    Specifications
    HS Code 843645
    Polymer Type High-density polyethylene (HDPE)
    Density 0.960 g/cm³
    Melt Flow Rate 8.0 g/10 min at 190°C/2.16 kg
    Melting Point 133°C
    Vicat Softening Temperature 125°C
    Heat Deflection Temperature 75°C at 0.45 MPa
    Tensile Yield Strength 28 MPa
    Elongation At Break >500%
    Flexural Modulus 1200 MPa
    Notched Charpy Impact Strength 6 kJ/m² at 23°C
    Hardness 65 Shore D
    Water Absorption <0.01% after 24 h
    Mold Shrinkage 1.5-3.0%

    As an accredited Sinopec-SK (Wuhan) HDPE T60-800 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec-SK (Wuhan) HDPE T60-800 is packed in 25 kg woven bags, 40 bags per pallet, totaling 1,000 kg.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Sinopec-SK (Wuhan) HDPE T60-800, 25 kg bags, palletized and shrink-wrapped, securely loaded into a 20′ FCL.
    Shipping Sinopec-SK (Wuhan) HDPE T60-800 ships as a non-hazardous thermoplastic resin. Standard packaging: 25 kg PP woven bags or 1 MT jumbo bags, palletized and containerized. Transport in clean, dry trucks, railcars, or ocean containers. Store away from moisture, heat, and direct sunlight. No special dangerous-goods handling required.
    Storage Store Sinopec-SK (Wuhan) HDPE T60-800 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, ignition sources, and strong oxidizers. Keep original bags sealed, palletized, and off the floor. Avoid punctures, contamination, and excessive stacking. Maintain clean handling areas and normal ambient temperatures. Rotate stock first-in, first-out. Follow local regulations and the manufacturer’s safety data sheet.
    Shelf Life Shelf life approximately 12 months under cool, dry, well-ventilated storage, away from direct sunlight, moisture, and contaminants, in original packaging.
    Application of Sinopec-SK (Wuhan) HDPE T60-800

    Across high-speed injection lines with clamp force from 1600 kN to 2200 kN and 45 mm general-purpose screws at L/D 22:1, T60-800 is processed at melt temperatures of 215 °C to 240 °C. The nominal melt flow rate of 8.0 g/10 min at 190 °C/2.16 kg per ASTM D1238 or ISO 1133-1 and the nominal density of 0.960 g/cm³ per ASTM D1505 or ISO 1183-1 support wall sections from 0.6 mm to 0.9 mm in dairy cups and deli containers. Cavity fill pressure is sustained between 65 MPa and 90 MPa when injection speed is set at 100 mm/s to 140 mm/s and the sprue bush orifice is 3.2 mm. Hold pressure of 30 MPa to 40 MPa is applied for 0.8 s to 1.5 s before gate freeze. A screw cushion of 4 mm to 8 mm is held to dampen pressure oscillation from the carriage manifold.

    Regrind from closed-loop sprues and runners is accepted up to 20 wt% with virgin pellet when melt filtration uses an 80 mesh screen pack. At addition above 30 wt%, gate blush appears on polished cavity surfaces and the melt-pressure trace shows high-frequency instability. The base resin normally requires no pre-drying when warehouse humidity is below 55 %RH. Above 60 %RH, pellet is dried at 80 °C for 2 h with dehumidified air at a dew point of -30 °C to avoid screw surging and inconsistent shot volume. Round cups are gated at four balanced points into the rim; gate vestige height below 0.3 mm prevents lid interference on high-speed filling lines.

    Food-contact converters apply a high-density polyethylene carrier colour masterbatch at 1.5 wt% to 2.5 wt% and, where faster crystallisation is required, a nucleating masterbatch at 0.05 wt% to 0.1 wt%. The nucleating package can reduce cooling time by 10 % to 15 % but may increase linear shrinkage variation across the cup wall. Finished articles are tested under EU Regulation (EU) No 10/2011 at overall migration < 10 mg/dm², under GB 4806.6-2016 at total migration < 10 mg/dm², and with the base olefin polymer referenced to FDA 21 CFR §177.1520(c). Additive compliance is verified separately with the masterbatch supplier.

    How Does Gate Freeze During Packing Limit Flatness in Stackable Logistic Crates?

    Ventilated logistic crates and agricultural totes from 35 L to 60 L are moulded on toggle presses with clamp force from 4000 kN to 6000 kN and tie-bar spacing above 800 mm. Four to six valve-gated hot runner drops feed the cavity with gate diameters of 3.0 mm to 4.0 mm. Melt temperature is set from 220 °C to 250 °C and mould temperature from 20 °C to 40 °C. When the hold-pressure timer is shorter than the gate freeze time, melt decompression inside the thick wall produces sink marks where base ribs intersect the sidewall. The resulting bottom flatness deviation exceeds 2.0 mm over a 600 mm diagonal in 45 L crates.

    For 45 L crates with nominal wall thickness from 2.5 mm to 3.5 mm, hold pressure is held at 28 MPa to 35 MPa for 10 s to 14 s, and cooling time is set to 18 s to 25 s. The valve gate is closed 0.3 s to 0.5 s before final hold-pressure decay to prevent material flow back into the hot runner. Ejection air blast plus eight or ten lifter cores releases the part at mould opening of 200 mm to 250 mm. In freezer loading, T60-800 without impact modification may not meet drop impact requirements at -20 °C. Notched Izod impact per ASTM D256 and environmental stress crack resistance per ASTM D1693 condition B should be requested from the lot certificate when crates are specified for cold-room or outdoor produce supply chains. Lot-specific shrinkage measured per ASTM D955 is used to correct rib layout because published data for this specific configuration is limited.

    When UN-Certified Pails Are Drop-Tested at Sub-Zero Temperatures

    For open-top pails and tight-head drums from 5 L to 25 L, T60-800 is processed on high-torque reciprocating screw presses with clamp force from 3000 kN to 5000 kN and shot capacity from 1200 g to 2500 g. Wall thickness ranges from 1.8 mm to 2.5 mm. Bottom corner radii are maintained above 3.0 mm to avoid notch-sensitive failure at the transition between base and sidewall. Melt temperature is set from 225 °C to 250 °C, with screw speed from 50 mm/s to 80 mm/s, back pressure from 0.8 MPa to 1.5 MPa, and hold pressure from 35 MPa to 45 MPa for 12 s to 20 s.

    Regrind content in UN-certified pails is limited to 15 wt% first-generation internal scrap after the gate and handle flash are ground. Higher regrind loads reduce low-temperature ductility and increase the failure rate in drop testing. The finished pail is conditioned at -18 °C for 24 h and drop-tested under the drop height specified in UN Model Regulations 6.1.5.3 for the declared packing group and liquid density. Pails with visible gate vestige or weld-line displacement around the handle region can pass at 23 °C and fail at -18 °C. Top-load compression is checked per ASTM D642; a 20 L open-top pail typically supports a top-load force above 800 N without sidewall buckling.

    T60-800 is not specified for prolonged contact with aromatic hydrocarbons, chlorinated solvents, or concentrated oxidising acids above 40 °C. For mildly acidic and alkaline aqueous formulations, compatibility is confirmed by weight change and tensile retention testing per ISO 175 or customer-specific protocols.

    When the same pellet is switched to a 24-cavity hot-runner closure tool, the limiting parameter shifts from injection pressure to gate vestige and holding-pressure stability. Melt temperature is held at 220 °C to 240 °C, mould temperature at 15 °C to 30 °C, and total cycle time from 12 s to 18 s. Valve-gate drops of 1.5 mm to 2.5 mm fill each closure at injection pressures below 90 MPa. The gates close 0.2 s to 0.4 s before hold pressure terminates. Gate-string vestige is maintained below 0.5 mm to avoid interference with the liner sealing surface.

    Closures and overcaps for dry powders and non-carbonated liquids are tested for leak integrity at 0.3 bar positive internal pressure and for removal torque from 1.5 N·m to 3.0 N·m after 24 h conditioning. Organoleptic panels follow ASTM E1870 for odour and taste transfer where food contact is declared. The base resin and additive package require clearance under FDA 21 CFR §177.1520, EU Regulation (EU) No 10/2011, and GB 4806.6-2016. T60-800 is not recommended for carbonated drink closures in long-term storage because shelf-life stress cracking may exceed the lot-specific environmental stress crack resistance capability.

    In Multi-Cavity Household Storage Tooling, Ejection Forces Determine Cycle Time

    In multi-cavity household storage tooling, the main process constraint is ejector pin drag on polished surfaces rather than maximum injection pressure. T60-800 is moulded at melt temperatures from 210 °C to 240 °C and mould temperatures from 20 °C to 35 °C. Draft angles above 1.0 ° on sidewalls and 3.0 ° on ribs allow release with ejection forces below 15 kN per 1000 g of part weight. Cooling time of 12 s to 22 s is adequate for drawer units, storage boxes, and hangers. Regrind loading up to 20 wt% is tolerated without significant process change; above this level, colour shift in pale tones becomes visible.

    Pallet Feet and Under-Block Moulding With High Regrind Fractions

    Distribution pallet components such as snap-in under-blocks, edge protectors, and pallet feet are injection-moulded from T60-800 on machines with clamp force from 2500 kN to 5000 kN. Part weight ranges from 200 g to 600 g with wall sections between 3.0 mm and 6.0 mm. The thick sections allow hold pressure to be reduced to 20 MPa to 30 MPa for 6 s to 12 s and total cycle time from 35 s to 50 s for a 400 g under-block. The grade accepts up to 30 wt% post-industrial regrind when screen packs and magnetic separators are maintained. Above 30 wt%, voiding at rib intersections and melt-pressure trace irregularity become measurable.

    Black compounds for outdoor-rated units use 1.5 wt% to 2.0 wt% carbon black masterbatch and are assessed under ISO 4892-2 cycle 1 for UV exposure. Compressive strength is measured per ASTM D642; a single under-block in a 1200 mm × 1000 mm pallet commonly withstands a top-load force above 1500 N before creep deformation becomes visible. Fit tolerances between the under-block snap feature and the deck are held within ±0.3 mm by compensating for post-mould shrinkage over 24 h per ASTM D955.

    Free Quote

    Competitive Sinopec-SK (Wuhan) HDPE T60-800 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec-SK (Wuhan) HDPE T60-800 is a high-density polyethylene injection-moulding grade supplied as natural pellets. The grade is defined by a nominal melt mass-flow rate of 8.0 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1 and a nominal density of 0.960 g/cm³ according to ISO 1183-1. These values position the product in thin-wall injection moulding, caps and closures, pails, crates, housewares and industrial containers where reduced filling pressure and shorter cycle time are primary processing requirements. The resin is manufactured at the Wuhan site of the Sinopec-SK joint venture. Lot-specific certificates of analysis should be consulted for batch values; values shown in this technical introduction are typical rather than specification limits.

    What distinguishes T60-800 from lower-flow HDPE injection grades in the same density band?

    At equal mould geometry and melt temperature, a higher melt mass-flow rate lowers apparent viscosity and reduces cavity-filling pressure. Field comparisons from thin-wall container lines using accumulator-assisted injection presses of 1500 kN to 2500 kN with hot-runner valve gates show that raising MFR from 4.0 g/10 min to 8.0 g/10 min can reduce peak injection pressure by 15 % to 25 % for wall thickness below 1.0 mm; however, published data for T60-800 in this exact configuration is limited, and mould-filling simulation should be used for tool-specific confirmation. Compared with lower-flow HDPE injection grades, T60-800 gives shorter fill time and lower residual gate stress but higher sensitivity to drool and valve-pin leakage. Unlike extrusion blow-moulding HDPE with MFR below 1.0 g/10 min, T60-800 lacks sufficient melt strength for parison stability and should not be used in continuous blow moulding.

    The typical property profile below is referenced to the relevant ISO methods and is abstracted from public technical data. These values are not lot-release limits; current certificates of analysis should be requested for production qualification.

    PropertyMethodTypical valueUnit
    Melt mass-flow rate, 190 °C/2.16 kgISO 1133-18.0g/10 min
    Density, 23 °CISO 1183-10.960g/cm³
    Tensile yield stress, 50 mm/minISO 527-226MPa
    Tensile elongation at breakISO 527-2>500%
    Flexural modulus, 2 mm/minISO 1781050MPa
    Notched Izod impact, 23 °CISO 180/A4.0kJ/m²
    Vicat softening temperature, A50ISO 306122°C
    Shore D hardnessISO 86863—

    Processing boundaries in high-speed thin-wall injection

    Melt temperature, mould temperature and injection velocity are interdependent. A typical barrel profile for a general-purpose reciprocating screw is rear 180 °C, centre 200 °C, front 210 °C, nozzle 215 °C; direct melt measurements by air shot should remain within 190 °C to 230 °C. Mould temperature should be held between 20 °C and 50 °C. At mould temperatures below 20 °C, surface skin freezing can interrupt flow in wall sections below 1.0 mm, increasing cavity pressure demand and producing flow marks. At melt temperatures above 230 °C, residence time becomes limiting; above 250 °C measurable chain scission, yellowing and odour formation can occur in unpigmented compound. Screw back pressure in the range 0.5 MPa to 1.0 MPa stabilises melt homogeneity; higher back pressure can raise melt temperature and shift melt mass-flow rate outside the intended window. Injection speed should be profiled to avoid gate blush; on thin-wall tools with 0.8 mm to 1.0 mm nominal wall, velocity-controlled filling is used rather than pressure-limited filling because the latter can produce hesitation marks before the cavity is filled.

    HDPE is not hygroscopic; pre-drying is normally not required for T60-800. If pellets are stored below ambient temperature and then opened under high-humidity conditions, surface condensation can introduce moisture that appears as splay and voids. Under those conditions, pellets should be allowed to reach ambient temperature before use; a mechanical dryer at 80 °C for 1 h may be used only when surface moisture is visible or when regrind has been exposed to moisture. Extended drying above 90 °C can oxidise the pellet surface and shift colour.

    Cavity pressure curves for high-flow HDPE show a characteristic switchover point: after switchover, pressure should rise to a defined holding level and remain above 30 MPa until gate freeze. If cavity pressure decays below 30 MPa before gate freeze, the part may exhibit sink. Tool trials with pressure sensors in the last filling point and gate insert are used to set switchover. Published data for this specific grade in instrumented tools is limited, but general high-flow HDPE behaviour indicates that switchover should occur at cavity fill percentages above 95 % to avoid overpacking and flash.

    Pressure-dependent shrinkage should govern tool cutting for T60-800. In 1.0 mm wall sections, gate freeze must be complete before holding pressure is released; gate freeze times below 2.5 s can produce sink, voiding and post-mould dimensional drift. Mould shrinkage measured to ISO 294-4 in the flow and transverse directions generally differs by 0.2 to 0.4 percentage points, reflecting orientation and crystallinity. The density of 0.960 g/cm³ corresponds to a highly crystalline matrix; unfilled natural T60-800 commonly shows total mould shrinkage of 1.5 % to 2.0 %, but published data for this specific grade is limited and cooling-channel layout should be verified with pressure-dependent PVT measurement. Warpage in rectangular thin-wall containers is aggravated by asymmetric cavity filling; inter-cavity fill imbalance above 0.05 s can produce visible distortion even when total shrinkage is within specification.

    Managing Regrind, Pigmentation and Hot-Runner Transients

    Regrind addition changes viscosity and impact retention. Hot-runner scrap and start-up waste from T60-800 tend to shift melt mass-flow rate upward by 0.5 g/10 min to 1.0 g/10 min after multiple heat cycles; therefore, regrind levels above 20 % may push the compound outside the intended processing window and reduce notched impact. The exact threshold for a specific article should be established by measuring MFR to ISO 1133-1 and notched Izod impact to ISO 180/A on moulded specimens from the intended regrind ratio. White masterbatches based on titanium dioxide at loadings above 4 % can raise injection pressure and reduce weld-line strength because they alter melt elasticity and local skin freezing. In hot-runner valve-pin systems, decompression distance should be sufficient to prevent drool; settings below 2 mm can produce stringing with this high-flow grade. Air vent depth and vent location should also be checked because faster cavity filling can trap gas in blind ribs.

    Production-scale failures observed on thin-wall packaging lines using high-flow HDPE include gate blush when velocity exceeds 300 mm/s, burn marks when vent depth is insufficient, and post-mould shrinkage after stacking when cooling time is shortened below 8 s for 1.0 mm walls. These failure modes are not unique to T60-800 but are amplified by its lower viscosity. The use of cavity pressure sensors and switchover by cavity pressure rather than screw position is recommended for process consistency. On accumulator-assisted machines, peak injection pressure should be recorded for each cycle; a drift above 10 % in peak pressure usually indicates gate blockage or melt temperature shift.

    The natural grade is stabilised for multiple heat histories, but its additive package is not optimised for long-term UV exposure; outdoor applications require an additional UV stabiliser masterbatch, and weathering performance must be tested to ISO 4892-2 or ASTM D2565-21. Natural T60-800 does not include slip or antiblock; caps and closures requiring torque release or low coefficient of friction typically require formulation with a slip additive at the converting line.

    When T60-800 replaces lower-flow HDPE in existing tooling

    Existing tools sized for MFR 2.0 g/10 min or 4.0 g/10 min may not require full redesign, but runner diameter, gate size and venting should be re-evaluated. The lower viscosity of T60-800 permits smaller runner cross-sections or lower packing pressure; however, the same lower viscosity can increase gate stringing and hot-tip drool. Cold-runner diameters can often be reduced by 10 % to 15 % relative to grades with MFR below 4.0 g/10 min, but this is mould-specific and must be confirmed by simulation. Gate size for thin-wall containers should not fall below 0.6 mm when nominal wall is 0.8 mm unless valve-gate speed is tightly controlled. The replacement also changes mould shrinkage and impact retention; holding pressure and cooling time should be re-qualified to ISO 294-4 and ISO 8256 for the target article.

    Regulatory status is article-specific. T60-800 is an olefin polymer that may be evaluated under 21 CFR 177.1520(c) for food-contact uses when the finished article is tested under the intended conditions of use; the manufacturer’s food-contact statement should be obtained before use. European food-contact assessment follows Regulation (EU) No 10/2011 and its overall migration limits; specific migration of additives must be verified on the finished article. Industrial supply is subject to REACH registration obligations and to REACH Article 33 communication when a candidate list substance is present above 0.1 % w/w. RoHS compliance for electrical and electronic applications should be confirmed by batch-level testing according to IEC 62321. These standards define the verification route; they do not by themselves confer product certification.

    In comparison with pressure-pipe HDPE grades classified under ISO 4427, T60-800 has lower long-term hydrostatic strength and lower environmental stress crack resistance, making it unsuitable for pressure pipe and fittings. Compared with extrusion blow-moulding HDPE with MFR below 1.0 g/10 min, T60-800 exhibits lower parison stability and higher drool tendency; replacement is valid only when a high-melt-strength coextrusion layer is validated. Compared with polypropylene thin-wall grades, T60-800 processes at lower melt temperature and offers a different balance of stiffness and low-temperature impact; direct substitution requires full article testing because density and shrinkage anisotropy differ. Published data for T60-800 in highly filled systems or in multilayer injection moulding is limited; these applications require qualification on the target production line rather than reliance on general HDPE property averages.