| HS Code | 489535 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.20 g/10 min |
| Tensile Yield Strength | 26 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | >600% |
| Flexural Modulus | 1100 MPa |
| Vicat Softening Temperature | 124°C |
| Brittleness Temperature | ≤-70°C |
| Environmental Stress Cracking Resistance Escr | >1000 h |
| Hardness Shore D | 65 |
| Water Absorption | <0.01% |
| Thermal Conductivity | 0.44 W/m·K |
| Dielectric Constant | 2.3 |
| Volume Resistivity | >1×10^16 Ω·cm |
As an accredited Sinopec Maoming HDPE HHM5502LW-GD factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Maoming HDPE HHM5502LW-GD packaging: 25 kg polypropylene woven bags, 40 bags per pallet, totaling 1,000 kg. |
| Container Loading (20′ FCL) | Loaded in 20′ FCL: Sinopec Maoming HDPE HHM5502LW-GD in 25 kg bags, 18 MT net, securely stowed and shrink-wrapped. |
| Shipping | Sinopec Maoming HDPE HHM5502LW-GD ships as a non-hazardous thermoplastic in 25 kg woven bags or 500–1,000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks, away from moisture, direct sunlight, and ignition sources. Standard sea/land freight applies; no special dangerous goods documentation required. |
| Storage | Store Sinopec Maoming HDPE HHM5502LW-GD in a cool, dry, clean, well-ventilated warehouse. Keep original bags sealed on pallets, off the floor, away from direct sunlight, rain, moisture, heat, flames, and incompatible materials. Avoid excessive stacking or package damage. Protect from contamination. Use first-in, first-out rotation and follow the supplier’s SDS recommendations. |
| Shelf Life | Typically 24 months when stored in original sealed packaging in a cool, dry, ventilated area, away from direct sunlight. |
Sinopec Maoming HDPE HHM5502LW-GD is processed in tight-head jerrycan tooling with a grooved-feed single-screw extruder having an L/D ratio of 24:1 delivering melt at 190–205 °C to an accumulator head. Parison length for a 280 g preform is controlled by mandrel movement programmed in six discrete points; the die gap opens from 2.2 mm to 3.8 mm during the final 40% of parison extrusion to correct diameter swell and sag. Blow pressure of 0.7–0.9 MPa is applied against a mould temperature of 15–25 °C, with a pinch-off land angle of 45° and cycle time of 85–110 s for 25 L nominal capacity. Formulation for outdoor stack storage uses a carbon black masterbatch at 2.0–2.5 wt%, a primary hindered phenol antioxidant at 0.10–0.15 wt%, and a process lubricant at 0.03–0.05 wt%; clean in-house regrind may replace up to 20 wt% of virgin resin without altering the UN drop-test response when melt mass-flow variation is held below ±0.5 g/s. Design-type qualification under UN Model Regulations Chapter 6.1 requires a 1.2 m drop for Packing Group II liquids after conditioning at –18 °C for 24 h, a 28-day stack test at 40 °C, and a leakproofness test at 20 kPa internal air pressure. The terminal articles are UN-marked 20 L and 25 L tight-head jerrycans of design type 3H1, used for hydrocarbon solvents, agricultural adjuvants, and liquid detergents in export transport. A practical boundary is that this monolayer structure is not suitable for high-vapour-pressure oxygenated solvents above 0.8 g/cm³ density or for sustained service above 50 °C internal fill temperature, because top-load creep and permeation loss exceed UN test margins. When the jerrycan pinch-off weld shows thickness below 3.5 mm at the chamfer transition, drop-test failure initiates at the weld; therefore parison programming must maintain weld thickness at or above 3.8 mm.
The dominant failure is traced to layer-ratio oscillation after 12–16 h of continuous three-layer extrusion, not to the EVOH resin itself. A five-layer die block is used to coextrude an outer virgin HHM5502LW-GD skin at 35 wt%, a maleic anhydride-grafted polyolefin tie at 2 wt%, an EVOH barrier at 3 wt%, a clean regrind core at 55 wt%, and an inner virgin skin at 5 wt%. Extruder set bands are kept at 180–210 °C for the HDPE streams and 200–220 °C for the tie resin, while the die head is maintained at 205–215 °C to prevent EVOH thermal cross-linking; residence time above 230 °C is limited to less than 90 s. Layer instability can be suppressed by maintaining a viscosity ratio between EVOH and HDPE melt streams of 0.8–1.2 at the die lip, measured by in-line capillary rheometry at 210 °C and 100 s⁻¹. Process air is supplied at 0.5 MPa with a pre-blow delay of 0.4 s; blow pressure reaches 0.8 MPa after mould closure, and the mould temperature is held at 18–22 °C to avoid embrittlement of the tie layer. Compliance for 1 L and 5 L agrochemical containers is evaluated through UN Model Regulations Chapter 6.1 for transport, combined with gravimetric solvent loss testing in xylene at 40 °C for 14 days and oxygen transmission measurement under ASTM D3985-17 at 23 °C and 0% RH. The terminal articles are wide-mouth 1 L and 5 L multilayer bottles for emulsifiable concentrates and oil-based pesticides, where the EVOH layer reduces xylene permeation relative to monolayer HDPE by approximately 60–75% at 3 wt% inclusion; published data for this specific grade in this configuration is limited, so a pilot 72-hour trial is required before film-layer targets are transferred. The pinch-off zone at the base cut edge exposes the EVOH layer; a post-mould flame treatment of 0.3 s or an internal sub-layer of regrind must cover exposed EVOH to prevent wicking delamination upon repeated thermal cycling between –10 °C and 45 °C.
In 750 mL to 5 L detergent and home-care packaging, the controlling property is environmental stress crack resistance rather than tensile yield. HHM5502LW-GD is processed on a dual-station shuttle blow moulder with 1+1 cavity tooling, melt temperature at the head of 185–200 °C, blow pressure of 0.6–0.8 MPa, and mould temperature of 10–20 °C. Screw speed is set to 40–60 rpm, producing a parison drop time of 2.8–3.6 s for a 62 g bottle; the shorter drop time relative to jerrycans allows a narrower die gap from 1.6 mm to 2.8 mm. Formulation for white detergent bottles includes titanium dioxide masterbatch at 1.0–1.5 wt%, antioxidant masterbatch at 0.10 wt%, and process aid at 0.02 wt%; use of post-consumer recyclate in the outer layer is limited to 15 wt% because higher incorporation increases parison width variability beyond ±1.2 mm at the mould parting line. ESCR screening is performed according to ASTM D1693-15, Condition A, with 10% Igepal CO-630 at 50 °C; acceptance criterion for serial release is F50 not less than 24 h, while the neck finish is checked separately under torqued closure at 2.0 N·m for 72 h. The terminal products are 750 mL trigger spray bottles, 1.5 L refill bottles, and 5 L laundry detergent jugs. An operational limitation is that condensation on the mould below 8 °C produces surface micro-voids that raise the coefficient of friction and mask the ESCR notch behaviour; chilled-water temperature is therefore maintained at 12 °C minimum.
A two-cavity shuttle line running 3.785 L containers at 4,800 shots per day must not be cooled below the ductile-brittle transition of the resin/regrind blend. For cold-climate windshield washer fluid, HHM5502LW-GD is compounded with 15 wt% milled post-consumer HDPE, 2.0 wt% blue colour masterbatch, and 0.05 wt% acid scavenger; regrind is screened to 4 mm maximum particle size and dried to less than 0.08% moisture before blending. Extrusion conditions use a melt temperature of 190–210 °C, an accumulator head volume of 1.2 L, and a shot weight of 98 g; mould temperature is set to 12–18 °C because higher mould temperatures extend cooling time without measurable improvement in cold impact. Differential cooling at the handle area is applied through segregated mould circuits to reduce residual stress, with cooling water set at 8–12 °C. Drop testing follows ASTM D5276-19 after conditioning at –30 °C for 48 h; the pass criterion is no fracture at a drop height of 1.0 m for a filled 3.785 L container, repeated on 10 specimens per lot. The terminal product is a 3.785 L windshield washer fluid bottle with a four-thread finish and induction-seal closure, shipped in ambient truck loads to northern distribution centres. The critical operational boundary is post-consumer recyclate content: above 25 wt%, the batch-to-batch high-load melt flow rate variation widens to ±2.5 g/10 min, producing parison length fluctuations of 4–6 mm and increasing drop-test failures at the handle gate; therefore recyclate proportion is clamped at 20 wt% unless in-line melt-flow homogenisation is installed.
For 10 L AdBlue dispensing packs, HHM5502LW-GD is selected for its low-extractables profile and wide processing window in monolayer extrusion blow moulding rather than for aggressive chemical barrier duty. Packaging compliance is governed by ISO 22241-4:2019 and by the diesel exhaust fluid supplier’s certificate of conformity; no post-consumer recyclate is used without written approval, because the standard requires traceability through the packaging supply chain. The formulation is restricted to an approved white masterbatch at 1.0 wt%, a stabiliser masterbatch at 0.10 wt%, and a processing aid at 0.02 wt%; all additives must be free of amines and heavy-metal stearates. The process uses a 750 g accumulator head, melt temperature of 190–205 °C, blow pressure of 0.7 MPa, and mould temperature of 15–20 °C; cycle time is 55–70 s. The terminal product is a 10 L semi-translucent white can with a 45 mm neck finish and a tamper-evident cap, filled at ambient temperature below 30 °C to avoid stress cracking around the handle bridge. The main boundary is outdoor storage: UV exposure beyond 6 months reduces impact strength, so the pack is overwrapped with a PE shrink film containing 5% carbon black or stored under roof.
Cap torque retention is often misinterpreted as a closure dimension issue; the actual failure mechanism is stress cracking in the neck finish caused by hoop stress from overthrust closures and hydrocarbon exposure in engine oil service. HHM5502LW-GD in 1 L and 4 L motor oil bottles is processed at melt temperature 185–200 °C, with blow pressure 0.6–0.8 MPa and mould temperature 10–16 °C. The neck finish is cooled independently to 6–10 °C to accelerate solidification and reduce post-mould shrinkage before the bottle enters the trim station. Formulation includes 2.5 wt% amber colour masterbatch and 0.08 wt% nucleating/clarifying package; no external lubricant is used because silicone-based slip agents can lower cap-off torque below the 1.1 N·m minimum retention requirement after 14 days at 50 °C. ESCR performance is screened under ASTM D1693-15, Condition A, in 10% Igepal CO-630 at 50 °C, with F50 accepted above 30 h for engine oil service; tensile yield of the moulded sidewall is tested under ASTM D638-14 at 50 mm/min to confirm not less than 20 MPa, and drop impact is tested under ASTM D5276-19 at 23 °C. The terminal articles are 1 L and 4 L opaque amber bottles with 38 mm and 45 mm necks, fitted with torque-controlled polypropylene closures. A documented incompatibility is the use of high-molecular-weight ester-based plasticising flushing compounds during colour changes; these can remain in the bottle surface and reduce cap torque retention by 15–20%, requiring a 2-hour purge with virgin HDPE at 210 °C.
| Application | Standard method | Critical threshold | Observed line failure mode |
|---|---|---|---|
| UN-rated jerrycan | UN Model Regulations Chapter 6.1 | 1.2 m PG II drop after –18 °C/24 h | Pinch-off weld thickness below 3.5 mm |
| Agrochemical barrier bottle | ASTM D3985-17 | Oxygen transmission rate target ≤ 0.5 cm³/(m²·day·atm) at 23 °C/0% RH | EVOH delamination at die lip during layer-ratio oscillation |
| Detergent bottle | ASTM D1693-15 | F50 ≥ 24 h in 10% Igepal at 50 °C | Base corner cracking under condensation below 8 °C |
| Windshield washer fluid bottle | ASTM D5276-19 | 1.0 m drop after –30 °C/48 h | Handle-gate fracture when PCR exceeds 25 wt% |
| AdBlue dispensing pack | ISO 22241-4:2019 | No post-consumer recyclate; fill below 30 °C | Handle-bridge stress cracking after prolonged outdoor UV |
| Lubricant bottle | ASTM D638-14, ASTM D1693-15 | Tensile yield ≥ 20 MPa; cap torque ≥ 1.1 N·m | Cap torque loss from ester-based flushing compound residue |
Competitive Sinopec Maoming HDPE HHM5502LW-GD prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Maoming HDPE HHM5502LW-GD is a high-molecular-weight, broad-molecular-weight-distribution ethylene-α-olefin copolymer supplied by Sinopec Maoming Petrochemical Co., Ltd. The resin is produced in a low-pressure slurry polymerization unit and is intended for extrusion processes in which a low melt-flow-rate HDPE is required to maintain parison stability, notch toughness, and environmental stress-crack resistance. Under ISO 1133-1:2022, the high-load melt mass-flow rate at 190 °C/21.6 kg is typically reported as 0.22–0.30 g/10 min; the high-load condition is used because a standard 2.16 kg test would produce values too low for routine quality control. The density at 23 °C, determined by ISO 1183-1:2019, is normally in the range 0.950–0.957 g/cm³. The material is supplied as pellets with an antioxidant and acid-scavenger package, and it generally does not require pre-drying when processed from sealed original packaging. When bags have been opened or stored at relative humidity above 60%, drying at 75–80 °C for 2–4 h is recommended to suppress moisture-related surface defects in large parisons. The grade is typically evaluated for large-volume blow molding and pressure-pipe extrusion; it is not generally recommended for injection molding because the high molecular weight and high melt viscosity require excessive filling pressures and induce orientation and packing variations.
In large-volume blow molding, HHM5502LW-GD can be processed on accumulator-head machines with shot capacities from 5 L to 2000 L. The resin’s high melt strength is intended to maintain wall thickness in long parisons and reduce uneven thinning in tall containers. Actual material distribution is controlled by the parison programming curve, and the die gap must be calibrated to produce an extrudate with uniform wall thickness at the target melt temperature. Molders should not substitute melt-temperature increases for proper die-gap and programming adjustments because that approach lowers melt strength and accelerates parison sag.
Unimodal HDPE blow molding resins with comparable density frequently show lower environmental stress-crack resistance and lower melt strength than this broad-molecular-weight-distribution product. The molecular weight distribution is designed so that a lower-molecular-weight fraction reduces melt viscosity under shear, while a higher-molecular-weight fraction contributes to tie-molecule formation between lamellae and therefore improves slow crack growth resistance. Because short-chain branching is preferentially located on the high-molecular-weight chains, the product exhibits a higher level of inter-lamellar connectivity than a conventional copolymer of the same density. This structural difference is reflected in the notched Charpy impact strength measured according to ISO 179-1:2010 and in the environmental stress-crack resistance measured under ASTM D1693-21 condition B using 100% Igepal at 50 °C. Compared with standard narrow-MWD grades, the product also displays higher die swell and lower parison sag for a given die gap and melt temperature; these effects must be compensated through parison programming rather than by increasing melt temperature. Another difference is the higher head pressure observed on the same extruder profile, which is a consequence of the high-molecular-weight tail and not necessarily an indication of poor melt quality.
The following property envelope is supplied for preliminary material selection and is not a lot-specific certificate of analysis. Lot-specific certificates of analysis may differ, particularly after exposure to reprocessed material or after storage beyond the manufacturer’s recommended shelf life.
| Property | Typical Range or Classification | Test Method |
|---|---|---|
| Density (23 °C) | 0.950–0.957 g/cm³ | ISO 1183-1:2019 |
| High-load melt mass-flow rate (190 °C/21.6 kg) | 0.22–0.30 g/10 min | ISO 1133-1:2022 |
| Tensile yield stress (50 mm/min, type 1B) | ≥23 MPa | ISO 527-2:2012 |
| Nominal tensile strain at break | >600% | ISO 527-2:2012 |
| Flexural modulus (2 mm/min) | 850–1000 MPa | ISO 178:2019 |
| Notched Charpy impact (23 °C, type 1 edgewise) | >35 kJ/m² | ISO 179-1:2010 |
| Environmental stress-crack resistance, 100% Igepal, 50 °C | >1000 h | ASTM D1693-21 |
| Oxidative induction time (210 °C) | >30 min | ISO 11357-6:2018 |
On a grooved-feed single-screw extruder with L/D 30:1 and a compression ratio of 2.5–3.5:1, the feed throat is normally maintained at 170–190 °C, the compression zone at 190–210 °C, and the metering zone at 210–230 °C. The melt temperature at the die entry should be controlled to 190–230 °C; excursions above 240 °C can accelerate oxidative degradation, reduce the high-molecular-weight fraction, and generate gels that damage pressure-pipe weld quality and blow-molded part appearance. Because the grade’s high-molecular-weight tail increases shear heating, screw speed and backpressure must be adjusted to prevent the melt from exceeding the setpoint despite lower barrel temperatures. A 90 mm single-screw extruder with L/D 30:1 is a common configuration for intermediate parison outputs; actual output must be established on the installed drive and die head. For accumulator-head blow molders with clamp forces above 2000 kN, shot-weight capacity should be checked against the required parison length and piston pressure. The high melt viscosity raises head pressure and can reduce shot-to-shot consistency if the accumulator ring or mandrel is worn. Pre-drying equipment with a dew point of -30 °C or lower is recommended when open storage cannot be avoided. Processors should not add waxes or external lubricants without evaluating their effect on weld-line strength; low-molecular-weight additives can migrate to the weld interface and reduce burst strength.
Batch-to-batch variability should be monitored by high-load melt mass-flow rate and density. A density shift of 0.002 g/cm³ can alter large-part shrinkage and warpage enough to require tooling compensation. On extrusion lines running above the extruder manufacturer’s recommended screw-speed window, the product can generate melt temperatures above the setpoint through viscous dissipation; barrel zone temperatures may need to be reduced by 5–10 °C per zone. If melt fracture appears at high output, reducing screw speed, opening the die gap, or increasing die temperature is preferable to adding unspecified process aids. Fluoropolymer-based processing aids may be evaluated at 300–500 ppm only after compatibility with the required weld strength and hydrostatic properties is confirmed.
High-molecular-weight broad-MWD HDPE exhibits time-dependent elastic recovery after the die exit. Die swell is higher than that of most unimodal grades of equivalent density, and actual values depend on die land length, land-length-to-gap ratio, shear rate, and melt temperature. Tooling designed for narrow-MWD HDPE may require die-gap adjustment or mandrel profile changes when this product is introduced. A die land-length-to-gap ratio below 10:1 may produce high swell but lower head pressure; ratios above 25:1 reduce swell but increase pressure drop. Parison sag is governed by zero-shear viscosity and the high-molecular-weight tail; the product is intended to permit longer parisons and larger containers without excessive wall-thickness loss. On accumulator-head machines, sag can be monitored by extruding a fixed parison and recording wall-thickness distribution over time. This measurement should be linked to a parison programming curve rather than to barrel temperature alone. Increasing melt temperature to reduce head pressure is not recommended because it lowers melt strength and accelerates sag. The head pressure measured on a given extruder profile can be 15–30% higher than that of a lower-molecular-weight HDPE of the same high-load melt mass-flow rate; this is a reported range from production-scale evaluation of similar broad-molecular-weight resins and is not a guaranteed offset for this specific product. When high head pressure is observed, processors should first reduce screw speed or increase die gap if part wall thickness targets allow; increasing die temperature without adjusting mandrel cooling may create internal weld lines in thick sections.
Tensile yield stress, elongation, flexural modulus, and notched Charpy impact are determined on compression-molded or injection-molded specimens after conditioning at 23 °C and 50% relative humidity for not less than 40 h unless the relevant standard specifies shorter conditioning. The combination of tensile yield stress above 23 MPa and flexural modulus between 850 MPa and 1000 MPa places the material in the stiff HDPE range, while the high impact strength and environmental stress-crack resistance support applications involving stacking, impact loading, and chemical exposure. Chemical resistance follows general HDPE behavior: the material is generally suitable for contact with aqueous acids, bases, salt solutions, and polar organic solvents at ambient or slightly elevated temperatures. Strong oxidizing acids, aromatic hydrocarbons, and chlorinated hydrocarbons can cause swelling or stress-cracking at elevated temperature. For containers holding surfactants or agricultural chemicals, the actual environmental stress-crack resistance must be evaluated with the specific formulation and closure design because the ASTM D1693-21 Igepal test is only a screening method. In pipe applications, slow crack growth resistance and resistance to notch propagation are more relevant than uniaxial tensile data; hydrostatic testing on notched or intact pipes is required to verify performance. The product’s low water absorption, typically below 0.01% at 23 °C for 24 h under ISO 62:2008, is not a unique differentiator but contributes to dimensional stability in humid service.
Lot-release testing for HHM5502LW-GD typically includes melt mass-flow rate, density, tensile yield stress, elongation at break, environmental stress-crack resistance, and oxidative induction time. Pipe producers may require additional hydrostatic tests, gel-count assessment, or carbon black dispersion analysis. A certificate of analysis is supplied with each shipment. Discoloration, black specks, or odor indicate processing degradation or contamination and should trigger gel-count assessment on extruded sheet or parison before the lot is used in pressure-rated components.
For pressure-pipe extrusion, the resin’s thermal stabilizer package is assessed by oxidative induction time at 210 °C under ISO 11357-6:2018 or ASTM D3895-19; values above 30 min are typical for grades intended for long-term water service, but oxidative induction time alone does not establish pressure rating. The antioxidant package may be consumed during processing; the oxidative induction time of regrind should be checked and should not fall below 20 min before re-extrusion into pressure pipe. Hydrostatic design basis is obtained by testing extruded pipe under ISO 9080:2012 and by classifying the material under ISO 12162:2009. This requires long-term hydrostatic data at multiple temperatures and pressures, not resin melt-flow-rate data. Pipe validation is typically performed at 20 °C, 60 °C, and 80 °C under ISO 1167-1:2006. For PE100 classification, the lower confidence limit σLPL at 20 °C for 50 years must be at least 10.0 MPa; however, this classification belongs to the pipe system and not to the resin alone. Published data for this specific grade configuration may not be available to the general public, particularly when certification is issued to the pipe producer rather than to the resin lot. Processors intending to mark pipe for drinking water or gas distribution must verify that the grade and the specific carbon black or color masterbatch meet the applicable national product standards, including ISO 4427 for water pipe and ISO 4437 for gas pipe. Regrind use in pressure pipe is restricted by product standards and manufacturer guidance; typical limits for in-line regrind in HDPE pressure pipe are often 10–20 wt%, but the governing standard and the pipe producer’s validated quality plan determine the maximum allowable fraction. Without lot-specific hydrostatic certification, the statement “PE100” should not be applied to this product unless the supplier has issued a formal classification document.
Existing tooling qualified for narrower-MWD HDPE may require a structured validation program because the product’s higher melt strength and elastic recovery alter parison swell, pinch-off weld formation, and mold-closing behavior. Blow molders should first run short shots at the low end of the melt-temperature window and compare parison length, wall thickness, and bottom flash. Pinch-off weld strength is influenced by molecular weight and cooling rate; if the mold pinch-off insert is worn or has insufficient compression, a high-molecular-weight melt may fail to displace trapped air and produce weak seams. Mold temperature is typically maintained at 10–40 °C for large parts; lower temperatures improve cooling time but can reduce weld-line toughness in thick sections. The material should not be mixed with generic low-density polyethylene or with recycled material of unknown stabilizer history, because phase incompatibility and acid-functional contaminants can reduce environmental stress-crack resistance unpredictably. For technical parts requiring continuously high stiffness, the broader molecular weight distribution does not reduce flexural modulus below the values shown in the table, but lot-to-lot differences in density and comonomer content do affect part shrinkage and warpage. Processors should measure mold shrinkage on the actual tool; published resin data are only a starting point. The grade is not recommended for rotational molding or for thin-wall injection molding, where its high melt viscosity would require high melt temperatures and degrade the stabilizer package. If outdoor service is specified, the molder must add or specify ultraviolet stabilization; unpigmented natural HDPE resin is not sufficient for prolonged exposure to sunlight.