    Specifications
    HS Code 776213
    Polymertype High-density polyethylene (HDPE)
    Meltflowrate 20 g/10 min (190°C/2.16 kg)
    Density 0.956 g/cm³
    Tensilestrengthatyield 25 MPa
    Elongationatbreak 500%
    Flexuralmodulus 1000 MPa
    Vicatsofteningtemperature 120°C
    Heatdeflectiontemperature 75°C
    Notchedizodimpactstrength 50 J/m
    Hardnessshored 60
    Meltingpoint 130°C
    Waterabsorption <0.01%
    Thermalexpansioncoefficient 1.2E-4/°C
    Dielectricconstant 2.3

    As an accredited Sinopec Shanghai HDPE CH2802 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Shanghai HDPE CH2802 is packed in 25 kg woven bags, typically 40 bags per pallet (1000 kg).
    Container Loading (20′ FCL) Sinopec Shanghai HDPE CH2802: 20′ FCL loading, typically 25 kg bags, approximately 18–20 MT per container.
    Shipping Sinopec Shanghai HDPE CH2802 is a non-hazardous polyethylene resin, typically shipped in 25 kg bags or jumbo bags on pallets. Transport in clean, dry containers or trucks. Keep dry, away from direct sunlight, heat, and contaminants. No special hazard classification required.
    Storage Store Sinopec Shanghai HDPE CH2802 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed, clean, and palletized. Prevent moisture, rain, and contamination. Avoid prolonged high temperatures and UV exposure. Use clean handling equipment; do not smoke or use open flames. Follow local fire and safety regulations.
    Shelf Life Typically 24 months if stored in original packaging, cool, dry, ventilated area, away from direct sunlight, heat, and moisture.
    Application of Sinopec Shanghai HDPE CH2802

    Sinopec Shanghai HDPE CH2802 enters monolayer extrusion blow moulding operations as a high-density polyethylene with a nominal density of 0.958 g/cm³ to ISO 1183-1:2019 and a reference melt mass-flow rate of 0.28 g/10 min at 190 °C under 2.16 kg to ISO 1133-1:2022. In detergent, personal-care and lubricating-oil packaging, the resin is converted without pre-drying when storage relative humidity is below 60% RH; at higher humidity, surface condensation on cold granulate can generate melt-stream voids and pinholing at the die exit. The standard formulation for an opaque 1 L to 25 L stackable jerrican includes 100 parts virgin CH2802, 2–5 wt% titanium-dioxide-based white masterbatch, and 0–25 wt% post-industrial flash regrind for non-dangerous-goods service. Processing is carried out on single-head shuttle blow moulders with 24:1 to 30:1 L/D barrier screws. Barrel zones are profiled from 160 °C at the feed throat to 205 °C at the die head, and melt temperature is held between 195 °C and 215 °C. Parison programming is used to narrow the die gap 10–15% at the pinch-off zone and to widen it 8–12% at the base chime. Mould cooling water is maintained at 10–18 °C, blow pressure is set at 0.6–0.8 MPa, and pre-blow delay is 0.3–0.7 s. The finished articles are stackable jerricans with calibrated neck finishes for screw-cap or foil-seal closures, drop-tested to ASTM D2463-15 and leak-tested at 20–30 kPa pneumatic pressure. CH2802 is not a general-purpose injection-moulding grade; converters should not substitute the resin into hot-runner piston machines without first confirming melt-index compatibility to ISO 1133-1:2022.

    What Causes Environmental Stress Cracking in Tight-Head Agrochemical Jerricans?

    In tight-head agrochemical jerricans, environmental stress cracking is governed by residual hoop stress at the pinch-off weld, wall-thickness distribution at the bottom chime, and the polar association of ester, ketone, or amide solvent constituents with polyethylene tie chains. For CH2802 in agrochemical service, the resin is compounded with 2–3 wt% carbon black masterbatch to provide ultraviolet screening at 0.2–0.4 mm wall stock; the masterbatch carrier is LLDPE-based to limit melt-index drift during repeated heat histories. The blow-moulding operation uses an accumulator head with 10–25 L shot capacity, a diverging die gap of 1.5–2.5 mm, and parison programming adjusted to maintain corner wall thickness above 0.8 mm in the handle area and above 1.2 mm at the bottom chime. Melt temperature must not exceed 215 °C to avoid chain scission and ESCR decay; barrel residence time is limited to 6–8 minutes. Mould cooling at 12–15 °C is maintained until demoulded surface temperature is below 65 °C, because hot parts ejected into stacking bins retain weld-line stress. The finished article is a 1 L, 5 L, or 20 L UN-certified jerrican for pesticide concentrates and plant-growth regulators. Transport conformance is evaluated under the UN Manual of Tests and Criteria, Part III, section 21 drop test at 1.2 m for packing group II, a hydraulic pressure test at 250 kPa for 30 minutes, and a stack test for 28 days at 40 °C under ADR Chapter 6.1. Low-temperature drop claims require conditioning at -18 °C before the impact cycle. Not every lot automatically satisfies UN certification; batch-specific ESCR values to ASTM D1693-15, condition B, 100% Igepal CO-630, 50 °C, must be tabulated against minimum wall thickness before release.

    Test or propertyStandard designationApplication-related parameter
    Melt mass-flow rateISO 1133-1:2022190 °C, 2.16 kg; parison sag control
    DensityISO 1183-1:2019Wall stiffness and top-load resistance
    Environmental stress-cracking resistanceASTM D1693-15 Condition B50 °C, 100% Igepal CO-630; agrochemical service
    Finished container drop impactASTM D2463-15Retail and UN drop performance
    Flexural modulusISO 178:2019Panel stiffness in flat-side jerricans
    Charpy notched impact strengthISO 179-1:2010Impact resistance at -20 °C

    Coextruded Barrier Skins: CH2802 Around an EVOH Core

    Coextruded barrier containers for solvent-based agricultural formulations use CH2802 in the outer and inner skin layers, while an ethylene-vinyl alcohol copolymer core suppresses permeation of xylene, cyclohexanone, and mixed aromatic solvents. A typical six-layer structure is 45 wt% outer CH2802, 3 wt% maleic-anhydride-grafted polyethylene tie resin, 3 wt% EVOH, 3 wt% tie resin, 25 wt% post-industrial CH2802 regrind, and 21 wt% inner CH2802. Coextrusion is performed on a six-extruder blow moulder with layer sequencing controlled by a spiral mandrel die; HDPE skin extruders are set from 190 °C to 215 °C, while EVOH is processed at 185–205 °C within its thermal stability window. The die head is held at 205 °C and the melt curtain is inflated at 0.65 MPa blow pressure. The terminal product is a 1 L, 5 L, or 10 L multi-layer bottle for xylene-based or ketone-based agricultural adjuvants. Barrier performance is characterised by gravimetric solvent-loss testing at 40 °C for 28 days; dimensional stability is checked by GB/T 13508-2011 and drop impact by ASTM D2463-15. EVOH layers are moisture-sensitive; pre-drying at 80 °C for 4–6 hours is mandatory when ambient relative humidity exceeds 40% RH. Direct food-contact use is not automatic; a food-contact compliance certificate to GB 4806.7-2016 or EU 10/2011 must be obtained from the resin supplier before such claims are made.

    On accumulator-head machines, open-top pails produced from CH2802 are processed when the part weight exceeds 600 g. The formulation for a water-based paint or adhesive pail is 100 parts CH2802, 4–6 wt% white masterbatch for light-blocking walls, and up to 35 wt% in-house regrind from trimmed rims and rejected pail walls, provided the product is not regulated as dangerous goods. For pails intended to hold flammable or corrosive preparations, regrind addition is limited to 15 wt% unless the re-qualified blend has been tested under the relevant transport regulation. The mould is a tapered bucket with rim, body, and base wall thicknesses held at 1.8 mm, 1.4 mm, and 1.2 mm respectively. Accumulator-head shot size is matched to the pail volume with a fill-to-shot ratio of 1.1:1 to 1.2:1; blowing pressure is 0.7–0.8 MPa. The terminal articles are 10 L, 20 L, and 30 L open-top pails with gasketed lids and steel locking rings for water-based coatings, adhesives, and construction admixtures. Top-load and stacking qualification uses ISO 12048:1994; pneumatic leakproofness is checked at 20 kPa with the lid locked.

    When Regrind Fractions Exceed 30 wt% in Monolayer Wall Stock

    When post-industrial flash and rejected container walls are re-extruded into monolayer wall stock, the critical variable is not melt index alone but the shift in die swell and parison sag caused by sheared and re-sheared polyethylene chains. At regrind fractions above 30 wt%, CH2802 wall stock exhibits measurable reductions in die swell at constant die gap, requiring an increase in die gap of 0.2–0.5 mm to maintain the same parison diameter. Melt pressure in the accumulator head falls by 5–15% as the molecular weight distribution narrows under repeated shear; operators compensate by lowering screw speed 10–20 rpm and raising the barrel temperature profile by 5–8 °C. The risk area is ESCR at the pinch-off weld: regrind-rich domains develop lamellar orientation that is less resistant to Igepal CO-630 stress cracking, so the addition rate for UN-certified jerricans is capped at the value specified in the certification test, commonly 20 wt% or lower. The process specification calls for granulator screens with 8–10 mm apertures, a densifier for spider-web flash, and blend homogeneity checks by melt index sampling per ISO 1133-1:2022. Published data for this specific configuration is limited; processors should run a 20-batch regrind stability trial measuring die swell, melt temperature uniformity, and drop impact under ASTM D2463-15 before releasing production.

    Diesel exhaust fluid containers demand a wall-thickness tolerance that prevents deformation during sealed hot-fill and subsequent cooling. CH2802 is converted into 5 L, 10 L, and 20 L automotive AUS 32 containers on shuttle blow moulders with 10–20 L shot capacity. The blowing grade is processed at 195–210 °C melt temperature and 12–18 °C mould temperature; the parison programmer is set to hold flat-panel walls above 0.7 mm and welded corners above 0.9 mm. The resin formulation for AUS 32 service uses 2–4 wt% of a blue masterbatch that does not contain amine, phenolic, or mineral-oil residues because leachates can poison selective catalytic reduction catalyst systems. Only in-house regrind from diesel exhaust fluid containers is permitted; regrind from lubricant or agrochemical containers is excluded because residual hydrocarbons cannot be washed from porous regrind surfaces. Containers are tested for leakproofness at 30 kPa, burst resistance above 100 kPa, and drop impact under ASTM D2463-15 after conditioning at -10 °C. The finished product is a closed-loop AUS 32 container with a tamper-evident neck, handled under ISO 22241-3:2017 guidance for handling and transport of NOx reduction agent.

    Free Quote

    Competitive Sinopec Shanghai HDPE CH2802 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Shanghai HDPE CH2802 is a high-density polyethylene resin engineered for extrusion blow moulding of rigid hollow parts. The grade is identified by the designation CH2802 and is supplied as stabilized pellet stock. Its nominal density of 0.950–0.954 g/cm³ when tested in accordance with ISO 1183-1:2019 and melt mass-flow rate of 0.25–0.35 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 place the resin in the medium-high molecular weight segment of HDPE blow moulding materials. The low melt flow rate indicates high melt viscosity and elevated melt strength, which are required for maintaining parison shape during accumulator-head or continuous-extrusion blow moulding of containers with capacities from approximately 5 L to 20 L.

    In industrial container production, CH2802 is selected where the part must combine stiffness, resistance to environmental stress cracking, and a sufficiently wide processing window. The resin is not intended for injection moulding because the same high melt viscosity that stabilizes the parison creates excessive pressure drop in runners and gates. This differentiation from high-flow HDPE injection grades is the most significant product-selection boundary.

    Property Profile and Melt Rheology

    The following data are representative of the grade’s nominal control envelope; lot-specific certificates of analysis remain the controlling document for production acceptance.

    PropertyTest MethodTypical Value
    DensityISO 1183-1:20190.950–0.954 g/cm³
    Melt mass-flow rate, 190 °C/2.16 kgISO 1133-1:20220.25–0.35 g/10 min
    Tensile yield stressISO 527-2:201225–29 MPa
    Elongation at breakISO 527-2:2012>500 %
    Flexural modulusISO 178:2019950–1200 MPa
    Charpy notched impact strength, 23 °CISO 179-1:20108–13 kJ/m²
    Vicat softening temperature, A50ISO 306:2022124–128 °C
    Environmental stress-cracking resistance, F50, 10 % Igepal CO-630ASTM D1693-15>200 h

    Melt rheology for CH2802 is characterized by a high melt-flow ratio between the 21.6 kg load and the 2.16 kg load, which is commonly used to infer molecular weight distribution. Higher ratios correspond to broader distribution and greater shear sensitivity. In this grade, the high-load melt index is typically 9–13 g/10 min, giving a melt-flow ratio near 30–40. Such shear sensitivity permits adequate extruder throughput while retaining enough low-shear viscosity to limit parison sag. The elevated environmental stress-cracking resistance is associated with the resin’s comonomer placement and molecular architecture; the producer maintains this property through control of short-chain branching rather than through high melt index alone.

    In laboratory specimens, yield stress and flexural modulus are influenced by cooling rate. Rapid quenching in cold moulds depresses crystallinity and modulus, while slow cooling in thick blow-moulded walls raises density and stiffness. Consequently, data from standard compression-moulded plaques should not be applied directly to blow-moulded containers without correcting for wall thickness and cooling history. The values in the table are for standard laboratory specimens prepared under controlled conditions; parts produced on commercial lines may exhibit different values because of orientation and cooling gradients.

    For extrusion blow moulding, the practical significance of the viscosity curve is most visible in wall-thickness control. The resin’s melt strength is sufficient to resist draw-down of the parison, but the processor must still compensate for sag through parison programming. Wall thinning is most severe near the bottom of large containers, where the parison carries the weight of the extruded melt for the longest period. CH2802 is formulated to reduce that sensitivity relative to lower-molecular-weight blow moulding grades, but it does not eliminate the need for programmed die gap adjustment.

    How Does CH2802 Differ from Injection and Film Grades?

    When compared with HDPE injection-moulding grades, CH2802 has a substantially lower melt mass-flow rate. Injection grades typically exhibit 8–20 g/10 min at 190 °C/2.16 kg, whereas CH2802 remains below 1 g/10 min. The resulting difference in viscosity determines process selection: injection grades fill thin walls under high shear, while CH2802 maintains a cohesive parison in low-shear, open-die conditions. The low MFR also reduces flow instability during inflation because melt is distributed by blowing rather than by injection velocity.

    Film-grade HDPE resins, by contrast, are often designed with lower melt strength and controlled gel levels for thin-gauge processing. Their molecular design targets bubble stability at high stalk heights and low neck-in during film blowing. CH2802 is not optimized for film extrusion; its rheology is tuned for sag resistance and wall-thickness uniformity in blow moulding. Attempting to use CH2802 in film converting equipment typically produces unstable bubble geometry and gauge variation.

    Within the blow-moulding HDPE family, CH2802 is differentiated from high-flow container grades by its higher melt strength and longer parison hang time. High-flow blow-moulding grades may be used for small bottles with shot weights below 1 kg and rapid cycling, while CH2802 is selected for larger parts where hang time exceeds a few seconds. The trade-off is that high melt strength can reduce output and increase melt temperature sensitivity; processors must balance die gap and parison programming to avoid excessive wall thickening at pinch-off zones.

    Compared with bimodal HDPE pipe resins, CH2802 is not formulated to meet PE100 long-term hydrostatic strength requirements such as ISO 9080. Pipe grades require long-term creep rupture performance and resistance to slow crack growth at 20 °C and 80 °C. CH2802 is selected for short-term manufacturing stability and environmental stress-cracking resistance in packaging, not for pressure-pipe design life.

    When Die Swell and Parison Sag Control Wall Thickness

    In extrusion blow moulding, wall-thickness distribution is governed by die swell and parison sag. Die swell is the radial expansion of the melt as it exits the die annulus; sag is the time-dependent elongation of the parison under its own weight. For CH2802, die swell must be characterized at the production die temperature, usually 180–210 °C, because laboratory capillary data at lower temperatures do not capture parison behavior. Sag is inversely related to melt viscosity and directly related to parison weight and hang time. Large containers therefore require parison programming where the die gap is varied during extrusion to compensate for sag and to thicken pinch-off areas.

    Typical barrel temperature profiles for CH2802 are 170–190 °C in the feed zone, 190–210 °C in the compression zone, and 200–215 °C at the die head. Actual set points vary with extruder size, screw speed, and accumulator capacity. Melt temperatures should remain below 230 °C; prolonged residence time above this threshold can generate gels and oxidized species that appear as surface defects or black specks. A purging grade of HDPE or LDPE should be used during shutdown to minimize stagnant material in the die head and accumulator.

    Accumulator-head machines with screw diameters of 60–90 mm and L/D ratios of 24:1–30:1 are commonly used for containers of 5–20 L. Single-station shuttle machines are suitable for smaller bottles when parison weight is below 1 kg. Mold temperature control is less critical for HDPE than for polypropylene, but maintaining a mold temperature of 15–40 °C improves dimensional stability and reduces sink marks opposite thick sections. Blow pressure should be sufficient to force the parison against the mold wall; typical values of 0.5–0.8 MPa are common, but thin-walled parts may require 0.6–1.0 MPa depending on wall thickness and melt temperature.

    Clean edge trim, tail flash, and nonconforming bottles can be blended with virgin CH2802. The blend fraction should remain below 20–30 % for demanding applications because repeated heat history increases gel levels and shifts MFR. When regrind is used, the melt temperature should be kept near the lower end of the range, and extruder back pressure should be monitored to detect viscosity drift. The resin is not hygroscopic, but condensation must be removed if sacks are stored in environments above 60 % relative humidity. Drying at 80 °C for 1–2 h is sufficient to reduce surface moisture below 0.05 %.

    Regulatory compliance for CH2802 must be verified against the lot-specific product documentation. As an ethylene polymer, the resin falls within the scope of FDA 21 CFR 177.1520 for olefin polymers, but a finding of compliance for a finished container requires migration testing under the intended conditions of use. Under REACH, the polymer itself is exempt from registration, while the imported monomers have registration obligations; articles containing CH2802 are subject to substance-of-very-high-concern communication duties only if a candidate-list substance exceeds 0.1 % w/w. RoHS 2011/65/EU restrictions on lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE are not expected to be triggered by the base resin, but recycled content and pigment masterbatch must be assessed separately.