    Specifications
    HS Code 579654
    Density 0.950-0.955 g/cm³
    Melt Flow Rate 190 C 5 0 Kg 0.50 g/10min
    Tensile Yield Strength ≥25 MPa
    Elongation At Break ≥600%
    Flexural Modulus ≥1000 MPa
    Notched Izod Impact Strength ≥20 kJ/m²
    Vicat Softening Temperature ≥120 °C
    Brittleness Temperature ≤-70 °C
    Oxidation Induction Time ≥20 min
    Carbon Black Content 2.0-2.5%
    Environmental Stress Crack Resistance ≥1000 h
    Moisture Content ≤0.03%
    Ash Content ≤0.05%
    Bulk Density ≥0.55 g/cm³
    Color Black

    As an accredited Sinopec Maoming HDPE HXB4505M factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE HXB4505M is packed in 25 kg PP woven bags with PE inner liner; 1000 kg jumbo bags available.
    Container Loading (20′ FCL) Sinopec Maoming HDPE HXB4505M 20′ FCL loading: 25kg bags, approx. 20–22 MT per container, palletized or loose, dry secure stowage.
    Shipping Sinopec Maoming HDPE HXB4505M is a non-hazardous high-density polyethylene resin, not regulated for transport. It ships in 25 kg woven bags or 1,000 kg jumbo bags, palletized and shrink-wrapped in containers or trucks. Store cool, dry, ventilated; avoid moisture, heat, and direct sunlight.
    Storage Store Sinopec Maoming HDPE HXB4505M in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags/containers tightly sealed, palletized, and off the floor. Prevent moisture, dust, and contamination. Observe safe stacking limits to avoid bag rupture or collapse. Use appropriate PPE, maintain good housekeeping, and follow the SDS.
    Shelf Life Typically 24 months when stored in original unopened packaging, in a cool, dry, ventilated area away from sunlight and moisture.
    Application of Sinopec Maoming HDPE HXB4505M

    Extrusion blow moulding of Sinopec Maoming HDPE HXB4505M for single-serve milk, pasteurised juice and dairy drink bottles is specified around a melt-temperature envelope of 185–205 °C and a die swell band of 20–35% at the parison die. The processing ranges cited below are representative for high-density polyethylene blow moulding grades with density near 0.945 g/cm³ and melt-flow rate near 0.45 g/10 min at 190 °C/2.16 kg; lot-specific certificates must be checked against ISO 1183-1:2019 and ISO 1133-1:2022. Food-contact status is not a resin-only property. Converters must verify that the supplied antioxidant and catalyst package is covered by lot-specific food-contact documentation under China GB 4806.6-2016, China GB 4806.7-2016 and EU Regulation (EU) No 10/2011, including overall migration below 10 mg/dm² in aqueous and acidic simulants. For white 250 mL milk bottles, a TiO₂-based masterbatch is typically metered at 2.0–3.0 wt%, and calcium carbonate filler addition is avoided to maintain drop-impact performance and weld-line strength. The parison programmer is set to deliver a top-section wall of 1.5–2.2 mm, a shoulder-section wall of 0.8–1.2 mm, and a sidewall target of 0.5–0.7 mm; finished shot weight for a 250 mL bottle is 8.5–10.5 g. Production lines use single-screw extruders with 55–75 mm screw diameter and 22:1–25:1 L/D ratio, typically with a barrier screw and Maddock mixer to control temperature rise. Die-head temperatures are held at 190–205 °C, mould temperatures at 15–25 °C, and blow air at 0.6–0.9 MPa. Cycle time for twin-station shuttle machines is 10–14 s per 250 mL two-cavity tool. Terminal products include 250 mL, 500 mL and 1 L dairy bottles with 0.45–0.60 mm sidewall thickness, tamper-evident neck finishes and no post-mould reaming.

    Pharmaceutical Container ESCR and Torque Retention Limits

    Syrup, oral liquid and tablet containers made from HXB4505M are qualified at tighter neck tolerances and more conservative environmental stress-crack resistance limits than food packaging. The material must be validated against USP <661.1> and Ph. Eur. 3.1.3 for polyolefins, with batch-specific certificates covering total ash, heavy metals and reducing substances. Where elemental impurity control is relevant, the converter should evaluate contributions under ICH Q3D using the packaging component as an indirect source. Tooling uses cut-slot neck finishes with 0.10–0.15 mm post-cool calibration rings and closed-loop parison weight control of ±0.5 g; a 100 mL syrup bottle is produced at 6.5–8.0 g shot weight with sidewall thickness 0.55–0.65 mm. Drop-impact testing follows ASTM D2463-15 at 0 °C and 1.2 m drop height, with acceptance criteria of no leakage through the closure or sidewall. Environmental stress-crack resistance is evaluated by ASTM D1693 Condition B using 100% Igepal CO-630 at 50 °C. Converters should establish product-specific failure limits with the actual fill fluid because syrups with high sugar content and pH 3.0–4.0 can accelerate cracking beyond the Igepal reference. Published failure-time data for this exact grade in multi-component oral syrups is limited. Closure torque retention on neck finishes must be checked after accelerated storage at 40 °C and 75% RH for 90 days; typical failure modes are cap back-off from resin creep in the neck or stress whitening at the thread base.

    Application sectorGoverning standard / regulationKey test or parameterBoundary used by converters
    Food and dairyFDA 21 CFR 177.1520; EU (EU) No 10/2011; China GB 4806.7-2016Overall migration, aqueous and acidic simulants; sensory panel<10 mg/dm²; no detectable off-taste
    PharmaceuticalUSP <661.1>; Ph. Eur. 3.1.3; ICH Q3DHeavy metals, non-volatile residue, ESCR, drop impactPh. Eur. limits; product-specific ESCR pass
    Personal careEU Regulation (EC) No 1223/2009; ASTM D1693; ISO 8295Fragrance-containing storage, ESCR, coefficient of frictionProduct-specific pass at 45 °C for 12 weeks
    Household and agrochemicalUN 3H1; UN Model Regulations Chapter 6.1; ASTM G154Drop at 1.2 m and -18 °C; hydraulic pressure 100 kPaNo leakage; no permanent deformation
    Industrial fluidsISO 22241-3:2017; ASTM D2684Cation leaching, aldehyde formation, weight lossAUS 32 limits; barrier retention validated

    In surfactant-heavy liquid packaging, the bottle sidewall is subjected to continuous hoop stress from filling-line torque and storage stacking while the product contact layer sees micelle-forming anionic systems at 9–15 wt% active surfactant. Shampoo, body wash and lotion bottles made from HXB4505M are typically monolayer and designed with a minimum sidewall thickness of 0.55 mm because thinner walls show rapid crack propagation at the label recess and parting line. Colour masterbatch addition ranges from 0.5 wt% for translucent natural bottles to 2.5 wt% for opaque pearlescent grades. A slip/antiblock package is introduced only when filling-line de-nesting and automated label application demand a coefficient of friction below 0.30, measured by ISO 8295. Continuous extrusion blow moulding machines with 60 mm extruder diameter and 24:1 L/D ratio operate at 190–205 °C melt temperature. Blow pressure is 0.7–0.9 MPa, mould temperature is 12–18 °C, and cycle times are 10–14 s for 200 mL bottles. The critical control point is parison hang time; parison drawdown greater than 15% in length before mould closing leads to thinning in the shoulder and lower drop-impact failure. Product qualification uses ASTM D1693 Condition B as a baseline, but storage of filled bottles at 45 °C for 12 weeks with the actual fragrance system is required before release. Published data for untreated HDPE in surfactant systems often underestimates failure time when fragrance solvents are absent. Terminal containers include 100 mL, 200 mL and 400 mL personal-care bottles with 24/410 and 28/410 neck finishes, matched to pump or flip-top closures.

    When High-pH Cleaning Agents and Agricultural Surfactants Reduce Bottle ESCR

    Detergent, chlorinated cleaner and agrochemical containers produced from HXB4505M operate under a narrower ESCR margin because the fill fluid can plasticise the amorphous tie phase and promote crack initiation at the inner surface. For liquid detergent and crop-protection formulations, monolayer HDPE is limited to bottles where the product is water-based and the solvent fraction consists of polar glycols or alcohols at <10 wt%; non-polar hydrocarbons above this level require fluorination or co-extruded barrier structures. Dangerous goods packaging must comply with UN 3H1 for rigid plastics, with drop, leakproofness and hydraulic pressure tests according to Chapter 6.1 of the UN Model Regulations. For agricultural products, label durability is tested under ASTM G154 UV cycling and field exposure. Carbon black masterbatch is metered at 2.0–3.0 wt% using a concentrate with 20–60 nm primary particle size to cut UV transmittance to <0.5% over 300–800 nm. Post-industrial regrind from the same process is capped at 30 wt% because higher fractions reduce ASTM D1693 Condition B failure time and increase die-pressure fluctuation. Accumulator-head blow moulding machines with 80–120 mm extruder diameter and 20:1–25:1 L/D ratio produce 1 L and 5 L jerry cans. Melt temperature is controlled at 195–210 °C, blow pressure at 0.7–1.0 MPa, and mould temperature at 10–20 °C. For 1 L detergent bottles, shot weight is 30–36 g and sidewall thickness is 0.55–0.85 mm; for 5 L jerry cans, shot weight reaches 180–220 g with wall thickness 1.2–1.6 mm. Terminal products include trigger-spray bottles, 1 L standalone bottles, and 5 L agrochemical jerry cans with closure necks tested for sustained hydraulic pressure at 100 kPa for 30 min.

    Which Barrier Layer Configuration Prevents Solvent Weight Loss in Small Industrial Containers?

    Small industrial containers for high-purity urea solution, windscreen washer fluid and diluted coolants require a barrier layer only when the fill fluid contains volatile oxygenated solvents or the customer specification imposes a water-loss limit below 6% over 12 months. Monolayer HXB4505M is adequate for water-based washer fluid with <15 wt% ethanol at 23 °C; weight loss is measured by ASTM D2684 on complete containers, not on film specimens. AdBlue/DEF containers must comply with ISO 22241-3:2017, with particular attention to cation leaching, aldehyde formation and total contaminant migration into the urea solution. Six-layer co-extrusion blow moulding uses an outer HXB4505M layer at 30–35 wt% of total structure, a regrind layer at 35–45 wt%, two tie layers at 1.5–2.0 wt% each, and an EVOH barrier at 2.0–3.5 wt%. The HDPE extruder is 65 mm with 25:1 L/D ratio and barrel profile 175–205 °C; EVOH is processed at 190–205 °C using a 30 mm extruder with 20:1 L/D and a low-shear screw to avoid gel formation. Blow air pressure is 0.8–1.0 MPa, mould temperature is 10–18 °C, and cycle time for a 5 L container is 16–22 s. The mould must provide positive pinch-off line cooling because EVOH layers can form semi-crystalline fragments that weaken the pinch seam; post-mould deflashing uses a rotating knife with ±0.5 mm flash allowance. Terminal products include 5 L AdBlue cans, 10 L coolant jugs, and 20 L windscreen washer pails with a wall thickness of 1.1–1.5 mm and barrier-layer distribution verified by microtome sectioning and polarised light microscopy.

    Container typeMelt temperatureBlow pressureMould temperatureWall thicknessCycle time
    250 mL food bottle185–205 °C0.6–0.9 MPa15–25 °C0.45–0.60 mm10–14 s
    100 mL pharmaceutical bottle185–205 °C0.6–0.8 MPa15–22 °C0.55–0.65 mm9–13 s
    200 mL personal care bottle190–205 °C0.7–0.9 MPa12–18 °C0.55–0.75 mm10–14 s
    1 L detergent bottle195–210 °C0.7–1.0 MPa10–20 °C0.55–0.85 mm12–16 s
    5 L barrier container190–205 °C0.8–1.0 MPa10–18 °C1.1–1.5 mm16–22 s

    Non-sterile diagnostic reagent bottles made from HXB4505M are produced in low-cavity shuttle machines because the neck geometry often includes a dropper tip with a 0.5–0.8 mm orifice and sidewall thickness 0.45–0.55 mm. The conversion is conducted at the lower end of the melt-temperature window, 185–195 °C, to maintain parison tear strength and reduce gel formation from long residence times. Filling solutions are typically phosphate-buffered saline at pH 7.2–7.4, Tris buffer at pH 8.0, or lyophilisation carriers containing <5 wt% sucrose; the bottle must show no pH shift and no turbidity after 60 °C storage for 14 days. Compliance follows EU Regulation (EU) 2017/746 for in vitro diagnostic medical devices only where the bottle is integrated into the device; otherwise, the relevant chemical and migration requirements are set under food or pharmaceutical references. A colour masterbatch is generally omitted to allow visual inspection of fill level and particulate contamination. Terminal products include 5 mL to 50 mL dropper bottles, reagent reservoirs and desiccant-containing closure bodies used in point-of-care cartridges.

    Free Quote

    Competitive Sinopec Maoming HDPE HXB4505M prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HDPE HXB4505M is a bimodal high-density polyethylene extrusion resin designed for pressure-pipe compounds where long-term hydrostatic strength and slow crack growth resistance govern material selection. Producer-published data sheets list a base resin density of 0.945 g/cm³ measured by ISO 1183-1, a melt mass-flow rate of 0.45 g/10 min at 190°C/5 kg measured by ISO 1133-1:2022, and a tensile yield stress of approximately 22 MPa measured on compression-moulded specimens according to ISO 527-2. The grade is normally supplied as natural resin without carbon black; pipe converters add a predispersed carbon-black masterbatch to achieve 2.0–2.5 wt% carbon black in the finished pipe compound. Under ISO 12162, compounds based on HXB4505M are positioned for PE100 classification, corresponding to a minimum required strength of 10.0 MPa at 20°C for 50 years. The structural basis for this classification is a bimodal molecular weight distribution, in which the low-molecular-weight fraction limits melt viscosity during extrusion while the high-molecular-weight fraction increases the density of load-bearing tie molecules between crystalline lamellae.

    What Distinguishes Bimodal HDPE from Conventional Unimodal Pipe Resins?

    In a conventional unimodal HDPE, a single broad peak in the molecular weight distribution dominates, and any increase in weight-average molecular weight to improve slow crack growth resistance also increases low-shear viscosity and requires higher extruder torque. In HXB4505M, the polymerisation architecture produces two distinct molecular weight fractions. The shorter chains provide shear thinning and acceptable haul-off speeds; the longer chains supply the tie molecules that bridge adjacent crystallites and transmit stress through the amorphous regions. Gel permeation chromatography with infrared detection on comparable bimodal pipe grades typically reports a weight-average molecular weight between 200,000 g/mol and 400,000 g/mol and a polydispersity index above 10, although published data for this specific configuration is limited. Under capillary rheometry at 190°C, apparent shear viscosity decreases sharply as shear rate increases from 1 s⁻¹ to 100 s⁻¹, a response that can be measured by the ratio of melt flow rate at 5 kg to melt flow rate at 2.16 kg. A higher ratio indicates more pronounced shear thinning and lower die-head pressure on grooved-barrel single-screw lines. The direct consequence is that a bimodal resin can retain a high weight-average molecular weight without exceeding the melt-pressure limits of a 30:1 to 36:1 L/D pipe extruder.

    At the conversion stage, grooved-barrel single-screw extruders with length-to-diameter ratios between 30:1 and 36:1 are preferred for HXB4505M-based compounds. Barrel zone settings typically begin near 180°C in the feed zone and increase to 210–230°C in the metering and head zones. Melt temperature measured by an immersion probe at the die entry should remain below 235°C to limit oxidative degradation and melt-flow-rate drift. A screen pack of 40/80/40 mesh is commonly inserted before the breaker plate to trap agglomerates while maintaining melt pressure no greater than 25 MPa. If the resin has been stored at relative humidity above 60%, pre-drying at 80°C for 2 h in a desiccant dryer with a dew point below -30°C is required to prevent surface moisture volatilisation and bubble formation in thick-walled pipe. Extruder screws without a barrier section and without shear-mixing elements can leave unmelted high-molecular-weight particles in the melt, producing visible gel defects in the pipe wall. Melt pressure before screen pack, haul-off speed, and pipe wall thickness should be monitored together, because a loss of melt strength at low screw speed may produce sag in large-diameter pipe and a wall-thickness variation exceeding ±0.5 mm on diameters above 315 mm.

    Long-Term Hydrostatic Strength and PE100 Classification

    PE100 classification is not a single batch test but a time-dependent extrapolation procedure defined by ISO 9080 and ISO 12162. A PE100 material must show a lower confidence limit of the stress-at-rupture at 50 years and 20°C of at least 10.0 MPa. For HXB4505M-based compounds, hydrostatic pressure testing is performed on pipe specimens according to ISO 1167, while notched-pipe testing under ISO 13479 is used to evaluate slow crack growth resistance. The notched-pipe test is especially relevant for trenchless installation and for systems exposed to point loads or third-party damage. In a typical PE100 acceptance sequence notched pipe specimens are exposed to a hoop stress of 0.8 MPa at 80°C and must exceed 165 h before failure. The bimodal high-molecular-weight tail retards the transition from ductile shear yielding to brittle crack propagation by increasing the number of stress-transmitting tie molecules in the interlamellar amorphous regions. For pipe dimensioning under ISO 4427, the design stress is 8.0 MPa for water at 20°C when the MRS of 10.0 MPa is divided by the standard service coefficient of 1.25. Finished pipes intended for Chinese water-supply applications may additionally be evaluated under GB/T 13663-2018, which references ISO 1167 and ISO 9080 for long-term strength verification.

    When Carbon Black Masterbatch Alters Density and UV Resistance

    Natural HXB4505M is not intended for outdoor service without ultraviolet stabilisation. For above-ground or exposed pressure-pipe applications, a carbon-black masterbatch is metered gravimetrically into the extruder at a let-down ratio that yields 2.0–2.5 wt% carbon black in the finished pipe wall. The addition of carbon black increases the compound density from approximately 0.945 g/cm³ to 0.955–0.960 g/cm³, and this shift must be used when converting batch mass into pipe length. Dispersion quality is assessed on microtomed sections according to ISO 18553, with a maximum acceptable rating of 3. Ultraviolet resistance is additionally verified by oxidation induction time at 210°C using differential scanning calorimetry according to ISO 11357-6; PE100 compounds intended for outdoor service typically require an OIT above 20 min. Volumetric dosing of carbon-black masterbatch is acceptable only if the bulk density fluctuation is controlled within ±5%, because larger variation shifts carbon-black content outside the specified window. Aggressive shear gaps below 0.5 mm should be avoided when incorporating carbon black, since excessive local temperature can consume the phenolic antioxidant package before the pipe reaches service.

    Compared with PE80 pipe grades, HXB4505M compounds support a higher pressure rating for the same wall thickness, or permit thinner walls at equal pressure. The design stress under ISO 4427 is 8.0 MPa for PE100 and 6.3 MPa for PE80 at 20°C. In buried pipelines, the higher slow crack growth resistance of bimodal PE100 avoids brittle fracture initiated at scratches from backfill or at butt-fusion bead irregularities. The trade-off is rheological: the higher molecular weight of HXB4505M lowers the maximum output on a given single-screw line relative to a PE80 resin, although the exact percentage depends on screw geometry, melt temperature, and die-head restriction. A lower-cost PE80 or PE63 resin may be sufficient for non-pressure drainage or low-stress industrial piping, but the selection of HXB4505M is justified where sustained hoop stress, fluctuating internal pressure, or high ambient temperature require retention of design stress beyond the capability of conventional unimodal resins.

    Batch-to-batch release tests for HXB4505M-based pipe compounds should include melt mass-flow rate per ISO 1133-1:2022, density per ISO 1183-1, carbon-black content and dispersion per ISO 6964 and ISO 18553, oxidation induction time per ISO 11357-6, and hydrostatic strength on extruded pipe per ISO 1167. Rheological verification on a parallel-plate oscillatory rheometer at 190°C between 0.01 rad/s and 100 rad/s is used to confirm that the high-molecular-weight fraction has not been degraded by excessive shear during compounding. A reduction in storage modulus at 0.01 rad/s of more than 15% relative to the reference lot indicates degradation of the high-molecular-weight tail and should trigger a review of screw geometry and melt temperature. Do not combine HXB4505M with recycled pipe regrind containing unknown restabiliser packages, because oxidative induction time may fall below 20 min under ISO 11357-6. Natural resin stored in transparent sacks should be protected from direct sunlight for periods exceeding 6 months, since pre-consumption antioxidant consumption can reduce long-term hydrostatic strength.

    Lot acceptance checklist for HXB4505M-based PE100 pipe compound
    PropertyTest methodAcceptance range
    Melt mass-flow rateISO 1133-1:20220.40–0.50 g/10 min at 190°C/5 kg
    Density, natural resinISO 1183-10.945–0.950 g/cm³
    Carbon black content, compoundedISO 69642.0–2.5 wt%
    Carbon black dispersionISO 18553rating ≤3
    Oxidation induction time, 210°CISO 11357-6>20 min
    Hydrostatic strength, 20°C/100 hISO 1167no failure at 12.4 MPa