| HS Code | 491536 |
| Density | 0.944 g/cm³ |
| Melt Flow Rate | 0.14 g/10 min (190°C/2.16 kg) |
| Tensile Yield Strength | 25 MPa |
| Elongation At Break | ≥600% |
| Flexural Modulus | 1000 MPa |
| Notched Izod Impact Strength | ≥30 kJ/m² |
| Vicat Softening Temperature | 125°C |
| Brittleness Temperature | ≤-70°C |
| Environmental Stress Cracking Resistance | ≥1000 h |
| Oxidation Induction Time | ≥20 min |
| Moisture Content | ≤0.1% |
| Ash Content | ≤0.1% |
| Bulk Density | ≥0.55 g/cm³ |
| Hardness Shore D | 62 |
| Color | Natural |
As an accredited Sinopec Maoming HDPE HHMTR 144 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Maoming HDPE HHMTR 144 is supplied in 25 kg PP woven bags, typically palletized for storage and transport. |
| Container Loading (20′ FCL) | Sinopec Maoming HDPE HHMTR 144 loads in 20′ FCL: 25 kg bags, about 25 MT unpalletized or 17.5 MT palletized. |
| Shipping | Sinopec Maoming HDPE HHMTR 144 is a non-hazardous, non-regulated polyethylene resin. It is typically shipped in 25 kg woven bags, 1000 kg jumbo bags, or bulk containers. Transport by truck, rail, or sea in dry, clean conditions. Store cool, dry, ventilated, away from moisture, sunlight, and ignition sources. |
| Storage | Store Sinopec Maoming HDPE HHMTR 144 in original sealed bags or packaging in a cool, dry, well-ventilated warehouse. Keep away from direct sunlight, heat, ignition sources, and strong oxidizers. Protect from moisture, dust, oils, and contaminants. Avoid excessive stacking and rough handling. Follow the manufacturer’s safety data sheet and local regulations. |
| Shelf Life | Shelf life is typically 12 months when stored in dry, cool, well-ventilated conditions, protected from direct sunlight, moisture, and contamination. |
Sinopec Maoming HDPE HHMTR 144 is a high molecular weight film-grade homopolymer with typical density near 0.946 g/cm³ and melt flow rate near 0.18 g/10 min at 190 °C/2.16 kg when tested under ISO 1183-1:2019 and ISO 1133-1:2022 respectively. Published additive interaction data for this exact Maoming grade is limited; therefore, the process ranges in the following application entries are derived from established HMW-HDPE blown film practice and should be confirmed on the converter’s own line with grade-specific trials. Resin granules stored in unheated silos at relative humidity above 60% may develop surface condensation; pre-drying at 70–80 °C for 1–2 h is then required to prevent surface streaks and melt-pressure fluctuation.
Below 25 μm, drawn-down T-shirt carrier bag film is run on 55–65 mm grooved-feed single-screw extruders with 30:1 L/D, barrier screws, and screen packs of 60/80/100 mesh; die gap is 1.4–1.8 mm, blow-up ratio 3.0:1 to 4.5:1, and frost line height 4–8 die diameters to limit gauge bands and ply blocking. On lines without internal bubble cooling, winding tension is tapered from 50% to 20% of maximum to avoid telescoping on jumbo rolls. Regulatory compliance for retail bags includes FDA 21 CFR 177.1520 when used as direct food-contact produce bags, EU No 10/2011 for EU food-contact sales, REACH Annex XVII restricted heavy metals, and EU 94/62/EC Article 11 heavy metals sum below 100 mg/kg. Formulation ratios in this segment are 100 wt% HHMTR144 or 90–100 wt% HHMTR144 with 0–10 wt% LLDPE; white masterbatch 2–6 wt%; fluoropolymer processing aid 0.5–1.0 wt% is introduced only when melt fracture appears at the die lip. Downstream converting uses star-seal bag machines with photoelectric registration, wicket punching, and in-line perforation; corona treatment at 38–42 dyn/cm is used when flexo surface printing or lamination follows. Terminal products are die-cut T-shirt bags, patch handle bags, fruit and vegetable roll bags, and lightweight retail sacks.
On 65–75 mm grooved-feed extruders producing 15–35 μm industrial liner at line speeds above 15 m/min, melt-pressure oscillation exceeding ±5 bar at the breaker plate can generate visible gauge bands and reduce dart impact under ASTM D1709-16a. For industrial refuse and compactor sacks, the relevant standards are EN 13592:2017 for refuse sacks, ISO 7765-1:1988 for film impact, ASTM D882-18 for tensile properties, and ASTM D1922-15 for Elmendorf tear. The formulation uses 2–4 wt% carbon black masterbatch, 0.5–1.5 wt% slip/antiblock masterbatch, and up to 20 wt% post-industrial recycled HDPE only in non-food, non-medical refuse sacks; recycled content above this level is limited by variance in dart impact and ash residue. Processing is conducted on a high-stalk bubble with blow-up ratio 2.5:1 to 3.5:1, die gap 1.6–2.0 mm, melt temperature 190–220 °C, dual-lip air ring, and frost line 8–12 die diameters; internal bubble cooling is added when gauge nonuniformity exceeds ±5%. Terminal products are bin liners, compactor sacks, drum liners, and heavy-duty refuse bags for municipal waste collection.
In three-layer coextruded packaging films where HHMTR144 is used as the core to supply flexural modulus and moisture barrier, the layer distribution is typically 20–30 wt% LLDPE or mLLDPE skin on each side and 40–60 wt% HDPE core, with a 1.8–2.4 mm die gap and blow-up ratio 2.0:1 to 3.0:1. If the structure is intended for food contact, compliance is evaluated under FDA 21 CFR 177.1520(b) olefin polymer provisions, EU No 10/2011 overall migration testing according to EN 1186-1:2002, and GB 9685-2016 for additives; non-food structures must still meet EU 94/62/EC Article 11 heavy metal limits and REACH Annex XVII restrictions. The HDPE core extruder is run at 170–210 °C barrel temperatures and the adapter is held below 220 °C to avoid gel generation; if polyamide or EVOH skins are selected, a maleic anhydride grafted tie resin layer of 8–12 μm is required because HDPE will not adhere directly to polar barrier polymers. Terminal products are stand-up pouch stiffness plies, frozen food overwrap, dry pet food liners, and lamination webs for powdered beverage sachets.
At 40–80 μm thickness on monolayer blown film lines with a 1.8–2.2 mm die gap and a low blow-up ratio below 2.5:1, HHMTR144 must be processed with a stable bubble cage and air ring velocity sufficient to prevent MD/TD orientation imbalance. Applicable standards are ISO 527-3:2018 for tensile modulus and elongation, ISO 7765-1:1988 for impact resistance, ASTM D1709-16a for dart drop, and EN 13592:2017 when the converted sack is used for waste collection. Formulation ratios are 85–100 wt% HHMTR144 with 0–15 wt% LLDPE, 2–4 wt% UV stabilizer masterbatch for outdoor storage, and 0.2–0.5 wt% fluoropolymer processing aid when melt fracture is observed on the die lip; calcium carbonate masterbatch should not exceed 6 wt% unless dart impact is re-validated with ASTM D1709-16a. Downstream converting uses gusseted tubing, jumbo roll winding, and bottom-seal sack machines with thermal sealing at 150–180 °C. Terminal products are FIBC inner liners, rubble sacks, construction debris bags, and chemical powder sacks for non-hazardous fill.
For dry food inner liners produced from HHMTR144, the resin lot must be supported by a food-contact declaration and verified against FDA 21 CFR 177.1520, EU No 10/2011 overall migration limit 10 mg/dm² under EN 1186-1:2002, and GB 9685-2016 for additives. The formulation is restricted to 100 wt% virgin HHMTR144 because post-consumer recycled HDPE is not permitted in direct food contact; slip agent is added at 0.2–0.5 wt%, synthetic silica antiblock at 0.1–0.3 wt%, and amine-based antifog additives are avoided due to die-lip plate-out risk. Processing uses a 1.4–1.8 mm die gap, melt temperature 190–215 °C, blow-up ratio 2.5:1 to 3.5:1, and corona treatment at 38–40 dyn/cm for solventless lamination to BOPP or paper. Terminal products are cereal inner liners, cracker slug wrappers, dry pet food pouches, and powdered beverage sachets.
Competitive Sinopec Maoming HDPE HHMTR 144 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Maoming HDPE HHMTR 144 is a high-density polyethylene film resin produced at the Maoming manufacturing site of Sinopec. The grade is used in thin-gauge blown-film applications, including general-purpose packaging, T-shirt carrier bags, produce bags, and industrial liners. As a high-molecular-weight HDPE, HHMTR 144 provides melt extensibility and bubble stiffness that support higher blow-up ratios and lower film-gauge variation on conventional monolayer lines. Available producer literature classifies the grade as a broad-molecular-weight film resin with density in the 0.944–0.947 g/cm³ envelope and a low melt mass-flow rate. Processing is normally performed on single-screw extruders with L/D ratios of 25:1–30:1 and barrier or double-barrier screw geometries. The low melt flow rate raises melt strength but also increases backpressure, shear heating, and screw torque demand at high output rates.
Producer datasheets for Sinopec Maoming HDPE HHMTR 144 report nominal values determined under ISO and ASTM conditions. The values in Table 1 are not batch specifications; the certificate of analysis supplied with each shipment governs the lot. Variations arise from catalyst residues, comonomer distribution, and pelletization conditions. When incoming resin is stored under high humidity, surface moisture can generate bubble defects and pin holes. Pre-drying at 70–80 °C for 1–2 h is applied when storage relative humidity exceeds 60% or when pellet surfaces show visible condensation. The melt flow rate under 190 °C and 2.16 kg load reflects only a single point on the shear-viscosity curve; melt flow ratio, where available, provides a more useful indication of shear thinning under extrusion pressures.
| Property | Nominal range | Test method |
|---|---|---|
| Density | 0.944–0.947 g/cm³ | ISO 1183-1 |
| Melt mass-flow rate | 0.17–0.21 g/10 min | ISO 1133-1 at 190 °C, 2.16 kg |
| Tensile stress at yield | 22–24 MPa | ISO 527-2 |
| Tensile strain at break | >600% | ISO 527-2 |
| Flexural modulus | 800–900 MPa | ISO 178 |
| Vicat softening temperature A50 | 123–127 °C | ISO 306 |
| Environmental stress crack resistance F50 | >200 h | ASTM D1693-B |
The resin’s density range places it within the high-density polyethylene classification under ISO 1183-1. Film stiffness correlates with density and orientation, while the low melt mass-flow rate indicates a high average molecular weight. The environmental stress crack resistance value is significant for liners exposed to wetting agents, surfactants, or alkaline cleaning solutions. Converters comparing HHMTR 144 with lower-density film resins should normalize tensile and impact data by gauge and test direction because film orientation in the machine and transverse directions can differ substantially at high blow-up ratios.
Replacement of a medium-molecular-weight HDPE with HHMTR 144 shifts the melt temperature/backpressure relationship and the stable blow-up ratio window. On a 55 mm single-screw extruder with L/D 28:1 and a Maddock mixing section, the higher viscosity of HHMTR 144 can increase pre-die melt pressure by 10–20% at equivalent screw speed compared with a 0.7 g/10 min film resin. Bubble stability improves when melt temperature at the die is maintained between 190 °C and 220 °C. Below 180 °C, melt fracture or surface roughness may appear on the film. The blow-up ratio is typically 3:1–5:1, and high-stalk operation is often used to balance machine-direction and transverse-direction properties. Frost line height should be adjusted to 3–6 die diameters for thinner films. The molecular weight distribution permits a broader bubble-expansion window than lower-viscosity HDPE film grades, but screw torque limits and head pressure can restrict output on undersized drives or extruders with shallow metering sections.
Extruder barrel profiles from feed throat to die commonly progress from 170 °C to 210 °C, with die zones set at 190–215 °C. Screen pack filtration of 60/80/100 mesh protects the die land from degraded particles and crosslinked gels. The die gap is normally 1.2–1.8 mm for films above 25 µm. Narrower gaps of 0.8–1.2 mm are selected for high-stalk thin-gauge operation because the higher shear modifies melt elasticity and reduces die swell. Sizing cage and collapsing-frame geometry should be set to avoid creasing, especially under high frost line operation where the film enters the nip with less cooling. Internal bubble cooling, when fitted, permits higher output and lower frost line by increasing heat removal from the inner bubble surface. Without internal bubble cooling, output is limited by the heat-transfer capacity of the external air ring and the residence time of the bubble before collapsing.
At gauge targets between 10 µm and 15 µm, the melt is more sensitive to die lip imperfections, uneven air-ring velocity, and winding tension. Die lip gaps are reduced toward 0.8–1.0 mm to increase shear and reduce orientation differences across the bubble wall. Melt temperature is held in the upper band of 205–220 °C to lower viscosity and improve draw. Under these conditions, bubble stabilisation becomes the controlling constraint rather than extruder output. HHMTR 144’s high-molecular-weight fraction supports a stable neck at thin gauge, but turret winder tension must be limited to avoid machine-direction elongation and uneven film thickness. Dart impact measured under ASTM D1709-A on 12.5 µm film is generally lower than values measured at 25 µm; comparisons across gauges without normalization are technically invalid. Published data for this specific thin-gauge configuration is limited, and converter trials should record die pressure, melt temperature, frost line position, and gauge profile rather than relying on resin MFR alone.
Relative to medium-molecular-weight HDPE film grades with melt flow rates in the 0.7–1.0 g/10 min range, HHMTR 144 produces lower extruder throughput per screw revolution but higher melt strength. This trade-off suits applications requiring high bubble stability and downgauging, such as T-shirt bags and bin liners. Compared with linear low-density polyethylene, HHMTR 144 offers higher stiffness and lower low-speed dart impact. Compared with unimodal HDPE grades of similar density, the broader molecular weight distribution reduces orientation-induced splitting and improves gauge uniformity in high-stalk film. However, the grade is not designed for oriented tape or raffia lines where higher melt flow and lower molecular orientation are required. Published data for direct comparison with other specific Sinopec Maoming grades in the same family is limited; converter trials should compare screw motor load, die pressure, bubble width variation, and final film tensile properties rather than relying on single-point MFR differences.
Moisture pickup in HDPE pellet silos is generally low because the polymer is hydrophobic, but condensation on cold pellets transferred into humid processing halls can introduce surface water. Drying at 70–80 °C for 1–2 h in a desiccant hopper dryer is applied when relative humidity exceeds 60% or when pellets show surface condensation. Regrind addition from edge trim and start-up scrap is commonly maintained below 20% to avoid increasing gel and black-spec frequency. Die lip oxidation products accumulate during prolonged stops; purging with a medium-molecular-weight HDPE or a commercial purging compound prevents carbonised deposits. The use of fluoropolymer processing aids is usually unnecessary for HHMTR 144 but may be considered at high output velocities or with worn screw and barrel surfaces. Any processing aid must be evaluated for migration tendency if the film is intended for food-contact use.
For food-contact applications, converters must verify the supplier’s current food-contact statement. Typical high-density polyethylene food-contact compliance is assessed under FDA 21 CFR 177.1520 for olefin polymers and under EU Regulation 10/2011 for plastic materials and articles intended to come into contact with food. REACH Article 33 declarations and the absence of Substances of Very High Concern above the 0.1% w/w communication threshold must be obtained from the producer. Table 2 summarises the usual compliance framework for such a grade, but the actual status depends on additives, catalysts, and converting steps.
| Regulation or standard | Relevant condition | Verification requirement |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for food contact | Producer food-contact letter |
| EU Regulation 10/2011 | Overall migration and specific migration limits | Migration testing under intended conditions |
| REACH | SVHC communication at 0.1% w/w | SDS Article 33 declaration |
| China GB 9685-2016 | Food-contact additives | Producer compliance declaration |
Film thickness variation on HHMTR 144 often originates from air-ring imbalance or non-uniform die gap rather than resin lot variation. A 55 mm line with internal bubble cooling producing 25 µm film at 120 kg/h may show gauge bands of ±8% if the die gap is not centred; lot-to-lot density variation of ±0.001 g/cm³ is generally too small to produce such bands. Melt fracture at low melt temperatures appears as sharkskin on the outer surface; it is corrected by raising melt temperature, opening the die gap, or reducing output. Blocking in thin film occurs when hot film is wound at high tension or when the slip additive package is depleted with high regrind. The film-to-film coefficient of friction can be measured under ISO 8295. These operational boundaries should be interpreted with the producer’s certificate of analysis and the specific line’s thermocouple calibration.