    • Product Name: Sinopec Maoming HDPE TR480M
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 852022
    Density 0.948 g/cm³
    Meltflowrate 190c 2 16kg 0.05 g/10 min
    Tensilestrengthatyield 25 MPa
    Elongationatbreak 600 %
    Flexuralmodulus 1000 MPa
    Notchedizodimpactstrength 300 J/m
    Vicatsofteningpoint 125 °C
    Brittlenesstemperature -70 °C
    Environmentalstresscrackingresistance >1000 h
    Hardnessshored 60
    Meltingpoint 130 °C
    Waterabsorption <0.01 %
    Thermalconductivity 0.4 W/m·K
    Dielectricconstant 2.3
    Bulkdensity 0.55 g/cm³
    Moisturecontent <0.1 %
    Ashcontent <0.05 %

    As an accredited Sinopec Maoming HDPE TR480M factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE TR480M is packaged in 25 kg polyethylene-lined woven bags, stacked on pallets for convenient transport and storage.
    Container Loading (20′ FCL) Sinopec Maoming HDPE TR480M in 20′ FCL: 25 kg bags, about 17 MT net, unpalletized; palletized loading may be lower.
    Shipping Sinopec Maoming HDPE TR480M is typically shipped as non-hazardous polyethylene pellets in 25 kg PP woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. It is transported in clean, dry 20-foot containers by sea or truck/rail. Store cool, dry, ventilated, away from sunlight, moisture, and contaminants.
    Storage Store Sinopec Maoming HDPE TR480M in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, heat, and ignition sources. Keep original packaging sealed to prevent moisture, dust, and contamination. Stack bags or pallets securely at moderate height. Avoid contact with strong oxidizers, oils, and incompatible chemicals. Use first-in, first-out inventory and follow local safety regulations.
    Shelf Life Store in cool, dry, well-ventilated area, sealed and away from sunlight; shelf life is typically 24 months in original packaging.
    Application of Sinopec Maoming HDPE TR480M

    In buried potable water networks, Sinopec Maoming HDPE TR480M is converted into solid-wall pressure pipe whose pressure class is governed by SDR, not by short-term tensile yield alone: SDR 17 corresponds to PN 10, and SDR 11 corresponds to PN 16 under ISO 4427-2:2019 and EN 12201-2:2011+A1:2023. The material is classified as PE100 through ISO 9080 extrapolation with an MRS of 10 MPa at 20°C for 50 years, and the pipe compound must also pass the notched-pipe test of ISO 13479 at 80°C and 4.0 MPa for not less than 500 h. Extrusion on a grooved-feed single-screw machine with L/D 30:1 to 36:1 is typical; barrel zones are held between 180°C and 210°C, head and die zones between 200°C and 210°C, and the melt stream at 200°C to 230°C is passed through an 80/120 mesh screen pack to remove char and gel particles. Backpressure ahead of the die pack is normally maintained in the 20–30 MPa range to stabilize output and prevent melt fracture. Potable-water pipe is produced with a blue pigment masterbatch at a letdown ratio of 2–4%; for outdoor storage, carbon black is added at 2.0–2.5 wt% and must show a dispersion rating no coarser than grade 3 when examined under ISO 18553. Joining uses butt fusion to ISO 21307:2017 with an interfacial fusion pressure of 0.15 MPa and bead-size verification on every joint. The bimodal molecular architecture is selected where high slow crack growth resistance is required in shifting soils and cold-water service.

    What Limits Gas Distribution Pipe Design Beyond Minimum Required Strength?

    The dominant constraint in natural gas distribution shifts from hydrostatic creep to rapid crack propagation resistance because a small impact puncture in a pressurized line can propagate axially faster than the gas decompression front if the pipe material lacks sufficient arrest capacity. TR480M pipe must meet ISO 4437-2:2014 for PE100 gas pipe, including the S4 critical pressure test under ISO 13477, the slow crack growth requirement under ISO 13479, and the long-term hydrostatic strength requirement under ISO 9080. Yellow masterbatch is added at a letdown ratio that does not reduce the compound's MRS below 10 MPa or alter the fusion parameter window. Typical operating pressures for SDR 11 PE100 gas distribution systems range from 0.4 MPa to 1.0 MPa, and all connections are made by electrofusion or butt fusion per ISO 21307:2017. Scrape-and-squeeze-off work on live mains requires the resin to tolerate local wall compression without initiating slow crack growth; the squeeze-off closing distance is limited to 80% of the outside diameter and release is controlled to avoid rapid re-expansion. The melt flow rate measured at 190°C under 5 kg load per ISO 1133-1:2022 places this grade in the 0.2–0.4 g/10 min range typical of bimodal PE100 pipe materials, balancing pipe extrusion output against sag resistance in large-diameter gas mains. Pipe produced for gas service is not transferred to potable water after off-spec wall thickness because the stabilizer package and pigment loading are matched to methane and odorant exposure rather than chlorine residual in drinking water.

    If the Pipe Carries Tailings Slurry, Wall Thickness Becomes the Primary Design Variable

    Slurry applications depart from clean-water design practice because the internal surface is subjected to continuous abrasion from quartz, pyrite, and coarse gangue particles moved by centrifugal pumps. TR480M is specified for tailings lines on the basis of strain tolerance and fused-joint continuity rather than tensile modulus; the wall thickness is deliberately increased beyond the SDR pressure rating to create a sacrificial wear allowance that protects the minimum required wall for connector loads and surge pressure. Slurry flow velocity is held between 2.0 m/s and 3.5 m/s because erosion rate in HDPE rises non-linearly when coarse particles exceed 200 μm and the impact angle concentrates at elbows, Y-branches, and blind-end laterals. Dredge and tailings lines are bedded per ASTM D2321-20 with select granular material; long-radius electrofusion fittings are used in place of injection-molded bends because the extra fitting wall and smooth transition reduce localized wear. Pressure surges from positive-displacement pumps are superimposed on the erosive load, so the system designer applies a surge allowance factor of 1.6 for intermittent service or 2.0 for cyclic operation against the PE100 MRS of 10 MPa. The outer surface is not the limiting degradation zone in this service; internal wall thinning at the invert and at directional changes is the controlling life parameter, and thickness verification is carried out with an ultrasonic thickness gauge at scheduled maintenance intervals.

    At ambient temperature, TR480M withstands a broad range of aqueous industrial fluids encountered in chemical plant drainage, process water transfer, and acid or caustic dosing lines, but the limiting compatibility boundary is not pH alone; it is the interaction of temperature, stress, and oxidizing species. Chemical resistance should be evaluated against ISO/TR 10358 and ASTM D543-21 using immersion coupons; published data for this specific resin formulation may be limited, so a site-specific immersion test at the maximum operating temperature is used for streams containing mixed solvents. Concentrated sodium hypochlorite, wet chlorine gas, fuming sulfuric acid, and strong oxidizing mixtures fall outside the available compatibility window for HDPE under stress. Aromatic hydrocarbons and chlorinated solvents reduce long-term stress crack resistance and are not carried in TR480M pressure lines unless the system is de-rated and protected by double containment. For industrial effluents with abrasive particulates, the same sacrificial wall-thickness method used in slurry service is applied. Joining methods are selected from butt fusion to ISO 21307:2017 or electrofusion sockets; flanged transitions to carbon steel use backing rings with full-face elastomer gaskets and torque is limited to the fitting manufacturer's declared sequence to avoid point loading the HDPE stub end.

    Trenchless Pullback and Overbend Survivability in Horizontal Directional Drilling

    Trenchless installation by horizontal directional drilling uses the pipe string itself as the pullback tensile member, which imposes a strict cap on axial force and outer-surface damage. The safe pull load for HDPE PE100 is calculated by ASTM F1962-20 using an allowable tensile stress at 20°C, not the short-term yield stress, and the pullback force is monitored with an inline load cell; field practice rejects drilling-fluid pressure that approaches the collapse threshold for the selected SDR because the pipe is under simultaneous tension and external mud pressure. The pipe string is fused above grade into one monolithic section using ISO 21307:2017 butt fusion, and the minimum allowable bending radius is maintained at 20–25 times outside diameter to keep outer-fiber strain below the long-term creep limit for PE100. Rock crossings require an annular space larger than the pipe outside diameter to prevent scoring; common inspection criteria reject axial scratches deeper than 10% of nominal wall thickness in pressure-rated HDPE. The same slow crack growth resistance that protects buried water and gas mains is relevant during post-installation pullback relaxation, because the pipe is locked into residual curvature and may remain under sustained tensile stress at the exit transition and connection to the carrier main for the operating life.

    Subaqueous HDPE strings require negative-buoyancy control rather than pressure resistance alone, because the pipe is floated into position and then sunk into a dredged trench where wave, current, and backfill loads act on the assembled string. TR480M pipe for marine outfall and intake service is compounded with carbon black at 2.0–2.5 wt% when exposed to sunlight during staged construction, with dispersion conforming to ISO 18553 grade 3 or better. Concrete ballast collars or bolted weights are spaced to maintain a submerged specific gravity of 1.05–1.10; the bending radius during S-lay and trench entry is kept at 20–25 times outside diameter to prevent local wall collapse and fusion bead stress. Butt fusion joints per ISO 21307:2017 allow the pipe to be assembled into a continuous string on shore before launch, eliminating underwater mechanical connections. External hydrostatic pressure at depth is checked against the pipe's collapse rating, and the design includes a minimum residual wall thickness after accounting for marine growth removal and anchor drag scoring. Published data for long-term marine exposure of this specific grade is limited, so inspection ports and wall-thickness monitoring points are included at diffuser and landfall transitions.

    Geothermal Borehole Loops Enter the Low-Temperature Service Window

    Because closed-loop ground-source heat pump circuits operate at low pressure and near-ambient temperatures, TR480M is used in vertical borehole loops and horizontal slinky configurations where sustained point loads from grout and rock contact become the controlling service condition. The resin's slow crack growth resistance is relevant because the pipe is installed in rough boreholes and is subjected to continuous contact with grout particles, rock edges, and thermal expansion cycles between 0°C and 40°C. Sustained operation above 60°C would move the material outside the PE100 long-term hydrostatic design envelope; therefore, this resin is not selected for high-temperature district heating circuits. Heat transfer fluids are water–propylene glycol or water–ethanol mixtures, and compatibility with these fluids falls within the HDPE chemical resistance window. Pipe joints are made by socket fusion or butt fusion to ASTM F2620-19 and ISO 21307:2017; the fusion bead is not trimmed on borehole U-bends unless the fitting manufacturer specifies bead removal for insertion clearance. The loop is pressure-tested before grouting, and the test pressure is held for the duration specified by local ground-source system codes while the borehole is still open to allow visual inspection of the transition from vertical pipe to trench header.

    Free Quote

    Competitive Sinopec Maoming HDPE TR480M prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HDPE TR480M is a bimodal high-density polyethylene resin supplied by Sinopec Maoming Petrochemical Company as a black pellet. The grade is classified as PE100 under ISO 12162 and is intended for pressure pipe extrusion in potable water, municipal gas, and industrial fluid networks. The product designation indicates a high-density polyethylene with a low melt flow rate, controlled carbon black loading, and hydrostatic design basis of 10 MPa at 20 °C for 50 years. The material is not a general-purpose injection-moulding or blow-moulding HDPE; its melt viscosity and molecular architecture are tailored for long-term creep and slow crack growth resistance in buried infrastructure. At molecular level, the bimodal distribution separates processability from slow crack growth resistance. In a unimodal HDPE, increasing molecular weight improves toughness but reduces melt flow; in a bimodal resin, the high-molecular-weight fraction can be large enough to impart slow crack growth resistance while the lower-molecular-weight fraction reduces melt viscosity under extrusion shear. TR480M therefore occupies the same classification as other PE100 products but is not automatically interchangeable with them for every pipe line or certification portfolio.

    Pipe-Grade Bimodal Architecture and Hydrostatic Classification

    The bimodal molar mass distribution of TR480M creates a processable high-molecular-weight structure. The high-molecular-weight fraction provides tie molecules that bridge interlamellar regions and resist crack propagation, while the lower-molecular-weight fraction improves melt flow under extrusion shear. In ISO 12162 classification, PE100 requires a lower prediction limit of hydrostatic strength of 10 MPa at 20 °C and 50 years from ISO 9080 regression. The resin must also satisfy minimum requirements under ISO 1167-1 for internal hydrostatic pressure at 20 °C and 100 h. ISO 9080 hydrostatic strength regression uses data at 20 °C, 40 °C, 60 °C and 80 °C for times up to 10,000 h or more. Extrapolation to 50 years is valid only if brittle failure modes dominate; ductile failure at high stress must be excluded from the regression where specified by the standard. A material with a regression line above 10 MPa but with low slow crack growth resistance may fail notched pipe tests. Therefore TR480M is evaluated with both hydrostatic pressure tests on unnotched pipe and notched pipe tests under ISO 13479. Typical reported density is 0.949 g/cm³ by ISO 1183-1. Melt flow rate tested at 190 °C and 5 kg load is in the range of 0.20–0.35 g/10 min under ISO 1133-1. Tensile yield strength is typically 23–25 MPa when measured by ISO 527-2, and elongation at break exceeds 600 %. Flexural modulus in the 900–1100 MPa range under ISO 178 contributes to pipe ring stiffness but does not replace ISO 9969 ring stiffness testing on finished pipe. Carbon black loading between 2.0 % and 2.5 % by mass, evaluated by ISO 6964, provides ultraviolet screening in outdoor storage. Dispersion quality is normally controlled to grade 3 or better according to ISO 18553 to avoid local stress concentrations.

    PropertyTest methodTypical reported value
    DensityISO 1183-10.949 g/cm³
    Melt flow rate, 190 °C, 5 kgISO 1133-10.20–0.35 g/10 min
    Tensile yield strengthISO 527-223–25 MPa
    Elongation at breakISO 527-2>600 %
    Flexural modulusISO 178900–1100 MPa
    Carbon black contentISO 69642.0–2.5 %
    Carbon black dispersionISO 18553≤ grade 3
    Oxidation induction timeISO 11357-6>30 min at 200 °C
    Environmental stress crack resistanceASTM D1693-15F50 >1000 h

    What Separates TR480M from PE80 and Conventional Injection-Moulding HDPE Grades?

    The primary difference between TR480M and PE80 is the hydrostatic design basis. PE80 has an MRS of 8 MPa, whereas PE100 has an MRS of 10 MPa. For a given pressure rating, PE100 pipe can have a lower wall thickness than PE80, reducing material demand and external diameter. This wall thickness reduction also increases internal bore at equal outside diameter, lowering fluid velocity at a given flow rate and reducing pumping energy. For water pipes, ISO 4427-2 provides minimum wall thicknesses for SDR series such as SDR 11, SDR 13.6, SDR 17, SDR 21 and SDR 26. PE100 allows the use of higher SDR values for a given pressure class compared with PE80, which translates into larger bore and lower hydraulic friction. Compared with conventional injection-moulding HDPE grades with melt flow rates of 5–20 g/10 min at 190 °C and 2.16 kg, TR480M has high melt viscosity and slow chain relaxation. Thin-wall injection moulding would require high melt temperatures and injection pressures that risk polymer degradation and incomplete mould filling. In pipe extrusion, the same high viscosity provides melt strength for vacuum calibration and reduces sag in large-diameter pipes. Compared with PE80 pipe materials, TR480M typically shows longer notched pipe failure times under ISO 13479. PE100 grade notched pipe specimens generally exceed 500 h at 80 °C and 0.92 MPa hoop stress; PE80 grades may fail earlier. Slow crack growth resistance of bimodal PE100 arises from the high-molecular-weight fraction and controlled short-chain branching, which increase tie-molecule density and reduce disentanglement under sustained stress. Carbon black content also differs from natural HDPE film grades; TR480M contains 2.0–2.5 % carbon black, while film grades are generally unpigmented or contain low pigment loading. This loading provides ultraviolet protection but makes the material unsuitable for applications requiring translucency or food-contact clarity.

    In potable water and gas distribution pipe extrusion, TR480M is run on single-screw extruders with grooved feed sections and barrier screws. Production machines commonly use L/D ratios of 30:1 to 33:1 and liquid-cooled grooved bushings to maintain feed-zone cooling. Barrel temperature settings from 180 °C in the feed section to 220 °C at the metering section are typically used. Die head and adapter temperatures are maintained between 210 °C and 230 °C. Melt temperature measured at the die exit should remain between 190 °C and 230 °C. Above 240 °C, chain scission accelerates, OIT decreases, and gel particle formation can cause surface defects and pipe microcracks. The upper temperature threshold is therefore an oxidative-stability boundary linked to ISO 11357-6 OIT. Vacuum sizing tanks and spray cooling baths with water temperatures from 15 °C to 25 °C are used to set outer diameter and wall thickness. Pipe dimensions for potable water are evaluated against ISO 4427-2; ring stiffness is measured by ISO 9969. The high melt viscosity of PE100 increases head pressure and shear heating. Operators monitor extruder motor load and melt pressure before the breaker plate; excessive screw speed can induce melt fracture and sharkskin on the pipe surface. If pellet moisture is present from condensation or storage at relative humidity above 60 %, pre-drying at 80 °C for 2–4 h in a hot-air or desiccant drier is applied. Drying prevents surface pitting and steam-induced voids during extrusion. Production-scale difficulties include batch-to-batch variation in melt flow rate and carbon black dispersion. When melt flow rate shifts upward by more than 0.05 g/10 min, wall thickness control and sag resistance may change; when carbon black dispersion exceeds grade 3, point-load resistance can deteriorate.

    When Buried Gas Mains Require Notched Pipe Resistance and Elevated-Temperature Derating

    For buried gas mains, pipes produced from TR480M are assessed against ISO 4437-3 and EN 1555-2. The hydrostatic design stress is derated when service temperature exceeds 20 °C. At 40 °C, PE100 pressure ratings are reduced by approximately 30–40 % relative to the 20 °C rating, depending on the pipe standard and safety factor. Rapid crack propagation resistance is evaluated with the S4 test of ISO 13477 at low temperature. PE100 gas pipes are formulated to resist long-running cracks that can propagate along a pressurised main. Slow crack growth resistance is evaluated by ISO 13479 notched pipe testing; PE100 grades generally exceed 500 h at 80 °C and 0.92 MPa hoop stress, although published TR480M-specific data for this configuration are limited. Notched pipe tests under ISO 13479 use a 110 mm pipe specimen with external longitudinal notches at four locations. The test is run at 80 °C and an internal pressure that produces a hoop stress of 0.92 MPa. For potable water service, the finished pipe must demonstrate migration behaviour appropriate to drinking-water contact under EN 12873-1 or national equivalents. TR480M should not be blended with amine-based antioxidant systems that can deplete the primary phenolic stabiliser or reduce OIT below 20 min at 200 °C. The addition of pro-oxidant additives for degradable film applications is incompatible because it would reduce hydrostatic design life. High levels of calcium carbonate filler or reprocessed material from unknown sources should be avoided unless the finished pipe is revalidated for hydrostatic strength and slow crack growth.

    Performance areaStandard / method
    PE100 classificationISO 12162
    Hydrostatic strength regressionISO 9080
    Hydrostatic pressure test, 20 °C, 100 hISO 1167-1
    Notched pipe slow crack growthISO 13479
    Rapid crack propagation resistanceISO 13477
    Potable water pipe material and dimensional requirementsISO 4427-2
    Gas pipe requirementsISO 4437-3 / EN 1555-2
    Drinking-water migration testingEN 12873-1
    Carbon black content and dispersionISO 6964 / ISO 18553
    Oxidative stabilityISO 11357-6

    At the conversion line, raw-material certificates for TR480M are reviewed for melt flow rate, density, carbon black content, carbon black dispersion, and OIT. Certificates should be traceable to the producer lot under ISO 9001 and ISO 14001 quality systems. Rotational moulding and injection moulding of this grade are generally impractical because melt viscosity is too high and the product is formulated for pipe extrusion. If regrind from pipe production is reused, clean, unpigmented or black PE100 regrind can be incorporated at low levels, but the blend’s melt flow rate and hydrostatic classification must be reaffirmed. Storage in unopened containers should be below 50 °C to limit antioxidant migration and surface oxidation. Under tropical conditions with relative humidity above 60 %, pre-drying is required. The grade is suitable for buried pipe only when carbon black content meets ISO 6964 and service temperature is below 20 °C; above-ground exposed pressure pipe requires additional UV and heat load assessment due to potential service temperatures above 20 °C. Published data for multi-layer co-extrusion of TR480M with other HDPE tie layers are limited; when multi-layer pipe is produced, interfacial adhesion and slow crack growth resistance should be validated on the finished pipe according to ISO 1167-1 and ISO 13479. These operational boundaries are derived from PE100 pipe resin behaviour and standard qualifiers, and they should be verified against the producer certificate for each lot.