidation induction time below the commonly applied 20 min at 200 °C, and cross-contamination with polypropylene or PVC must be excluded because weld-line delamination and reduced slow crack growth resistance appear in subsequent butt fusion joints.

    How Does Slow Crack Growth Resistance Govern Gas Pipe Service Life?

    Gas distribution pipe manufactured from Sinopec Yangzi HDPE 4902T is qualified under ISO 4437-2:2014 and EN 1555-2, with North American export specifications referencing ASTM D2513 and material cell classification under ASTM D3350. The decisive failure mechanism is slow crack growth rather than short-term hydrostatic burst; therefore product standards apply the notched pipe test of ISO 13479 at 80 °C under 4.6 MPa, and PE100 grades are commonly required to exceed 500 h failure time in this test. The ISO 9080:2012 regression curve must predict a 20 °C/50-year lower confidence limit of at least 10 MPa. In gas pipe formulation, carbon black masterbatch is added at 5.0–6.25 phr to achieve 2.0–2.5 wt% final carbon black, preserving outdoor storage stability without creating micro-dispersion defects that lower notched pipe resistance. A coextruded yellow identification stripe is applied through a second 25–45 mm extruder using a gas-grade yellow concentrate at 2–4 wt% of the stripe layer, with stripe thickness controlled at 0.2–0.5 mm; the stripe compound must not introduce contaminants that migrate into the pressure-bearing pipe wall. Extrusion differs from municipal water pipe in its demand for tighter melt pressure stability: on a 75 mm grooved-feed extruder, output is deliberately reduced to maintain die pressure fluctuation below ±1.0 MPa. Barrel temperature is profiled at 180–205 °C, die temperature at 200–215 °C, and cooling water at 18–25 °C. Terminal products include SDR 11 and SDR 17 gas mains from 32 mm to 630 mm, coiled service pipe up to 125 mm, and transition-ready spigot ends for electrofusion and butt fusion. Jointing must follow ISO 21307:2017; fusion below 5 °C ambient temperature without documented procedure qualification is outside the validated operating window.

    ApplicationProduct standardQualification testCritical numerical limit
    Potable water pipeISO 4427-2:2019ISO 9080:2012 long-term hydrostatic strength10 MPa MRS at 20 °C/50 years
    Gas distribution pipeISO 4437-2:2014 / ASTM D2513ISO 13479 notched pipe test≥500 h at 80 °C/4.6 MPa
    Industrial pipeISO 15494:2015Chemical resistance list and ASTM D1693 ESCRFluid-specific derating required
    Pipe material classificationISO 12162MRS classification10 MPa PE100

    Mining Slurry and Dredge Line Pipe: Erosion–Stress Crack Interaction

    In slurry and dredge pipe service, HDPE 4902T is converted into thick-wall pressure pipe governed by ISO 15494:2015, with North American inspection practice often referencing ASTM F714 for diameter-ratio-based pressure ratings. The formulation remains carbon black-stabilized at 2.0–2.5 wt% final content, but melt quality is the controlling variable: 0.02–0.05 wt% fluoropolymer processing aid is permitted only when melt fracture appears on small die gaps, and in-house scrap rework should be limited to 10–20 wt% because repeated heat histories reduce slow crack growth resistance in high-solids service. Production differs from municipal pipe in that wall thickness frequently exceeds 30–60 mm, forcing low screw speed and reduced output to avoid sagging. A 90 mm grooved-feed extruder with L/D 33 produces outer diameters up to 800 mm at 195–215 °C melt temperature; the calibration sleeve is lengthened to 1.0–1.5 m and spray cooling is staged at 20–30 °C to limit internal residual stress. Terminal products include floated and flanged HDPE dredge pipes, mine tailings lines, coal slurry transfer pipe, and pit dewatering risers. The governing operational boundary is not short-term burst but combined slow crack growth from internal pressure and erosion from solid particles; design therefore derates hydrostatic service pressure by slurry density and by an abrasion allowance specified in the piping design code. Butt fusion of thick-wall slurry pipe requires reduced planing torque, longer soak time, and pressure holding time extended by 30–50% relative to thin-wall pipe.

    Pressure wastewater force mains manufactured from HDPE 4902T use the same product standards as potable water, ISO 4427-2:2019 and EN 12201-2, but the qualification emphasis shifts to chemical resistance and surge tolerance rather than taste and odor. The formulation is carbon black masterbatch at 5.0–6.25 phr to produce 2.0–2.5 wt% final carbon black, with no additional antioxidant masterbatch because the reactor stabilizer package retains an oxidation induction time above 20 min at 200 °C after processing. In this application, the extrusion line is configured for thicker SDR 11 and SDR 17 pipe from 90 mm to 1000 mm outside diameter, using grooved-feed single-screw extruders of 60–120 mm diameter and L/D 33–36. Melt temperature is kept between 195 °C and 215 °C, and the calibration/cooling section is extended to manage residual stress; cooling water temperature is controlled at 20–30 °C to avoid rapid skin solidification that produces inner-wall shrinkage voids. Terminal product types include sewage force mains, lift station discharge lines, and offshore outfall pressure sections. Hydrogen sulfide and disinfectant exposure require that the pipe not be joined to PVC or lined metallic spools with adhesives; electrofusion fittings must be rated for the same pressure class and commodity. Published data for long-term oxidation under chlorinated wastewater exposure with this specific grade is limited, so design should select chlorine-resistant PE100 compound inventories where residual chlorine exceeds 1.0 mg/L under continuous service.

    When Wall Thickness Exceeds 60 mm in Water Transmission Pipe

    Large-diameter water transmission pipe from HDPE 4902T is governed by ISO 4427-2:2019, and the central production conflict is thermal residual stress: when wall thickness exceeds 60 mm, the outer skin solidifies while the core remains molten, creating shrink-induced stress unless multi-layer cooling or internal water cooling is used. The formulation uses the same carbon black masterbatch addition of 5.0–6.25 phr for 2.0–2.5 wt% final carbon black, while UV stabilization is supplied by the masterbatch itself. Production equipment is typically a 120–150 mm grooved-feed single-screw extruder with L/D 30–36 and a barrier screw, operated at 60–70% of thin-wall maximum output to prevent melt fracture and sag. Melt temperature at die entry is held at 190–205 °C, lower than standard pipe to increase melt strength, and die head pressure can exceed 40 MPa on large heads. Calibration uses vacuum at −0.5 to −0.9 bar and multi-stage spray tanks with water at 15–25 °C; total cooling length often exceeds 40 m for diameters above 800 mm. Terminal products are SDR 17/PN10 and SDR 21/PN8 transmission mains, raw water intake lines, and desalination outfalls, up to 1600 mm where extrusion tooling and transport constraints permit. Any interruption exceeding 3–5 min during thick-wall extrusion creates radial interfaces and must be scrapped. Butt fusion of such thick sections requires strict adherence to ISO 21307:2017, with extended heating and cooling times calculated from interfacial pressure and wall thickness.

    ParameterPotable water pipeGas distribution pipeThick-wall slurry/transmission pipe
    Melt temperature200–220 °C190–215 °C190–205 °C
    Die head pressure, 60–90 mm extruder25–35 MPa25–35 MPa with ±1.0 MPa fluctuation limit40 MPa and above on large dies
    Cooling water temperature15–25 °C18–25 °C15–25 °C staged
    Vacuum calibration−0.3 to −0.8 bar−0.3 to −0.8 bar−0.5 to −0.9 bar
    Carbon black masterbatch addition5.0–6.25 phr5.0–6.25 phr5.0–6.25 phr

    Industrial Chemical Transfer Lines and the Slow Crack Growth Margin

    In industrial chemical transfer service, the governing material property for HDPE 4902T is not melt flow but environmental stress crack resistance and chemical compatibility. The applicable product standard is ISO 15494:2015, material classification remains PE100 under ISO 12162, and chemical resistance is assessed through supplier resistance charts or ISO 4433 immersion testing. Black chemical pipe is formulated with 5.0–6.25 phr carbon black masterbatch to reach 2.0–2.5 wt% carbon black; where carbon black is prohibited by fluid purity or color requirements, unpigmented natural pipe is produced without carbon black, but outdoor storage life is reduced unless shielded from ultraviolet exposure. Extrusion of chemical pipe uses a 60–90 mm grooved-feed single-screw line with melt temperature of 200–220 °C, die head pressure of 25–35 MPa, and close-tolerance vacuum sizing because dimensional stability controls electrofusion joint quality. Terminal products include pressure pipe for dilute acids, caustic soda, brine, and process water; however, strong oxidizing acids, aromatic solvents, and chlorinated hydrocarbons lie outside the chemical resistance envelope of high-density polyethylene. Jointing is electrofusion or butt fusion to ISO 21307:2017; solvent cement is not permitted. Continuous contact with wetting agents, silicone oil, or certain alcohols can reduce slow crack growth resistance significantly, so ASTM D1693 or ISO 22088-1 data for the specific fluid must be reviewed before service pressure is quoted.

    Free Quote

    Competitive Sinopec Yangzi HDPE 4902T prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Yangzi HDPE 4902T is a bimodal high-density polyethylene pipe-grade compound manufactured by Sinopec Yangzi Petrochemical Co., Ltd. The grade is formulated for solid-wall pressure pipe extrusion and is commonly supplied as a black compound with UV-stabilising carbon black. Published datasheets list a nominal density of 0.949 g/cm³ by ISO 1183-1:2019 and a melt flow rate of 0.25 g/10 min at 190°C under a 5 kg load by ISO 1133-1:2022. Under the pipe material classification system of ISO 12162:2009, the material is positioned as a PE100 compound, indicating a minimum required strength of 10 MPa at 20°C for a 50-year service life. This classification separates the grade from PE80 pipe compounds, which carry a minimum required strength of 6.3 MPa, and from general-purpose HDPE blow-moulding or film resins that are not tested for long-term hydrostatic strength.

    What Limits Long-Term Hydrostatic Performance in 4902T?

    Long-term hydrostatic performance is evaluated by the regression method of ISO 9080:2022, in which pipe specimens are subjected to internal hydrostatic pressure at multiple temperature levels until failure. The PE100 designation requires that the lower predictive limit at 20°C and 50 years remain at or above 10 MPa. For 4902T, the bimodal molecular weight distribution contributes a high-molecular-weight fraction that increases resistance to craze propagation and slow crack growth. In notched pipe testing to ISO 13479:2022, conducted at 80°C under the hoop stress specified for PE100, the grade is designed to exceed the minimum failure time applied to PE100 compounds. Published data for this specific configuration is limited, and converters should generate batch-specific hydrostatic regression data when qualifying a new extrusion line. The supplier certificate of analysis typically reports oxidation induction time above 20 min at 210°C by ISO 11357-6:2018, which is an indirect indicator of stabiliser retention during processing.

    Extrusion behaviour on production-scale equipment is dominated by the grade’s high low-shear viscosity and strong shear-thinning response. On grooved-feed single-screw extruders with an L/D ratio of 30:1 to 36:1, a barrier screw, and a spiral mandrel pipe die, melt temperature at die entry is normally maintained between 200°C and 230°C. The drive system must accept the torque required to plastify the material; experience on lines with 40 mm to 90 mm screw diameter indicates that barrel heating and cooling capacity of at least 1.5 kW/kg of output is needed to prevent screw slip and pressure oscillation. A 40 μm screen pack upstream of the die is used to retain gel particles and carbon black agglomerates. Die pressure above 350 bar can induce shear heating and reduce melt homogeneity; therefore, throughput should be limited when the melt pump suction pressure exceeds the stabiliser limit. The material should not be held above 240°C for more than 15 min, because thermal-oxidative chain scission can reduce the oxidation induction time below the 20 min value measured to ISO 11357-6:2018. Regrind inclusion should not exceed 20% unless notched pipe performance and OIT are re-qualified, as repeated thermal cycles consume antioxidant and increase gel content.

    Moisture management on the line is limited because HDPE does not hydrolyse. However, surface condensation on pellets stored outdoors can create steam-induced surface defects in the melt. If ambient relative humidity exceeds 60%, a hopper dryer at 80°C for 1 h removes surface moisture. Carbon black dispersion in the finished pipe wall is controlled by the masterbatch let-down ratio and the shear history in the screw. Poor dispersion creates local stress concentrations that reduce slow crack growth resistance and can be detected by grading to ISO 18553:2002.

    When This Grade Replaces a Unimodal PE80 or PE100 Compound

    Relative to a conventional unimodal PE80 pipe compound with a design stress of 6.3 MPa, 4902T provides a higher hydrostatic design basis of 8.0 MPa at 20°C for 50 years under ISO 4427-2:2019 design rules. The resulting wall thickness at a given pressure is approximately 20% lower for 4902T, which changes critical dimensions and reduces material demand per metre of installed line. Compared with a typical unimodal PE100 grade of similar density, 4902T has a lower melt flow rate under 190°C/5 kg, which corresponds to higher melt strength during free-form extrusion of thick-wall pipe. In practice, this difference reduces sag in spiral-wound and large-diameter pipe heads, but the lower flow also raises specific energy input during plastication. The bimodal distribution gives a broader shear-thinning response: apparent viscosity decreases more sharply at die shear rates above 100 s⁻¹, which allows linear output while retaining low-shear viscosity for dimensional stability.

    Differentiation from non-pipe HDPE grades is equally sharp. Blow-moulding grades typically show melt flow rates above 0.50 g/10 min under 190°C/5 kg and are not tested for hydrostatic design basis. Film grades with densities in the range 0.940–0.948 g/cm³ lack the 10 MPa minimum required strength of a PE100 compound. Metallocene-catalysed medium-density polyethylene grades may offer high slow crack growth resistance, but their lower density reduces tensile yield strength and long-term creep modulus. A converter evaluating a switch from such a resin must recalibrate pipe SDR, ring deflection calculations, and weld parameters, because the higher crystallinity of 4902T changes thermal conductivity and cooling shrinkage.

    Nominal Property Profile and Test Methodology

    Property Test method Unit Published typical value
    Density at 23°C ISO 1183-1:2019 g/cm³ 0.949
    Melt flow rate at 190°C/5 kg ISO 1133-1:2022 g/10 min 0.25
    Tensile stress at yield ISO 527-2:2012 MPa 23
    Elongation at break ISO 527-2:2012 % >600
    Flexural modulus ISO 178:2019 MPa 950
    Carbon black content ISO 6964:2019 % by mass 2.0–2.5
    Oxidation induction time at 210°C ISO 11357-6:2018 min >20

    Values shown are representative of published datasheets and do not constitute batch release limits. Batch-specific certificates of analysis and hydrostatic regression curves to ISO 9080:2022 form the definitive acceptance criteria for pressure pipe qualification.

    Buried pressure pipe service involves internal pressure, soil deflection, and point loads. The material’s flexural modulus of 950 MPa by ISO 178:2019 is only one input in ring deflection calculations under ISO 4427-2:2019; long-term creep modulus at 50 years is lower and must be used for structural calculations. For water at 20°C, design stress 8.0 MPa yields SDR 11 for PN16 service. At 40°C, derating factors reduce the admissible pressure by approximately 30%, which directly affects maximum operating pressure. The compound’s carbon black content at 2.0–2.5% by ISO 6964:2019 provides ultraviolet screening for above-ground sections, but prolonged direct exposure should be evaluated by oxidative degradation tests such as ISO 4892-2:2013 for the specific exposure environment.

    The relevant standards do not replace hydrostatic batch testing.

    Standard/regulation Purpose/condition Application in qualifying 4902T
    ISO 9080:2022 Hydrostatic strength regression at multiple temperatures Establishes 50-year strength
    ISO 12162:2009 Pipe material classification PE100 designation
    ISO 13479:2022 Notched pipe test at 80°C Slow crack growth resistance
    ISO 4427-2:2019 PE water pipe dimensions and hydrostatic design SDR selection
    EN 12201-2:2024 European pressure pipe requirements CE marking support
    GB/T 13663.2-2018 China water supply pipe specification Local compliance
    FDA 21 CFR 177.1520 Olefin polymer compositional requirement Food-contact article basis

    Compliance with these standards is not purely compositional. The extruder line must demonstrate process capability indices for wall thickness and hydrostatic performance. A pipe producer may not claim conformity to ISO 4427-2:2019 simply by moulding a material that meets MRS; the finished pipe must pass batch hydrostatic and notched pipe tests. This distinction is frequently underestimated when switching from a generic HDPE extrusion grade to a pressure-pipe compound.

    Batch-to-batch variation in melt flow rate of ±0.03 g/10 min can produce measurable die pressure changes in closed-loop extrusion. A melt pump with pressure control loop is recommended when wall thickness tolerance must be held within +0.5 mm, because the pump compensates for small viscosity differences. The main failure modes observed on production lines are melt fracture at die entry if output is pushed beyond the shear stress limit, and shrinkage variation if the cooling water temperature is not controlled between 10°C and 20°C. Neither failure mode is unique to 4902T, but the higher molecular weight and narrower processing window of a bimodal pipe compound make closed-loop temperature and melt pressure control more critical than for lower-viscosity PE80 or general-purpose extrusion grades.

    Rapid crack propagation in a pressurised pipe is assessed by small-scale or full-scale tests. Under ISO 13477:2008, a pre-cracked pipe is impacted at a defined internal pressure and temperature. The grade’s density and bimodal architecture influence the ductile-to-brittle transition; published data for this specific configuration is limited, and pipe manufacturers should determine the critical pressure and temperature for each diameter and SDR series. This is particularly relevant for pipes above 315 mm OD intended for low ambient temperature service.

    Slow crack growth resistance is not predicted by melt flow rate alone. A unimodal resin of the same density and melt flow rate may fail earlier because the molecular weight distribution is narrower and the high-molecular-weight tail is shorter. The slow crack growth resistance of 4902T arises from tie-chain density and disentanglement resistance in the amorphous phase. In bimodal resins, the high-molecular-weight fraction increases the number of load-bearing tie molecules, which extends failure time under ISO 13479:2022 at 80°C. The notched pipe test is therefore more relevant than melt flow rate for qualifying a pipe grade for buried service. Converters that blend 4902T with off-spec or non-pipe HDPE regrind risk reducing the high-molecular-weight fraction below the level required to meet PE100 notched pipe performance.

    For large-diameter solid-wall pressure pipe, the main processing bottleneck is sag. On a spiral mandrel die head with an outside diameter above 900 mm, the melt front must retain geometry during solidification. The high melt strength of 4902T allows wall thickness tolerances within +0.5 mm when die centring and calibrator vacuum are correctly set. The material is not suitable for rotomoulding or blown film because the melt flow rate at 190°C/2.16 kg is below the minimum required for those processes. Storage under high humidity does not require desiccant drying, but surface moisture on pellets should be removed by a hopper dryer at 80°C for 1 h if the ambient relative humidity exceeds 60%.

    Top