| HS Code | 774442 |
| Density | 0.948–0.951 g/cm³ |
| Melt Flow Rate | 0.08 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | ≥24 MPa |
| Elongation At Break | ≥600% |
| Flexural Modulus | ≥1000 MPa |
| Notched Izod Impact Strength | ≥30 kJ/m² |
| Vicat Softening Temperature | ≥120°C |
| Brittleness Temperature | ≤-70°C |
| Environmental Stress Cracking Resistance | ≥1000 h |
| Hardness | ≥60 Shore D |
| Water Absorption | ≤0.01% |
| Dielectric Constant | 2.3 |
| Volume Resistivity | ≥1×10^16 Ω·cm |
| Melting Point | 130°C |
| Thermal Conductivity | 0.4 W/(m·K) |
As an accredited Sinopec Qilu HDPE DGDA6098 / 6098 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Qilu HDPE DGDA6098/6098 is typically packed in 25 kg PP woven bags, available in 25 metric ton lots. |
| Container Loading (20′ FCL) | 20′ FCL container loading for Sinopec Qilu HDPE DGDA6098/6098: 25 kg bags, palletized, shrink-wrapped, securely stowed, moisture-protected. |
| Shipping | Sinopec Qilu HDPE DGDA6098/6098 is shipped as non-hazardous high-density polyethylene pellets. Standard packaging includes 25 kg woven bags, 500–1000 kg jumbo bags, or bulk truck/container. Store in a cool, dry, well-ventilated area. Avoid moisture, contamination, and direct sunlight. Not regulated as dangerous goods for sea, road, or rail transport. |
| Storage | Store Sinopec Qilu HDPE DGDA6098 / 6098 in a cool, dry, well-ventilated warehouse. Keep original bags or containers sealed, palletized, and off the floor. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources, strong oxidizers, incompatible chemicals, and foodstuffs. Follow local regulations and the manufacturer’s SDS. Use first-in, first-out stock rotation. Avoid outdoor storage. |
| Shelf Life | Under cool, dry, ventilated storage away from sunlight, Sinopec Qilu HDPE DGDA6098/6098 has a typical shelf life of 24 months. |
Sinopec Qilu DGDA6098 is processed on monolayer high-stalk blown-film lines dedicated to thin-gauge T-shirt carrier sacks. The resin is charged to a grooved-feed extruder with a barrier screw of 24:1 to 30:1 L/D and a die gap of 0.8 mm to 1.2 mm. The bubble is set at a blow-up ratio of 4.0:1 to 5.0:1 and the stalk height is held at 6 to 8 die diameters. Melt temperature measured at the die lip is controlled from 200 °C to 230 °C; sustained excursions above 240 °C produce oxidation gels and die-lip deposits in the tack-down seal area of the film. Film thickness is drawn to 8 µm to 15 µm. Tensile properties are recorded to ASTM D882, dart impact to ASTM D1709 Method A, and Elmendorf tear to ASTM D1922. The converter seals T-shirt sacks at 130 °C to 155 °C with a dwell time of 0.2 s to 0.4 s. The end products are retail carrier sacks, produce bags, and laundry bags. The dominant processing failure is MD/TD orientation imbalance: high-stalk operation raises MD tensile strength but depresses MD tear in thin film, so seal bars are set along the TD axis where elongation is more uniform. For food-contact retail use, FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 migration testing must be verified for the finished structure. Incoming pellet surface moisture is kept below 0.05 wt%; when condensation appears on cold pellets, hopper-air purging at 70 °C for 1 h to 2 h is applied before extrusion.
When 20 wt% to 40 wt% LLDPE is coextruded as skin layers over a DGDA6098 core, the structure is run on a three-layer blown-film line with separate core and skin extruders. The LLDPE skins are processed at 185 °C to 210 °C, while the HDPE core is maintained at 200 °C to 225 °C. If the melt temperature differential between the core and skin streams exceeds 25 °C, interfacial instability appears at the die as wavy gauge bands near the frost line. The core is metered at 60 wt% to 80 wt% and the skins at 20 wt% to 40 wt%. The resulting refuse sack film is produced at 20 µm to 40 µm. Dart impact is tested to ASTM D1709 Method A, slow puncture to ASTM D5748, and seal strength to ASTM F88. The HDPE core supplies yield stress and stiffness; the LLDPE skins contribute TD tear and heat-seal strength. The terminal products are drawstring refuse sacks, star-seal kitchen bags, and higher-gauge garbage sacks. The known limitation is that HDPE-rich structures can exhibit lower dart impact at frost-line heights above 8 die diameters, so the air ring and chilled-air flow are adjusted to maintain the frost line within the high-stalk window. Compliance for heavy-metal content is screened against EU Directive 94/62/EC packaging standards for the final converted sack.
| Standard / Regulation | Test Method or Clause | Application Boundary |
|---|---|---|
| ASTM D1238 | 190 °C/2.16 kg | Incoming lot MFR verification for film-line lot release |
| ASTM D882 | Film tensile, secant modulus | MD/TD orientation control on high-stalk bubble |
| ASTM D1709 | Method A | Dart impact for thin-gauge film and filled grades |
| ASTM D1922 | Elmendorf tear | MD/TD tear balance and regrind acceptance |
| ASTM D5748 | Slow puncture resistance | Refuse sacks and heavy liners |
| ASTM D2578 | Surface wetting tension | Corona-treated lamination webstock |
| EU Regulation 10/2011 | Migration testing | Food-contact final structure verification |
| 21 CFR 177.1520(c) | Olefin polymers | US food-contact use after formulation-specific review |
Calcium carbonate masterbatch is let down into DGDA6098 at 5 wt% to 25 wt% on monolayer film lines fitted with a static mixer or cavity transfer mixer in the metering section. The filler suppresses film necking, increases opacity, and improves dead-fold in opaque retail packaging. During the trial, the density of the filled film is measured to ASTM D1505 and is expected to rise from the unfilled resin value of 0.949 g/cm³ to the range of 1.05 g/cm³ to 1.20 g/cm³ at 25 wt% CaCO₃, depending on masterbatch carrier resin and particle size. Haze and opacity are evaluated under ASTM D1003 and ISO 14782. Filler addition also raises melt pressure and torque on the extruder main drive; the screen pack is typically upgraded to a 60/100/60 mesh configuration to trap undispersed filler agglomerates. At loadings above 30 wt%, dart impact measured to ASTM D1709 and MD tear measured to ASTM D1922 commonly decline below retail bag acceptance limits in thin-gauge film. End products are opaque retail packaging, mailers, laundry bags, and industrial covers where paper-like stiffness and low light transmission are required. Food-contact status again requires verification under 21 CFR 177.1520(c) and EU Regulation 10/2011; the masterbatch additives must be specified in the migration test because CaCO₃ itself does not automatically confer compliance.
Post-industrial edge trim and start-up film are recycled back into non-food liner film on lines with a screen changer and a gear pump. The reinjection ratio of regrind to virgin DGDA6098 is held at 10 wt% to 20 wt% for standard runs. If the ratio exceeds 20 wt%, the melt flow rate is monitored to ISO 1133-1:2022 condition 190 °C/2.16 kg because repeated heat history increases the MFR and narrows the bubble stability window. The regrind must be ground to a uniform particle size below 8 mm to avoid uneven feeding; dust and fines are removed with a cyclone. A continuous screen changer with 100 µm or 150 µm screen packs is required to remove gel contamination. The resulting film is specified at 30 µm to 60 µm for non-critical trash can liners and industrial waste bags. Quality tests are limited to visual gel rating, gauge profile, and puncture resistance to ASTM D5748. Because the reincorporation of regrind can increase gel formation, converters must not use this stream for food-contact or high-speed T-shirt sack applications without additional melt filtration and migration testing.
Heavy-duty industrial liners and can liners are converted from DGDA6098 film in the gauge range 50 µm to 100 µm. The process uses a lower blow-up ratio of 3.0:1 to 3.5:1 to reduce the TD orientation and increase the film's carrying strength along the machine direction. Die gap is widened to 1.2 mm to 1.5 mm to maintain melt homogeneity at higher gauge. Secant modulus at 1% strain is measured to ASTM D882; this value is used as the release criterion for down-gauge projects. Puncture propagation tear is tested to ASTM D2582 on a high-speed puncture apparatus fitted with a 50 mm/min crosshead. The film is slit and sealed into heavy-duty liners, construction debris bags, and agricultural bulk packaging. The key processing constraint is the frost line: as gauge exceeds 60 µm, the bubble must be cooled with a dual-lip air ring and internal bubble cooling to prevent blocking at the collapsing frame. Additive packages should not exceed 1,500 ppm of total slip and antiblock, because higher concentrations produce plate-out on the collapsing shields and reduce film adhesion. The converted liners are tested for seam strength to ASTM F88 and for loaded burst resistance under factory-specific vacuum-lift trials.
For lamination webstock and garment-bag construction, DGDA6098 film is treated by corona discharge to a wetting tension of at least 38 mN/m, measured to ASTM D2578. The corona treater is placed on-line between the collapsing frame and the winder; treatment intensity is adjusted according to line speed and film gauge. The film is then printed with flexographic or gravure presses, and the ink adhesion is checked with tape-pull tests referenced to ASTM F2252. The HDPE film is used as an outer web in envelope windows, garment bags, and publication mailers because of its moisture resistance and dead-fold. The lamination adhesive is selected from polyurethane or acrylic grades; an epoxy-cured polyurethane system is not recommended where amine migration could generate interlayer delamination at the heat-seal jaw. The finished laminate is tested for bond strength under ASTM F904 on a tensile tester with a 200 N load cell. End products include envelope windows, garment bags, and non-food printed mailers. The known limitation is that corona treatment decays with storage; the web must be printed or laminated within 7 days of treatment, or retreatment is required. Film thickness is held at 12 µm to 25 µm for window and garment applications.
Competitive Sinopec Qilu HDPE DGDA6098 / 6098 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Qilu HDPE DGDA6098, also designated grade 6098 in domestic commercial listings, is a high-molecular-weight high-density polyethylene resin positioned for high-stalk blown film extrusion. The grade is characterized by a nominal density of 0.950 g/cm³ under ISO 1183-1:2019 and a nominal melt mass-flow rate of 0.11 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022. The corresponding high-load melt mass-flow rate at 190 °C/21.6 kg is approximately 8.0 g/10 min, producing a high-load/standard flow ratio near 73:1. This rheological signature places the material outside conventional injection molding and pipe extrusion; it is instead weighted toward melt strength, high-stalk bubble stability, and downgauged film toughness.
Commercial production on this grade is reported in T-shirt style carrier bags, refuse sacks, industrial liners, and thin-gauge packaging films with thicknesses from 10 µm to 30 µm. In those formats, the resin is typically processed on single-screw blown-film lines with die diameters from 50 mm to 400 mm, die gaps from 1.2 mm to 2.5 mm, and blow-up ratios from 3:1 to 5:1. The broad molecular weight distribution permits a tall stalk, commonly 6 to 10 die diameters in neck height, which aligns melt orientation ahead of the frost line and shifts the film tear balance. Published production data for line speeds above 80 m/min with thickness below 12 µm remains limited; such performance depends on air-ring configuration, internal bubble cooling, and collapse-frame geometry rather than resin alone.
The low standard MFR of 0.11 g/10 min increases specific energy input relative to a 0.7 g/10 min general-purpose HDPE film grade. Melt temperature measured at the adapter is normally maintained between 190 °C and 230 °C. Below 185 °C, the die-lip shear rate can exceed the critical shear rate for shark-skin melt fracture, producing regularly spaced transverse ridges on the film surface. Above 240 °C, oxidative chain scission and gel-particle formation become time-dependent defects; residence times above 10 min at 240 °C can increase the high-load MFR and reduce bubble tear resistance. Extruder temperature profiles are therefore set as a rising profile from hopper to die, for example 170–180 °C in the feed section, 190–200 °C in the compression zone, 200–210 °C in the metering zone, and 190–210 °C at the die. These values are starting references for a 90 mm single-screw extruder with a 24:1 to 30:1 L/D barrier screw; they do not replace line-specific calibration.
Head pressure is a critical limitation. Because the high-molecular-weight fraction increases melt viscosity at low shear, breaker-plate and screen-pack selection typically uses a 60/80/100 mesh screen sequence and a working head pressure below 45 MPa. A pressure increase greater than 5 MPa at unchanged screw speed during a production run usually indicates screen-pack blinding, insufficient feed-zone temperature, or feed-section material blockage. Operators also monitor screw amperage, but amperage is not a substitute for melt temperature. Excessive screw speed intended to compensate for low melt temperature produces melt-pressure fluctuation and can cycle bubble diameter by more than ±5%, creating measurable film-thickness variation on online capacitance gauges.
Internal bubble cooling and dual-lip air rings are preferred over single-lip air rings at high output. With a 250 mm die and a blow-up ratio of 4:1, frost-line height is typically adjusted between 4 and 8 die diameters above the die. A lower frost line may quench the bubble too early, raise transverse-direction tear, and reduce dart impact. A higher frost line can produce bubble wander, gauge bands at the collapsing frame, and unstable layflat width. The exact setting is governed by melt temperature, ambient air temperature, and cooling-air dew point, not by a fixed machine recipe.
The following values are nominal representative data for the base resin; lot-specific specification limits may be obtained from the manufacturer’s certificate of analysis. Incoming raw-material testing should use the stated standard revision, because test speed, specimen thickness, and conditioning affect reproducibility. Values should not be interpreted as guaranteed maxima or minima for every production lot.
| Property | Standard | Nominal value | Unit |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 0.11 | g/10 min at 190 °C/2.16 kg |
| High-load melt mass-flow rate | ISO 1133-1:2022 | 8.0 | g/10 min at 190 °C/21.6 kg |
| Density | ISO 1183-1:2019 | 0.950 | g/cm³ |
| Tensile stress at yield | ISO 527-2:2012 | 22 | MPa |
| Tensile strain at break | ISO 527-2:2012 | >500 | % |
| Dart impact, Method A | ASTM D1709-16a | 150 | g at 25 µm |
| Vicat softening temperature, A50 | ISO 306:2013 | 124 | °C |
| Melting temperature, DSC | ISO 11357-3:2018 | 131 | °C |
For food-contact applications, the base resin may be evaluated under FDA 21 CFR 177.1520 for olefin polymers. A supplier declaration is required because additive packages, catalyst residues, and film fabrication conditions may affect extractables. In the European Union, migration is evaluated on the finished article under EU 10/2011 and its amendments; total migration limits are 10 mg/dm² for general food contact and lower for specific food categories. REACH registration status should be confirmed through the Safety Data Sheet and SVHC declaration; the grade contains no intentionally added substances above 0.1 wt% in candidate-list categories. Packaging waste compliance follows national recycling streams; the resin is not intended for medical implant or pharmaceutical use.
Film converters sometimes blend DGDA6098 with 10–30 wt% LDPE or LLDPE to modify tear balance, seal initiation, and hand feel. The addition of LDPE at 20 wt% can lower die pressure and reduce frost-line sensitivity, but it also reduces yield strength and may increase blocking unless an anti-block masterbatch is added at 0.5–1.0 wt% based on silica content. These are starting ratios, not universally stable formulations. Batch-to-batch variance in comonomer content, catalyst residue, and pellet geometry can shift effective melt pressure and bubble stability; a lot-specific rheometer trace should be checked before high-speed commercial introduction.
The primary differentiator of DGDA6098/6098 is the combination of low standard MFR and moderate high-load MFR. Compared with a general-purpose HDPE film grade with a standard MFR of 0.6–1.2 g/10 min, the DGDA6098 standard MFR is roughly one-sixth to one-tenth as high, leading to higher melt pressure and higher melt strength. Compared with a typical injection molding HDPE with MFR in the 7–20 g/10 min range, the present grade cannot fill thin-wall molds and is outside the injection molding design window. Compared with an HDPE pipe grade of similar density, the pipe grade is formulated for hydrostatic strength and slow crack growth resistance; film dart impact and downgauging behaviour are not guaranteed by the same molecular architecture.
| Parameter | DGDA6098/6098 | General-purpose HDPE film | HDPE injection molding |
|---|---|---|---|
| MFR 190 °C/2.16 kg, ISO 1133-1 | 0.11 g/10 min | 0.6–1.2 g/10 min | 7–20 g/10 min |
| High-load MFR 190 °C/21.6 kg, ISO 1133-1 | 8.0 g/10 min | 15–30 g/10 min | not usually specified |
| Density, ISO 1183-1 | 0.950 g/cm³ | 0.948–0.955 g/cm³ | 0.950–0.965 g/cm³ |
| Primary process | high-stalk blown film | low-stalk or high-stalk blown film | injection molding |
| Typical thin-gauge film failure mode | ductile drawing in dart impact | lower puncture energy at equal gauge | not applicable |
In film service, the failure mode of a low-MFR high-molecular-weight film differs from that of a lower-molecular-weight film at the same gauge. DGDA6098 film tends to yield and draw rather than fail by brittle crack propagation in drop-impact testing under ASTM D1709-16a. In tear testing under ISO 6383-2, the orientation imposed by a high stalk typically increases machine-direction tear resistance, while transverse-direction tear resistance may be lower unless the blow-up ratio is raised. This anisotropic balance is a property difference, not a processing defect; converters should set dart-impact and tear targets on the finished film rather than on pellet MFR alone.
The grade should not be stored in unheated silos where condensed moisture can wet the pellet surface. Unlike hygroscopic engineering resins, HDPE does not require desiccant drying for absorbed water, but surface condensation from cold pellets in warm humid air can introduce pinholes in film. If pellets have been stored below the dew point, a surface-drying step at 60–70 °C for 2–4 h using desiccant air with a dew point of -20 °C or lower is recommended before film extrusion. Avoid combination with amine-based additives or strongly oxidizing color concentrates that have not been stability tested; such combinations can promote yellowing or gel formation during long runs. Post-industrial trim may be reprocessed at 10–20 wt% if dust and fines are controlled by melt filtration; higher regrind fractions typically increase gel count and widen gauge variation. These are processing restrictions observed on production-scale lines; they do not modify the published chemical resistance or food-contact status.