Sinopec Shanghai Hdpe Sh850

Sinopec Shanghai HDPE SH850

    • Product Name: Sinopec Shanghai HDPE SH850
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 164684
    Density 0.954 g/cm³
    Melt Flow Rate 7.0 g/10 min
    Tensile Strength At Yield 25 MPa
    Tensile Strength At Break 20 MPa
    Elongation At Break 500%
    Flexural Modulus 1000 MPa
    Notched Izod Impact Strength 50 J/m
    Vicat Softening Point 125 °C
    Heat Deflection Temperature 80 °C
    Shore D Hardness 65
    Mold Shrinkage 1.5-3.0%
    Water Absorption <0.01%
    Dielectric Strength 20 kV/mm
    Volume Resistivity >10^16 Ω·cm
    Dielectric Constant 2.3
    Melting Temperature 130-135 °C

    As an accredited Sinopec Shanghai HDPE SH850 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Shanghai HDPE SH850 is packed in 25 kg PE-lined woven bags, 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL loading: Sinopec Shanghai HDPE SH850, 25 kg bags, palletized, approximately 17 MT net, shrink-wrapped and secured for ocean export.
    Shipping Sinopec Shanghai HDPE SH850 is shipped as non-hazardous thermoplastic resin pellets in 25 kg PP bags or 500/1000 kg jumbo bags, palletized or bulk. Transport by truck, container, or rail in dry conditions; keep away from moisture, sunlight, heat, and contamination. No special DG declaration required. Store in a cool, ventilated warehouse. Handle with care.
    Storage Store Sinopec Shanghai HDPE SH850 in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, heat, flames, and strong oxidizers. Keep original bags sealed, palletized, and off the floor. Avoid prolonged UV exposure and excessive stacking. Maintain clean handling to prevent contamination. Use first-in, first-out stock rotation. Ambient temperature storage is recommended; avoid temperatures above 40°C.
    Shelf Life Shelf life is typically 24 months from manufacture when stored unopened in a cool, dry, ventilated area away from sunlight.
    Application of Sinopec Shanghai HDPE SH850

    Stackable Crates and Returnable Handling Totes

    Returnable crates moulded from Sinopec Shanghai HDPE SH850 are produced in steel tools with two to four direct sprue gates or short hot-runner drops. Incoming resin density is checked under ISO 1183-1:2019; typical high-density polyethylene values fall between 0.945 g/cm³ and 0.965 g/cm³. Melt mass-flow rate is verified under ISO 1133-1:2022 at 190 °C and 2.16 kg. The exact lot value is read from the certificate of analysis and used to adjust shot weight and hold time. The melt temperature at the nozzle is maintained between 210 °C and 245 °C. The barrel thermal profile is set with a feed zone at 180 °C, a compression zone at 215 °C, and a metering zone at 230 °C to 245 °C. Mould surface temperature is held between 18 °C and 35 °C using closed-circuit chilled water. Injection velocity is set to complete cavity filling within 0.8 s to 1.2 s for nominal wall thicknesses from 2.0 mm to 3.5 mm. Peak injection pressure is recorded for each shot; values are normally between 80 MPa and 120 MPa. Holding pressure is initially set at 55 % to 65 % of peak injection pressure and then decayed over 5 s to 8 s. Gate freeze must be confirmed by part weight stabilisation before the cooling timer is shortened. Regrind from sprues and rejected crates is added at levels up to 30 wt%. Higher regrind fractions reduce dart impact resistance and increase sidewall warpage in stackable totes. The moulded crate is dimensionally measured after 48 h of ambient conditioning at 23 °C and 50 % relative humidity. Moulding shrinkage along the flow direction typically falls between 1.4 % and 2.0 % when measured according to ISO 294-4:2018. Tensile yield strength of moulded plaques is verified under ASTM D638-14; values in the range of 22 MPa to 32 MPa are expected for high-density polyethylene of this category. Stacking lugs and hand grips are gated through the rim to avoid knit lines in load-bearing corners. Draft angles on sidewalls are held at 1.5° to 3.0° to reduce ejection friction. If the crate is exported to the European Union, packaging heavy metal limits under Directive 94/62/EC apply, with a combined lead, cadmium, mercury, and hexavalent chromium limit below 100 mg/kg. REACH Annex XVII restrictions on polycyclic aromatic hydrocarbons apply if post-consumer recycled material is used in the blend.

    How Does SH850 Behave in Thin-Wall Food Packaging Moulds?

    Thin-wall food packaging produced from Sinopec Shanghai HDPE SH850 is injection moulded at nominal wall thicknesses from 0.40 mm to 0.80 mm. The cavity filling stage must complete before the flow front freezes. Fill time is limited to 0.15 s to 0.40 s for oval tubs and rectangular trays. The material is processed at nozzle temperatures between 220 °C and 245 °C. The mould surface temperature is controlled between 12 °C and 30 °C using a pressurised closed-circuit chiller. Peak injection pressure in thin-wall cavities normally reaches 90 MPa to 130 MPa. Hold pressure is tuned by gate-seal observation; weight stabilisation after hold pressure removal indicates gate freeze. For food-contact packaging supplied to the United States, the product must comply with 21 CFR §177.1520, which covers olefin polymers. For European Union food-contact applications, Regulation (EU) No 10/2011 applies. The overall migration limit is 10 mg/dm² when tested according to EN 1186-1:2002. Specific migration of additives and pigments is verified under EN 13130-1:2004 when the additive is not covered by a generic restriction. Colour concentrates must be formulated with food-contact-grade carriers and additive loading levels that do not raise extractables above the specific migration limits in Annex I of Regulation (EU) No 10/2011. Residual monomers and oligomers are usually below detectable limits for high-density polyethylene. Organoleptic testing according to ISO 13302:2003 may be requested for sensitive dairy or bakery applications.

    Nominal wall thickness (mm)Melt temperature (°C)Mould temperature (°C)Peak injection pressure (MPa)Hold pressure (MPa)Fill time (s)
    0.40–0.55220–23512–20110–13045–600.15–0.30
    0.55–0.75225–24015–25100–12540–550.20–0.35
    0.75–0.90230–24520–3090–11535–500.25–0.40

    High-volume closure moulding lines processing Sinopec Shanghai HDPE SH850 are configured with 48- to 96-cavity valve-gated hot-runner tools. Cavity fill time for a 28 mm PCO 1881 neck finish is typically 0.08 s to 0.20 s. Mould temperature is maintained at 5 °C to 18 °C to reduce cap skirt sticking and stabilise the tamper-evident band undercut. Melt temperature at the nozzle is held at 215 °C to 240 °C. Back pressure is set to 0.3 MPa to 0.8 MPa. High back pressure raises shear work and increases the likelihood of premature environmental stress cracking along the knurl. Screw decompression after plasticising is set to 2 mm to 5 mm to prevent drooling from the hot runner. ESCR is assessed according to ASTM D1693-15e1 in 10 % Igepal CO-630 solution at 50 °C. A failure time below 48 h indicates excessive orientation in the tamper-evident groove or an incompatible additive package. Opening torque for a 28 mm closure is measured between 0.7 N·m and 2.0 N·m. Slip agent loading is controlled at 0.05 wt% to 0.12 wt%. Levels above 0.15 wt% migrate to the sealing surface and compromise gas chromatography headspace analysis. Torque retention is verified by repeated application at 1.8 N·m for 10 cycles after 24 h conditioning at 23 °C. Leak testing is performed according to ASTM D4991-07(2015) with a vacuum of 15 kPa to 30 kPa on capped glass or PET bottles. Closure systems intended for carbonated soft drinks and edible oil must comply with 21 CFR §177.1520 and Regulation (EU) No 10/2011. The additive package must not contain phthalates restricted under REACH Annex XVII.

    Industrial Pallet Moulding Requires Controlled Packing Pressure Decay

    Industrial pallet moulds processing Sinopec Shanghai HDPE SH850 are characterised by long flow lengths and thick deck sections. The nozzle temperature is set at 230 °C to 255 °C. The mould cooling system is divided into zones; water temperature is held at 10 °C to 25 °C. Deck thickness between 8 mm and 20 mm extends cooling time to 45 s to 90 s. Packing pressure is the key variable. A high initial packing pressure of 70 MPa to 90 MPa is applied for 5 s to 10 s, followed by a linear decay to 30 MPa over 20 s to 35 s. The decay profile reduces gate-area sink without overpacking the ribs. Gate freeze is verified by weight stabilisation. If part weight continues to increase after the pressure decay interval, the gate is not sealed and the holding time is extended until weight remains within 0.2 % over three consecutive shots. Clamp force is calculated from the projected pallet area and peak cavity pressure. For a 1,200 mm × 1,000 mm pallet with a projected area of 1.2 m², a cavity pressure of 30 MPa calls for a minimum clamp force of 36,000 kN. Structural acceptance is evaluated under ISO 8611-1:2021. Bending deflection under a uniformly distributed load is measured with linear variable differential transformers placed at mid-span. Racking load tests use conditions selected by the user-specified storage system. Published data for this specific SH850 pallet configuration is limited, so the racking load rating must be established by instrumented testing rather than extrapolation from datasheet tensile values. Warpage after demoulding is controlled by fixturing for 24 h to 48 h at 20 °C to 25 °C. Post-mould shrinkage in the deck thickness can reach 2.0 % to 2.5 % if mould temperature exceeds 25 °C. Anti-slip rubber inserts are over-moulded only after plasma or flame treatment of the HDPE surface to raise surface energy above 42 mN/m.

    In high-volume houseware and storage article production, the material is processed at nozzle temperatures from 210 °C to 240 °C. Mould surfaces are cooled to 15 °C to 30 °C. Injection velocity is set to fill the part in 0.5 s to 1.5 s for wall sections between 1.0 mm and 2.5 mm. Pigment masterbatches with a polyethylene carrier are preferred. Let-down ratios are maintained at 1 % to 4 %. Inorganic pigments such as titanium dioxide are used at 2 % to 3 % when opacity is required. High-molecular-weight hindered amine light stabiliser is added at 0.2 % to 0.5 % for outdoor storage articles. Phenolic antioxidant is added at 0.05 % to 0.10 % to protect the melt during compounding. Articles with living hinges, such as tool cases or accessory boxes, should be gated along the hinge axis to avoid molecular orientation perpendicular to the flexural axis. Continuous service temperature above 65 °C leads to creep, warpage, and loss of interference fit in snap-fit closures. Housewares intended for repeated dishwasher exposure should be designed with a maximum wall thickness of 2.0 mm and should not be exposed to drying cycles above 80 °C. The crystalline morphology of HDPE undergoes partial melting and recrystallisation above this threshold, which increases shrinkage and distorts flat lids. Moulded-in stress is checked by annealing samples at 80 °C for 1 h. Warpage greater than 1.5 mm over a 300 mm span indicates excessive orientation. Articles that contact food directly are excluded from this segment unless the masterbatch and processing aids comply with 21 CFR §177.1520 and Regulation (EU) No 10/2011.

    When Open-Top Pails Are Moulded with In-Mould Labels

    In-mould labelling of open-top pails imposes constraints on melt temperature, label substrate, and ejection mechanics. The label stock is selected from 50 μm to 90 μm biaxially oriented PP or a PP/PE laminate with a low-melting ethylene copolymer seal layer. Label ink and overprint varnish must withstand cavity temperatures up to 60 °C and melt front temperatures of 210 °C to 230 °C. The label is robotically inserted and electrostatically pinned. Charge decay must be less than 60 s to prevent label displacement during injection. Melt temperature is kept below 230 °C to avoid label film shrinkage. This reduction in melt temperature increases peak injection pressure by 8 % to 15 % compared with unlabelled pails of identical geometry. Hold pressure is set between 40 MPa and 55 MPa for pail walls from 1.2 mm to 2.2 mm. The mould is cooled to 10 °C to 20 °C and the cooling time is extended by 5 s to 10 s relative to unlabelled production. Label adhesion is evaluated after 24 h conditioning at 23 °C and 50 % relative humidity. A peel strength below 0.5 N/15 mm may indicate inadequate heat seal activation. Filled pails of 20 L are drop tested at -18 °C from 0.8 m according to ASTM D5276-19. Cracks in the rim or label delamination constitute failure. Pails intended for foodservice or bulk food ingredients must comply with 21 CFR §177.1520 and Regulation (EU) No 10/2011. Label adhesives and inks must also meet the specific migration conditions of Annex I of Regulation (EU) No 10/2011. Volatile compounds from solvent-based inks can increase taint and should be avoided. Handle attachment by metal wire or plastic grip is inserted after moulding. Interference fit between the handle boss and the pail ear must be checked after 72 h because post-mould shrinkage can reduce grip retention.

    Free Quote

    Competitive Sinopec Shanghai HDPE SH850 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Shanghai HDPE SH850 is a high-density polyethylene grade produced by Sinopec Shanghai Petrochemical Co., Ltd. and classified for extrusion blow moulding of small to medium containers. The grade designation SH850 refers to a narrow molecular weight distribution resin in the ethylene copolymer family. Producer-issued certificates of analysis provide lot-specific values for melt index, density, and additive package; therefore, the numerical ranges in this document are class-typical for HDPE blow moulding resins and should be confirmed against the current SH850 technical data sheet. The material is not a general-purpose injection or film resin, and its utility arises from controlled melt strength and parison stability rather than from high flow or high draw-down capability.

    Density is normally determined by ISO 1183-1, and melt flow rate by ISO 1133-1:2022 under 2.16 kg at 190°C. For HDPE blow moulding grades in the same class, density commonly falls between 0.955 g/cm³ and 0.960 g/cm³, while melt index commonly falls between 0.3 g/10 min and 0.5 g/10 min. Tensile yield stress measured by ASTM D638-14 is typically in the range 23 MPa to 30 MPa, and flexural modulus by ISO 178:2019 typically lies between 900 MPa and 1200 MPa. These values support container stiffness, top-load capacity, and dimensional stability after cooling.

    What Limits the Processing Window for SH850 in Continuous Extrusion Blow Moulding?

    On continuous extrusion blow moulding machines, the practical processing window is bounded by melt temperature, die-head pressure, and parison sag. Melt temperature in the SH850 class is usually set between 180°C and 220°C, with the die head maintained within 5°C of the melt stream. At temperatures above 230°C, reductions in melt strength can produce parison draw-down, while temperatures below 170°C can raise die-head pressure and create sharkskin or melt fracture on the parison surface.

    Extruder selection follows the same practice as other HDPE blow moulding resins: a barrier-type single-screw machine with a length-to-diameter ratio of 24:1 to 30:1 is standard. The feed section should be cooled and grooved to stabilise solids conveying. Melt pressure measured before the screen pack on a 65 mm extruder frequently ranges from 150 bar to 250 bar when running small containers, but machine geometry and throughput alter these values. A progressive pressure rise of 5–10 bar at constant screw speed indicates screen-pack loading, which can reduce output and increase melt temperature through shear heating. Published data for SH850 across every clamp force and die configuration is limited; process validation on the target machine is therefore required.

    When the grade is run on shuttle blow moulding equipment with accumulator heads producing 5 L to 25 L containers, parison programming exerts more influence on wall thickness than the resin’s basic rheology. In production-scale trials, wall thickness measured with an ultrasonic gauge or Hall Effect sensor can show a sidewall standard deviation of 0.10 mm to 0.20 mm, but values above 0.25 mm generally indicate parison sag, die swell variation, or incorrect programming. The accumulator head should be set to deliver a fast parison drop with minimal pre-forming time, because blow moulding HDPE grades in this class exhibit measurable sag when hang time exceeds a few seconds at high melt temperature.

    Flash and pinch-off quality are secondary indicators. A pinch-off seam that is translucent or notched under a 10x optical comparator usually reflects insufficient melt strength, excessive melt temperature, or a worn pinch-off insert. Wall sections below 0.4 mm may require higher blow pressure or a different blow moulding grade, particularly in containers with sharp radii or deep handles.

    Melt Strength, Die Swell, and Parison Stability in SH850

    Blow moulding grade design is controlled through molecular weight distribution and comonomer placement. The narrow molecular weight distribution associated with SH850 class resins reduces chain entanglement relative to broad-distribution high-molecular-weight film grades, but the resin must retain enough extensional viscosity to prevent thinning during parison extension. Melt strength is not fully captured by melt index; it is inferred from parison hang time, melt tension, or dynamic rheological data. Class-typical die swell for HDPE blow moulding resins lies between 10% and 30% depending on shear rate, die land length, and melt temperature. Excessive die swell produces flash at the parting line. Insufficient die swell weakens the pinch-off weld and alters bottle handle regions.

    When the resin is compared with a high-load melt index injection-moulding HDPE, the lower melt index of blow moulding grades reduces melt flow into thin-wall sections but improves parison integrity. The result is that SH850 is suitable for containers with wall thicknesses from approximately 0.5 mm to 3.0 mm, depending on tool design and blow ratio. In extrusion blow moulding, blow pressure is commonly set between 6 bar and 10 bar, with blow time adjusted to achieve adequate cooling of the pinch-off and base regions.

    PropertyTest methodClass-typical range for HDPE blow moulding gradesRelevance to SH850 processing
    DensityISO 1183-10.955–0.960 g/cm³Controls top-load, permeation, and part weight
    Melt flow rateISO 1133-1:20220.3–0.5 g/10 minAffects die-head pressure and parison hang time
    Tensile yield stressASTM D638-1423–30 MPaProvides short-term wall stiffness after forming
    Flexural modulusISO 178:2019900–1200 MPaPredicts container rigidity and stacking resistance
    Environmental stress-cracking resistanceASTM D1693-15 condition BGenerally 10–100 h F50Defines chemical resistance boundaries relative to pipe grades
    Brittleness temperatureASTM D746-20Below -60°CIndicates low-temperature impact behaviour during transport

    The values above are class-level indicators for HDPE blow moulding resins and are not a substitute for the SH850 lot certificate. They illustrate the specification logic used by converters when qualifying containers against a target top-load requirement or drop-impact standard.

    If SH850 Is Compared With Pipe-Grade PE100 and Film-Grade HDPE

    PE100 pipe grades are differentiated by bimodal molecular weight distribution and high environmental stress-cracking resistance under ASTM D1693-15 condition B, often exceeding 1,000 h F50 in notched constant-strain testing. Blow moulding grades such as SH850 are optimised for melt strength and die swell, and their ESCR values are generally lower because the molecular architecture is not designed for long-term internal pressure at 20°C, 50 years service. Film-grade HDPE grades are typically designed for high draw-down and bubble stability, with higher melt index or different density ranges, whereas SH850 class resins are selected for parison hang time and container wall uniformity. The comparison is not a quality hierarchy; it is a mismatch of molecular parameters to the fabrication process.

    Processing propertySH850 blow moulding classPE100 pipe classFilm HDPE class
    Melt flow rate under ISO 1133-1:20220.3–0.5 g/10 min0.2–0.4 g/10 min0.5–1.0 g/10 min
    Density under ISO 1183-10.955–0.960 g/cm³0.959–0.965 g/cm³0.950–0.960 g/cm³
    ESCR under ASTM D1693-15Lower, process-orientedHigh, often > 1,000 h F50Moderate, application-dependent
    Primary processing demandParison stability and die swell controlLong-term creep and crack resistanceBubble stability and draw-down
    Typical failure modeParison sag, pinch-off weaknessSlow crack growth, creep ruptureBubble instability, gauge variation

    The table is comparative at the class level. Grade-specific differences between SH850 and another producer’s blow moulding resin may still exist in comonomer type, antioxidant package, and residual catalyst content, which must be checked through the safety data sheet and lot inspection report.

    Regulatory Compliance and Food-Contact Boundary Conditions

    Sinopec Shanghai HDPE SH850 must be evaluated against FDA 21 CFR 177.1520 for olefin polymers when used in food-contact containers, but compliance is not an intrinsic resin property; it depends on the full package construction, processing aids, and migration testing under EU 10/2011 if shipped into European markets. The resin is typically within the scope of REACH and RoHS for heavy-metal restrictions, but converters must verify additive composition with the supplier's safety data sheet. Pre-drying is not normally required for HDPE blow moulding; however, if storage occurs at relative humidity above 60% and condensation is present on pellets, a drying step at 70°C for 2 h may be used to avoid surface defects caused by moisture steam pockets.

    Chemical resistance follows the general HDPE expectation: the resin is resistant to many aqueous salt solutions, dilute acids, and alkalis, but it is unsuitable for continuous immersion in strong oxidising acids, aromatic hydrocarbons, or halogenated solvents, which can cause softening or environmental stress-cracking. Contact with amine-based additives should be avoided in the melt unless compatibility is proven, because they can disturb antioxidant function and prematurely shift the melt-flow stability of the compound.

    In moulding operations that require regrind re-use, the addition of up to 30 wt% of clean, unpigmented regrind is commonly accepted for HDPE blow moulding grades, but higher percentages reduce parison strength and can shift die swell. The operational boundary for regrind content in SH850 should be established by measuring ESCR and top-load on the finished container, because dried-in stresses and contaminant particles accumulate with rework cycles.