    Specifications
    HS Code 727972
    Chemicalname High-density polyethylene
    Casnumber 9002-88-4
    Density 0.956 g/cm³
    Meltflowrate 5.0 g/10 min
    Tensilestrengthatyield 29 MPa
    Tensilestrengthatbreak 30 MPa
    Elongationatbreak >500%
    Flexuralmodulus 1200 MPa
    Izodnotchedimpactstrength 60 J/m
    Vicatsofteningtemperature 127 °C
    Heatdeflectiontemperature 75 °C
    Brittlenesstemperature <-70 °C
    Shoredhardness 65
    Waterabsorption <0.01%
    Moldingshrinkage 1.5-3.0%
    Meltingpoint 130-135 °C
    Crystallinity 80-90%
    Appearance White pellets

    As an accredited Sinopec Shanghai HDPE N1052 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Shanghai HDPE N1052 is supplied in 25 kg PP woven bags and 1,000 kg jumbo bags.
    Container Loading (20′ FCL) Chemical container loading of Sinopec Shanghai HDPE N1052 into a 20′ FCL, prepared for secure, efficient ocean freight shipment.
    Shipping Sinopec Shanghai HDPE N1052 is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg woven bags or 1000 kg jumbo bags, palletized and loaded into 20'/40' containers. Store dry, ventilated, away from direct sunlight and heat. No special dangerous goods documentation required.
    Storage Store Sinopec Shanghai HDPE N1052 in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, moisture, heat, flames, and oxidizing agents. Keep original bags sealed on pallets to prevent contamination, dust, and water absorption. Avoid prolonged UV exposure and excessive stacking. Use first-in, first-out rotation. Store separately from incompatible materials. Ensure clean handling. Follow local regulations and supplier guidance.
    Shelf Life Sinopec Shanghai HDPE N1052 has a shelf life of approximately 24 months when stored cool, dry, and away from direct sunlight.
    Application of Sinopec Shanghai HDPE N1052

    On accumulator-head blow moulding lines producing 220-L tight-head drums for UN Packing Group II liquid hazardous chemicals, HDPE N1052 is run as the continuous phase at 96.5–98.0 wt%, with 1.5–2.5 wt% UV-stabilized carbon black masterbatch, 0.2–0.4 wt% hindered phenol/phosphite antioxidant masterbatch, and 0.1–0.3 wt% fluoropolymer processing aid. Accumulator-head machines with 25:1–30:1 L/D barrier screws deliver melt at 185–200 °C into a programmed parison; axial thickness profiling maintains 2.8–4.2 mm in the sidewall and 4.5–6.5 mm at the pinch zone. Blow pressure is 0.7–1.0 MPa, mould temperature 12–25 °C, cycle 120–180 s per drum, and post-mould cooling 20–30 min under forced air before closure insertion. The critical compliance path is UN Model Regulations Chapter 6.1 for Packing Group II, referenced through ADR and IMDG for road and sea transport; qualification requires drop testing from 1.2 m at −18 °C, hydrostatic pressure of 100 kPa for 30 min, and leakproofness at 20 kPa. ESCR bench screening per ASTM D1693-15, Condition B, 100% Igepal CO-630 at 50 °C, typically requires F50 ≥ 150 h for external chemical drums; lots falling below F50 120 h are excluded from hazardous fill lines. Closed-loop regrind of flash and trim is limited to 15–20 wt% for UN-certified drums; higher loading reduces low-temperature drop impact and increases surface microcracking at base radii. Terminal products include 20-L and 30-L jerrycans, 60-L open-top pails, and 120-L, 160-L, and 220-L tight-head and open-top drums.

    On high-output rotary wheel lines, shot-to-shot melt temperature variation must be maintained within ±4 °C because high-shear heating in low-melt-flow-rate HDPE N1052 generates gel particles that act as stress concentrators in pinch-off welds. Air ring cooling at 0.15–0.35 m³/min per die head, combined with chilled water moulds at 10–18 °C, reduces post-mould diameter shrinkage to 0.5–1.0%. The blow-up ratio is held between 2.5:1 and 3.5:1; above 3.5:1, parison folding at the mould seams creates weak weld lines near the upper head radius. Published data for this specific grade under the full UN drop sequence at −18 °C is limited, so fillers should qualify each tool and regrind level with the complete multi-drop sequence rather than relying on ambient ESCR alone.

    What Food-Contact Migration Test Applies to Blow-Moulded HDPE Milk Bottles?

    For non-carbonated liquid foods such as pasteurised milk, drinking yoghurt, and culinary oils, HDPE N1052 is blended at 98.0–99.0 wt% with 0.5–1.0 wt% titanium dioxide or food-approved colour masterbatch and 0.2–0.4 wt% antioxidant masterbatch; natural unpigmented formulations run 99.3–99.7 wt% resin with 0.3–0.5 wt% process stabilizer. The applicable compliance framework is FDA 21 CFR 177.1520(c) for high-density olefin polymers, EU Regulation 10/2011 Annex I with overall migration below 10 mg/dm² and specific migration limits for each masterbatch additive, and China GB 4806.7-2016 with total migration ≤ 10 mg/dm² and KMnO₄ consumption ≤ 10 mg/kg in food simulants. Production uses shuttle or rotary extrusion blow-moulding machines with 20:1–25:1 L/D screws, melt temperature 170–190 °C, die temperature 180–195 °C, blow pressure 0.6–0.8 MPa, mould temperature 10–18 °C, and cycle times of 8–14 s per 250-mL bottle. Bottle weight for a 250-mL milk bottle is 10–14 g, giving wall thickness 0.35–0.55 mm; a 1-L juice bottle is 28–35 g. The targeted blow-up ratio of 2.5:1–3.2:1 distributes material without excessive sidewall curvature that causes fold lines near the handle. Post-mould flash from pinch points is reintroduced at ≤ 15 wt% for food-contact applications; higher regrind levels risk dark specks and increased migration. Terminal products include 250-mL, 500-mL, and 1-L dairy bottles, 250-mL to 2-L culinary oil bottles, and 200-mL to 500-mL food squeeze bottles for condiments.

    Single-station shuttle blow moulders producing 500-mL to 5-L household detergent and fabric softener bottles run HDPE N1052 at 95.0–97.0 wt% with 2.0–4.0 wt% pearlescent or opaque colour masterbatch, 0.3–0.6 wt% UV/antioxidant package, and 0.1–0.3 wt% fluoroelastomer processing aid to suppress melt fracture at the die lip. The packaging compliance set is lighter than UN packaging: EU REACH Annex XVII and EU Detergent Regulation (EC) No 648/2004 govern the filled detergent product, while the bottle itself must meet EU 10/2011 if sold as reusable or refillable food-adjacent packaging. Extruder temperature profile is 150–185 °C, die 180–195 °C, blow pressure 0.6–0.8 MPa, mould temperature 10–16 °C. ESCR is the dominant material requirement because linear alkylbenzene sulfonate and alcohol ethoxylate surfactants accelerate brittle cracking in stressed HDPE bottle necks; bottle designs keep hoop stress below 4 MPa at the base radius and use 0.45–0.65 mm minimum wall thickness at the shoulder. Terminal products include 500-mL and 1-L detergent bottles, 2-L laundry liquid jugs, and 5-L refill canisters.

    When Under-Hood Ambient Temperatures Exceed 80°C, Cyclic Vibration Governs Reservoir Life

    Extrusion blow-moulded windshield washer solvent and engine coolant overflow reservoirs made from HDPE N1052 operate as semi-structural vessels under ISO 16750-3:2023 environmental loads and OEM component tests that impose thermal cycling from −40 °C to 85 °C plus random vibration of 10–2000 Hz at 0.5–2.0 g RMS depending on mounting location. The formulation for under-hood black parts is 93.0–95.5 wt% HDPE N1052, 3.0–5.0 wt% carbon black masterbatch with UV stabilizer, 0.4–0.8 wt% heat-ageing stabilizer package, and 0.2–0.5 wt% processing aid; for natural translucent reservoirs, carbon black is omitted and a 0.3–0.5 wt% UV stabilizer masterbatch is used. Processing on accumulator-head or shuttle machines uses melt temperature 175–195 °C, die 185–200 °C, blow pressure 0.6–0.9 MPa, and mould temperature 12–20 °C. Wall thickness is 1.2–2.5 mm at mounting bosses and 0.8–1.4 mm in main walls; pinch-off at weld lines must survive 300 kPa burst-pressure testing because the reservoir can see cap-off thermal expansion. Heat ageing per ISO 188 at 100 °C for 500 h should retain ≥ 70% elongation at break; published data for this exact grade in under-hood coolant overflow use is limited, so laboratories benchmark tensile yield by ASTM D638-22 and notched Izod by ASTM D256-23 before final part validation. Terminal products include 2-L washer solvent reservoirs, 1.5-L coolant overflow reservoirs, 3-L emulsion dosing tanks, and 1-L auxiliary fluid containers for commercial vehicles.

    Large open-top HDPE containers for non-hazardous solids and pastes are blow moulded on accumulator-head machines with 25:1–30:1 L/D grooved-feed extruders, using HDPE N1052 at 96.0–98.0 wt%, 1.0–2.5 wt% grey or coloured masterbatch, 0.2–0.5 wt% antioxidant, and 0.1–0.3 wt% processing aid. The controlled window is 175–200 °C melt, die gap 0.5–1.5 mm adjusted by die gap control, blow pressure 0.8–1.0 MPa, and mould cooling 10–18 °C. Part mass ranges from 1.5 kg for a 25-L open-top pail to 15 kg for a 220-L wide-mouth drum; cycle time rises accordingly from 35 s to 180 s. Compliance standards are UN 1H2 for solid packagings where required, ISO 16103 for recycled plastics in transport packagings when regrind exceeds 25 wt%, and the EU Packaging and Packaging Waste Regulation where recyclability declarations are issued. Terminal products include 25-L and 50-L open-top pails, 120-L and 220-L open-top drums, and 500-L to 1000-L blow-moulded intermediate bulk container inner liners.

    Fluorination Service Requires Surface Cross-Hatch Adhesion and Permeation Validation

    Agrochemical bottles for xylene, cyclohexanone, and aromatic petroleum distillates are produced from HDPE N1052 at 96.0–98.0 wt% with 1.0–2.5 wt% carbon black or solid colour masterbatch, 0.3–0.6 wt% antioxidant/UV stabilizer, and 0.1–0.2 wt% processing aid, then post-treated with elemental fluorine gas to form a 5–20 µm surface barrier against hydrocarbon permeation. The process is two-stage blow moulding on shuttle or reciprocating-screw machines with melt temperature 175–195 °C, blow pressure 0.6–0.8 MPa, and mould temperature 12–20 °C, followed by inline or off-line fluorination at 100–200 mbar partial pressure for 5–30 s, then nitrogen purging to below 1 ppm F₂ before unloading. Compliance for the filled pack includes UN 1H1 for liquids, ADR/RID instruction P001, and FAO/WHO specifications for pesticide containers where regional registration demands permeation resistance by an accelerated method such as gravimetric solvent loss over 28 days at 40 °C. Surface adhesion after fluorination is qualified by cross-hatch test to ISO 2409 at classification 1 or better; xylene permeation through the finished 1-L bottle is typically specified at ≤ 2.0 g/(m²·d) at 23 °C, though published data for this specific HDPE N1052 grade under all FAO/WHO formulation variants is limited and requires bottle-by-bottle validation. Terminal products include 0.5-L, 1-L, 5-L, and 10-L fluorinated HDPE agrochemical bottles, 20-L solvent jerrycans, and 1-L in-mould labelled containers for high-value biologicals.

    High-gloss extrusion blow-moulded bottles for shampoo, body wash, and hand soap are produced on shuttle machines with HDPE N1052 at 97.0–98.5 wt%, 1.5–2.5 wt% colour masterbatch, 0.2–0.4 wt% antioxidant, and 0.1–0.3 wt% processing aid; processing is limited to 170–190 °C melt because pearlescent masterbatches containing mica/titanium dioxide raise shear viscosity and generate surface roughness above 190 °C. The container must satisfy EU Cosmetics Regulation (EC) No 1223/2009 Article 17 by not altering the cosmetic formula or releasing substances above REACH Annex XVII thresholds; for export to FDA-regulated markets, the natural resin must be covered by FDA 21 CFR 177.1520(c). Terminal products include 200-mL and 500-mL shampoo bottles, 250-mL body wash bottles, 1-L hand soap refills, and 500-mL lotion bottles with flip-top or pump closures.

    Free Quote

    Competitive Sinopec Shanghai HDPE N1052 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Shanghai HDPE N1052 is a high-density polyethylene injection-molding grade produced at the Shanghai Petrochemical complex. The resin is supplied as free-flowing lenticular pellets and is specified to a nominal melt mass-flow rate of 10 g/10 min when determined at 190 °C under 2.16 kg load per ISO 1133-1:2022, and a nominal density of 0.952 g/cm³ per ISO 1183-1:2019. These values place the grade in the high-flow segment of HDPE intended for thin-section injection molding, where short cycle times, adequate melt filling, and reproducible part mass are required. The molecular architecture associated with this flow class reduces chain entanglement relative to blow-molding and pipe grades, lowering injection pressure demand but also reducing melt strength and environmental stress-crack resistance. The following technical profile is assembled from public material data for the N1052 designation, typical high-flow HDPE injection grades, and standard ISO test methods; lot-specific certificates govern final acceptance.

    How Does N1052 Differ from Pipe and Film Grade HDPE?

    High-density polyethylene grades are differentiated primarily by melt flow rate, molecular weight distribution, density, and comonomer content. Pipe grades such as PE 100 typically carry MFR below 0.5 g/10 min and bimodal molecular weight distributions for slow crack growth resistance. Blown film grades operate at MFR between 0.2 g/10 min and 2.0 g/10 min to preserve bubble stability. N1052, by contrast, is designed for fast injection filling; its higher MFR lowers viscosity under shear and permits shorter filling and holding times. The trade-off is a reduction in ultimate extensional ductility and ESCR when compared with PE 100 pipe resins. The grade is therefore not interchangeable with pipe extrusion or blown film resins, even though all three may share similar density ranges.

    Comparative MFR and Density Bands by HDPE Processing Class
    Grade classNominal MFR (ISO 1133-1:2022)Nominal density (ISO 1183-1:2019)Primary processing routeCritical limitation
    Sinopec Shanghai HDPE N105210 g/10 min0.952 g/cm³Injection moldingReduced ESCR and melt strength
    PE 100 pipe grade0.2–0.5 g/10 min0.950–0.960 g/cm³Pipe extrusionLong cycle time if injection molded
    HDPE blown film grade0.2–2.0 g/10 min0.948–0.952 g/cm³Film blowingExcessive melt strength not suitable for thin-wall filling

    In high-cavitation production of caps, closures, and thin-wall dairy containers, the grade is processed on hydromechanical or electric injection molding machines with screw L/D ratios of 18:1 to 22:1 and a short compression zone. A reverse-taper non-return valve is typically selected to minimize shot-weight variation. Barrel temperature settings from rear to nozzle are normally maintained between 180 °C and 230 °C, with the nozzle held at 215 °C to 230 °C. Mold temperature is controlled at 20 °C to 60 °C; lower mold temperatures shorten cooling time but may increase warpage in flat-sided containers. Injection pressure required depends on flow length and wall thickness; for a 1.2 mm wall section, melt pressure at the nozzle commonly falls between 60 MPa and 90 MPa. For multi-cavity tools with projected area of 200 cm² per cavity and cavity pressure of 35 MPa to 45 MPa, a 32-cavity mold may require clamp force between 2240 kN and 2880 kN. Production machines in the 2500 kN to 3000 kN class are commonly selected for such configurations.

    Melt Rheology and Shear Sensitivity

    The high melt flow rate of N1052 does not imply Newtonian behavior. Capillary rheometry at 190 °C shows a shear-thinning profile typical of linear HDPE; apparent viscosity declines from a low-shear plateau of roughly 900 Pa·s to 180 Pa·s at 1000 s⁻¹. This sensitivity permits effective filling of thin ribs and hinge regions. On the production floor, the practical consequence is that increasing injection velocity can reduce pressure drop through gate lands, but excessive shear heating above 240 °C may initiate oxidative degradation and surface splay. In molds with hot-runner systems, internal runner temperatures should be limited to 220 °C to 240 °C, and residence time at temperature should be less than 5 min. Published isothermal crystallization data for HDPE with similar density indicate half-times of 5 s to 10 s at 110 °C; this rapid crystallization governs cooling time and post-filling dimensional stability.

    When the Melt Temperature Drops Below 190 °C

    At melt temperatures below 190 °C, viscosity increases rapidly and the risk of short shots in long flow paths rises. Molding trials on stack molds with 32 cavities and 0.8 mm wall thickness have shown that melt temperature variation of ±5 °C at the nozzle is sufficient to shift part mass by 0.3 g to 0.6 g. Therefore barrel zone control should maintain a tolerance of ±3 °C on the metering zone and ±2 °C on the nozzle adapter. When processing in high-humidity environments above 60 % RH, pellet surface moisture can generate splay; hopper drying at 80 °C for 2 h is recommended before extended production runs. The same drying condition is advised after outdoor warehouse storage in unsealed containers.

    The tensile and flexural property envelope of Sinopec Shanghai HDPE N1052 is evaluated under standard ISO conditioning at 23 °C and 50 % relative humidity. Typical values include a tensile yield stress of 26 MPa per ISO 527-2:2012, tensile elongation at break above 100 %, flexural modulus of 1150 MPa per ISO 178:2019, and Charpy notched impact strength of 3.5 kJ/m² per ISO 179-1:2010. These values reflect a high-density polyethylene with limited short-chain branching, giving stiffness but reducing low-temperature impact compared with LLDPE. At -20 °C, notched impact values decrease; the grade is therefore not generally specified for impact-dominated subzero service.

    Representative Property Matrix for Sinopec Shanghai HDPE N1052
    PropertyTest methodTypical value
    Melt mass-flow rateISO 1133-1:202210 g/10 min
    DensityISO 1183-1:20190.952 g/cm³
    Tensile yield stressISO 527-2:201226 MPa
    Tensile elongation at breakISO 527-2:2012>100 %
    Flexural modulusISO 178:20191150 MPa
    Charpy notched impact strength, 23 °CISO 179-1:20103.5 kJ/m²
    Vicat softening temperature, 50 °C/h, 50 NISO 306:2022125 °C
    Heat deflection temperature, 0.45 MPaISO 75-2:201375 °C
    Mold shrinkage, flow directionISO 294-4:20182.0 %–2.5 %

    Post-mold shrinkage is anisotropic and depends on gate location, wall thickness, and mold temperature. In flat rectangular containers with 1.0 mm to 1.5 mm wall thickness, flow-direction shrinkage measured after 48 h at 23 °C is typically 0.2 to 0.4 percentage points higher than transverse-direction shrinkage. This dimensional asymmetry should be compensated in tooling by differential cavity scaling. For closure threads, the high mold shrinkage of HDPE relative to polypropylene requires verification of thread engagement after 24 h post-molding, because continued secondary crystallization can shrink the closure diameter by an additional 0.1 % to 0.3 %.

    Compliance Status in Food-Contact and Electrotechnical Applications

    For food-contact uses, the base resin is represented as complying with FDA 21 CFR 177.1520(c)3.1a and EU 10/2011 as amended, provided that overall migration limits of 10 mg/dm² are respected. In thin-walled packaging, actual migration is governed by diffusion kinetics and the high crystallinity of HDPE; the low solubility of the matrix in aqueous and acidic simulants limits mass transfer. For electrical enclosures and cable management components, the grade is assessed against IEC 60695-2-12 glow-wire flammability only with flame-retardant modification; the unmodified grade is not classified for UL 94 V-0.

    Chemical resistance is typical of high-density polyethylene: continuous exposure to dilute acids, alkalis, and polar solvents at ambient temperature causes limited property loss, but swelling occurs in aliphatic and aromatic hydrocarbons. In caps and closures for household chemicals, the grade is used only when closure liners provide barrier function. Stress-cracking resistance under constant strain in 10 % Igepal CO-630 solution is lower than that of medium-density and high-molecular-weight HDPE grades; published data for this specific configuration is limited, so lot-specific environmental stress-crack resistance should be confirmed when the application involves wetting agents or detergents.

    Compared with isotactic polypropylene, N1052 has lower heat deflection temperature, lower flexural modulus, and higher notched impact strength at ambient temperature. The density advantage of HDPE becomes relevant in closures where part weight reduction is linked to cavity count and cycle time. Compared with linear low-density polyethylene, N1052 offers higher tensile yield stress and flexural modulus but lower puncture resistance and lower dart impact capacity. These differences are material-class properties rather than grade-specific defects, and they determine that N1052 is selected for rigid thin-wall parts rather than flexible packaging or impact-dominated applications.

    For incoming resin qualification, the producer's lot certificate reports melt mass-flow rate, density, and typically tensile yield stress. Lot-to-lot MFR variation is controlled within ±0.5 g/10 min around the nominal value, which supports stable injection pressure and part mass in production. If the resin is stored in unopened original packaging in a dry indoor environment below 50 % RH, it can normally be processed without drying. Once a package is opened, the material should be consumed within 24 h or kept in sealed hopper dryers to avoid surface moisture pickup, which can produce splay in fast-cycle molding.