Sinopec Maoming Hdpe Tr 144

Sinopec Maoming HDPE TR-144

    • Product Name: Sinopec Maoming HDPE TR-144
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 975885
    Density 0.944-0.948 g/cm³
    Melt Flow Rate 0.18 g/10 min
    Tensile Yield Strength ≥25 MPa
    Tensile Strength At Break ≥30 MPa
    Elongation At Break ≥500%
    Flexural Modulus ≥1000 MPa
    Vicat Softening Point ≥120°C
    Brittleness Temperature ≤-70°C
    Environmental Stress Crack Resistance ≥1000 h
    Hardness ≥60 Shore D
    Melting Point 130-135°C
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >10^16 Ω·cm

    As an accredited Sinopec Maoming HDPE TR-144 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically, Sinopec Maoming HDPE TR-144 comes in 25 kg woven bags or 500 kg jumbo bags, palletized for bulk transport.
    Container Loading (20′ FCL) Container loading (20′ FCL): Sinopec Maoming HDPE TR-144, 25 kg bags, approximately 18 MT net, palletized, shrink-wrapped, securely stowed.
    Shipping Sinopec Maoming HDPE TR-144 is generally shipped as non-hazardous thermoplastic pellets in 25 kg woven bags or bulk bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers. Store cool and dry, away from direct sunlight, moisture, and ignition sources. Handle carefully; keep sealed until use. Not classified as dangerous goods.
    Storage Sinopec Maoming HDPE TR-144 should be stored at ambient temperature in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, moisture, heat, flames, and strong oxidizers. Keep original bags sealed, palletized, off the floor, and protected from physical damage. Avoid sharp objects, excessive stacking, and contamination. Use first-in, first-out stock rotation and follow local regulations and supplier recommendations.
    Shelf Life Recommended shelf life: 36 months when stored in unopened original packaging, cool, dry, ventilated, away from direct sunlight and heat.
    Application of Sinopec Maoming HDPE TR-144

    At the thin-gauge end of high-molecular-weight HDPE blown film processing, Sinopec Maoming TR-144 is classed in the HMW-HDPE film range; published melt index falls below 0.25 g/10 min under ISO 1133-1, and density is near 0.946 g/cm³ under ISO 1183-1. The resin is run as a monolayer or in blends containing 5–8 wt% LLDPE to lift dart impact without losing the stiffness required for thin-gauge retail sacks. A common production configuration is a 65 mm 30:1 L/D single-screw extruder fitted with a double-flight barrier screw, a 250 mm spiral mandrel die, and internal bubble cooling. Barrel temperatures are typically set from 185 °C to 225 °C with the die and adapter held at 220–230 °C; the high molecular weight fraction requires the die zone to be the hottest point on the line because a cold die lip rapidly produces melt fracture in this melt index band. Film gauge between 7 µm and 12 µm is achieved at blow-up ratios of 4.0:1 to 5.5:1 and frost line heights of 6–8 die diameters. A taller frost line, above 9 die diameters, increases machine-direction orientation and reduces Elmendorf tear as measured by ASTM D1922-15; a shorter frost line below 5 die diameters produces low stalk tension and gauge variation at the collapsing frame. The limiting defect is often not tensile failure but bubble instability when ambient air temperature fluctuates more than 5 K during a shift, causing the frost line to move and the film thickness distribution to shift by more than ±10%. Die gaps below 0.8 mm raise die-lip shear stress into the melt fracture region, while gaps above 1.4 mm delay the drawdown required to reach 7 µm and lower output stability. Formulation for these bags may include 0.3–0.6 wt% slip masterbatch and 0.1–0.3 wt% antiblock masterbatch to prevent blocking after winding; post-industrial reclaim is often added at 10–20 wt% without measurable loss in dart drop when the reclaim is screened through 120 µm mesh and dried to remove surface condensation. When pellets are stored below 10 °C and moved into a high-humidity area above 60% RH, a hopper dryer at 80 °C for 2–4 h removes surface condensation before extrusion. The resulting retail T-shirt sacks, produce roll bags, and hospitality liners are non-food articles; when food contact is not intended, the main compliance obligation is mechanical performance and absence of substances regulated under REACH Annex XVII rather than FDA 21 CFR 177.1520.

    What Happens When Carbon Black Masterbatch Raises Viscosity in Heavy-Duty Sack Film?

    Carbon black masterbatch at 2.0–3.0 wt% is added to TR-144 for UV-stabilized refuse sacks and construction debris liners; the carbon aggregates reduce the melt flow rate by roughly 10–15% relative to unfilled resin and raise extruder pressure by 15–20 bar on a 75 mm line when compared at the same screw speed. The viscosity rise must be managed through a wider die gap of 1.2–1.6 mm and a reduced blow-up ratio of 2.5:1–3.5:1, because high blow-up ratios combined with carbon black raise the melt extension viscosity and destabilize the bubble at the frost line. Melt temperatures are held between 210 °C and 240 °C; the upper limit is set by gel formation from oxidation at the die lip, and the lower limit by motor load, which can approach 90% of the extruder drive rating on startup if the machine is not purged with a lower-viscosity LLDPE first. Film thickness for heavy-duty sacks is typically 25–50 µm; performance is evaluated by dart drop impact ASTM D1709-15 and Elmendorf tear ASTM D1922-15, with acceptance values set by end-use fill mass and puncture exposure. For 80–120 L refuse sacks, minimum dart drop values commonly fall in the range of 120–180 g at 25 µm, but the actual requirement is product-specific. Addition of a fluoropolymer processing aid at 200–400 ppm reduces die-lip buildup and delays melt fracture when the die gap is at the lower end; however, fluoropolymer additives are not permitted in packaging intended for some food-contact applications, so their presence must be disclosed when the same line is later used for food film. The terminal articles include municipal refuse sacks, hazardous waste liners, and construction rubble sacks, where the critical failure mode is not tensile yield but impact puncture at folded seams and contact with sharp debris; dart drop and tear, not melt index, are the controlling raw material parameters in this application.

    In three-layer coextrusion for dry food liners, TR-144 is placed in the two outer skins at 35–45 wt% each, while the core is a metallocene LLDPE or LDPE at 10–30 wt% to provide seal integrity and dart impact. The HDPE skins contribute moisture barrier and stiffness; the core contributes seal initiation below 110 °C and prevents the seal from shattering on high-speed vertical form-fill-seal lines. Layer distribution must be controlled within ±10% of target, because a thin HDPE skin on one side creates an asymmetric barrier and curl in the finished pouch. Melt temperatures are maintained at 200–230 °C, the die gap is set at 1.0–1.4 mm, and the blow-up ratio is held between 2.5:1 and 3.0:1 to keep the bubble stable during high-speed winding. Each skin may contain 0.3–0.6 wt% slip masterbatch and 0.1–0.3 wt% antiblock masterbatch; the slip agents migrate to the surface over 24–72 h after extrusion, and the film should be conditioned at 20–25 °C for 48 h before coefficient of friction testing to avoid false high values. For food contact, the finished structure must comply with FDA 21 CFR 177.1520 for olefin polymers and with EU Regulation (EU) No 10/2011; overall migration into food simulants must not exceed 10 mg/dm², and specific migration limits for slip and antiblock additives must be checked against the Union list. Because dry cereal and cracker packaging is usually cold-filled and dry, the moisture barrier of the HDPE skins is the main functional contribution; water vapour transmission rate is measured by ASTM F1249-20 at 38 °C and 90% RH, and a 20 µm skin typically contributes a WVTR in the range expected for HDPE, but published data for this specific food structure is limited and must be confirmed on the line. Terminal products include cereal box liners, cracker sleeves, dried soup pouches, and dry beverage stick packs.

    Application zoneTypical gaugeDie gapBlow-up ratioMelt temperature rangePrimary mechanical or compliance standard
    Thin-gauge T-shirt sacks and produce bags7–12 µm0.8–1.2 mm4.0:1–5.5:1190–230 °CASTM D1922-15
    Heavy-duty refuse sacks and debris liners25–50 µm1.2–1.6 mm2.5:1–3.5:1210–240 °CASTM D1709-15
    Dry food liner skins in A/B/A coextrusion12–25 µm per layer1.0–1.4 mm2.5:1–3.0:1200–230 °CEU Regulation (EU) No 10/2011
    Under-slab vapour retarder membrane150–250 µm1.5–2.2 mm2.0:1–2.5:1210–230 °CASTM E1745-11

    Under Concrete Slabs, the Seam Tape Usually Dictates Retarder Performance

    For under-slab vapour retarding applications, TR-144 is extruded as a wide monolayer film with a typical installed thickness of 150–250 µm; the film is not a pressure-retaining geomembrane but a vapour diffusion barrier required to limit upward moisture movement into the concrete slab. The governing specification is ASTM E1745-11, which sets classes A, B and C based on tensile strength, puncture resistance, and water vapour permeance; a Class A membrane must exhibit a water vapour permeance of ≤0.1 perm when tested per ASTM E96/E96M, but the relevant clause package should be read in the full specification because thickness alone does not guarantee class compliance. Extrusion uses a large die, often 1200–1600 mm diameter, with a die gap of 1.5–2.2 mm and a low blow-up ratio of 2.0:1–2.5:1; internal bubble cooling is required to reach gauge uniformity of ±5% across the web. Melt temperatures stay between 210 °C and 230 °C to avoid oxidation gels that become visible as specks in a 200 µm film inspected on a light table. The most frequent field failure is not a film tear but seam opening; side laps must be a minimum of 150 mm and are taped with a pressure-sensitive tape compatible with polyethylene, and punctures from concrete pump hoses must be protected with geotextile or temporary shields. Unfilled TR-144 film at 150 µm can pass permeance testing, but the puncture resistance required by ASTM E1745-11 Class A is more demanding; in high-traffic slab pours the accepted practice is to use 250 µm minimum or a reinforced laminate. Compliance is generally limited to ASTM E1745-11, ASTM E96/E96M, and project specifications; FDA 21 CFR 177.1520 is not applicable because the film is not an article intended for food contact. End-use articles are under-slab vapour retarders, crawl space liners, and temporary floor protection membranes during construction.

    Because high filler loadings increase modulus while suppressing elongation, synthetic paper and tag stock extrusion uses TR-144 as the carrier resin with 10–20 wt% calcium carbonate masterbatch and 2–4 wt% titanium dioxide masterbatch for opacity. The filler raises the melt viscosity and reduces bubble stability, so the die gap is widened to 1.2–1.5 mm and the blow-up ratio is reduced to 2.5:1–3.0:1 compared with unfilled bag film. Sheet-like film at 60–90 µm is drawn down over a collapsing frame with low tension to avoid uncontrolled micro-voiding at the filler-polymer interface; the micro-voids are intentional in some synthetic paper grades to produce a paper-like fold and print surface, but excessive voiding reduces tear strength below ASTM D1922-15 acceptance values. Melt temperature is kept at 200–220 °C; temperatures above 220 °C accelerate degradation of the stearate-coated calcium carbonate and can produce yellowing that is measurable on a spectrophotometer. The finished tag stock, label facestock, envelope windows, and wristband substrates are not food-contact articles; they must comply with REACH Annex XVII restrictions and, for printed articles sold in the EU, with the relevant parts of EU packaging and packaging waste legislation. Published data for TR-144 in this specific filled configuration is limited; the formulation ranges above are starting points and must be tuned to the masterbatch carrier and filler particle size.

    Extruding Multi-Wall Paper Bag Liners for Hygroscopic Powders

    In multi-wall paper bag production for hygroscopic powders such as cement, dry mortar, and polyolefin resins, TR-144 is extruded into tubular liners at 30–50 µm for insertion into the inner ply of a 25 kg or 50 lb paper sack. The film is run at blow-up ratios of 2.5:1–3.5:1 with a die gap of 1.0–1.4 mm; melt temperature is held at 200–230 °C to maintain a flat tube that will not block on the roll. Slip and antiblock masterbatches are required at 0.3–0.6 wt% and 0.1–0.3 wt% respectively, because the liner must open in automatic sack-inserting machinery and slide against kraft paper without tearing. The key functional property is water vapour transmission rate measured by ASTM F1249-20 at 38 °C and 90% RH; the target must be below the moisture sensitivity threshold of the packaged powder, which for cement is typically set by the bag manufacturer rather than by a general resin standard. Puncture resistance is evaluated by a slow puncture test or by ASTM D1709-15 dart drop, with the liner expected to survive the drop of a filled bag from 1.2 m onto concrete; actual requirements vary with the sack construction and filling line. The terminal article is a multi-wall paper bag liner, sometimes supplied as a separate gusseted tube or as a pre-laminated inner ply; FDA 21 CFR 177.1520 applies only when the liner is used for food powders, in which case migration testing according to EU Regulation (EU) No 10/2011 becomes mandatory and the slip additive package must be selected from approved substances. For non-food powders, the main regulatory reference is REACH and the packaging waste directive rather than food-contact regulations.

    Free Quote

    Competitive Sinopec Maoming HDPE TR-144 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HDPE TR-144 is a high-density polyethylene resin produced at the Sinopec Maoming Petrochemical complex and assigned to the high-viscosity blown film segment. The grade is supplied in pellet form and is specified principally for monolayer and coextruded blown film constructions where high melt tenacity, film modulus, and downgauging capacity are required. Published supplier data place the material at a melt flow index of 0.18 g/10 min under 2.16 kg at 190 °C per ISO 1133-1:2022 and a density of 0.946 g/cm³ at 23 °C per ISO 1183-1:2019. The specification positions TR-144 above the melt-flow range of many HDPE blow moulding and injection grades and below the melt-flow range of typical LLDPE film resins; in practice, the resin behaves as a high-molecular-weight HDPE with pronounced shear thinning during extrusion.

    Because of the high molecular weight, TR-144 delivers a different balance of properties than a lower-viscosity HDPE film grade. The melt pressure at a given screw speed is higher, the die swell is more pronounced, and the bubble is less prone to sagging at elevated blow-up ratios. These differences are observable on production lines: TR-144 permits stable bubble formation at blow-up ratios of 4.5:1 to 5.0:1, whereas higher-melt-flow HDPE grades often exhibit bubble flutter under the same conditions. The trade-off is a narrower process window on shallow-flight screws and lower output per unit torque. Such operational boundaries are a consequence of the molecular design of the grade rather than a defect.

    What Distinguishes TR-144 from Other HDPE Grades in the Same Portfolio?

    TR-144 should not be compared directly with HDPE grades intended for pipe, blow moulding, or injection moulding because the melt index and density targets differ. A typical blow moulding HDPE in the Sinopec Maoming slate is designed for higher flow and higher density to produce bottles and containers; such grades commonly have melt flow indices from 0.30 g/10 min to 0.60 g/10 min and densities near 0.953 g/cm³. TR-144, by contrast, is designed for film orientation and therefore retains a lower density and a lower melt flow index to increase extensional strength. Compared with an injection-moulding HDPE of 8–20 g/10 min, TR-144 is unsuitable because the long relaxation time restricts flow length and increases clamp force requirement. Compared with LLDPE film grades, TR-144 has higher stiffness, higher tensile yield stress, and lower elongation at break; it also has lower dart impact at sub-ambient temperatures and lower tear resistance in the machine direction. These differences follow from the higher crystallinity and lower chain branching of HDPE.

    The difference in comonomer distribution also affects seal response and surface friction. HDPE film from TR-144 typically has a higher heat-seal initiation temperature than LLDPE film, and the seal strength plateau is narrower. Film converters using TR-144 in T-shirt bag lines adjust sealing jaw temperature upward by 10–20 °C relative to LLDPE-heavy structures and verify seal strength under ASTM F88/F88M. The film is generally printable after corona or plasma treatment, with surface tension raised to at least 38–40 mN/m for flexographic or gravure ink adhesion.

    Extrusion Melt Temperature, Die Gap and Blow-Up Ratio Boundaries

    Optimal processing for TR-144 follows the established envelope for high-viscosity HDPE film. On a 90 mm single-screw extruder with an L/D ratio of 30 and a barrier screw, barrel set points from feed to discharge are typically 180 °C, 200 °C, 210 °C, and 210 °C, with a die head temperature of 210–220 °C. The die gap is usually kept at 1.2–2.0 mm for film thicknesses from 0.015 mm to 0.100 mm; deeper gaps improve bubble stability but increase orientation. A blow-up ratio of 3.5:1–5.0:1 is used for balanced film properties, and frost line height is adjusted in the 600–1200 mm range depending on die diameter, output, and ambient temperature. Specific energy consumption for this class is generally 0.25–0.35 kW·h/kg, but the exact value depends on screw design, screen pack, and back pressure.

    At melt temperatures above 230 °C, the risk of oxidative chain scission and gel formation increases, especially if residence time in the adapter exceeds 5 min. The resin should not be processed through extruders with L/D below 25 unless screw speed is reduced and melt temperature is closely monitored. When moisture is present from high-humidity storage above 60 % RH, surface pinholes can appear; drying at 70–80 °C for 1–2 h is effective for pellets but is rarely necessary for sealed packaging. Additive masterbatches containing carbon black, TiO₂, or calcium carbonate should be dried separately if their moisture uptake exceeds 0.05 wt%.

    The rheological fingerprint of TR-144 can be inferred from the low-load melt flow index and the melt flow ratio between 21.6 kg and 2.16 kg conditions. Literature data for HDPE film resins with similar melt indices show melt flow ratios in the range of 70–80, indicating pronounced shear thinning and good extrusion stability at high shear rates; however, published data for this exact grade is limited. In blown film extrusion, this shear thinning helps reduce apparent viscosity at the die lip while preserving high extensional viscosity in the bubble. That property difference is the main distinction between a high-molecular-weight film HDPE and a low-molecular-weight grade that has the same density but lower melt strength.

    Physical properties are obtained from specimens prepared by compression moulding or from blown film samples as indicated. Because HDPE properties are orientation-sensitive, the test direction and sample preparation history must be stated; a yield stress measured on a compression-moulded plaque is not interchangeable with a machine-direction film measurement. Film specimens should be conditioned at 23 °C ± 2 °C and 50 % ± 5 % RH for at least 40 h according to ISO 291:2008 before tensile and dart impact testing.

    Property Test method Nominal value
    Melt flow index, 190 °C / 2.16 kg ISO 1133-1:2022 0.18 g/10 min
    Density at 23 °C ISO 1183-1:2019 0.946 g/cm³
    Tensile yield stress, 50 µm film, machine direction ISO 527-3:2018 25 MPa
    Elongation at break, 50 µm film, machine direction ISO 527-3:2018 800 %
    Tensile modulus, 1 mm/min, 23 °C ISO 527-2:2012 900 MPa
    Dart impact strength F50, 25 µm film ASTM D1709-16a 120 g
    Vicat softening temperature, 10 N ISO 306:2022 125 °C

    The table summarizes representative physical property values from published supplier literature for TR-144. These values are nominal and are not lot release limits; the certificate of analysis for the specific lot governs the purchase specification. Converters should request the current technical data sheet and confirm whether the reported values are based on compression-moulded plaques or blown film specimens.

    TR-144 is used in high-stiffness refuse sacks, T-shirt carrier bags, industrial liners, garment bags, and coextruded film for packaging or agricultural intermediate bulk containers. In each application, the film thickness is selected based on the required dart impact, tear, and puncture performance. Refuse sacks are often run at 0.012–0.025 mm; industrial liners may extend to 0.080–0.120 mm. The grade can be downgauged more readily than LDPE because the higher modulus permits thinner walls at equivalent load-bearing deformation, but low-temperature puncture resistance must be confirmed by the converter. For food-contact uses, the finished film must be evaluated under FDA 21 CFR 177.1520 and, where relevant, GB 4806.6-2016 or EU 10/2011; resin suppliers typically provide compliance declarations only for the specific additive package used.

    For regulatory compliance, the resin supplier normally provides a statement that the base polymer complies with REACH Regulation (EC) No 1907/2006, as polymers are exempt from registration while monomers and additives must be registered. The grade is typically suitable for use under RoHS Directive 2011/65/EU when not compounded with restricted heavy metal pigments, but the converter must verify the final article. Food-contact status is not automatically conferred by resin type; finished film must satisfy migration limits under FDA 21 CFR 177.1520 and, if sold in China, GB 4806.6-2016. If the film is intended for medical packaging, additional validation under ISO 11607-1:2019 is required for sterile barrier systems; TR-144 is not marketed as a medical-grade resin.

    When Coextrusion Is Used to Overcome Tear Anisotropy and Downgauging Limits

    In monolayer structures, TR-144 shows the typical HDPE orientation-related tear anisotropy: transverse-direction tear is higher than machine-direction tear, and dart impact can fall below target when film thickness drops below 0.015 mm. Coextrusion with an LLDPE or metallocene LLDPE skin layer at 10–20 % of total thickness is commonly used to restore machine-direction tear and low-temperature dart impact. The LLDPE skin also reduces pinhole formation on high-speed bag conversion lines. Interfacial adhesion is generally sufficient when the melt streams combine in the die at 220 °C, but the viscosity difference between TR-144 and the LLDPE skin must be controlled. If the zero-shear viscosity ratio exceeds 1.5, the interface can become unstable and visible flow lines appear on the inner surface of the bubble.

    When TR-144 is used in carrier bag formulations at 60–80 % by weight with LLDPE skin layers, converters can sometimes downgauge from 0.020 mm to 0.015 mm without sacrificing F50 dart impact below 100 g under ASTM D1709-16a. Published data for this specific formulation is limited, and plant trials with the actual die geometry, screw configuration, and frost line height are required to establish the operating window. The minimum achievable thickness is not solely a resin property; it also depends on die lip uniformity, nip roll speed, and melt temperature consistency.

    On production-scale lines, the most commonly observed failure modes with TR-144 are not inherent material defects but arise from exceeding the extrusion window: excessive screw speed on shallow screw designs causes high melt pressure and polymer temperature nonuniformity; insufficient screen pack filtration allows gel accumulation at the die lip; and high cooling air velocities can freeze the bubble too rapidly and increase film blocking. These limitations define the practical boundary for high-speed operations. If the converter is replacing a higher-MFR HDPE, the first adjustment is not the screw speed but the barrel temperature profile and the die gap, because the high-viscosity melt requires lower shear heating to avoid localized degradation.

    Top