Sinopec Tianjin Hdpe T60 800

Sinopec Tianjin HDPE T60-800

    • Product Name: Sinopec Tianjin HDPE T60-800
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 748891
    Density G Cm3 0.960
    Melt Flow Rate G 10min 190 C 2 16kg 8.0
    Tensile Yield Strength Mpa ≥25
    Elongation At Break ≥500
    Flexural Modulus Mpa ≥1000
    Notched Izod Impact Strength J M ≥40
    Vicat Softening Temperature C ≥120
    Heat Deflection Temperature C ≥70
    Shore D Hardness ≥60
    Melting Point C 130-135
    Crystallinity 80-90
    Water Absorption ≤0.01
    Environmental Stress Crack Resistance H ≥1000
    Volume Resistivity Ω Cm >1E16
    Dielectric Constant 2.3
    Ash Content ≤0.1
    Moisture Content ≤0.1
    Bulk Density G Cm3 0.55-0.60
    Form Pellets
    Color Natural
    Processing Method Injection Molding

    As an accredited Sinopec Tianjin HDPE T60-800 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Tianjin HDPE T60-800 is packaged in 25 kg PE-lined woven bags, securely stacked at 1,000 kg per pallet.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Sinopec Tianjin HDPE T60-800, 25 MT net, 25kg bags, palletized, shrink-wrapped, seaworthy export packing.
    Shipping Sinopec Tianjin HDPE T60-800 is a non-hazardous HDPE resin. Shipped in 25 kg PP woven bags or 1,000 kg jumbo bags, palletized and stretch-wrapped, loaded into 20'/40' FCL containers from Tianjin port. Store dry, away from moisture, sunlight, and heat. HS code: 3901.20. No special dangerous goods documentation required.
    Storage Store Sinopec Tianjin HDPE T60-800 in a cool, dry, well-ventilated warehouse, protected from direct sunlight, rain, moisture, heat, and ignition sources. Keep original packaging sealed and palletized; avoid dust, oil, and chemical contamination. Stack securely without excessive height. Use clean handling equipment. Do not expose to open flames or prolonged ultraviolet radiation. Observe stock rotation and manufacturer’s shelf-life recommendations.
    Shelf Life Shelf life is 24 months from production when stored in original packaging, dry, cool, well-ventilated area, away from direct sunlight.
    Application of Sinopec Tianjin HDPE T60-800

    In returnable logistics crates, Sinopec Tianjin HDPE T60-800 is processed as a high-flow injection molding grade with a melt flow index of 8.0 g/10 min under ASTM D1238-13 Procedure A at 190 °C/2.16 kg and a nominal density of 0.960 g/cm³ under ISO 1183-1:2019. The combination of high flow and high density allows filling of complex ribbed sidewalls and lattice floors without moving to a random copolymer or lower-density grade that would sacrifice top-load stiffness. In a 600 mm × 400 mm bottle crate with wall thickness from 2.5 mm to 3.2 mm, the longest melt flow path from a central sprue or edge fan gate frequently reaches 420 mm. Cavity pressure measured at the end of fill typically lies between 35 MPa and 45 MPa; for a projected part area of 0.24 m², the resulting clamp force requirement is 8,400 kN to 10,800 kN. The barrel temperature profile is commonly set at 190 °C, 210 °C, 220 °C, and 230 °C from rear to nozzle, while mold coolant is held at 8 °C to 20 °C. Shot weight is normally kept between 50 % and 70 % of barrel capacity to avoid residence times above 5 min, which can induce oxidation and odor at nozzle temperatures near 230 °C. Post-industrial regrind from sprue and rejects can be reincorporated at up to 20 wt% for non-food crates after drying to 0.05 % moisture and screening through a 4 mm mesh; higher regrind percentages introduce melt viscosity variability and can reduce weld-line impact performance under ASTM D256-10 Method A. Terminal products in this segment include stack/nest bottle crates, dairy transport crates, bakery trays, produce crates, and collapsible logistics boxes. For products not in direct food contact, REACH Article 33 communication is required only if an SVHC is present above 0.1 % w/w; for crates intended for indirect food logistics, end-product surface cleanliness and overall migration follow the customer’s specified food hygiene protocol rather than a single resin-level limit.

    What Operational Boundary Appears First When Thin-Wall Dairy Tubs Are Molded at a Nominal 8.0 g/10 min?

    The first operational boundary in thin-wall dairy packaging is gate freeze-off time versus cavity pack pressure. For a 200 ml round yogurt cup with a wall thickness of 0.55 mm, filling time of 0.08 s to 0.15 s at injection velocity 250 mm/s to 400 mm/s is short enough to reach the rim before freeze-off, but the process window requires holding pressure of 45 MPa to 60 MPa to compensate 1.5 % to 2.0 % volumetric shrinkage. Mold temperature between 15 °C and 30 °C is used for cycle time control; dropping coolant below 10 °C can produce a frozen skin layer that delaminates near the gate during pressure transfer. The grade’s density of 0.960 g/cm³ contributes to rim stiffness and stackability in single-serve cups, but the same high density reduces dart-drop toughness relative to lower-density polyethylene grades. Food-contact compliance for this segment is not met by the resin alone; converters must test the final article under FDA 21 CFR 177.1520, EU Regulation (EU) No 10/2011 with its amendments, and GB 4806.7-2016 where applicable. Overall migration into aqueous food simulants is limited to 10 mg/dm² or 60 mg/kg under EU 10/2011 Annex V. Terminal products include yogurt cups, cottage cheese tubs, single-serve creamer cups, and disposable dessert containers. The use of the grade in hot-filled or microwaveable containers is not advisable without thermal distortion verification under ASTM D648-16, because HDPE homopolymer softens at elevated temperatures and may show rim warpage above 70 °C under sustained load.

    The following compliance and property anchor points frame thin-wall food-service qualification rather than substituting for end-use migration testing:

    Standard / regulationMeasurement scopeRelevant limit or value
    ASTM D1238-13 Procedure AMelt flow index at 190 °C/2.16 kg8.0 g/10 min
    ISO 1183-1:2019Density0.960 g/cm³
    FDA 21 CFR 177.1520Olefin polymers in food-contact articlesEnd-test migration required; no single resin limit
    EU Regulation (EU) No 10/2011Overall migration into food simulants10 mg/dm² or 60 mg/kg
    GB 4806.7-2016Polyethylene food-contact materialsTotal migration 10 mg/dm²; additive SML applies

    Closure molding for 28 mm tamper-evident beverage caps exploits the same melt flow index to fill buttress threads and pilfer band undercuts at injection pressures from 80 MPa to 110 MPa in 24-cavity or 48-cavity cold-runner or hot-runner molds. Cap skirt thickness is commonly set between 0.85 mm and 1.00 mm, and the high density of T60-800 provides the necessary radial stiffness for removal-torque consistency. A polyolefin-based color masterbatch is typically added at 1.5 wt% to 2.0 wt% in an LLDPE carrier; loadings above 3 wt% can shift the effective melt flow index and should be validated case by case. The grade is best restricted to non-carbonated beverage closures, dry pharmaceutical caps, and overcaps because its homopolymer structure has lower environmental stress crack resistance than hexene-1 or butene-1 copolymer HDPE grades. Where closures contact aggressive detergent formulations, essential oils, or high-chlorine water, the specific grade must be qualified with ASTM D1693-15 bent strip ESCR testing in the packaged product matrix; published ESCR data for this exact grade under those conditions is limited. Application torque on capping lines is usually set at 1.2 N·m to 2.5 N·m, with removal torque measured between 1.5 N·m and 3.0 N·m after 24 h at 23 °C; actual torque values depend on cap geometry, liner type, and bottle neck finish. Compliance for food-contact caps uses FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011; pharmaceutical caps additionally require USP General Chapter 661.1 extraction and leachables evaluation. Terminal products include still-water caps, dairy bottle closures, overcaps for sports bottles, and moisture-protective screw caps for dry pharmaceuticals.

    When a Straight-Sided Industrial Pail Lid Is Gated Centrally in a Two-Plate Tool

    Central gating of a 20 L pail lid with a nominal diameter of 300 mm and wall thickness 2.0 mm forces radial melt flow and creates a shrinkage profile that differs between the gate region and the periphery. Differential cooling often produces flatness deviation of 1.5 mm to 3.0 mm across the lid diameter if holding pressure is constant and cooling is uneven; a decaying hold profile from 50 MPa to 25 MPa over 5 s to 8 s reduces overpacking near the central sprue. Coolant temperature is maintained at 12 °C to 18 °C, with high-flow bubbler channels or conformal cooling around the gasket groove and tamper-evident hinge to balance heat removal. The processed lid is normally ejected at a surface temperature below 65 °C to avoid post-ejection distortion in stack cooling racks. For pails used as non-hazardous liquid containers, article-level tests include ASTM D648-16 for heat deflection, ASTM D790-17 for flexural stiffness across the lid, and ASTM D1693-15 for environmental stress cracking when the package may contact oils or hydrocarbon-based liquids. If hazardous goods packaging is required, the filled pail must be qualified under UN 1H1 or 1H2 performance tests, including drop, stacking, and leakproofness as prescribed by ADR 6.1 or 49 CFR 178.500; the resin itself is not certified, only the final packaging system can be certified. Terminal products in this segment include 5 L to 25 L industrial pails, agricultural chemical buckets, building material containers, and food ingredient pails with tamper-evident lids.

    Houseware storage articles such as desktop drawers, laundry baskets, and utility boxes are molded with wall thicknesses of 2.0 mm to 3.0 mm, where the high density of 0.960 g/cm³ provides surface hardness and dimensional stability; cycle time is controlled mainly by part ejection temperature of 60 °C to 70 °C rather than by a narrow melt-pressure window.

    Free Quote

    Competitive Sinopec Tianjin HDPE T60-800 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Tianjin HDPE T60-800 is a pelletized high-density polyethylene resin identified by the grade designation T60-800. The nominal density is 0.960 g/cm³ and the melt flow rate is reported under ISO 1133-1:2022 at 190°C/5.0 kg as 0.80 g/10 min; these values are release-controlled and vary within production tolerances. The resin is supplied for extrusion conversion, primarily in PE100 pressure-pipe and thick-section profile applications. It is not intended as a thin-wall injection molding material. The high molecular weight design gives the material a high low-shear viscosity and slow crack growth resistance; the exact rheological profile must be confirmed from the batch certificate before line setup. Published data for this specific configuration is limited in some secondary application areas, and qualification trials should use lot-specific data rather than class-typical values.

    What Limits the Melt Temperature Window in Single-Screw Extrusion?

    The practical melt temperature boundary is set by oxidative degradation above 240°C and incomplete fusion below 195°C. On a grooved-barrel single-screw extruder with an L/D ratio of 30:1 to 36:1, barrel setpoints are maintained from 180°C at the feed throat to 220°C in the metering zone. The die head is set at 210°C to 225°C. Melt temperature at the die entry should remain below 230°C; continuous operation above 240°C accelerates thermo-oxidative chain scission and forms oxidized gel particles on the screw root and breaker plate. Below 195°C, the high molecular weight fraction remains incompletely fused, producing surface roughness and poor weldline strength in the pipe wall.

    The grooved feed section of 3D to 5D axial length must be water-cooled to prevent premature melting and feed bridging. The compression ratio of the screw is typically 2.5:1 to 3.0:1; barrier flights separate the solid bed from the melt pool. If a standard three-zone screw is used without barrier elements, output stability may degrade because the material's high viscosity at low shear resists melting and creates pressure oscillations at the die. A gear pump operating at constant discharge pressure can isolate the die from screw-generated pulsations and improve wall-thickness control at die throughput above 400 kg/h. Screen pack pressure at the breaker plate is monitored and typically remains below 15 MPa before filter replacement. A mesh configuration of 60/80/120 is acceptable for gel removal; a pressure rise of more than 10 MPa over a 24-hour run indicates a need to reduce melt temperature or verify stabilizer dispersion.

    Pre-drying is not mandatory at controlled indoor relative humidity below 50%. If pellets are stored in unheated warehouses or exposed to relative humidity above 60%, drying in a desiccant hopper dryer at 70°C to 80°C for 2 to 4 hours reduces surface moisture below 0.005 wt%. Drying above 90°C risks pellet softening and bridging in the hopper. The resin should not be blended with amine-containing masterbatches unless validated, because alkaline additives can disturb the stabilizer system and shorten oxidative induction time.

    Hydrostatic Strength, Slow Crack Growth, and PE100 Classification

    Long-term pressure performance is assessed under ISO 9080 and ISO 12162. A PE100 material class requires an extrapolated 50-year hydrostatic strength of at least 10.0 MPa at 20°C. Pipe extruded from T60-800 is subjected to sustained internal pressure testing under ISO 1167 at 20°C, 60°C, and 80°C; failure is required to be ductile rather than brittle within the specified test windows. The notched pipe test under ISO 13479 at 80°C and 4.6 MPa is used to confirm resistance to slow crack growth in the presence of a defined axial notch. This property is the principal differentiator from many unimodal HDPE resins. Slow crack growth resistance depends on tie-molecule density between lamellae; the bimodal molar mass distribution of the T60-800 class retains a high molecular weight fraction that increases crack pinning and decreases crack-tip advance.

    The high molecular weight fraction contributes to slow crack growth resistance, while the low molecular weight fraction improves shear thinning. Melt flow rate alone does not capture this balance; oscillation rheometry at 190°C is used to track the crossover modulus and the high molecular weight tail. An upward shift in crossover modulus outside the control limit may indicate crosslinking or high gel content. Batch consistency is also checked by oxidative induction time under ISO 11357-6 at 200°C; a value below the agreed minimum indicates antioxidant depletion during processing or storage.

    Indicative property windows and test designations for T60-800
    Property Test method Class-typical window Condition
    Density ISO 1183-1 0.959–0.961 g/cm³ 23°C
    Melt flow rate ISO 1133-1 0.70–0.90 g/10 min 190°C/5.0 kg
    Tensile yield stress ISO 527-2 24–28 MPa 50 mm/min, Type 1B
    Elongation at break ISO 527-2 greater than 600% 50 mm/min
    Flexural modulus ISO 178 1100–1300 MPa 2 mm/min
    Charpy notched impact ISO 179-1/1eA 25–40 kJ/m² 23°C
    Oxidative induction time ISO 11357-6 at least 20 min 200°C, O₂
    Vicat softening temperature ISO 306/A50 125–128°C 10 N, 50°C/h
    Hardness Shore D ISO 868 65–70 15 s

    Direct substitution of T60-800 for a general-purpose HDPE blow molding grade is not recommended. Blow molding resins with densities of 0.945–0.955 g/cm³ and melt flow rates at 2.16 kg between 0.2 g/10 min and 0.7 g/10 min are formulated for parison melt strength and surface finish, not for hydrostatic design basis. T60-800 shows a higher low-shear viscosity and a stronger shear-thinning response, which is beneficial in thick-wall pipe but causes short-shot behavior in thin-wall injection molds. In capillary rheometry at 190°C, apparent viscosity can drop by 60% to 80% between shear rates of 10 s⁻¹ and 1000 s⁻¹; the exact curve must be taken from the converter's own lot data because rheology varies with batch and carbon black content.

    When T60-800 Replaces PE80 in Buried Pressure Networks

    Compared with a PE80 resin, T60-800 permits higher design stress for the same service lifetime. Under EN 1555 and ISO 4427, PE100 pipe can be designed with a thinner wall than PE80 for the same nominal pressure, reducing mass per metre and installation weight. The trade-off is that the higher molecular weight raises melt viscosity and requires a more robust extrusion drive. In field failure analysis, PE100 grades are differentiated by their resistance to brittle crack propagation in low-temperature environments. The pipe-grade resin is tested for resistance to rapid crack propagation under ISO 13477; a critical pressure lower than the operating pressure at 0°C is unacceptable for gas distribution. Published data for T60-800 under ISO 13477 should be obtained from the resin supplier or pipe certification body before gas-network qualification.

    Comparison of material classes
    Material class Density Melt flow rate condition Design basis Main limitation
    T60-800 PE100 pipe resin 0.959–0.961 g/cm³ 0.80 g/10 min at 190°C/5.0 kg 10.0 MPa MRS High melt viscosity; UV stabilization required for outdoor exposure
    PE80 pipe resin 0.945–0.955 g/cm³ 0.5–1.0 g/10 min at 190°C/5.0 kg 8.0 MPa MRS Thicker wall required at equivalent pressure rating
    General-purpose HDPE injection resin 0.958–0.965 g/cm³ 8–20 g/10 min at 2.16 kg Not pressure-rated Low slow crack growth resistance; unsuitable for pressure pipe

    Fabricating Large-Diameter Thick-Wall Pipe on Grooved-Barrel Lines

    Large-diameter pipe extrusion of T60-800 places specific demands on the calibration system. For diameters above 400 mm and wall thickness above 30 mm, vacuum spray cooling is used to remove heat at the outer surface, while internal air pressure maintains roundness. The high melt strength prevents sagging in the unsupported distance between the die and the sizing sleeve. However, residual thermal stress in thick walls can arise if the outer surface is quenched below 40°C while the inner wall remains above 120°C. Therefore, cooling tanks are operated with stepwise water temperatures from 35°C to 60°C, followed by a final spray section at 20°C. Production lines running T60-800 at high output may require torque-limited screw speeds above 80 min⁻¹; the screw design must avoid excessive shear heating. Wall thickness distribution is measured by ultrasonic gauges after the second cooling tank to maintain tolerances in accordance with ISO 4427-2 or EN 1555-2.

    Release testing includes oxidative induction time at 200°C under oxygen; the value must exceed 20 min. The base pellet is stabilized with a hindered phenolic primary antioxidant and a phosphite secondary antioxidant. The stabilizer package is optimized for pipe extrusion residence times of 2 to 8 min; longer residence times at high temperature can consume the antioxidant and create a yellowness shift. In black pipe production, carbon black masterbatch should have a particle size below 25 nm and a volatile content below 0.1 wt% to avoid microvoids at the carbon black-polymer interface.

    Food-contact use is not assumed from the base resin designation. If the finished pipe or profile is intended for potable water, the converter must verify organoleptic and migration compliance under the relevant national transposition of the EU Drinking Water Directive or FDA 21 CFR 177.1520. The natural resin formulation may require additional UV stabilisers for outdoor storage exceeding 12 months; carbon-black compounds with 2.0 wt% to 2.5 wt% well-dispersed carbon black provide the required UV resistance under ISO 16871. Processing above 250°C should be avoided even for short residence times because the stabilizer system is not designed for high-temperature coating or lamination processes.

    Top