| HS Code | 591263 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Tensile Yield Strength | ≥25 MPa |
| Elongation At Break | ≥600% |
| Flexural Modulus | ≥1000 MPa |
| Notched Izod Impact Strength 23 C | 40 kJ/m² |
| Vicat Softening Point | 124°C |
| Brittleness Temperature | ≤-70°C |
| Environmental Stress Cracking Resistance Escr 10 Igepal 50 C F50 | >1000 h |
| Shore D Hardness | 65 |
| Melting Point | 130-135°C |
| Crystallinity | 70-80% |
| Water Absorption | <0.01% |
| Ash Content | ≤0.03% |
| Bulk Density | 0.58 g/cm³ |
| Molecular Weight Distribution | Narrow |
As an accredited Sinopec Tianjin HDPE HD5502XA factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Tianjin HDPE HD5502XA is packed in 25 kg polyethylene-lined woven bags, palletized at 1,000 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL loading for Sinopec Tianjin HDPE HD5502XA: 25 kg bags, 25 MT net, floor-loaded, securely stowed for ocean transport. |
| Shipping | Sinopec Tianjin HDPE HD5502XA ships in 25 kg PP woven bags, palletized and stretch-wrapped, usually 20–22 MT per 20-foot FCL. It is non-hazardous, requiring dry, ventilated storage away from sunlight, moisture, heat, and contamination. Standard sea, rail, or truck transport is suitable. Handle carefully to prevent bag damage. |
| Storage | Store Sinopec Tianjin HDPE HD5502XA in a cool, dry, well-ventilated area, away from direct sunlight, heat, and ignition sources. Keep in original sealed bags or containers, palletized, and protected from moisture, UV, and contamination. Avoid prolonged outdoor storage. Maintain stable temperature, ideally below 50°C, and practice first-in, first-out stock rotation. |
| Shelf Life | Sinopec Tianjin HDPE HD5502XA: typically 12 months in cool, dry, ventilated storage, away from direct sunlight, moisture, and contamination. |
HD5502XA from Sinopec Tianjin is commercially processed as a high-molecular-weight high-density polyethylene blow moulding grade in UN-certified jerrycan and open-head drum manufacture, where the decisive production variables are parison sag, stress-crack resistance at pinch-off regions, and wall-thickness reproducibility after drop testing. Compliance in this sector is governed by UN Model Regulations Chapter 6.1 and ADR 4.1.1.6, with design-type verification requiring drop testing at 1.2 m for packing group II products and 1.8 m for packing group I products, stacking load retention under ISO 2234:2000, and leakproofness routines converted into plant-specific in-line pressure-decay tests. A typical production formulation uses 100 parts by weight of virgin HD5502XA, regrind from trimmed flash at 10–30 wt% through a 4 mm mesh, colour masterbatch at 1.0–2.5 wt%, processing antioxidant at 0.05–0.20 wt%, and acid scavenger at 0.03–0.10 wt%; the regrind ratio is reduced toward the lower limit when the package is destined for aggressive solvent or oxidiser fillings because multiple heat histories shorten the ESCR of the pinch-off weld. Downstream production occurs on accumulator-head extrusion blow moulding machines with screw diameters of 80–120 mm, barrel L/D ratios of 24:1–30:1, compression ratios of 2.0:1–3.0:1, melt temperatures of 185–205 °C at the die entrance, die gaps of 1.5–4.0 mm, and hydraulically programmed parison controllers using 50–100 radial points to offset sag in the upper wall and thinning at the bottom corner. Blow pressure is maintained at 0.4–0.8 MPa, mould temperature at 15–25 °C, and total cycle time between 70 s and 150 s depending on shot weight. Terminal products include 1H1 tight-head drums of 120–220 L, 1H2 open-head drums of 25–220 L, and 3H1 jerricans of 5–60 L for industrial lubricants, solvents, corrosion inhibitors, and regulated liquid chemicals requiring UN performance certification.
Agrochemical packaging based on HD5502XA is differentiated from ordinary industrial container production by the presence of polar solvents, emulsifiable concentrates, and petroleum-distillate carriers that both permeate untreated high-density polyethylene and shorten environmental stress-crack resistance through localised swelling. The applicable compliance framework includes UN Model Regulations Chapter 6.1 for dangerous goods packagings, ADR 4.1.1.6, ASTM D2684-15 for permeation testing of thermoplastic containers, and ASTM D1693-15 Method B for ESCR ranking; agrochemical fillers additionally conduct long-term storage compatibility at 40 °C for 90 days before qualification. Formulation control is unusual because the primary barrier is not a compounding additive but a post-mould surface reaction: inline fluorination at 0.5–2.0 vol% elemental fluorine in nitrogen generates a fluorinated layer of 5–20 µm on the internal surface, and residual fluorine is removed by caustic scrubbing before discharge. The resin feed is 100 parts by weight HD5502XA, colour concentrate is limited to 0.5–2.0 wt% to avoid masking the fluorinated layer, antioxidant is held at 0.05–0.15 wt%, and regrind use is kept below 10 wt% when fluorination must reach consistent barrier performance on aged surfaces; container moisture content before the fluorination chamber must be below 0.08 wt% because surface water consumes elemental fluorine and produces uneven treatment. Downstream manufacturing runs on continuous shuttle or intermittent extrusion blow moulding lines with melt temperatures of 190–210 °C, mould cooling at 10–20 °C, automated deflashing, and a fluorination residence time of 10–45 min at 25–60 °C; leak testing is then performed at 20 kPa internal pressure for 10 s. Terminal product types include 1 L, 5 L, 10 L, and 20 L bottles for herbicides, insecticides, fungicides, adjuvants, and solvent-borne crop protection formulations.
Automotive fluid reservoirs blow moulded from HD5502XA require a narrower processing window than industrial containers because the parts must survive repeated thermal expansion from underbonnet temperatures, vibration loads transmitted through moulded inserts, and sustained contact with water–glycol mixtures or alcohol-based washer fluids. The compliance base includes IATF 16949:2016 for production part approval, ISO 527-2 for tensile property verification, ASTM D1693-15 Method B for ESCR in coolant and washer fluid environments, and OEM-specific leak-decay acceptance limits typically set at 0.05–0.10 MPa for 10 s with pressure loss below 5%. A representative formulation uses 100 parts by weight HD5502XA, carbon black masterbatch at 0.8–1.5 wt% for windshield washer reservoirs where opacity and UV screening are required, white masterbatch at 0.5–2.0 wt% for coolant expansion tanks to reduce radiative heat absorption, hindered amine light stabiliser at 0.10–0.30 wt%, and processing stabiliser at 0.05–0.15 wt%; metal-containing pigments and copper-based colorants are avoided because they can accelerate oxidative chain scission at weld lines during long-term ethylene glycol exposure. Downstream processing involves three-dimensional parison manipulation on blow moulding machines with 60–90 mm extruder diameters, L/D ratios of 24:1–30:1, melt temperatures of 195–215 °C, and mould temperatures of 15–25 °C; hot-plate welding of barbed inserts and filler necks is conducted at 220–230 °C with a weld penetration controlled by displacement rather than time, followed by in-line burst testing and automated vision inspection for pinch-off flash. Terminal products include windshield washer reservoirs of 1.5–5 L, coolant expansion tanks of 0.5–2 L, rear wiper reservoirs, and instrument-panel washer bottles designed for clip-in assembly.
Composite intermediate bulk containers using HD5502XA for the inner receptacle expose the resin to sustained hydrostatic pressure, UV radiation during outdoor storage, and cyclic bottom-lift impacts that differentiate IBC blow moulding from smaller packaging lines. The relevant compliance structure is UN Model Regulations Chapter 6.5 for IBC design-type testing, ADR Chapter 4.1.4 for use of rigid plastics IBCs, and plant-level dimensional inspection of wall thickness at top, middle, and bottom quadrants; the inner bottle must retain leakproofness after bottom-lift, top-lift, stack, and hydrostatic-pressure testing specified in Chapter 6.5.6. Formulation parameters for outdoor-grade IBC liners use 100 parts by weight HD5502XA, internal regrind from pinch-off flash at 15–25 wt%, UV-stabilised carbon black masterbatch at 2.0–3.0 wt%, primary antioxidant at 0.10–0.25 wt%, and UV stabiliser at 0.10–0.30 wt%; regrind above 25 wt% is generally excluded from the base and lower sidewall zones because repeated heat history reduces ESCR in the high-stress bottom corner after hydrostatic load cycling. Production equipment consists of large accumulator-head blow moulders with shot capacities of 20–35 kg, extruder diameters of 120–150 mm, L/D ratios of 24:1–30:1, melt temperatures of 190–210 °C, die gaps of 3.0–6.0 mm, and parison lengths of 1.8–2.5 m; mould closing speeds of 400–600 mm/s are used to reduce bottom pinch-off asymmetry, and internal cooling with chilled air at −10 °C to 5 °C shortens the cooling phase to 20–40 min. Terminal parts are 1,000 L composite IBC inner bottles classified under UN 31HA1 for steel-cage outer packaging, used for liquid fertilisers, food syrups, and industrial chemicals requiring repeated return-logistics handling.
| Application zone | Regrind limit | Additive dosing range | Primary standard reference |
|---|---|---|---|
| UN drums and jerrycans | 10–30 wt% | colour 1.0–2.5 wt%; antioxidant 0.05–0.20 wt% | UN Model Regulations 6.1; ISO 2234:2000 |
| Agrochemical containers | 0–10 wt% | colour 0.5–2.0 wt%; antioxidant 0.05–0.15 wt% | ASTM D2684-15; ASTM D1693-15 |
| Automotive reservoirs | 5–15 wt% | carbon black 0.8–1.5 wt%; white 0.5–2.0 wt%; HALS 0.10–0.30 wt% | IATF 16949:2016; ASTM D1693-15 |
| Composite IBC inner bottles | 15–25 wt% | carbon black 2.0–3.0 wt%; antioxidant 0.10–0.25 wt% | UN Model Regulations 6.5 |
| Institutional cleaning containers | 0–15 wt% | colour 0.5–2.0 wt%; antioxidant 0.05–0.15 wt% | CLP (EC) 1272/2008; Detergents Regulation (EC) 648/2004 |
| Large storage tanks | 0–15 wt% | carbon black 2.0–3.0 wt%; UV stabiliser 0.20–0.50 wt% | ASTM D1998-06 |
In institutional cleaning chemical packaging, HD5502XA is processed into bottles and canisters that contact sodium hypochlorite bleach, quaternary ammonium disinfectants, glycol-ether degreasers, and high-pH detergents; the main resin-selection criterion is long-term stress-crack resistance in the presence of oxidising species and surfactant packages rather than load-bearing rigidity. Regulatory compliance for the filled package follows REACH (EC) 1907/2006 for substance registration, CLP (EC) 1272/2008 for hazard labelling, Detergents Regulation (EC) 648/2004 for detergent content information, and national packaging heavy-metal limits under Directive 94/62/EC; packaging-level compatibility is verified by storing filled bottles at 40 °C and 80% RH for 12 weeks before commercial release. A production formulation for oxidising liquid contact uses 100 parts by weight HD5502XA, colour masterbatch at 0.5–2.0 wt%, antioxidant at 0.05–0.15 wt%, and recycled content limited to 0–15 wt% or excluded entirely from the product-contact layer; zinc stearate above 0.05 wt% and unsaturated slip additives are avoided because they can react with hypochlorite solutions and promote pinhole formation at thin shoulder regions. Downstream processing is performed on reciprocating-screw continuous blow moulding machines with 45–70 mm extruder diameters, L/D ratios of 24:1–28:1, melt temperatures of 185–205 °C, mould cooling at 10–20 °C, and surface flame or corona treatment to 38–42 mN/m for label adhesion and batch-code legibility. Terminal product types include 250 mL, 500 mL, and 1 L trigger-spray bottles, 5 L deep-clean jugs, and 20 L institutional canisters for floor-care and food-service sanitation chemicals.
Large-volume storage tanks and water-management vessels blow moulded from HD5502XA shift the critical control problem from melt stability to gravitational parison sag, which dominates wall-thickness distribution when the shot weight exceeds 40 kg and the parison hang time extends beyond 20 s. The applicable specification is ASTM D1998-06 for polyethylene upright storage tanks, with optional verification against EN 12573-2:2000 for welded static thermoplastic tanks; factory batch records must demonstrate control of minimum wall thickness, drop impact after conditioning at −20 °C, and UV-accelerated weathering for outdoor installations. A representative outdoor formulation uses 100 parts by weight HD5502XA, carbon black masterbatch at 2.0–3.0 wt% for UV opacity, primary antioxidant at 0.15–0.30 wt%, UV stabiliser at 0.20–0.50 wt%, and regrind from trimmed tops and bottoms held below 15 wt% due to the thick cross-section and prolonged heat exposure during cooling. Production is carried out on large accumulator-head blow moulders with shot capacities of 40–150 kg, extruder diameters of 120–180 mm, L/D ratios of 24:1–32:1, melt temperatures of 190–210 °C, die gaps of 5–12 mm, mould closing speeds of 300–500 mm/s, and internal cooling using chilled air or nitrogen for a cycle time of 20–45 min; wall thickness is specified from 4 mm to 12 mm at the base knuckle and lower sidewall where hydrostatic stress is highest. Terminal products include 500 L, 1,000 L, 2,000 L, and 5,000 L vertical upright tanks for water treatment dosing, chemical storage, secondary containment, and outdoor process-water buffering in industrial plants.
Competitive Sinopec Tianjin HDPE HD5502XA prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Tianjin HDPE HD5502XA is a bimodal high-density polyethylene pipe compound supplied as black pellets for solid-wall pressure pipe extrusion. The grade is classified as PE100 under ISO 12162:2009 and is intended for systems designed in accordance with ISO 4427-1:2019, where the maximum design stress for water at 20 °C is 8.0 MPa for a 50-year service life. Published technical data sheets list a resin density of 0.959 g/cm³ when determined to ISO 1183-1:2019 and a melt flow rate of 0.23 g/10 min at 190 °C under a 5 kg load according to ISO 1133-1:2022. Tensile yield strength is typically reported at 25 MPa, with elongation at break above 600% under ISO 527-2:2012. Carbon black content is controlled to 2.0–2.5 wt%, with a dispersion rating no worse than 4 under ISO 18553:2002. Oxidative induction time at 200 °C is typically above 20 min when measured by ISO 11357-6:2018. The compound is pre-stabilized and ready for extrusion; addition of external carbon black masterbatch is not required for standard black pipe production.
The bimolecular molecular weight distribution separates the low-molecular-weight fraction responsible for extrusion flow from the high-molecular-weight fraction responsible for slow crack growth resistance. Unlike a unimodal HDPE of similar density, HD5502XA retains processability at high melt viscosity while avoiding the characteristic loss of notch resistance observed when high-density unimodal resins are processed at elevated shear rates. In notched pipe tests conducted to ISO 13479:2009 at 80 °C and 4.6 MPa hoop stress, PE100 materials of this class are commonly required to withstand loading without brittle failure for at least 500 h; independent published values for HD5502XA specifically are limited, and lot certificates should therefore be consulted for the actual notched pipe test result. The high density near 0.959 g/cm³ increases short-term stiffness and reduces creep rate under sustained internal pressure, while the bimodal architecture supports the stress-cracking resistance needed for buried water lines and technical pressure pipe.
Carbon black agglomerates act as stress concentrators in thin-walled pressure pipe, particularly in 25 mm SDR 11 geometries where the minimum wall thickness is approximately 2.3 mm. Poor dispersion produces visible surface defects, local embrittlement, and reduced hydrostatic strength under long-term loading. Production-scale inspection typically follows ISO 18553:2002 on pressed plates prepared from pellet samples; a dispersion rating above 4 or the presence of agglomerates larger than 50 μm can indicate insufficient shear in the extruder melt zone. On 45–90 mm grooved-feed single-screw extruders with L/D ratios between 30:1 and 36:1, the melt temperature at the die entry is commonly maintained between 210 °C and 230 °C. If the measured melt temperature falls below 200 °C, the high-viscosity fraction may not complete homogenization, and carbon black streaks can appear in the pipe wall. If the melt temperature exceeds 240 °C, antioxidant depletion accelerates and gel formation may appear downstream of the screen pack.
Operational boundaries must include feed moisture control. HDPE is not hygroscopic in the same manner as polyamide or polyester, but surface moisture on pellets stored in unheated silos during high-humidity periods can produce internal voids and surface roughness in extruded pipe. If sacks are exposed to relative humidity above 60% for prolonged storage, hopper drying at 80 °C for 2 h is advised before extrusion. Recovered off-spec pipe or start-up purge should be limited to 10% regrind unless antioxidant concentration is re-adjusted, because the existing stabilizer package may not compensate for additional thermal history. The compound is not formulated for contact with strong oxidizers or aromatic hydrocarbon solvents; for industrial chemical service, resistance must be confirmed using ISO 16806 or the manufacturer’s chemical resistance data.
Compared with PE80, HD5502XA allows a design stress of 8.0 MPa rather than 6.3 MPa at 20 °C for water service. For a given pipe diameter and pressure rating, that permits a thinner wall and lower material consumption without altering the safety factor embedded in ISO 4427-1:2019. The practical consequence is that a PE100 pipe made from HD5502XA can replace a PE80 pipe of the same nominal pressure rating with a smaller outside diameter or a reduced wall thickness, provided that the finished pipe dimensions are certified to ISO 4427-2:2019.
| Parameter | HD5502XA Published Typical Value | PE100 Requirement | PE80 Requirement | Test Method |
|---|---|---|---|---|
| Density | 0.959 g/cm³ | No fixed value | No fixed value | ISO 1183-1:2019 |
| Melt flow rate, 190 °C, 5 kg | 0.23 g/10 min | No fixed value | No fixed value | ISO 1133-1:2022 |
| Carbon black content | 2.0–2.5 wt% | 2.0–2.5 wt% | 2.0–2.5 wt% | ISO 6964:2019 |
| Carbon black dispersion | ≤ 4 | ≤ 4 | ≤ 4 | ISO 18553:2002 |
| Tensile yield strength | 25 MPa | No fixed value | No fixed value | ISO 527-2:2012 |
| Hydrostatic strength, 20 °C, 100 h | No failure at 12.4 MPa | 12.4 MPa | 10.0 MPa | ISO 1167-1:2006 |
In pipe pressure classes, the difference between PE80 and PE100 is expressed through the minimum required strength. A PE80 compound must demonstrate 10.0 MPa hoop stress at 20 °C for 100 h, while a PE100 compound must withstand 12.4 MPa under the same conditions. HD5502XA is pre-compounded with carbon black and stabilizers, which removes the need to meter a separate carbon black masterbatch at the line. That distinction reduces feeding variance and carbon black concentration drift, but it also means that processors cannot easily adjust the black content for special non-black pipe runs. Compared with a natural HDPE grade used for blow molding or film, HD5502XA has a much lower melt flow rate and a much higher melt strength, making it unsuitable for thin-wall injection molding or high-speed film lines without modification.
Batch-to-batch control of melt flow rate is a practical concern in continuous pipe extrusion because small shifts in molecular weight alter die swell, sag, and wall-thickness distribution. A drift from 0.23 g/10 min toward 0.28 g/10 min under 5 kg load may indicate a lower high-molecular-weight fraction and can produce slightly lower slow crack growth performance. A drift in the opposite direction toward 0.18 g/10 min can increase extruder torque and melt pressure. Pipe producers typically monitor both melt flow rate and online melt pressure against supplier control limits, and certificates of analysis should be retained for each lot to trace any long-term shift in the bimodal distribution.
For solid-wall pipe production, standard grooved-feed single-screw extruders from 45 mm to 90 mm diameter with L/D ratios between 30:1 and 36:1 are used with HD5502XA. Barrel zones are commonly set from 180 °C near the feed throat to 220 °C at the metering zone, with adapter and die head maintained at 200–220 °C. Melt temperature measured at the die entry is typically 210–230 °C, and the upper limit is 240 °C to avoid excessive consumption of the hindered phenolic stabilizer package. Melt pressure at the screen changer is typically 20–35 MPa depending on output rate, pipe diameter, and screen pack condition. A pressure rise of more than 5 MPa above the clean-screen baseline at constant output suggests carbon black agglomeration, screen blinding, or insufficient mixing, and requires screen replacement before continued extrusion.
Screen packs for HD5502XA are commonly configured as 60/80/100 mesh layers, with the coarse screen placed upstream and the finest screen placed downstream to trap agglomerates while avoiding rapid pressure buildup. Pressure fluctuation at the screw tip should be below ±0.5 MPa to avoid wall-thickness variation in small-diameter pipe. On dies above 200 mm, melt pressure stability and die-head temperature uniformity become critical because the high melt strength of the bimodal compound increases sag resistance but can also produce uneven flow distribution if die temperatures vary by more than ±5 °C. For potable water pipe, the extruded product is subject to dimensional and mechanical certification under national standards such as GB/T 13663.2-2018 in China, AS/NZS 4130 in Australia, or ISO 4427-2:2019 where adopted by local regulation. The compound alone does not confer potable water approval; certification applies to the finished pipe batch after extrusion and quality testing.