| HS Code | 692088 |
| Density | 0.945 g/cm³ |
| Melt Flow Rate | 0.18 g/10 min |
| Tensile Yield Strength | 23 MPa |
| Elongation At Break | 500% |
| Flexural Modulus | 900 MPa |
| Vicat Softening Temperature | 122 °C |
| Environmental Stress Crack Resistance | >1000 h |
| Notched Izod Impact Strength | 200 J/m |
| Hardness | 65 Shore D |
| Water Absorption | 0.01% |
| Dielectric Constant | 2.3 |
| Volume Resistivity | >1×10^16 Ω·cm |
As an accredited Sinopec Maoming HDPE TR144-GD factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Maoming HDPE TR144-GD is supplied in 25 kg polyethylene-lined woven bags, stacked on pallets for bulk transport. |
| Container Loading (20′ FCL) | Seaworthy 20' FCL container loaded with Sinopec Maoming HDPE TR144-GD in 25 kg bags, palletized, securely stowed for chemical transport. |
| Shipping | Sinopec Maoming HDPE TR144-GD is non-hazardous and ships as general cargo in 25 kg woven bags, usually palletized or loose-loaded. Standard FCL ocean freight uses 40HQ containers, loading about 25–28 MT. Store dry, ventilated, away from sunlight, moisture, and heat. Normal export handling applies. |
| Storage | Store Sinopec Maoming HDPE TR144-GD in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags closed and palletized to prevent moisture, dust, and contamination. Avoid prolonged high temperatures and stacking damage. Use first-in, first-out stock rotation. Handle with clean equipment; no food, drink, or smoking in storage areas. Protect from mechanical damage. |
| Shelf Life | Sinopec Maoming HDPE TR144-GD: store cool, dry, ventilated, away from sunlight; recommended shelf life is 24 months in unopened original packaging. |
Cold-water municipal networks processed from TR144-GD typically target the PE 100 classification under ISO 12162:2023 and the pipe material requirements of EN 12201-2:2011+A1:2018, because the 50-year design strength must remain above the lower prediction limit derived from ISO 9080:2022 regression. The compound is prepared with 93.0–94.6 wt% virgin TR144-GD, 5.0–6.3 wt% of a 40 wt% carbon black masterbatch to give 2.0–2.5 wt% carbon black in the final wall, and 0.4–0.7 wt% of an antioxidant/processing-aid masterbatch; the dosing ratio is set gravimetrically and checked by ash content every 2 h. Extrusion on a 60 mm grooved-barrel single-screw machine with L/D 30:1 and barrel temperatures from 180°C to 210°C produces a melt at 200–215°C, while the die head is held at 190–205°C; downstream vacuum calibration at −0.2 bar to −0.5 bar and spray cooling at 15–20°C maintain wall-thickness tolerance within ±0.2 mm on 110 mm pipe. The central process conflict is thermal: exceeding 220°C oxidises the outer layer and shifts hydrostatic strength downward, while operating below 190°C produces sharkskin on the die land and unresolved plastication defects. Pre-drying at 80°C for 2 h is required if moisture measured by Karl Fischer exceeds 0.03 wt%, because water vapour in the melt appears as microvoids that lower slow crack growth resistance in hydrostatic testing. Finished product types include SDR 11 and SDR 17 PE100 pipes from 25 mm to 630 mm, supplied in coils for service lines and in 6 m or 12 m straight lengths for mains, with compliance documentation covering NSF/ANSI/CAN 61, AS/NZS 4020:2018, and GB/T 17219 where potable-water contact approval is mandatory.
Gas distribution imposes the tightest rapid crack propagation control because a small through-wall crack can propagate along a pipeline at sonic velocity. Pipe compounds in this sector are formulated with 93.0–94.5 wt% TR144-GD, 5.0–6.2 wt% of a 40 wt% carbon black masterbatch, and 0.5–0.8 wt% of a heat-stabiliser masterbatch; the final wall must contain 2.0–2.5 wt% carbon black as specified in ISO 4437-2:2024 for UV and weathering resistance, and no post-consumer recyclate is permitted in the pressure wall under ISO 4437-1:2024. Extrusion runs at melt temperature 205–215°C through a spiral mandrel die with 16–32 ports depending on outside diameter; die gap is held at 1.0–1.5 mm for 110 mm OD, and haul-off speed is slaved to ultrasonic wall-thickness measurement so that SDR 11 tolerance is maintained from +0.2 mm to −0.0 mm. The critical conflict on production lines is that high melt temperatures improve melt homogenisation but accelerate additive consumption; operators monitor melt mass-flow index under ISO 1133-1:2022 condition T every 4 h, and a drift above 0.25 g/10 min at 190°C/5 kg is treated as incipient degradation or feed contamination. Rapid crack propagation is assessed by ISO 13477:2008 S4 testing at 0°C, while slow crack growth is measured by ISO 13479:2022 notched pipe testing; both must be included in the initial type-test report before first article approval. Finished products include SDR 11 black PE100 gas pipes from 20 mm to 400 mm, supplied as 50 m or 100 m coils for small diameters and 6 m or 12 m sticks for larger diameters, designed for maximum operating pressures from 1.0 MPa in small-diameter networks to 0.4 MPa in large-diameter distribution lines, with ASTM D2513-24 governing the North American export specification.
Low-pressure industrial effluent lines carrying acids, alkalis, and mixed organic streams impose chemical resistance demands that exceed potable water service, and TR144-GD is selected only after confirming compatibility at the expected service temperature and concentration. In dilute inorganic acid and neutralised wastewater service, the extrusion formulation is compounded with 92.7–94.5 wt% TR144-GD, 5.0–6.3 wt% of a 40 wt% carbon black masterbatch, and 0.5–1.0 wt% of an acid-neutralising stabiliser masterbatch; the final carbon black level may be reduced to 1.5–2.0 wt% where electrostatic dissipation is not required, but that decision must be verified against ISO 15494:2015 industrial polyethylene piping requirements and the specific chemical resistance data. Because published data for TR144-GD in aggressive organic media is limited, pipe manufacturers normally run immersion testing according to ISO 4433-1:2019 at the actual concentration and temperature before quoting service life. Extrusion proceeds on a grooved-barrel single-screw line with barrel temperatures 190–210°C, melt temperatures 200–215°C, and a breaker-plate screen pack of 80/120/80 mesh to trap gels; the pipe is calibrated under vacuum and then cut into 6 m sticks for butt fusion. Wall-thickness calculation for industrial effluent uses the same hydrostatic design basis as water pipe but applies a chemical service factor, and the resulting pipe is often derated from PN 16 to PN 10 or PN 6 for solvents or oxidising streams. Terminal products include PN 10 and PN 16 flanged spool assemblies, fabricated elbows, and straight PE100 pipe from 32 mm to 315 mm, used in chemical plant effluent containment, plating-line wastewater transfer, desalination brine discharge, and neutralised acid waste headers. The operational boundary is explicit: TR144-GD is not suitable for strong oxidising acids above 40°C nor for continuous exposure to aromatic hydrocarbons, and such services require a higher-fluorine polymer barrier or an alternative material.
Mining tailings and dredge slurry lines from TR144-GD use the same PE100 hydrostatic design basis but must account for wall loss from internal abrasion, so pipe specifiers apply a service factor and often select SDR 11 or SDR 17 walls with a sacrificial wear allowance. The compound for thick-wall black pipe is formulated with 92.5–94.2 wt% TR144-GD, 5.0–6.3 wt% of a 40 wt% carbon black masterbatch to reach 2.0–2.5 wt% wall carbon black, and 0.8–1.2 wt% of a process-stabiliser/external-lubricant masterbatch to hold melt pressure stable during long thick-wall runs. Extrusion on 75–150 mm grooved-barrel single-screw extruders with melt pumps and L/D 33:1 to L/D 36:1 keeps melt temperature at 195–210°C; wall thickness up to 60 mm demands stepwise cooling after the vacuum calibration tank to reduce frozen-in stress, because residual stress accelerates slow crack growth when the outer wall is scratched by ore particles. Production bottlenecks are primarily throughput limitations at high wall thickness and sag of the unsupported pipe between die and calibrator; belt haul-offs with six-point contact are used instead of conventional two-wheel pullers above 400 mm OD. Published data for TR144-GD slurry abrasion life is limited because wear rate depends on particle angularity, velocity, and solids concentration; site-specific abrasion tests or a wear allowance of 2–5 mm beyond the pressure wall is common practice but must be confirmed by operators. Terminal product types include SDR 17 and SDR 21 tailings lines from 110 mm to 1000 mm, mine dewatering mains, dredge discharge pipe, and flanged adapters for slurry pumps, with butt fusion and electrofusion joints qualified under ISO 4427-2:2019, ISO 13479:2022, and ASTM D3350-24 cell classification.
Pressurised agricultural irrigation mains extruded from TR144-GD are dimensionally centred on SDR 17 to SDR 26, where the governing variables are pump-pressure cycling, soil load, and long-term ultraviolet exposure rather than elevated temperature. The pipe compound comprises 93.2–94.7 wt% TR144-GD, 5.0–6.2 wt% of a 40 wt% carbon black masterbatch for 2.0–2.5 wt% final carbon black, and 0.3–0.6 wt% of a UV-stabiliser/processing-aid masterbatch; a blue co-extruded stripe is often added only as a code marking for non-potable water. Extrusion uses a single-screw grooved-barrel line at barrel temperatures 180–205°C, melt 195–210°C, and vacuum calibration at −0.2 bar to −0.4 bar; wall thickness is recorded continuously by ultrasonic sensors, and the puller speed is trimmed for every 0.5% change in line speed to hold outer diameter within ±0.3 mm. The main field failure mode is not hydrostatic collapse but third-party mechanical damage during trenching and soil movement, so installation standards such as ISO 4427-5:2019 govern bedding and backfill rather than material formulation. Finished product types include 75 mm to 400 mm PE100 irrigation mainlines, sub-mainline sections, reversible flanged connections for diesel pump suction and discharge, and saddle-branch outlets; these are sold in 6 m and 12 m sticks and in larger coils for smaller diameters where transport permits.
Ground-source heat pump loops fabricated from TR144-GD rely on the PE100 hydrostatic design basis because the loop is a closed pressure system that must survive 50 years buried in soil at temperatures normally below 20°C. The compound is kept at 93.5–94.6 wt% TR144-GD, 5.0–5.8 wt% of a 40 wt% carbon black masterbatch, and 0.4–0.7 wt% of an antioxidant masterbatch; no plasticiser or processing slip additive is used because low-molecular-weight additives can migrate to the pipe surface and complicate heat-fusion joints. Coil extrusion on 25–50 mm OD dies at melt temperature 195–210°C and vacuum sizing at −0.3 bar to −0.5 bar produces SDR 11 wall thicknesses from 2.3 mm to 4.6 mm, with automatic coilers running at 25–60 m/min for 300 m or 600 m coils. The operational boundary is temperature: PE100 pressure rating decreases above 20°C, and the pipe is not rated for direct geothermal heat extraction above 60°C; therefore the application is limited to low-temperature ambient ground loops. Published data for TR144-GD in geothermal service is limited, so qualification is based on the PE100 classification under ISO 12162:2023 and hydrostatic type testing under ISO 9080:2022, not on a geothermal-specific long-term creep database. Terminal products include U-bend ground loops, pond and lake loops, manifold headers, and socket-fused loop headers for ground-source heat pump arrays.
Competitive Sinopec Maoming HDPE TR144-GD prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Maoming HDPE TR144-GD is a high-density polyethylene resin supplied by Sinopec Maoming Petrochemical Company as a pelletized film-extrusion grade. The designation identifies a high-molecular-weight HDPE film material; the suffix GD denotes a production or additivation variant, and the producer’s certificate of analysis should be consulted for exact nomenclature and lot traceability. The resin is intended for thin-gauge blown film applications in which high melt strength, controlled density, and downgauging capability are required. Because lot-to-lot variation exists, the values in Table 1 should be read as representative published ranges, not as specification limits. Where compliance decisions depend on a property, converters should use the lot-specific certificate of analysis.
Representative property ranges for Sinopec Maoming HDPE TR144-GD are summarized below.
| Property | Test method | Typical range |
|---|---|---|
| Melt mass-flow rate, 190 °C / 2.16 kg | ISO 1133-1:2022 | 0.22–0.30 g/10 min |
| Density, 23 °C | ISO 1183-1:2019 | 0.945–0.948 g/cm³ |
| Tensile stress at yield | ISO 527-2:2012 | ≥22 MPa |
| Elongation at break | ISO 527-2:2012 | ≥500% |
| Dart drop impact F50, 25 μm film | ASTM D1709-15a Method A | 120–180 g as processed |
| Environmental stress-crack resistance F50, 100% Igepal CO-630 | ASTM D1693-15 | ≥500 h |
| Vicat softening temperature A50 | ISO 306:2013 | 122–127 °C |
The combination of density and low melt mass-flow rate places TR144-GD close to other high-molecular-weight HDPE film grades but with a relatively narrow density specification. The low melt index indicates high melt viscosity and makes the resin unsuitable for injection molding or high-flow extrusion. Published gel permeation chromatography data for similar grades indicate a bimodal molecular weight distribution; this architecture increases the high-molecular-weight fraction responsible for melt strength while the lower-molecular-weight fraction contributes processability. Capillary rheometry is not included in the standard datasheet, but similar resins exhibit pronounced shear thinning, which keeps extrusion backpressure manageable in grooved-feed single-screw extruders. Density of 0.945–0.948 g/cm³ indicates limited short-chain branching, typically introduced by low levels of α-olefin comonomer, and produces higher crystallinity and stiffness than linear low-density polyethylene film grades. Film property comparisons should use ISO 527-3 rather than ISO 527-2 because the latter reports resin tensile values on compression-moulded specimens, whereas blown-film orientation and thickness dominate final performance.
High-stalk extrusion is the preferred processing mode for TR144-GD. In this geometry, the bubble rises several die diameters before reaching the frost line, which aligns the high-molecular-weight fraction and builds machine-direction orientation. Single-screw extruders with L/D ratios of 25:1 to 30:1, barrier screws, and Maddock-style dispersive mixers are commonly used. Melt temperature at the die lip is maintained between 180 °C and 210 °C, with a narrower target of 185–200 °C when gauge variation must remain below ±1 μm. Below 175 °C, sharkskin and melt fracture appear as fine surface roughness that reduces gloss and tear resistance. Above 220 °C, residence time becomes critical because thermo-oxidative degradation generates visible gels that cause pinholes and screen-pack pressure rise.
Die gap recommendations vary with film thickness. For film between 15 μm and 80 μm, die gaps of 1.2 mm to 2.2 mm are typical. A gap below 1.0 mm raises wall shear rate and may exceed the critical shear rate for sharkskin; capillary rheometry suggests this threshold lies near 500–800 s⁻¹ at 190 °C for this density class. Blow-up ratio is normally set between 3:1 and 5:1. High-stalk bubbles tolerate the upper end because the resin’s strain hardening resists bubble flapping. Frost line height of 6–10 die diameters balances machine-direction and transverse-direction properties. Excessively high frost lines increase blocking tendency and reduce line speed; excessively low frost lines produce low machine-direction tear resistance.
Pre-drying is not usually required for resin taken directly from sealed bags at ambient humidity. If pellet surface condensation occurs after storage in unheated warehouses, hot-air drying at 70–80 °C for 1–2 h is sufficient to remove surface moisture. Continuous melt temperatures above 250 °C should be avoided. Slip and antiblock masterbatches at 2–5 wt% are common in commercial bag film because the base grade is not supplied with high levels of pre-dispersed slip additives. Screen packs of 80/120/80 mesh trap degraded particles; pressure drop across the screen pack should be monitored to detect gel accumulation. Film-to-film coefficient of friction after masterbatch addition should be checked per ISO 8295, and haze should be checked per ISO 14782.
For converters evaluating TR144-GD as a direct replacement for LLDPE-rich film structures, the response to melt drawing differs. The high-molecular-weight HDPE exhibits greater strain hardening, which supports bubble stability, but its extensional viscosity is more temperature-sensitive. Melt pressure on a 65 mm extruder with a 200 mm die and 1.8 mm die gap has been reported to become the limiting variable before screw speed when melt temperature is below 190 °C. Production lines designed for LLDPE may require screw and die-temperature profile changes rather than simple material substitution.
Optical properties of HDPE remain lower than LLDPE. Haze measured per ISO 14782 on 25 μm film is typically above 15% unless special chill-roll or high-gloss processing is used. Gloss is measured per ISO 2813; surface roughness increases haze and reduces gloss. Converters seeking high-clarity film should not use TR144-GD as the sole resin. Water vapour transmission rate of HDPE is lower than LDPE and LLDPE because of higher crystallinity, but oxygen transmission is higher than PET and PA. Since published permeation data for this specific grade at commercial thickness is limited, WVTR should be tested per ASTM E96/E96M-16 when barrier performance is critical. Heat-seal initiation temperature is typically higher than LLDPE, usually above 135 °C depending on sealing equipment, dwell time, and film thickness; seal strength should be tested per ASTM F88/F88M-15.
Substitution of TR144-GD for monomodal film-grade HDPE with similar density generally increases melt strength and bubble stability while retaining stiffness. The bimodal molecular weight distribution provides a more pronounced extensional strain-hardening response, which permits higher stalk height without bubble vibration. This behavior is not directly captured by the melt index; converter trials with haul-off force measurement and bubble geometry are required. Compared with monomodal HDPE of the same density, TR144-GD typically exhibits higher dart impact and environmental stress-crack resistance because the high-molecular-weight fraction improves fibrillation resistance. However, the same molecular structure can lower machine-direction tear resistance at high blow-up ratios. Dart impact, Elmendorf tear per ISO 6383-2, tensile properties per ISO 527-3, and haze per ISO 14782 should be measured on the actual film line before conversion.
Pipe-grade HDPE products are not interchangeable with TR144-GD. Pipe grades are classified by long-term hydrostatic strength under ISO 9080 and are formulated for sustained internal pressure service. TR144-GD has not been classified for pipe pressure service and should not be used in pressure piping. Blow-molding grades have higher melt indices, usually above 0.5 g/10 min, and balanced parison hang characteristics. TR144-GD is unsuitable for large-part blow molding because its low flow generates high extruder backpressure and short parison hang times. Injection-grade HDPE with melt indices above 4 g/10 min fills thin-wall cavities at moderate pressures, whereas TR144-GD would require impractically high injection pressures and would freeze prematurely.
Compared with linear low-density polyethylene film grades used in high-toughness sacks, TR144-GD provides higher modulus and lower elongation at break. It therefore suits applications requiring stiffness and dimensional stability but not puncture-dominated service. For sharp-object trash liners or agricultural bags with high puncture exposure, LLDPE-rich blends are preferred. Some converters use TR144-GD as the stiffening component in blends with C4 or C8 LLDPE; blend ratios are site-specific and depend on sealing requirements and dart impact targets. Published data for this specific grade in post-consumer recycled HDPE blends is limited, so compatibility should be verified with melt filtration, gel count, and film tear testing.
Industrial liner and T-shirt bag operations running TR144-GD on 65 mm extruders with 200 mm dies and 1.8 mm die gaps have demonstrated stable production in the 20–30 μm thickness range. Film gauge control should be maintained within ±1 μm because dart impact and tear resistance of thin HDPE are strongly thickness-dependent. Applications requiring outdoor UV stability must include carbon black or hindered amine light stabilizer masterbatch; the base resin is not intended for long-term outdoor exposure without stabilization. For direct food-contact use, the final film must satisfy FDA 21 CFR 177.1520 or EU Regulation 10/2011 migration limits depending on the target market. Converters are responsible for proving conformity because processing aids, masterbatches, and recycled content change the regulatory status. Storage limitations include keeping pellets below 40 °C, avoiding direct sunlight, and using sealed original packaging. Once bags are opened, the resin should be used promptly, and conditioned storage is recommended in humid tropical locations to avoid surface moisture pickup.