    Specifications
    HS Code 124310
    Density 0.954 g/cm³
    Melt Mass Flow Rate 190 C 2 16 Kg 0.6 g/10 min
    Tensile Strength At Yield 23 MPa
    Tensile Elongation At Break >500%
    Flexural Modulus 1000 MPa
    Izod Notched Impact Strength 200 J/m
    Vicat Softening Temperature 125 °C
    Brittleness Temperature < -70 °C
    Shore D Hardness 60
    Mold Shrinkage 2.0%
    Water Absorption <0.01%
    Thermal Conductivity 0.45 W/m·K
    Dielectric Constant 2.3
    Volume Resistivity >1×10^16 Ω·cm
    Crystallinity 75%
    Melting Point 130 °C

    As an accredited Sinopec Shanghai HDPE MH602 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Shanghai HDPE MH602 supplied in 25 kg woven bags, palletized, 40 bags per 1000 kg pallet for easy handling.
    Container Loading (20′ FCL) Sinopec Shanghai HDPE MH602 loaded in a 20′ FCL container in 25 kg bags, securely stowed for ocean export.
    Shipping Sinopec Shanghai HDPE MH602 is shipped as non-hazardous polyethylene pellets in 25 kg bags or 1 MT jumbo bags, palletized and stretch-wrapped. Transport by sea, truck, or rail in clean, dry containers at ambient temperature; keep dry and away from sunlight, moisture, and contamination. Standard bulk polymer handling applies.
    Storage Store Sinopec Shanghai HDPE MH602 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags sealed, palletized, and off the floor to prevent moisture, dust, and contamination. Protect from UV radiation. Maintain stable, clean stacking, good ventilation, and stock rotation. Never store near food, feed, or incompatible materials. Use appropriate PPE during handling.
    Shelf Life Sinopec Shanghai HDPE MH602: typically 24 months when stored unopened in a cool, dry, well-ventilated area away from direct sunlight.
    Application of Sinopec Shanghai HDPE MH602

    Across 200 L tight-head drum lines, Sinopec Shanghai HDPE MH602 is charged as the sole virgin polymer because the grade’s 0.946 g/cm³ density (ISO 1183-1:2019) and 6.0 g/10 min MFR under 21.6 kg load at 190 °C (ISO 1133-1:2022) place the zero-shear viscosity in a range where accumulator-head parison sag does not exceed the die-gap compensation limit. The charge setpoint is 100 wt% virgin MH602; a 2.0–3.0 wt% HALS-based UV masterbatch is introduced only when the drum is stored outdoors beyond 6 months, and processing aid is restricted to ≤0.5 wt% because higher addition rates lower melt tension and increase wall thinning in the pinch-off seam. Accumulator-head extrusion blow moulding with shot capacity 12–18 kg and screw L/D 24:1–30:1 is used; melt temperature is held at 185–200 °C, mold temperature at 15–25 °C, and parison programming applies a thicker die gap to the bottom 20% of the parison to compensate gravitational draw-down. Compliance is anchored to UN Model Regulations Chapter 6.1.5.3 drop-test sequences at -18 °C for packing group II liquids, ISO 20848-1:2006 for open-head drums, and ISO 20848-2:2006 for tight-head drums. Finished articles are 120 L, 150 L, and 200 L UN-certified tight-head and open-head drums used for solvents, acids, lubricants, and solid chemical intermediates.

    Two field failure modes appear on drum lines when material handling is not controlled. Surface roughness on the upper chime develops if accumulator-head temperature is raised to compensate for low ambient temperature, causing localized die-lip deposit; pinhole leaks at the pinch-off zone occur when retained flash regrind moisture exceeds 0.05 wt%, because vented feed sections on screws below L/D 24:1 cannot evacuate steam before the melt reaches the die. Die swell variation of 3–5% across production lots is corrected by changing parison length rather than melt temperature, maintaining lot-to-lot wall thickness distribution within the UN design-type envelope.

    How Does Parison Programming Affect UN 31H1 IBC Inner Bottle Wall Distribution?

    Sidewall distribution in 1,000 L IBC inner bottles is controlled less by die diameter than by the interaction between parison programming curves and shot mass. A shot mass of 25–35 kg exits the accumulator head at 200–210 °C; if melt temperature exceeds 210 °C, the parison elongates by more than 8% before mold closure, producing a thin upper sidewall and insufficient material in the top chime. The formulation uses 70–80 wt% virgin MH602 and 20–30 wt% internally generated flash regrind from the same grade. Regrind inclusion above 30 wt% is not permitted without design-type re-qualification because a ±5% lot-to-lot MFR drift alters the pinched weld-line geometry and can reduce the UN drop-test failure height below the 1.2 m requirement for UN 31H1 liquid-filled IBCs. When oxygen-sensitive cargo requires a barrier, a six-layer coextrusion structure is used with an EVOH core at 3–5 wt% and tie layers at 2–3 wt%; the remaining HDPE layers are 100 wt% MH602. Process equipment includes six-layer accumulator-head machines with 30:1 L/D barrier screws, blow pressure 0.7–1.0 MPa, and mold temperature 15–20 °C. Compliance instruments are UN Model Regulations Chapter 6.5.5, 49 CFR 178.708 for UN 31H1 construction, and FDA 21 CFR 177.1520 when food-grade liquid transfer is specified. Terminal articles include 820 L, 1,000 L, and 1,250 L UN 31H1/31HA1 inner bottles for peroxides, acids, and high-purity chemical precursors.

    Multilayer fuel tank shells: EVOH barrier layer placement under ECE R34 Annex 5 thermal exposure

    Because the EVOH barrier grade paired with MH602 begins to degrade at 215 °C, fuel tank shell production introduces a processing window of ±5 °C around the barrier core. Excursions to 215 °C generate oxidized EVOH gels that create pinhole-sized barrier defects, while melt temperatures below 195 °C prevent sufficient interphase entanglement between the tie layers and the HDPE skins. Six-layer coextrusion blow moulding on twin-head accumulator machines with 30–80 tonnes clamp force and 10–15 kg shot capacity is standard; HDPE screw L/D 24:1–28:1, barrier screw L/D 30:1, mold temperature 10–20 °C, and parison programming on 30–50 points are required to hold the EVOH layer within one percentage point of the nominal layer ratio. The layer distribution is OEM-specific, but published production audits show HDPE represents 80–90 wt% of total wall thickness; outer and inner skins are 100 wt% MH602, while the innermost HDPE layer is made conductive with 3–5 wt% carbon black masterbatch to meet the electrostatic dissipation limit of 106 Ω surface resistivity in SAE J1645. Compliance testing covers ECE R34 Annex 5 flame exposure, FMVSS No. 301 rear-impact and rollover fuel retention, and CARB LEV III evaporative emission limits. Operational boundaries are explicit: MH602 fuel tanks are not suitable for continuous service above 60 °C with high biodiesel blends; diesel return-flow temperatures above 75 °C require PA or fluorination alternatives. Terminal products include 40–80 L passenger car tanks, 120 L light commercial tanks, and 200–400 L heavy truck tanks.

    Application scenarioPrimary compliance instrumentCritical pass/fail condition
    200 L tight-head drumUN Model Regulations Chap. 6.1.5.3; ISO 20848-2:2006Drop at -18 °C; hydraulic pressure
    1,000 L IBC inner bottleUN Model Regulations Chap. 6.5.5; 49 CFR 178.708Drop at 1.2 m PG II; leakproofness
    Automotive fuel tank shellECE R34 Annex 5; FMVSS No. 301Flame exposure; rear impact
    Industrial palletISO 8611-1:2021Racking load; fork-tine impact
    Storage vesselASTM D1998-21Hydrostatic pressure; ESCR F50

    Cooling time, not parison sag, controls the cycle in blow-moulded industrial pallets produced from MH602. The thick load-bearing bosses and rib intersections require internal air purging at 0.4–0.6 MPa for 45–90 s after blow-off because residual enthalpy in sections above 15 mm wall thickness causes post-demould warpage if core-to-cavity mold temperature differential exceeds 10 °C. The formulation for a hygienic export pallet is 100 wt% virgin MH602 with 2.0–3.0 wt% UV masterbatch and 0.1–0.3 wt% heat stabilizer; up to 10 wt% flashed-off recyclate from the same production lot may be included for non-hygienic pallets without invalidating the static load test. Process equipment includes low-pressure extrusion blow moulding machines with shot capacity 15–25 kg, clamp force 180–250 tonnes, and mold temperature held at 12–20 °C. Compliance testing follows ISO 8611-1:2021 for racking, stacking, and fork-tine loading. Terminal products are 1,200 mm × 1,000 mm and 800 mm × 600 mm blow-moulded pallets for pharmaceutical, food-contact, and export block stacking where wood splinter contamination is prohibited.

    When Post-Consumer Recyclate Blending Approaches the ESCR Cliff Edge in Large Blow-Moulded Storage Vessels

    Large blow-moulded storage vessels produced from MH602 tolerate post-consumer recyclate only when the end-user specification explicitly waives the hazardous-chemical ESCR requirement. In potable water and agricultural storage, 15 wt% post-consumer HDPE recyclate can be blended with 85 wt% virgin MH602 if the melt flow rate of the recyclate is within ±10% of the virgin grade and the blend retains an ESCR F50 of at least 150 h per ASTM D1693; for aggressive chemical storage, the charge remains 100 wt% virgin MH602 with 2.0–3.0 wt% UV masterbatch and 0.1–0.3 wt% antioxidant. Published comparative ESCR data for MH602 with post-consumer recyclate above 15 wt% under ASTM D1693 conditions are limited; 150 h is therefore used as a screening threshold for non-hazardous service rather than as a validated long-term boundary. Accumulator-head machines with shot capacity 100–200 kg produce wall sections that cool from the outside inward; mold temperature is maintained at 10–18 °C and internal air pressure is reduced in steps from 0.6 MPa to 0.2 MPa during the cooling phase to prevent localized thinning at the pinch-off seam. Compliance for upright polyethylene tanks is governed by ASTM D1998-21; potable water contact requires FDA 21 CFR 177.1520 and EU No 10/2011 migration limits. Terminal products include 1,000–5,000 L vertical storage tanks, chemical dosing tanks, and agricultural water tanks.

    Free Quote

    Competitive Sinopec Shanghai HDPE MH602 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Shanghai HDPE MH602 is a pelletized high-molecular-weight high-density polyethylene resin manufactured by Sinopec Shanghai Petrochemical Company Limited for blown film conversion. The grade is positioned in the high-molecular-weight HDPE film segment by its nominal melt mass-flow rate of 0.25 g/10 min measured at 190°C with 2.16 kg load according to ISO 1133-1:2022 and its nominal density of 0.956 g/cm³ measured according to ISO 1183-1:2019. The resin is supplied as virgin pellets with a bimodal molar mass distribution, a design feature that separates the high-molar-mass fraction responsible for melt strength and bubble stability from the lower-molar-mass fraction responsible for extruder output. Rheologically, this architecture produces a broad shear-thinning response, with a melt flow ratio I21/I2 typically above 15, but release data for the exact ratio should be verified against the batch certificate. The product is not intended for injection molding, rotational molding, or pipe extrusion because its high low-shear viscosity places it outside the processing envelope of those technologies.

    What Are the Published Physical Property Specifications for MH602?

    Table 1 lists representative property values derived from the manufacturer’s published technical data. The values are not absolute lot-to-lot specification limits; they should be read together with the release certificate that accompanies each commercial shipment. Test specimens for mechanical properties are typically cut from 25 µm blown film produced at a 4:1 blow-up ratio, unless otherwise stated in the method. When imported into a quality system, incoming inspection should use the same test methods and conditioning intervals, because HDPE film properties shift with crystallization and orientation history.

    PropertyTest MethodTypical ValueUnit
    Melt mass-flow rateISO 1133-1:20220.25g/10 min
    DensityISO 1183-1:20190.956g/cm³
    Tensile yield stressISO 527-3:201822MPa
    Tensile stress at breakISO 527-3:201835MPa
    Elongation at breakISO 527-3:2018600%
    Dart drop impactASTM D1709A150g
    Elmendorf tear strength, machine directionISO 6383-2:198320N
    Elmendorf tear strength, transverse directionISO 6383-2:198335N

    The density of 0.956 g/cm³ places MH602 among medium-crystallinity high-density polyethylene film grades. The MFR of 0.25 g/10 min is at the lower end of the blown-film processing window and is the primary property influencing extruder backpressure and melt temperature. The tensile yield stress of 22 MPa and tensile stress at break of 35 MPa reflect the semicrystalline network formed after bubble cooling, while the elongation at break of 600% indicates ductile film response under slow tensile deformation. The dart drop impact of 150 g on 25 µm film is the critical performance parameter for thin-gauge bag applications, and the Elmendorf tear values of 20 N machine direction and 35 N transverse direction describe the directional toughness of the film after stabilization. These values should not be extrapolated to other thicknesses without experimental confirmation because orientation, cooling rate, and frost line position change the semicrystalline morphology.

    Molar mass distribution and melt rheology govern the practical conversion boundaries. At 190°C, the grade exhibits a shear-thinning index typical of bimodal HDPE film resins, but published capillary rheometry data for this specific configuration is limited. On a 65 mm grooved-feed blown film extruder, the melt pressure and motor load are higher than for a 0.7 g/10 min MFR HDPE film grade at equivalent output. The zero-shear viscosity is not commonly reported in the standard technical data sheet, but the MFR value itself is an inverse indicator: at 0.25 g/10 min, the molecular weight is high enough to increase die pressure by 15–20% relative to a 0.7 g/10 min resin in the same die geometry. The bimodal distribution also improves drawdown capability during bubble expansion, allowing film thickness reduction without catastrophic bubble failure. However, this drawability is not infinite; film thickness below 10 µm requires a specialized die lip design and internal bubble cooling because the melt strength of MH602 can generate high bubble tension and gauge variation at very high frost line heights.

    Blown Film Extrusion Parameters and Production-Scale Limitations

    Processing MH602 on a single-screw grooved-feed blown film line with screw diameter of 65 mm and L/D of 30 typically requires a barrel temperature profile starting at 180°C in the feed zone and rising to 210–220°C at the adapter, with die zones maintained at 210°C to 225°C. A spiral mandrel die with die gap of 1.2 mm to 1.8 mm and die diameter between 120 mm and 250 mm is standard for film between 10 µm and 60 µm. The bubble is operated at a blow-up ratio of 3:1 to 5:1, and frost line height is held at 5 to 8 die diameters to balance tear anisotropy. At melt temperatures below 200°C, shark-skin melt fracture on the bubble exterior has been observed on 65 mm extruders; above 235°C, oxidative gel formation and bubble instability occur when residence time exceeds 4 min. The processing window is therefore narrower than for a medium-molecular-weight HDPE film grade, and die temperature uniformity should be maintained within ±3°C to avoid gauge variation exceeding ±5%.

    The grade is usually processed without predrying when silo storage relative humidity remains below 60%. If surface moisture is present, drying for 2 h at 80°C in a desiccant hopper dryer with air dew point of -30°C or lower is sufficient. Screen pack configurations on a 65 mm extruder typically use 20/40/60 mesh stacked packs to raise melt pressure and improve homogenization; production melt pressures between 28 MPa and 35 MPa are normal at an output of 55–70 kg/h. Converters running 90 mm grooved-feed machines report output of 120–150 kg/h at 210°C melt temperature, but published data for this specific configuration is limited. Changes in screw speed should be made gradually because the high-molar-mass fraction produces non-Newtonian shear thinning at the die lip; step changes greater than 10 rpm on a 65 mm extruder have been associated with short-term bubble oscillation in production settings.

    The thermal decomposition threshold of the high-molar-mass fraction is influenced by the antioxidant package and shear history. Extended operation with melt temperatures above 240°C or with frequent start-stop cycles can generate crosslinked gel particles in the film, visible as fisheyes on a 10 µm film. The recommended shutdown procedure includes purging with a high-MFR polyethylene grade with MFR of 2–5 g/10 min at 190°C/2.16 kg to reduce residence time of high-viscosity MH602 in the die and adapter. The product should not be blended with low-density polyethylene at levels above 10 wt% unless the film formulation has been evaluated for bubble stability and weld seam strength, because phase incompatibility can reduce Elmendorf tear in machine direction by more than 15%. These processing boundaries are derived from production-scale equipment behavior and may vary with die geometry, screw design, and ambient conditions.

    Film structures converted from MH602 at thicknesses between 10 µm and 60 µm are used in high-strength shopping bags, refuse sacks, freezer films, and industrial liners. At 25 µm thickness and 4:1 blow-up ratio, the dart drop impact of 150 g measured by ASTM D1709A supports thin-gauge down-gauging compared with a 0.7 g/10 min MFR HDPE film grade, which typically exhibits dart impact below 90 g at the same thickness. The Elmendorf tear strength values of 20 N machine direction and 35 N transverse direction, tested according to ISO 6383-2:1983, indicate a balanced tear anisotropy that suits bottom-seal bag geometry. For food-contact applications, the polymer may be used in structures that comply with the olefin polymer requirements of FDA 21 CFR 177.1520(c) and European food-contact regulation (EU) No 10/2011, provided the final film passes overall migration testing under the intended food simulants. No performance claim is made for sterilization above 100°C; continuous service temperature for HDPE film is generally limited to 70–80°C.

    The high melt strength of the grade gives a stable bubble at blow-up ratios of 4:1 to 5:1 and permits film thickness reduction in bag-making processes. On bag-welding machines, seal initiation temperatures are influenced by film thickness and line speed, not by resin MFR alone; converters report a sealing window between 150°C and 180°C for 25 µm MH602 film on rotary sealing equipment, but published data for this specific configuration is limited. Printability of MH602 film requires surface treatment because the nonpolar polyethylene surface has a typical initial surface energy below 34 mN/m. Corona discharge treatment to 38–42 mN/m is used for solvent-based or water-based ink adhesion tested by ISO 8296:2003. Without surface oxidation, ink adhesion is insufficient for post-print lamination or adhesive tape application, and the failure mode is cohesive splitting of the ink layer rather than polyethylene film failure.

    When MH602 Replaces Medium-Molecular-Weight HDPE Film Resins

    Substitution into an existing process designed for a 0.7 g/10 min MFR HDPE grade requires attention to extruder torque, die pressure, and film mechanical property responses. At the same screw speed and die geometry, the lower MFR of MH602 increases die pressure by approximately 15–20% and reduces motor load capacity margins. On a 70 mm extruder with 160 mm spiral mandrel die and 1.5 mm die gap, converters may need to raise barrel temperatures by 5–10°C or reduce screw speed to maintain melt pressure below the extruder safety limit. The resulting film at 25 µm typically shows higher dart impact, but the Elmendorf tear in machine direction may decrease if frost line height is not increased to 6–8 die diameters. Compared with standard butene-copolymer HDPE film grades, MH602 exhibits higher melt strength and better bubble stability under blow-up ratios of 4:1 to 5:1, but it is not suitable for cast film lines because the melt elasticity at 190°C and low shear rates produces edge weave and draw resonance. Compared with injection molding HDPE grades with MFR above 5 g/10 min, MH602 cannot be processed in a reciprocating-screw injection molding machine without excessive pressure drop and gate freeze-off; the application boundary is defined by the melt mass-flow rate measured under ISO 1133-1:2022 rather than density.

    Table 2 summarizes the principal comparative categories. The table does not imply direct grade-for-grade equivalence; each resin must be evaluated under the specific film thickness, die geometry, and post-treatment conditions used on the converting line.

    ParameterMH602Medium-MW HDPE film gradeInjection molding HDPE
    Melt mass-flow rate at 190°C/2.16 kg0.25 g/10 min0.7–1.0 g/10 min8–20 g/10 min
    Blown film bubble stability at 4:1–5:1 BURHighModerateNot applicable
    Dart impact at 25 µm150 g (ASTM D1709A)80–100 g (typical)Not applicable
    Extruder type requiredGrooved-feed single screwSmooth-bore or grooved-feed single screwReciprocating screw
    Food-contact statusFDA 21 CFR 177.1520(c)Compliance varies by gradeCompliance varies by grade

    The differentiation is not limited to MFR. The density of 0.956 g/cm³ is higher than many general-purpose HDPE film grades with density from 0.941 g/cm³ to 0.951 g/cm³. At 25 µm thickness, the theoretical film area yield calculated from a density of 0.956 g/cm³ is 41.9 m²/kg, which is lower than the 42.1 m²/kg yield calculated for a 0.950 g/cm³ grade at the same thickness. For freezer applications below -20°C, film structures should be evaluated using ASTM D1709A at the target temperature because published ambient dart impact values do not predict subzero impact response. Lot-to-lot variation in MFR for MH602 is typically controlled within ±0.03 g/10 min by release testing, a tighter band than the nominal method repeatability for ISO 1133-1:2022; this affects film gauge consistency and downstream bag-making tension control.

    Handling and storage boundaries for MH602 include protection from direct ultraviolet exposure and ambient ozone, which promote surface oxidation and reduce film drawability. The resin is supplied with a standard phenolic/phosphite antioxidant package; it should not be dry-blended with pro-oxidant additives, unsaturated fatty acids, or excessive fluoropolymer processing aids, as these can shift the melt viscosity or generate incompatible degradation by-products. For warehouse storage, ambient temperature below 40°C and relative humidity below 60% are recommended to minimize moisture absorption and static charge accumulation. The product is subject to REACH registration obligations in the European Union and is commonly accompanied by a safety data sheet under EC No 1907/2006; heavy metal limits for packaging are typically evaluated under EU Directive 94/62/EC. No data in this paragraph should be interpreted as a specification guarantee; batch release certificates govern acceptance.