Sinopec Maoming Hdpe Hhm5502st

Sinopec Maoming HDPE HHM5502ST

    • Product Name: Sinopec Maoming HDPE HHM5502ST
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 162231
    Density 0.954 g/cm³
    Melt Flow Rate 0.20 g/10 min (190°C/2.16 kg)
    Melting Point 130-135 °C
    Vicat Softening Temperature 125 °C
    Tensile Yield Strength ≥25 MPa
    Elongation At Break ≥600%
    Flexural Modulus ≥1000 MPa
    Notched Izod Impact Strength ≥30 kJ/m²
    Hardness 60-65 Shore D
    Environmental Stress Crack Resistance >1000 h
    Brittleness Temperature ≤-70 °C
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >10^16 Ω·cm
    Thermal Conductivity 0.45 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2×10^-4 /°C

    As an accredited Sinopec Maoming HDPE HHM5502ST factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE HHM5502ST is packed in 25 kg woven bags, also supplied in 1000 kg jumbo bags.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Sinopec Maoming HDPE HHM5502ST supplied in 25 kg bags; approximately 25 MT per 20′ FCL, unpalletized.
    Shipping Sinopec Maoming HDPE HHM5502ST ships as non-hazardous high-density polyethylene resin. Standard packaging: 25 kg PP/PE bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Typically loaded into 20' or 40' containers. Store in a cool, dry, ventilated area, away from direct sunlight, heat, and moisture.
    Storage Store Sinopec Maoming HDPE HHM5502ST in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep sealed bags or containers closed, palletized, and protected from moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking pressure. Use clean handling equipment; maintain good housekeeping. No smoking or ignition sources. Store at ambient temperature.
    Shelf Life Typically 12 months from production when stored unopened in a cool, dry, ventilated place, away from direct sunlight and heat.
    Application of Sinopec Maoming HDPE HHM5502ST

    Extrusion blow moulding of Sinopec Maoming HDPE HHM5502ST into UN-rated tight-head and open-head containers for agrochemical adjuvants, water-treatment chemicals and liquid detergent intermediates places the resin as the dominant continuous phase rather than a minor additive. A representative production formulation is 100 parts by mass virgin HHM5502ST combined with 10–25 parts clean in-house regrind generated exclusively from the same grade, plus 1.0–3.0 wt% of a high-density PE-compatible liquid colour or masterbatch based on total batch weight. The regrind ceiling is set at 25 wt% because higher recycle fractions have been observed on single-station shuttle machines to increase parison surface defects and reduce die-swell consistency when the regrind melt flow rate exceeds 0.5 g/10 min under ASTM D1238 at 190°C/2.16 kg. The industry compliance framework for these containers includes UN Model Regulations Chapter 6.1 for 1H1 non-removable-head and 1H2 removable-head plastics drums and jerricans, ADR/RID 6.1, and drop-stack testing under ISO 2248 or ASTM D5276; lot release requires a signed certificate of analysis addressing density by ASTM D1505, melt flow rate by ASTM D1238, tensile yield by ASTM D638, notched Izod impact by ASTM D256, and environmental stress crack resistance by ASTM D1693 condition B. Processing on a single-station or dual-station shuttle blow moulding line with a grooved-barrel extruder of L/D ≥ 24:1 uses a barrel temperature profile of 180°C at the feed throat to 205°C at the metering section, head and die zones at 190–205°C, and a mould temperature of 10–40°C. A parison programmer with a die gap range of 0.5–3.5 mm is required to compensate for sag on containers above 20 L; blow pressure is maintained at 0.6–0.8 MPa and blow-up ratio is held between 2.5:1 and 4:1 to avoid excessive thinning of the chime area. Finished products include 10–30 L open-head pails, 20–25 L jerrycans, 30–60 L tight-head drums, and dosing containers for agricultural and water-treatment fluid concentrate. The operational boundary is that HHM5502ST is not suitable for continuous exposure to strong oxidising acids, aromatic solvents, or chlorinated hydrocarbons at ambient and elevated temperatures; pre-drying at 80°C for 1–2 h is advisable only when storage relative humidity exceeds 80% and visible surface condensation is present.

    Does HHM5502ST Remain Within EU 10/2011 and FDA 21 CFR 177.1520 Migration Limits for Food-Contact Blow Moulding?

    HDPE HHM5502ST is processed as the base resin in monolayer extrusion blow moulding of short-shelf-life food-contact holloware where the food simulant migration limits of EU Regulation (EU) No 10/2011 and the olefin polymer provisions of FDA 21 CFR 177.1520 apply, alongside China GB 4806.7-2016. The formulation is typically 97.5–99.0 wt% virgin HHM5502ST with 1.0–2.5 wt% titanium dioxide white masterbatch; if colour is not required, the resin may be run without any additive package provided the line has been purged and the food-contact status is documented in the lot changeover record. Anti-block and slip additives are generally avoided at above 0.2 wt% because such additives can alter the organoleptic panel outcome and raise total migration values under EU 10/2011 long-term storage testing at 40°C for 10 days. The downstream process uses reciprocating-screw continuous extrusion blow moulding with a 24:1 L/D screw and Maddock mixing section, feed throat at 170°C, barrel zones at 175–200°C, die head at 185–200°C, and mould temperature at 8–25°C. Blow air is supplied at 0.5–0.7 MPa, blow-up ratio is held at 2:1–3:1 for handleware bottles, and wall thickness is maintained between 0.6 mm and 1.5 mm for 500 mL to 5 L containers. Pinch-off trim is in-line granulated and reintroduced at 10–15 wt% only if the trim has not been exposed to oil, cardboard dust, or secondary operations. Finished product types include 1–5 L edible oil bottles, sauce bottles, vinegar bottles, and 500 mL–2 L condiment handleware. The grade is not suitable for hot-fill above 60°C or retort processes because HDPE undergoes excessive deformation and oxygen permeation rises; aseptic cold-chain fills are the upper thermal limit.

    Automotive Washer Reservoirs, Coolant Overflow Tanks and Low-Temperature Impact Validation

    In automotive engine-compartment blow moulding, HHM5502ST functions as a monolayer material for windshield washer reservoirs, coolant overflow bottles and headlamp washer tanks, where the part-level compliance chain is governed by OEM specifications derived from ISO 16750-4 for low-temperature service, VDA 270 odour rating, and DIN 75201 fogging; material-level mechanical validation follows ASTM D638 for tensile yield and ASTM D256 for notched Izod impact at -30°C. The formulation is 96.5–98.0 wt% HHM5502ST, 2.0–3.5 wt% carbon black masterbatch with a PE carrier, and 0.1–0.3 wt% hindered amine light stabilizer masterbatch; a 0.05–0.1 wt% processing antioxidant is added when regrind exceeds 20 wt% and the part wall thickness exceeds 2.5 mm. The process uses accumulator-head machines because the welded pinched areas and varying wall thickness of reservoirs require programmable parison control with a die gap of 0.5–4.0 mm; melt temperature is kept at 190–210°C, mould temperature at 10–30°C, and blow pressure at 0.6–0.8 MPa. Wall thickness at the lowest pinch-off and insert areas is held above 2.0 mm to pass -30°C drop impact after thermal ageing under ISO 16750-4. Finished products are 2–6 L windshield washer reservoirs, 1–3 L coolant overflow tanks, and rear-window wash containers. The material is not appropriate for fuel-contact components or underhood parts exposed to continuous temperatures above 90°C, because HDPE exhibits creep and softening above its Vicat softening temperature.

    Application scenarioCompliance anchorsMaterial and part test standardsBinding process limit
    UN-rated industrial chemical containersUN Model Regulations Chapter 6.1, ADR/RID 6.1, ISO 2248ASTM D1505, ASTM D1238, ASTM D638, ASTM D256, ASTM D1693In-house regrind ≤ 25 wt%; parison die gap 0.5–3.5 mm
    Food-contact blow mouldingEU 10/2011, FDA 21 CFR 177.1520, GB 4806.7-2016ASTM D1238, ASTM D638, ASTM D256Melt temperature ≤ 200°C; clean trim reintroduction ≤ 15 wt%
    Automotive reservoirs and overflow tanksISO 16750-4, VDA 270, DIN 75201ASTM D638, ASTM D256 at -30°CMinimum wall thickness 2.0 mm; continuous service ≤ 90°C
    Pharmaceutical solid-dose bottlesUSP <661.1>, Ph. Eur. 3.1.3, ICH Q3DASTM D1238, ASTM D638, differential pressure leak test 10–20 kPaNo external lubricant; no post-mould trimming that introduces particulate contamination
    Marine floats and buoysASTM D1693, ISO 4892-2ASTM D638, ASTM D256, accelerated weathering 2,000 hUV masterbatch ≤ 6 wt%; no post-consumer recyclate of unknown additive history

    Pharmaceutical solid-dose and dry powder containers blow-moulded from HHM5502ST are validated under USP <661.1> plastic packaging systems and European Pharmacopoeia monograph 3.1.3 for polyolefins, with elemental impurity limits aligned to ICH Q3D. The dominant formulation is 99.0–100 wt% HHM5502ST with 0–1.0 wt% white PE-compatible masterbatch; no external lubricant is added because trace slip agents can interfere with drug product stability assays and change the contact angle of the internal wall. The extrusion blow moulding process is run in an ISO Class 8 cleanroom or equivalent controlled environment using dedicated resin silos and filtered blow air at 0.45–0.60 MPa, with melt temperature between 175°C and 195°C to reduce thermal degradation odour and low-molecular-weight extractables. Multi-cavity moulds with polished 0.8–1.2 mm wall thickness are used for 50–500 mL round packer bodies; post-mould handling includes air-ionization, in-line leak detection at 10–20 kPa differential pressure, and immediate bagging. Finished product types include 50–500 mL dry oral solid-dose bottles, 250–1000 mL effervescent tablet tubes, and desiccant canisters for diagnostic strip packaging. The grade is not suitable for parenteral, ophthalmic, or liquid formulations requiring low oxygen transmission below 100 cm³/(m²·d·bar), because monolayer HDPE does not provide an oxygen barrier.

    ESCR and UV Ageing Boundaries in Accumulator-Head Marine Float Moulding

    For marine buoy and float moulding, HHM5502ST is selected where the part must survive long-term water immersion, wave-induced flexure, and ultraviolet exposure without stress cracking. The formulation is 94.0–97.0 wt% HHM5502ST, 3.0–6.0 wt% UV-stabilized black or zinc-oxide masterbatch, and 0.1–0.3 wt% antioxidant masterbatch; the additive package is pre-dispersed at a letdown ratio not exceeding 6 wt% to avoid localized agglomerates that act as crack-initiation sites. Accumulator-head blow moulding with a grooved-barrel extruder of L/D 25:1–30:1 and head die gap 2.0–6.0 mm is used; melt temperature is held at 180–205°C, with the upper limit controlled to prevent gel formation during long cycles. Blow pressure of 0.5–0.7 MPa and mould temperature of 15–35°C are set according to wall thickness, which ranges from 3.0 mm to 8.0 mm on floats. Finished products include navigation buoy bodies, fender floats, and hose support floats. The compliance foundation is ASTM D1693 condition B for environmental stress crack resistance and ISO 4892-2 for UV ageing; published data for this specific configuration is limited for multi-year marine field performance, so part qualification should include a production trial with 2,000 h accelerated weathering and drop impact at -20°C. Avoid combination with amine-based additives or certain hindered phenolic packages that can bloom and reduce weld-line strength.

    Free Quote

    Competitive Sinopec Maoming HDPE HHM5502ST prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HDPE HHM5502ST is a high-density polyethylene film-extrusion grade produced at the Maoming petrochemical complex in Guangdong, China. Published grade literature and distributor datasheets list a typical melt mass-flow rate of 0.35 g/10 min when measured at 190 °C under 2.16 kg piston load according to ASTM D1238-20 or ISO 1133-1:2022, and a nominal density of 0.955 g/cm³ under ASTM D1505-18 or ISO 1183-1:2019. The material is intended for stalk-bubble blown film conversion, particularly thin-gauge high-strength carrier bags, bin liners, and industrial packaging. In comparison with injection-moulding HDPE grades displaying melt-flow indices above 4 g/10 min, HHM5502ST is not suitable for high-flow filling or complex moulds. In comparison with high-molecular-weight blow-moulding grades, the resin is tuned for film drawing rather than parison sag resistance.

    Rheological Boundaries and Stalk-Bubble Extrusion Stability

    On production-scale grooved-feed extruders with screw diameters from 45 mm to 90 mm and length-to-diameter ratios of 25:1 to 30:1, the low melt-flow index of HHM5502ST produces elevated melt pressure at the screen pack and die inlet. Processors should anticipate higher specific energy input than a 1.0 g/10 min unimodal film HDPE. Melt-temperature set points are typically maintained between 180 °C and 220 °C; sustained operation above 230 °C can increase gel formation from oxidative degradation, while operation below 170 °C may leave insufficiently melted particles that appear as shark-skin or die lines. Because high-density polyethylene is not strongly hygroscopic, drying is not normally required before extrusion, but pellets stored outdoors under RH > 80% or cooled after silo transfer should be dried at 70–80 °C for 1–2 h to remove surface condensation.

    The stalk-bubble process for this molecular-weight class typically operates with a die gap of 1.2–1.8 mm, a blow-up ratio of 3:1 to 5:1, and a frost-line height adjusted to maintain film optics and tensile isotropy. Excessively low frost-line height increases machine-direction orientation, lowering transverse elongation and tear resistance; excessively high frost-line height destabilizes the stalk and causes film-width variation. Melt filtration with screen packs of 60/100/60 mesh or finer is commonly used to remove crosslinked particles, but finer screens increase backpressure. Published data specific to gel counts and melt-pressure drift for HHM5502ST under different screen-pack configurations is limited, and start-up campaigns should establish a process baseline on each film line.

    Table 1. Typical trade-literature property profile.

    PropertyTest methodTypical value
    Melt mass-flow rate, 190 °C/2.16 kgASTM D1238-20 / ISO 1133-1:20220.35 g/10 min
    DensityASTM D1505-18 / ISO 1183-1:20190.955 g/cm³
    Tensile yield strengthASTM D638-14 / ISO 527-3:201828 MPa
    Elongation at breakASTM D638-14 / ISO 527-3:2018800%
    Dart drop impact F50ASTM D1709-15a / ISO 7765-1:200485 g

    In thin-gauge grocery bag conversion at film thicknesses from 12 µm to 25 µm, the combination of 0.955 g/cm³ density and the higher molecular weight of HHM5502ST provides stiffness that permits downgauging without the excessive fold-creasing of lower-density LLDPE. Automatic bag-making machines operating at line speeds above 150 cycles/min require consistent film slip and uniform gauge profile; gauge band variation outside ±5% across the web increases seal-bar misregistration and reject rates. The resin must be evaluated with the specific slip and antiblock masterbatch because neat high-density polyethylene exhibits higher coefficient of friction than many converters require. Published data for HHM5502ST in high-speed bag machines is limited to converter reports rather than standardized test results; dart impact and tensile yield data cannot substitute for sealing-bar temperature optimization and dwell-time studies.

    Why Is HHM5502ST Classified as a High-Molecular-Weight Film Resin Instead of a Blow-Moulding Resin?

    HHM5502ST differs from generic unimodal film HDPE grades with melt-flow indices near 0.8–1.0 g/10 min in the way molecular weight distribution and comonomer placement affect bubble stability and impact. A lower melt-flow index indicates longer chains, which raises melt viscosity and confers higher dart impact at equal density and gauge; however, it also narrows the operating window for output rate on extruders with limited torque. Compared with blow-moulding HDPE grades that have similar melt-flow indices but are optimized for parison sag resistance, HHM5502ST is formulated to permit drawing into films below 25 µm without catastrophic melt fracture or bubble collapse. Direct published data comparing HHM5502ST with Sinopec Maoming HHM5502LW or earlier HHM5502ST predecessors under identical blown-film conditions is limited; side-by-side converter trials are required to establish differences in die-lip deposit rate, gel count, and bag-machine seal strength.

    The difference from injection-grade high-density polyethylene is more pronounced. Injection HDPE with melt-flow indices above 10 g/10 min has low melt viscosity for thin-wall filling but insufficient melt strength for stalk-bubble extrusion. If HHM5502ST were substituted into an injection moulding process, short shots would be expected in multi-cavity tools because the melt would freeze before filling thin sections. Conversely, injecting a high-flow HDPE into a blown film line would not allow a stable bubble and would sacrifice toughness. The operational boundary for HHM5502ST is therefore blown film and possibly thick sheet extrusion where melt strength is valued, but not injection moulding or thin-wall injection applications.

    Table 2. Regulatory applicability checklist for the unpigmented base resin.

    Regulatory instrumentScopeApplicability to HHM5502ST
    21 CFR 177.1520(c)Olefin polymer food-contact useBase resin falls within defined olefin polymer class; finished film must meet extractive limitations and end-use restrictions.
    EU Regulation 10/2011Plastic food-contact materialsCompliance depends on overall migration and specific migration tests on finished film.
    RoHS Directive 2011/65/EULead 1000 mg/kg, cadmium 100 mg/kg, mercury 1000 mg/kg, hexavalent chromium 1000 mg/kgNot intentionally added; certificate of analysis required for batch-level confirmation.
    REACH EC 1907/2006SVHC assessmentPellet suppliers should confirm absence of SVHC above 0.1% w/w.

    Post-industrial reclaim of HHM5502ST film can be re-extruded into the same structure at addition levels up to 30 wt% when the scrap is clean, dry, and free of polypropylene labels. Above 30 wt%, accumulation of oxidized material from repeated heat histories may raise gel counts and reduce dart impact. Printed film scrap introduces ink-binder degradation products that deposit on the die lip; if printed scrap is used, finer melt filtration below 80 mesh is required. Published data specific to HHM5502ST at high reclaim ratios is limited, so the 30 wt% limit is a conservative industrial guideline rather than a material specification.

    When HHM5502ST Is Coextruded with Metallocene LLDPE in Heavy-Duty Sacks

    In coextruded structures where HHM5502ST forms the stiff core or outer layer and a metallocene LLDPE skin provides seal initiation and dart impact, melt-viscosity matching at the die is a primary process variable. The HDPE layer operates in the 190–220 °C melt-temperature range, while the metallocene skin layer may require a lower melt temperature to avoid degradation and die-lip build-up. If the viscosity ratio between the layers exceeds approximately 3:1, interfacial instability may appear as wavy interlayer boundaries or local haze. Published data for HHM5502ST in these exact coextruded structures is limited; establishing the stable operating envelope requires flat-die or spiral-mandrel die trials with melt-pressure transducers installed at each extruder output.

    The die gap in coextrusion should not be set below 1.0 mm for high-molecular-weight HDPE layers because melt fracture at the die lip can propagate into the mLLDPE skin. Purging between HHM5502ST and polypropylene-containing reclaim is necessary; polypropylene contamination above 2 wt% in the HDPE layer reduces dart impact and can create visible gel-like inclusions. Screw purges with a high-flow HDPE are commonly used before shutdown to displace high-viscosity HHM5502ST from the barrel and die channels.

    Storing HHM5502ST in Hot Climates

    Pellets stored in railcars or silos in southern China summer conditions can reach surface temperatures above 60 °C. Although the base resin contains antioxidant and acid scavenger packages, extended storage at 60 °C for more than 12 weeks may increase yellowness index and gel formation, especially if exposed to ultraviolet light through translucent packaging. End users should avoid storing HHM5502ST near ozone-generating electrical equipment because ozone attack can initiate surface cracking and reduce film integrity. Published data for HHM5502ST in hot-weather storage is limited; warehouse trials with yellowness index measured under ASTM E313-20 and gel count under ISO 18553 are advisable for long-cycle procurement.

    For film-grade acceptance testing, properties are measured on 25 µm or 40 µm laboratory blown film produced under controlled conditions. A typical test protocol includes tensile properties under ASTM D882-18 or ISO 527-3:2018, dart impact under ASTM D1709-15a, and tear resistance under ASTM D1922-15. The values obtained are not intrinsic material properties because they depend on blow-up ratio, frost-line height, and draw-down ratio. Comparing HHM5502ST with another HDPE film resin therefore requires identical film preparation conditions; otherwise differences in dart impact and tear can exceed 30% from processing alone.

    In heavy-duty industrial liner applications with film thicknesses between 50 µm and 120 µm, HHM5502ST contributes stiffness and puncture resistance, but the final puncture performance depends on gauge uniformity, blow-up ratio, and frost-line control. Agricultural silage film or outdoor geotextile applications require an additional UV stabilizer masterbatch because the base resin is not designed for extended outdoor exposure; without UV stabilization, service life may fall below 12 months in direct sunlight. The resin is not recommended for potable-water pipe, pressure gas, or medical device applications unless the finished product passes all applicable extractive and mechanical endurance standards, including but not limited to ISO 9080 and ISO 10993 series where relevant.

    Top