Sinopec Wuhan Hdpe Pn049 030 122

Sinopec Wuhan HDPE PN049-030-122

    • Product Name: Sinopec Wuhan HDPE PN049-030-122
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 834541
    Product Name Sinopec Wuhan HDPE PN049-030-122
    Manufacturer Sinopec Wuhan Petrochemical Company
    Polymer Type High Density Polyethylene (HDPE)
    Grade Classification PE100 pipe grade
    Density 0.949 g/cm3
    Melt Flow Rate 0.30 g/10 min (190°C/5 kg)
    Tensile Strength At Yield >=25 MPa
    Elongation At Break >=350%
    Flexural Modulus >=1000 MPa
    Vicat Softening Temperature >=120°C
    Oxidation Induction Time >=20 min
    Carbon Black Content 2.0-2.5%
    Environmental Stress Crack Resistance >=5000 h
    Moisture Content <=0.05%
    Ash Content <=0.1%
    Bulk Density >=0.50 g/cm3
    Color Black
    Hydrostatic Strength MRS 10.0 MPa
    Thermal Conductivity 0.4 W/(m·K)
    Water Absorption <=0.01%

    As an accredited Sinopec Wuhan HDPE PN049-030-122 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Wuhan HDPE PN049-030-122 is typically packed in 25 kg woven bags or 1,000 kg jumbo bags.
    Container Loading (20′ FCL) 20′ FCL container loaded with Sinopec Wuhan HDPE PN049-030-122 in 25 kg bags, palletized, shrink-wrapped, and securely stowed for export.
    Shipping Sinopec Wuhan HDPE PN049-030-122 is shipped as non-hazardous high-density polyethylene resin pellets, typically in 25 kg bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport by truck or container as general cargo. Keep dry, ventilated, away from sunlight, heat, moisture, and contamination. No special UN hazard classification required.
    Storage Store in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, moisture, heat, flames, and strong oxidizers. Keep original bags sealed and palletized off the floor and away from walls. Avoid prolonged UV exposure and excessive stacking. Use first-in, first-out stock rotation. Maintain clean, dry handling areas to prevent contamination. Handle gently to avoid bag damage and dust generation.
    Shelf Life Shelf life is 24 months when stored in dry, ventilated conditions, away from direct sunlight and heat.
    Application of Sinopec Wuhan HDPE PN049-030-122

    Pressure retention limits in PE100 potable water distribution systems

    In potable water pressure piping, the 50-year hydrostatic design basis of PN049-030-122 is established through long-term creep rupture testing under ISO 9080:2012, which assigns the material a minimum required strength of 10 MPa at 20 °C for PE100 compounds. Finished pipes are dimensionally and mechanically qualified under ISO 4427-2:2019 and EN 12201-2:2011+A1:2013, while material contact with drinking water is assessed under NSF/ANSI/CAN 61:2023, FDA 21 CFR 177.1520, and GB/T 13663.2-2023. During extrusion, the resin is typically blended with a blue masterbatch at a loading of 1–2 wt% to produce the standard blue stripe or solid blue pipe; in co-extruded structures, post-consumer recycled polyethylene is confined to the outer non-water-contact layer at mass fractions up to 30 wt%, while the inner layer remains 100% virgin resin in accordance with the hydrostatic stress-cracking clauses of ISO 4427-1:2019. Processing on single-screw extruders with a screw length-to-diameter ratio of at least 30:1 and a barrier mixing section is required to homogenise the bimodal molecular weight distribution without excessive shear heating; barrel temperatures are held between 180 °C and 220 °C, with melt temperatures at the die land maintained between 200 °C and 220 °C to avoid surface melt fracture and internal void formation. Vacuum calibration is applied at −0.04 MPa to −0.06 MPa in a multi-stage spray cooling tank with water temperatures between 15 °C and 25 °C, and haul-off speeds are adjusted from 0.5 m/min to 2.5 m/min depending on outside diameter. Finished pipe dimensions span dn20 mm to dn1200 mm, with standard dimension ratios of SDR11, SDR17, and SDR26, corresponding to nominal pressure ratings of PN16, PN10, and PN6.3 when operating at 20 °C with water. The slow crack growth resistance of the bimodal resin, measured as notched pipe test failure exceeding 1,000 h at 80 °C and 4.6 MPa per ISO 13479:2022, is the principal performance characteristic that distinguishes this grade from unimodal HDPE in long-term potable water service.

    Natural gas distribution networks impose a more severe set of rapid crack propagation and slow crack growth requirements than water service, and PN049-030-122 is processed into solid-wall pipe conforming to ISO 4437-3:2022, EN 1555-2:2021, and GB 15558.1-2023, with material classification verified through full-scale rapid crack propagation testing under ISO 13477:2022 at 0 °C and critical pressure thresholds. In gas pipe compounds, carbon black masterbatch is added at 2.0–2.5 wt% to achieve a carbon black content of 2.0–2.5 wt% in the pipe wall, as specified in the carbon black dispersion clauses of ISO 4437-1:2022; a yellow stripe masterbatch is co-extruded at 0.3–0.5 wt% for identification, while the oxidation induction time of the stabilised resin must exceed 20 min at 200 °C when tested under ISO 11357-6:2023. The extrusion process for gas pipe typically uses a grooved-feed single-screw extruder with L/D 33:1 and a low-shear barrier screw to deliver melt at 200–230 °C through a spiral mandrel die, with screen packs of 60/80/100 mesh installed to trap gel particles that could initiate brittle failure. Vacuum sizing is followed by ultrasonic wall-thickness monitoring to maintain ovality within ±1.5% of nominal outside diameter, because gas pipes must withstand internal pressures up to 1.0 MPa for testing and operate continuously at 0.4 MPa or lower in distribution networks. Finished products range from dn20 mm to dn630 mm, with SDR11 and SDR17.6 dimension ratios, supplied in black or black with yellow co-extruded stripes, and qualified for butt-fusion and electrofusion jointing according to the weldability annexes of ISO 4437-3:2022. The bimodal comonomer placement in PN049-030-122 provides the tie-molecule density required to arrest fast crack propagation at the temperatures encountered in buried gas service, which is the critical safety boundary that excludes many alternative PE pipe grades from this application.

    When thick-walled electrofusion fittings require low-shear melt homogeneity

    For injection moulded PE100 fittings, the low melt flow rate of 0.30 g/10min at 190 °C/5 kg on PN049-030-122 forces processors to rely on controlled screw shear rather than elevated barrel temperatures to achieve cavity fill, and the resin is typically processed in injection moulding machines with a screw L/D of 20:1 to 25:1 and a compression ratio of 2.5:1. Barrel temperature profiles are set with the rear zone at 180–200 °C, the centre zone at 200–220 °C, and the front zone and nozzle at 210–230 °C; melt temperatures above 240 °C initiate oxidative chain scission that reduces the slow crack growth resistance required for pipe network integrity. Mould temperature is maintained between 10 °C and 40 °C, and injection pressures of 100–140 MPa with hold pressures of 60–80 MPa are applied, with multi-stage injection velocity profiles used to prevent jetting and freeze-off in sections thicker than 20 mm. Masterbatch loading for coloured fittings is limited to 0.5–2 wt%, and regrind content is not permitted to exceed 10 wt% unless the reclaimed material is generated from the same lot and verified by hydrostatic testing, because thick-wall fitting bodies must withstand the same 10 MPa minimum required strength classification as adjoining pipe. Fittings are qualified under ISO 4427-3:2019 for water supply and ISO 4437-3:2022 for gas distribution, with additional requirements for electrofusion sockets under EN 12201-3:2011+A1:2012 and butt fusion reducers under ASTM D3261-22. Finished terminal components include electrofusion couplers, spigot tees, saddle branches, and butt-fusion stub ends in diameter ranges of dn20 mm to dn630 mm, with pressure ratings matched to SDR11 and SDR17 pipe systems. The primary processing defect observed in production-scale runs is void formation at the intersection of the fitting body and the heating-wire zone, which is controlled by maintaining a minimum melt cushion of 3–5 mm and a screw back pressure of 0.5–1.0 MPa during plastication.

    Trenchless installation and close-fit pipe rehabilitation consume PN049-030-122 in the form of solid-wall pipes that must tolerate surface scoring during pullback through horizontal directional drilling boreholes, and the pipe design is governed by ASTM F1962-22 for pulling load calculations, ISO 11298-1:2018 for water network renovation, and ISO 11299-1:2018 for gas network renovation. The resin is compounded with 2.0–2.5 wt% carbon black masterbatch to provide long-term UV resistance when pipe is stored above ground before installation, and a fluoropolymer processing aid at 0.05–0.1 wt% is introduced during extrusion to reduce melt fracture and produce a smooth external surface that lowers friction during borehole insertion. The pipe manufacturing process follows the same single-screw extrusion parameters as pressure water pipe, with melt temperatures of 200–230 °C and vacuum calibration, but the finished pipe is then subjected to butt-fusion welding on site at a plate temperature of 210–230 °C and an interfacial pressure of 0.15–0.25 MPa, with cooling times calculated from wall thickness using the cooling rate tables in ISO 21307:2017. During pullback, contractors follow curvature radius limits specified in ASTM F1962-22 design curves, and post-installation integrity is confirmed by hydrostatic pressure testing at 1.5 times the operating pressure for a minimum of 1 h per ISO 11298-1:2018. Terminal finished products are continuous lengths of dn200 mm to dn800 mm SDR11 or SDR17 PE100 pipe, used as replacement water mains, gas distribution lines, and slip-lining sleeves inside degraded cast iron or steel pipelines. The slow crack growth resistance of the bimodal resin is critical here because surface scratches act as stress concentrators during the entire service life, and the resin’s high tie-molecule density reduces the ductile-to-brittle failure transition even when notch depth approaches 0.1 mm on the pipe exterior.

    Slurry abrasion and chemical resistance data for PE100 industrial piping

    Industrial slurry and chemical transfer lines made from PN049-030-122 are specified where low internal pressure fluctuations and abrasive particulates coexist, although published abrasion-resistance data for this exact grade is limited compared with elastomer-modified PE compounds. The governing standards for industrial polyethylene piping include ISO 15494 for industrial plastics piping systems, ASTM F714-22 for high-density polyethylene pipe in water and wastewater service, and ISO 9080:2012 for long-term hydrostatic strength derivation. For outdoor installations, the resin is dry-blended with 2.0–2.5 wt% carbon black masterbatch to meet UV weathering expectations, while indoor or buried lines can be extruded without carbon black using a natural stabilised compound, with no recycled content permitted when the conveyed fluid is classified as a hazardous chemical under local regulations. Extrusion of thick-wall industrial pipe uses a single-screw extruder with L/D 33:1 to 37:1, a grooved feed bushing, and a melt pump to stabilise output to ±1%; melt temperatures are controlled at 200–230 °C, and die head pressures commonly reach 20–40 MPa on diameters above DN/OD 500 mm. The terminal pipe geometries are DN/OD 110 mm to DN/OD 1000 mm, with dimension ratios from SDR11 to SDR26, giving pressure ratings from PN6 to PN16. In mineral slurry transport, the primary operational boundary is that HDPE exhibits lower mass loss under wet sliding abrasion than PVC-U or cast iron, but the absence of a standardised slurry abrasion test method for PE means that end users must validate performance through loop testing with actual particle size distributions rather than relying on published generic wear factors.

    Can PE100 resin sustain long-term hydrostatic pressure in seawater desalination brine lines?

    Seawater cooling and desalination brine discharge lines require a PE100 resin with high hydrostatic endurance in saline and chlorinated environments, and PN049-030-122 is qualified against the same minimum required strength of 10 MPa criterion as potable water pipe materials under ISO 9080:2012, with pipe dimensions governed by ISO 4427-2:2019 and ASTM F714-22. Because the resin does not require plasticisers or metal-based stabilisers that could leach into brine, the only compounding step for outdoor marine exposure is the addition of 2.0–2.5 wt% carbon black masterbatch to limit UV degradation during above-ground assembly; oxidation induction time is verified to exceed 20 min at 200 °C per ISO 11357-6:2023 for long-term thermal stability in warm seawater. The extrusion process for large-diameter marine pipe uses a 33:1 L/D single-screw extruder with a spiral mandrel die and melt temperatures of 200–230 °C, followed by vacuum calibration tanks of 6–10 m in length to maintain roundness on diameters up to dn2000 mm, and cooling water temperatures held at 15–25 °C to minimise residual stress that could accelerate environmental stress cracking in chlorine-bearing seawater. Finished terminal products include submarine intake and outfall lines, desalination plant brine discharge pipes, and power plant cooling water conduits, typically in sizes of dn200 mm to dn2000 mm and dimension ratios of SDR17 or SDR26. The operational boundary in desalination brine is that free chlorine residuals above 2 ppm at continuous exposure should be independently validated for material compatibility, because published long-term data for chlorinated brine contact on this grade is limited and the governing standards do not assign a specific chlorine resistance class for PE100.

    Free Quote

    Competitive Sinopec Wuhan HDPE PN049-030-122 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Wuhan HDPE PN049-030-122 is a bimodal high-density polyethylene pressure pipe grade intended for black compound extrusion in water and gas distribution. The product is classified as PE100 under ISO 12162, with a nominal base resin density of 0.949 g/cm³ when measured by ISO 1183-1:2019 and a melt mass-flow rate of 0.30 g/10 min at 190 °C under 5 kg per ISO 1133-1:2022. The grade is positioned for pipes evaluated against ISO 4427-2 for water transport and ISO 4437-2 for gaseous fuel distribution. Published representative values from producer technical documentation list a minimum required strength of 10.0 MPa at 20 °C for 50 years under ISO 9080:2012, placing the material in the PE100 hydrostatic design class rather than the older PE80 class. The resin is typically compounded with 2.0–2.5 wt% carbon black according to ISO 6964 to provide ultraviolet stabilization for long-term outdoor storage and buried service.

    Which Hydrostatic Design Class and Pipe Certification Standards Apply to PN049-030-122?

    As a PE100 material, PN049-030-122 is evaluated against the hydrostatic test ladder of ISO 9080:2012 and the classification scheme of ISO 12162. The 10 MPa minimum required strength at 20 °C for 50 years is not a service limit but a design stress basis. Pipe pressure ratings derive from the ISO 4427-2 equation P = 2 × MRS / (C × (SDR − 1)), where C is 1.25 for water. At SDR 11 the calculated nominal pressure rating is 16 bar; at SDR 17 the rating is 10 bar; at SDR 21 the rating is 8 bar. For gas service under ISO 4437-2, the same SDR geometries are generally assigned lower operating pressures because the design coefficient for combustible fluid service is larger than the water-service coefficient and national codes impose further limits. Slow crack growth resistance is assessed through the notched pipe test of ISO 13479, in which pipe specimens are subjected to 4.6 MPa hoop stress at 80 °C in a wetting agent. PE100 pipe compounds of this molecular architecture typically exceed 165 h in the notched pipe test before brittle failure, but published data for this specific Sinopec Wuhan grade at every stress level remains limited. Rapid crack propagation performance, when required for gas pipe, is characterized by the S4 method of ISO 13477 at 0 °C.

    The bimodal molecular weight distribution of PN049-030-122 creates two distinct chain populations: a low molecular weight fraction that lowers melt viscosity and improves processability, and a high molecular weight fraction that raises the density of load-bearing tie molecules between crystalline lamellae. The mechanistic result is increased resistance to slow crack propagation under constant hoop stress. Equipment-specific behavior on grooved-feed single-screw extruders indicates that this distribution lowers melt pressure sensitivity at high screw speeds compared with unimodal HDPE of similar 0.30 g/10 min melt flow, although molecular orientation in thick-walled pipe remains a processing constraint.

    Representative values from Sinopec technical documentation are summarized below. These values are typical of the base resin and black pipe compound; lot-to-lot variation should be confirmed on the inspection certificate for each delivery.

    PropertyTest methodRepresentative value
    Melt mass-flow rate, 190 °C/5 kgISO 1133-1:20220.30 g/10 min
    Density, base resinISO 1183-1:20190.949 g/cm³
    Carbon black contentISO 69642.0–2.5 %
    Tensile stress at yield, 50 mm/minISO 527-2:2012 type 1B23 MPa
    Tensile strain at breakISO 527-2:2012 type 1B>600 %
    Flexural modulus, 2 mm/minISO 178:2019800 MPa
    Charpy notched impact strength, 23 °CISO 179-1:2010/1eA26 kJ/m²
    Charpy notched impact strength, -30 °CISO 179-1:2010/1eA11 kJ/m²
    Oxidation induction time, 200 °CISO 11357-6:2018>30 min

    Extrusion of PN049-030-122 is typically performed on single-screw extruders with 30:1 to 33:1 L/D ratios and grooved feed zones. Die melt temperature should remain between 200 °C and 230 °C. At melt temperatures above 240 °C, oxidative degradation begins to consume the antioxidant package, and the measured oxidation induction time can fall below the 20-min pipe standard minimum after prolonged residence time. On grooved-feed lines, screw speeds above 120 rpm may generate melt temperature overshoot in the metering section, particularly when barrel zones are set to compensate for high melt pressure. Pre-drying is not normally required when the resin is stored in intact packaging below 60% relative humidity; material exposed to ambient moisture at higher humidity should be surface-dried at 80 °C for 2 h to avoid surface splay. During die assembly, the melt pressure drop through the spiral mandrel should be monitored at the die entry because the high molecular weight fraction increases die swell and can alter wall thickness control in the vacuum calibration tank.

    Primary pipe applications include municipal potable water distribution, raw water transfer, industrial liquid transport, and gaseous fuel distribution where the design stress and temperature limits of PE100 are accepted. In continuous water service at 20 °C, the long-term hydrostatic strength under ISO 9080:2012 supports design stress calculations rather than short-term burst tests. For gas distribution, operational limits are typically 40 °C maximum continuous temperature, and design codes impose lower pressure ratings than water service because of the safety factors associated with combustible fluids. The carbon black content stabilizes the pipe against ultraviolet embrittlement during outdoor storage; however, prolonged exposure to strong oxidizing chemicals at concentrations above the limits defined in ISO/TR 10358 can consume the antioxidant package and initiate surface cracking. The grade is compatible with dilute acids, alkalis, and aqueous salt solutions at ambient temperatures, but it is not recommended for continuous immersion in strong oxidizing media. Aromatic hydrocarbons, chlorinated solvents, and some synthetic oils cause swelling and loss of mechanical strength. When used in mine dewatering or industrial effluent, the end user should verify chemical resistance at the specific concentration and temperature using ISO 4433-1 immersion testing or supplier chemical resistance data.

    Slow Crack Growth Resistance and the Bimodal Molecular Weight Distribution

    Unlike blow-molding HDPE resins with melt flow rates of 1.0–10 g/10 min or injection-molding grades with melt flow rates above 20 g/10 min, PN049-030-122 is not optimized for thin-wall blow molding or high-cavitation injection molding. Its 0.30 g/10 min melt flow rate, high molecular weight, and broad bimodal distribution are selected for long-term hydrostatic creep resistance and slow crack propagation resistance in extruded pipe. When compared with commodity HDPE used in caps or containers, the PE100 product exhibits longer notched pipe failure times under ISO 13479 and higher resistance to internal pressure creep at 80 °C, but it requires higher melt pressure and is less suited to long-flow-length injection tools. The high tie-molecule concentration between lamellar crystals reduces microcrack propagation under constant hoop stress, which is the dominant failure mechanism in buried pressure piping.

    When a PE80 Line Converts to PE100, the Same SDR Yields Higher Pressure Capacity

    Relative to a PE80 compound with an MRS of 8.0 MPa, PN049-030-122 permits a thinner wall at identical operating pressure or a higher pressure at identical SDR. For an SDR 11 water pipe, the calculated nominal rating moves from 12.8 bar for PE80 to 16 bar for PE100 under ISO 4427-2 using the 1.25 design coefficient. For this reason, conversion of an existing PE80 extrusion line to PN049-030-122 requires recalculation of pipe wall thickness to maintain the same hydraulic performance and adjustment of haul-off speed because the lower melt flow rate of this PE100 grade reduces throughput at identical screw speed and melt pressure.

    SDRCalculated water service nominal pressure at 20 °C
    SDR 920 bar
    SDR 1116 bar
    SDR 13.612.5 bar
    SDR 1710 bar
    SDR 218 bar
    SDR 266.4 bar

    Within the PE100 family, grades with higher melt flow rates, such as 0.45 g/10 min or 0.50 g/10 min, offer lower extrusion pressure and higher maximum line speed for thin-wall pipe. PN049-030-122, at 0.30 g/10 min, is positioned toward the high-molecular-weight end of the PE100 processing window; this can reduce die drool but may require a longer barrel temperature profile. Published data comparing the exact slow crack growth performance of this Sinopec Wuhan grade with higher-MFR PE100 alternatives is limited, but the reduced melt flow rate is generally associated with a higher tie-molecule density and longer notched pipe survival times under ISO 13479. Processors should confirm inspection-certificate values for melt flow rate, oxidation induction time, and carbon black content before qualifying replacement of an incumbent PE100 resin in certified drinking-water or gas pipe production.

    Top