    Specifications
    HS Code 775413
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.35 g/10 min
    Tensile Yield Strength ≥ 24 MPa
    Elongation At Break ≥ 600%
    Flexural Modulus ≥ 1000 MPa
    Notched Izod Impact Strength ≥ 30 kJ/m²
    Environmental Stress Cracking Resistance ≥ 1000 h
    Vicat Softening Temperature ≥ 120 °C
    Brittleness Temperature ≤ -70 °C
    Shore D Hardness 65
    Melting Point 130 °C
    Water Absorption < 0.01%

    As an accredited Sinopec Wuhan HDPE HD5502S factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Wuhan HDPE HD5502S is supplied in 25 kg net-weight polyethylene woven bags, palletized and stretch-wrapped for secure bulk handling.
    Container Loading (20′ FCL) Sinopec Wuhan HDPE HD5502S is packed in 25kg bags and loaded into 20ft FCL containers, typically 25 metric tons per container.
    Shipping Sinopec Wuhan HDPE HD5502S is a non-hazardous high-density polyethylene resin. It is supplied in 25 kg bags or 500–1000 kg jumbo bags, palletized, stretch-wrapped, and shipped in 20'/40' containers by sea/land. Not regulated as dangerous goods; keep dry, away from heat and UV. Standard freight conditions apply.
    Storage Store Sinopec Wuhan HDPE HD5502S in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and moisture. Keep original bags sealed on pallets; avoid contact with oils, chemicals, and strong odors. Maintain moderate temperature, use first-in-first-out, and observe stacking limits. Protect from UV exposure and humid conditions. Do not store near oxidizing agents or odorous materials.
    Shelf Life Shelf life is typically 24 months when stored in a cool, dry, well-ventilated area, away from direct sunlight and moisture.
    Application of Sinopec Wuhan HDPE HD5502S

    In 20 L UN-certified tight-head jerrican production, HD5502S is processed on accumulator-head shuttle blow molders with single-screw extruders of L/D 24:1 to 30:1 and compression ratios between 3.0:1 and 3.5:1. The melt temperature is maintained at 180–210 °C, while the die head temperature is set 5–10 °C below melt to reduce parison sag and stabilize die swell. Finished packages must pass UN Model Regulations Chapter 6.1.5 performance tests, including a 1.2 m drop height for Packing Group II liquids and a 100 kPa internal pressure hold for 30 min; lot release also references ASTM D1693-15b Condition B environmental stress-cracking resistance at 50 °C in 10% Igepal CO-630. The formulation is 100 parts HD5502S virgin resin with 1.5–2.5 wt% UV-stabilized color masterbatch and a maximum of 25 wt% clean in-house regrind of the identical grade; masterbatch loading above 3.0 wt% is avoided because it can reduce ESCR and impact strength in chime corners. Parison programming with 5–10 discrete thickness steps compensates for thinning at the shoulder and pinch-off zones, targeting 1.8–2.2 mm sidewall and 2.5–3.0 mm shoulder thickness. Terminal outputs include 1 L, 5 L, 10 L, and 20 L UN-marked jerricans and 60 L open-head drums with gasketed EPDM closures.

    When Does a Reciprocating Screw Blow Molder Reduce Pinch-Off Failures in Automotive Washer Reservoirs?

    Automotive washer reservoir conversion on a reciprocating screw blow molder introduces a weld-line integrity limit because the part wall thickness varies from 1.5 mm to 3.0 mm at the pinch-off. HD5502S is compounded with 100 parts base resin, 1.0–2.0 wt% heat-stabilized color masterbatch, and 0.5–1.0 wt% UV stabilizer masterbatch; total masterbatch content is limited to 3.0 wt% to avoid reducing pinch-off seam strength. On a 65 mm screw with L/D 24:1, the melt temperature is held at 175–195 °C, mold coolant inlet temperature is 8–12 °C, and blow pressure is 0.5–0.7 MPa. The pinch-off knife is set to leave residual flash of 0.3–0.5 mm; flash below 0.2 mm correlates with leakage at the weld line during ASTM D543-21 immersion testing in methanol-based washer fluid. OEM qualification commonly applies ISO 16750-4 thermal cycling from −40 °C to 80 °C and ASTM D648 heat deflection verification for underhood exposure. Terminal products include 3 L, 4.5 L, and 5 L windshield washer reservoirs, auxiliary fluid reservoirs, and integrated cap assemblies.

    In agricultural pesticide container conversion, a dual requirement of solvent stress-cracking resistance and prolonged outdoor UV endurance governs the formulation. HD5502S is let down at 100 parts with 1.0–2.5 wt% UV stabilizer masterbatch and 1.0–2.0 wt% pigment masterbatch; total non-resin fraction is maintained below 4.0 wt% because higher loadings reduce melt strength and create parison drawdown instability on narrow-neck bottles. Extrusion blow molding on a long-stroke accumulator machine with L/D 24:1 uses barrel zone temperatures from 160 °C to 200 °C, a die temperature of 185–205 °C, and a mold temperature of 10–20 °C. Leak tightness is verified at 20 kPa compressed air, and container closure integrity is tested with the actual pesticide formulation for 48 h at 40 °C; lot acceptance requires 95% retention of top-load capacity after immersion. Compliance references UN Model Regulations Chapter 6.1, FAO/WHO Guidelines for the Packaging and Storage of Pesticides, and 40 CFR 156.150 child-resistant closure requirements for US registrations. Terminal products are 1 L, 5 L, 10 L, and 20 L narrow-mouth bottles with induction-seal or desiccant closures.

    Institutional Cleaning Chemical Bottles Demand Torque-Verified Child-Resistant Closures

    Institutional cleaning chemical bottle production from HD5502S is typically a low-complexity continuous shuttle operation at 100 parts resin and 1.0–2.0 wt% pigment masterbatch, processed at melt temperatures of 175–195 °C and blown into 1 L and 5 L trigger-spray bottles, where ISO 8317:2015 child-resistant closure testing and EU Regulation (EC) No 1272/2008 CLP child-resistant packaging provisions govern the final package.

    Application segmentCore standard/codeCritical test parameterAcceptance criterion
    UN-certified jerricansUN Model Regulations 6.1.5Drop height Packing Group II1.2 m, no leakage
    Automotive washer reservoirsASTM D543-21Immersion in methanol-based washer fluidNo stress cracking after 48 h at 40 °C
    Agricultural pesticide containersFAO/WHO packaging guidelinesClosure integrity with actual formulation95% top-load retention after 48 h at 40 °C
    Institutional cleaning bottlesISO 8317:2015Child-resistant closure testingPer ISO 8317:2015 child/adult protocol
    Large tight-head drumsUN Model Regulations 6.5Hydraulic pressure hold100 kPa for 30 min, no leakage
    Multi-layer barrier bottlesASTM D3985Oxygen transmission rate at 23 °C, 50% RH< 5 cm³/(m²·day·atm)
    PCR non-food bottlesEN 15343:2007Recyclate traceability and MFR stabilityMFR variation within ±15% of virgin grade

    When the shot weight exceeds 8 kg on large-part accumulator-head machinery, the bottleneck shifts from melt plastication to parison sag. HD5502S is processed at 100 parts with 0.5–1.0 wt% antioxidant masterbatch and up to 15 wt% clean in-house regrind; higher regrind fractions above 20 wt% are not recommended for 220 L tight-head drums because melt strength loss can increase sidewall thinning at the top chime. The extruder is a 120 mm grooved-feed single-screw unit with L/D 30:1, running barrel temperatures from 165 °C to 200 °C and a die head at 185–200 °C; parison wall thickness after expansion is 6–10 mm before mold closing, and blow pressure is 0.6–0.9 MPa. Mold cooling water is held at 12–18 °C, and cycle time for a 220 L tight-head drum is typically 300–420 s. Compliance testing follows UN Model Regulations Chapter 6.5 for rigid plastics IBC inner containers and Chapter 6.1 for large drums; periodic design qualification requires a 1.2 m drop test on the top chime and a 100 kPa hydraulic pressure hold for 30 min. Terminal products are 120 L, 150 L, and 220 L tight-head drums and 1000 L IBC bottle inserts.

    If Multi-Layer Coextrusion Is Deployed for Oxygen-Sensitive Industrial Fluids

    Multi-layer blow molding for oxygen-sensitive industrial fluids uses HD5502S as the structural outer layers because its parison melt strength supports a 5–6 layer structure without encapsulation defects. The total HD5502S fraction is commonly 55–65 wt% of the bottle wall, with EVOH barrier at 3–5 wt%, tie-layer adhesive at 2–4 wt%, and regrind layer at 20–30 wt%; each layer ratio is confirmed by layer thickness measurement to prevent EVOH discontinuity. Coextrusion blow molding requires separate extruders for each layer: a 80 mm main extruder for HD5502S, a 35 mm barrier extruder, and a 25 mm tie-layer extruder, feeding a multi-layer die head at 190–210 °C. The process window is narrow: if the barrier layer drops below 3 wt%, oxygen transmission rate measured by ASTM D3985 at 23 °C and 50% RH rises above 5 cm³/(m²·day·atm); if the HD5502S outer layer fraction exceeds 70 wt%, interlayer adhesion measured by ASTM F904 may become the failure mode due to shear history differences. Published data for this specific HD5502S/EVOH/tie-layer combination is limited; therefore first-article qualification must include peel testing per ASTM F904 under 23 °C and 50% RH before line approval. Compliance for industrial fluids packaging also requires UN Model Regulations Chapter 6.1 and, where applicable, REACH Article 33 communication for substances of very high concern in the final article. Terminal products are 5 L, 10 L, and 20 L multi-layer bottles for oxygen-sensitive solvents, adhesives, and chemical intermediates.

    SegmentHD5502S loadingAdditive/masterbatch loadingMelt temperature rangeBlow pressure
    UN jerricans100 parts1.5–2.5 wt% UV colour180–210 °C0.6–0.9 MPa
    Automotive washer reservoirs100 parts1.0–2.0 wt% colour + 0.5–1.0 wt% UV175–195 °C0.5–0.7 MPa
    Agricultural pesticide containers100 parts1.0–2.5 wt% UV + 1.0–2.0 wt% pigment160–200 °C0.5–0.8 MPa
    Institutional cleaning bottles100 parts1.0–2.0 wt% pigment175–195 °C0.5–0.7 MPa
    Large tight-head drums100 parts0.5–1.0 wt% antioxidant + up to 15 wt% regrind165–200 °C0.6–0.9 MPa
    Multi-layer barrier bottles55–65 wt% of wallEVOH 3–5 wt% + tie 2–4 wt%190–210 °C0.6–0.8 MPa
    PCR non-food bottles60–80 wt%20–40 wt% PCR + 1.0–2.0 wt% compatibilizer175–200 °C0.5–0.7 MPa

    Closed-Loop Post-Consumer Recyclate Blending in Non-Food Containers

    For closed-loop post-consumer recyclate blending in non-food containers, the start point is 60–80 wt% virgin HD5502S and 20–40 wt% cleaned post-consumer HDPE, with 1.0–2.0 wt% compatibilizer masterbatch and 0.5–1.0 wt% antioxidant masterbatch to compensate for oxidative degradation of the recyclate fraction. The recyclate must meet EN 15343:2007 traceability requirements for plastics recycling and the packaging waste recovery provisions of EU Directive 94/62/EC; each lot requires melt flow rate testing per ISO 1133-1:2022 Method A to keep lot-to-lot MFR variation within ±15% of the virgin grade. On a continuous shuttle blow molder, the use of 40 wt% post-consumer recyclate raises the melt pressure at constant screw speed by 8–15% and may require a 5–10 °C reduction in the feed-zone temperature to avoid over-shearing; blow pressure is maintained at 0.5–0.7 MPa. Terminal products are 1 L, 5 L, and 20 L non-food cleaning chemical bottles, automotive aftermarket fluid bottles, and non-hazardous industrial packaging where food-contact approval is not required.

    Free Quote

    Competitive Sinopec Wuhan HDPE HD5502S prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Wuhan HDPE HD5502S is a pelletized high-density polyethylene blow moulding resin produced at Sinopec Wuhan Petrochemical’s ethylene complex. The grade is positioned for extrusion blow moulding of rigid containers in the 0.5 L to 20 L class. Class-representative values for this molecular-mass region are a melt mass-flow rate of 0.25 g/10 min to 0.35 g/10 min when measured at 190 °C under 2.16 kg in accordance with ISO 1133-1:2022, and a density of 0.950 g/cm³ to 0.956 g/cm³ when determined in accordance with ISO 1183-1:2019. Published data for this specific configuration is limited; the manufacturer’s technical datasheet and lot-specific certificate of analysis should be used for die design, mould quoting, and process validation because additive package, catalyst residuals, and production-line condition can shift rheological and mechanical values by several percent.

    The main commercial uses are automotive lubricant bottles, household and industrial chemical containers, and agricultural chemical packaging. These service environments make environmental stress crack resistance a primary fitness-for-use criterion. A density of 0.950 g/cm³ to 0.956 g/cm³ provides a balance between container stiffness, top-load performance, and slow stress-crack resistance. The resin is processed on shuttle-type and accumulator-head blow moulding machines. Starting conditions are established on class-equivalent lines with a 65 mm single-screw extruder, 24:1 L/D screw, and a converging blow-head die. Melt temperature at the die exit is typically held between 180 °C and 200 °C. Blow-up ratio is set between 2.0:1 and 3.0:1, and mould temperature is controlled between 10 °C and 30 °C. These are not intrinsic resin limits; they are process boundaries observed across blow moulding grades of similar melt flow and density.

    On a single-station shuttle machine, cycle time for a 5 L container is typically 25 s to 40 s depending on wall thickness, mould cooling, and flash removal. Extruder screw speed is commonly set between 50 rpm and 80 rpm for a 65 mm machine. Initial machine settings derived from class-equivalent HDPE grades are as follows:

    Production-scale batch-to-batch variation in melt mass-flow rate of ±0.03 g/10 min is not unusual for this resin class. When a lot arrives at the upper or lower limit of the specification band, container weight and wall-thickness distribution can shift. Closed-loop parison length control, in-line container weighing, or trimming of the extrusion temperature by ±5 °C is used to compensate. If high ambient humidity persists above 60% relative humidity, surface moisture from storage can generate splay in the pinch-off region. A desiccant dryer set at 80 °C for 2 h reduces this risk; routine pre-drying of HDPE is otherwise unnecessary.

    What Limits Parison Stability in HD5502S Blow Moulding?

    Parison stability is the primary controls issue. The melt-flow ratio, MFR at 21.6 kg divided by MFR at 2.16 kg, is an indirect indicator of molecular weight distribution breadth. Medium-molecular-weight blow moulding HDPE in this class commonly exhibits melt-flow ratios between 25 and 35. A value above 35 indicates greater shear sensitivity and can produce faster drawdown; a value below 25 may raise back-pressure but improves parison hang time. The mould designer should request the producer’s melt-flow ratio and die-swell data rather than infer parison performance from MFR alone.

    On single-station shuttle machines, parison sag is observed as progressive increase in wall thickness from the tail to the top of the container. With a die gap of 1.2 mm to 2.0 mm and parison length exceeding 0.5 m, die swell and drawdown interact non-linearly. The practical corrective sequence is to lower the melt temperature by 2 °C to 5 °C, reduce the blow-up ratio, or adjust the parison programming curve. Increasing die gap alone does not correct sag because it alters both die swell and thickness distribution.

    Thermal history also limits the window. A melt temperature above 210 °C at the die exit can increase gel speck formation and shift colour. Residence time in the accumulator head or screw should not exceed 10 min at 200 °C; longer residence can generate oxidized material at the pinch-off weld and degrade environmental stress crack resistance. Purging after high-flow injection moulding HDPE should use a blow moulding HDPE of similar MFR, not a polypropylene or filled purge compound, to avoid delamination at the pinch weld.

    Blown containers are routinely leak-tested at internal air pressure between 30 kPa and 50 kPa. Pinch-weld failure during this test indicates inadequate melt temperature, contaminated material, improper flash trimming, or excessive moisture at the pinch-off zone. Top-load strength of rigid containers can be measured according to ASTM D2659 or ISO 12048. Drop impact testing at 0 °C or −20 °C is relevant for agricultural chemical containers because HDPE impact resistance decreases with temperature.

    Mechanical property differentiation among HDPE grades is not captured by density alone. Blow moulding HDPE in this density range is class-reported at tensile stress at yield between 24 MPa and 30 MPa according to ISO 527-2:2012, and flexural modulus between 900 MPa and 1200 MPa. Environmental stress crack resistance determined with ASTM D1693-15 in 10% Igepal CO-630 at 50 °C varies with comonomer type and molecular weight distribution; a unimodal blow moulding resin may show an order-of-magnitude lower F50 value than a bimodal large-part grade with lower density. Published data for HD5502S specifically should be obtained from the producer because ESCR is influenced by comonomer length, catalyst residuals, and additive package.

    Class-level differentiation of HDPE conversion processes
    Resin classMelt mass-flow rate, ISO 1133-1Density, ISO 1183-1Dominant processing equipmentPrincipal defect
    Blow moulding, HD5502S class0.25–0.35 g/10 min0.950–0.956 g/cm³Shuttle or accumulator-head blow moulding, 20:1–30:1 L/DParison sag, pinch-weld variation
    Injection moulding HDPE4–20 g/10 min0.955–0.965 g/cm³Reciprocating-screw injection moulding, cold runnerJetting, sink marks
    Film HDPE0.5–1.5 g/10 min0.940–0.950 g/cm³Blown-film die, BUR 3:1–5:1Melt fracture, bubble flutter
    Large-part blow moulding HDPE0.1–0.2 g/10 min0.945–0.952 g/cm³Accumulator-head machine, 80–120 mm extruderGel specks, ESCR loss

    Quality-control testing for blow moulding HDPE should include melt flow, density, tensile yield, flexural modulus, impact resistance, and ESCR. The table below lists the relevant method designations and class-representative ranges.

    Quality-control matrix for blow moulding HDPE
    PropertyTest methodClass-representative rangeRelevance to container use
    Melt mass-flow rateISO 1133-1:20220.25–0.35 g/10 minControls extrusion pressure and parison drawdown
    DensityISO 1183-1:20190.950–0.956 g/cm³Controls stiffness, top-load, and chemical resistance
    Tensile stress at yieldISO 527-2:201224–30 MPaRelates to container burst and pinch-weld strength
    Flexural modulusISO 178:2019900–1200 MPaGoverns stacking stiffness and panel rigidity
    Notched Charpy impactISO 179-1:20105–10 kJ/m² at 23 °CIndicates service impact resistance
    ESCR, F50ASTM D1693-15producer-dependentControls chemical stress-crack resistance

    Compared with high-flow injection moulding HDPE, the HD5502S-class material has a much lower MFR and higher melt viscosity. Injection grades with MFR between 4 g/10 min and 20 g/10 min are unsuitable for parison formation because their low melt strength permits excessive drawdown of a 0.2 m parison even at low head pressure. Conversely, HD5502S is not intended for thin-wall injection moulded closures requiring high flow length-to-wall thickness ratio and short cycle. Attempts to run it in a multi-cavity closure mould with 0.8 mm wall thickness often produce short shots or high injection pressure unless the melt temperature is raised above the recommended blow moulding window.

    Differences from film-grade HDPE are equally significant. Film resins commonly use a density of 0.940 g/cm³ to 0.950 g/cm³ and a broader molecular weight distribution to stabilize the blown-film bubble. HD5502S-class density of 0.950 g/cm³ to 0.956 g/cm³ improves top-load and stack performance for rigid containers but would reduce dart impact and tear resistance in a film application. Differences from large-part blow moulding grades are primarily molecular weight and ESCR; large-drum resins often use MFR values below 0.2 g/10 min and bimodal molecular weight architecture for stress-crack resistance in heavy-walled drums.

    When HD5502S Replaces a High-Flow Injection Moulding Grade in Plant Trials

    Direct substitution is rarely successful without process modification. The screw design for injection moulding HDPE usually uses a metering section optimized for low viscosity; a blow moulding grade with MFR near 0.30 g/10 min increases torque, back-pressure, and residence time. Plant trials should begin by reducing screw speed to limit shear heating and by setting the barrel profile 10 °C to 20 °C hotter in the feed zone than a typical injection grade profile. When the target is a large thick-walled structural part rather than a thin-wall closure, the material may be acceptable, but the gate size and runner diameter must be increased to accommodate the higher viscosity.

    For the intended blow moulding application, the controlling specification is a combination of MFR, density, and melt-flow ratio rather than density alone. A resin with a MFR of 0.30 g/10 min supports a longer parison without drawdown than a resin with MFR of 0.45 g/10 min at the same melt temperature. This permits faster mould closure and a more uniform pinch-off. The trade-off appears as higher extruder discharge pressure and increased energy consumption. In a corrugated mould with a pinch-off flash pocket, a narrow die-swell distribution reduces flash variation; the operator can maintain a constant flash thickness by adjusting the die gap within 1.0 mm to 2.5 mm.

    Multilayer barrier containers may employ HD5502S as the structural layer. In a three-layer structure with an EVOH barrier layer and a maleic-anhydride-grafted tie layer, the HDPE structural layer should be processed within the adhesive’s thermal stability window. The tie-layer vendor normally specifies a maximum melt temperature of 220 °C; excessive temperature reduces adhesion and may generate odour compounds. The converter should confirm that the container’s material identification for recycling is marked 02 HDPE per ISO 11469 or the applicable national packaging marking scheme.

    Clean in-house regrind from tops and tails can be blended up to 20 wt% when approved by the resin producer, provided the regrind is free of dust, label adhesive, and oil contamination. Higher regrind levels reduce ESCR and impact resistance at the pinch weld. Outdoor exposure for agricultural chemical containers typically requires a UV-stabilized variant or masterbatch addition of hindered amine light stabilizer at 0.1 wt% to 0.3 wt%, otherwise HDPE loses impact resistance after prolonged sunlight exposure.

    Chemical compatibility follows general high-density polyethylene limits. HD5502S should not be used for strong oxidizing acids at elevated temperature, continuous service with halogenated solvents, or long-term storage of strong aqueous surfactant systems at elevated temperature because environmental stress cracking can occur at moulded-in stress concentrations. For food-contact applications, a lot-specific food-contact statement is required; the statement should identify the applicable paragraph of 21 CFR 177.1520 or the appropriate European Union regulation, and specify any limits on food type, temperature, or container size. In the absence of such a statement, the material should be limited to non-food industrial chemical containers.