| HS Code | 200304 |
| Polymer Type | High Density Polyethylene (HDPE) |
| Comonomer | 1-Hexene |
| Density | 0.955 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Tensile Yield Strength | 26 MPa |
| Elongation At Break | ≥600% |
| Flexural Modulus | 1100 MPa |
| Vicat Softening Temperature | 125°C |
| Brittleness Temperature | ≤ -70°C |
| Environmental Stress Cracking Resistance Escr | >1000 h |
| Hardness | 66 Shore D |
| Melting Point | 130°C |
| Mold Shrinkage | 1.5-3.0% |
| Water Absorption | <0.01% |
As an accredited Sinopec Maoming HDPE HHM5502LW factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Maoming HDPE HHM5502LW is supplied in 25 kg polypropylene woven bags, palletized and stretch-wrapped for industrial shipment. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Sinopec Maoming HDPE HHM5502LW in 25 kg bags, palletized/floor-loaded, shrink-wrapped, sealed dry container, with loading photos. |
| Shipping | Sinopec Maoming HDPE HHM5502LW is shipped as a non-hazardous thermoplastic resin in 25 kg woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. It moves by truck, rail, or sea container; store cool, dry, away from sunlight, moisture, and contamination. No special dangerous goods documentation required. |
| Storage | Store Sinopec Maoming HDPE HHM5502LW in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and ignition sources. Keep original bags or containers tightly closed to prevent moisture, dust, and contamination. Palletize, stack securely, and avoid prolonged UV exposure. Store at ambient temperature, away from oxidizers or strong acids. Maintain clean handling areas and follow local regulations. |
| Shelf Life | Sinopec Maoming HDPE HHM5502LW has a typical shelf life of 24 months under cool, dry, ventilated storage away from sunlight. |
Sinopec Maoming HDPE HHM5502LW moves through downstream extrusion blow moulding plants as a high-molecular-weight, high-density polyethylene with a nominal melt flow rate of 0.25 g/10 min under ISO 1133-1:2022 and a density of 0.955 g/cm³ under ISO 1183-1:2019. The resin enters accumulator-head extrusion blow moulding cells with first-in, first-out accumulator design, grooved-feed extruders, and mould closing units sized for 25 L to 1000 L industrial containers. On a 200 L tight-head drum line, HHM5502LW is plasticated through a 24:1 L/D single-screw extruder with barrel temperatures ramped from 170°C at the feed throat to 200°C at the metering section, while the accumulator head is held between 195°C and 210°C. The high-molecular-weight fraction in the grade provides a parison with sufficient melt strength to be blown against a water-cooled aluminium mould at 0.7 MPa to 0.9 MPa blow air pressure without tear initiation at the pinch-off line. Converter qualification for UN 3H1 drum performance applies drop impact at -18°C per 49 CFR 178.509 and stack load testing under ISO 2234; the specification cannot be met from resin properties alone because wall thickness distribution, die swell, and pinch-off weld quality remain machine-dependent. Environmental stress crack resistance is measured as F50 under ASTM D1693-15 Condition B in 10% Igepal CO-630 at 50°C; values observed on laboratory compression-moulded specimens are not directly transferable to blown articles, and published data for this specific configuration is limited. The density of 0.955 g/cm³ fixes a crystalline fraction that raises flexural modulus toward 1100 MPa under ISO 178:2019, which improves top-load and stacking performance on 200 L drums but reduces ductile behaviour at low temperature compared with lower-density HDPE grades. Converters accepting this trade-off typically select HHM5502LW for chemical packaging where column strength, hydrocarbon resistance, and environmental stress crack resistance are weighted more heavily than subzero impact.
At head temperatures below 190°C, the apparent melt viscosity of HHM5502LW rises steeply because the high-molecular-weight chains retain longer relaxation times in the die land region. The immediate production-scale failure mode on 25 L jerry can tools is sharkskin surface roughness concentrated at the die exit, followed by weld-line splitting at the pinch-off zone when the melt temperature drops further during parison formation. Die land shear stress is controlled by reducing screw speed to 18–25 rpm on a 24:1 L/D extruder and by widening the die gap from 1.5 mm to 2.5 mm; however, a die gap above 3.0 mm produces wall thickening at the container shoulder and accelerates parison drawdown because the swell compensation is no longer matched to the programmed shot volume. The acceptable operating band for the accumulator head is normally ±5°C around the nominal setpoint, and an excursion below this band increases screw back-pressure and torque demand beyond 85% of drive capacity on small machines. When the melt temperature is raised above 225°C, gel particles from minor thermal-oxidative crosslinking can appear in the melt stream; these gels are visible as pinholes in the top-load region of a 30 L tight-head container after sectioning. Plant data from accumulator-head lines with 24:1 L/D screws show that increasing screw speed from 20 rpm to 35 rpm raises melt temperature by 4–7°C through viscous dissipation, and this temperature gain must be offset by reducing barrel zone 3 temperature by 3–5°C. The same sub-190°C condition may also force the accumulator plunger to fill more slowly, extending cycle time by 4–7 s and reducing output on rotary-wheel machines. Without a static mixer or barrier screw, the outer parison surface can be 3–5°C hotter than the melt core, producing asynchronous die swell and measurable wall thickness variability around the container circumference.
On rotary-wheel blow moulding machines producing 1 L to 5 L monolayer lubricant and agrochemical bottles, HHM5502LW is processed with a short accumulator stroke and parison programming to maintain a target sidewall thickness of 0.8 mm to 1.2 mm and 1.5 mm to 2.0 mm at the handle pinch-off. The application environment requires resistance to aliphatic hydrocarbons, ester-based lubricant additives, and chlorinated pesticide carriers; HDPE provides hydrocarbon resistance but is not resistant to strongly oxidising formulations such as 5% sodium hypochlorite at 50°C for indefinite service. Top-load and column strength are determined by bottle geometry, not resin alone; qualification should use ASTM D2659-16 at 10 mm/min compression speed to compare empty and filled containers. Batch-to-batch melt flow variation should be held within ±0.03 g/10 min under ISO 1133-1:2022, because drift outside this range alters wall thickness distribution in the bottle base and reduces cap-torque retention after migration of surface lubricants. Closure systems containing ethylene-propylene-diene monomer liners may interact with the bottle neck finish; converter trials should monitor sealing torque loss after 14 days at 40°C. The same high-molecular-weight fraction that improves ESCR also complicates colourant dispersion in thin-walled bottles; masterbatch carriers should be high-density PE with a melt flow rate within ±0.15 g/10 min of the base resin to avoid local viscosity mismatch and weld-line weakening. Agrochemical formulations containing xylene or cyclohexanone can reduce ESCR of polyethylene; therefore, container qualification for these solvents should include finished-article ESCR testing rather than reliance on resin F50 values.
When the parison hang time exceeds 12 s on a 25 L jerry can tool, the unsupported melt column begins to draw down under its own mass; the resulting wall thickness variation produces a thinner top corner and a thicker base pinch-off. HHM5502LW has sufficient high-molecular-weight tails to resist drawdown better than lower-molecular-weight film grades, but the benefit is lost if the die gap is opened too far to compensate. Pressure programming should deliver a parison thickness profile that is 0.3–0.5 mm thicker in the top section than the base before blowing. On accumulator-head machines, hang time is controlled by reducing head tooling temperature to 195°C while maintaining extruder output, or by increasing shot size so that the accumulator plunger fills and discharges quickly. A hang time above 15 s at 210°C head temperature causes visible parison elongation and weld-line thinning; at this point the operator must either lower melt temperature or increase tooling diameter, because higher melt temperature alone reduces die swell and accelerates sag. The interaction between melt temperature and hang time is non-linear; converter trials show that a 5°C reduction in head setpoint can extend the maximum usable hang time by 2–3 s without improving tear resistance at the pinch-off. For 200 L open-head drums with tall parison lengths, the same extension is achieved with internal parison cooling and programmed die-gap profile changes, not by raising the melt temperature; excessive melt temperature reduces wall thickness at the top chime and increases parison length variability. The shortcoming of a wide die-gap compensation strategy is that it creates a heavier base weld line and longer cycle cooling time in that region, increasing total mould closed time by 8–12 s.
Blow-moulded industrial water storage tanks with nominal volume from 200 L to 1000 L are produced from HHM5502LW when the end use requires stiffness and ESCR rather than low-temperature impact at -40°C. For outdoor UV exposure, natural HHM5502LW does not contain sufficient light stabiliser for permanent sun exposure; converters must compound with 2%–2.5% carbon black masterbatch of compatible high-density PE carrier, and dispersion should be checked by ISO 4892-2:2013 accelerated weathering with a 500 h exposure condition. Immersion in potable water is subject to extraction and organoleptic testing under EN 1622:2006 and local drinking-water approvals; the resin by itself does not carry automatic certification. For industrial water at 50°C with chloramine residual above 2 mg/L, surface microcracking can initiate at weld lines; this is accelerated by internal stress and should be assessed with ASTM D1693-15 after immersion in chlorinated water rather than by visual inspection alone. The flexural modulus of 1100 MPa under ISO 178:2019 provides adequate buckling resistance for vertical tanks but is not sufficient for unsupported horizontal storage vessels above 3000 L; ribbed wall design is required. The same grade can be used for immersion service in dilute mineral acids below 25% concentration at ambient temperature, but continuous exposure to concentrated nitric acid or oxidising acid mixtures above 40% at 40°C is outside the long-term chemical resistance boundary of polyethylene. Welded or fusion-bonded joints on HHM5502LW tanks should be considered the critical ESCR zone because orientation and residual stress differ from the blow-moulded wall.
Compliance for HHM5502LW downstream articles is application-specific and is not conferred by resin sales specification alone. The following matrix lists the governing methods that converters commonly use to qualify finished blow-moulded containers; inclusion in the matrix does not constitute a regulatory approval for the resin. For UN packaging, the full package design qualification governs drop impact, leakproofness, hydraulic resistance, and stacking performance on production tooling. For food-contact or potable-water use, the finished article must be tested for overall migration and organoleptic properties; the base olefin polymer may be referenced under FDA 21 CFR 177.1520(c) or Regulation (EU) No 10/2011, but no automatic food-contact status is granted without article-specific testing.
| Qualification area | Governing method or clause | Operational boundary for HHM5502LW |
|---|---|---|
| UN plastic drum drop impact | 49 CFR 178.509 at -18°C | Wall thickness distribution and pinch-off geometry must be validated on production tooling |
| UN leakproofness | 49 CFR 178.604 | Applies to tight-head packagings; closure torque is application-specific |
| Environmental stress crack resistance | ASTM D1693-15 Condition B, 10% Igepal, 50°C | Laboratory values are not directly transferable to finished container corners |
| Melt flow rate | ISO 1133-1:2022, 190°C/2.16 kg | Incoming resin control; drift above ±0.03 g/10 min alters parison drawdown |
| Density | ISO 1183-1:2019 | Nominal 0.955 g/cm³; used for stiffness and barrier consistency |
| Food-contact olefin polymer | FDA 21 CFR 177.1520(c) | Compliance is conditional; extraction and end-use temperature limits must be confirmed |
| EU food-contact overall migration | Regulation (EU) No 10/2011 | Not granted automatically; article-specific migration testing required |
Competitive Sinopec Maoming HDPE HHM5502LW prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Maoming HDPE HHM5502LW is a high molecular weight, high-density polyethylene blow moulding resin produced through low-pressure ethylene polymerization. The grade is characterized by a density of 0.956 g/cm³ when measured according to ISO 1183-1:2019 and a melt flow rate of 0.25 g/10 min at 190 °C under 2.16 kg load using ISO 1133-1:2022. The producer identifies the material as a bimodal HDPE, in which a high molecular weight fraction contributes to parison stability and environmental stress crack resistance (ESCR), while a lower molecular weight fraction provides shear-induced flow during extrusion. The resin is supplied in pellet form and is used primarily in extrusion blow moulding of large rigid containers, industrial packaging, and chemical drums. Published data for this grade indicates negligible moisture absorption; routine drying is not required unless surface condensation has occurred after storage in high-humidity conditions.
At a melt flow rate of 0.25 g/10 min, the resin belongs to the high molecular weight end of extrusion blow moulding grades. Bimodal architecture produces a broad molecular weight distribution that increases shear thinning during plastication and retains high extensional viscosity during parison formation. The low melt flow rate reduces injection moulding compatibility but provides the melt elasticity required for accumulator-head and shuttle press processes. The high molecular weight fraction is associated with tie-molecule formation between crystalline lamellae, which improves slow crack growth resistance. At a density of 0.956 g/cm³, stiffness remains sufficiently high for dimensional stability. At this density, the mass fraction crystallinity calculated from density correlation is approximately 65–70%, corresponding to a peak melting endotherm near 130–135 °C measured by differential scanning calorimetry using ISO 11357-3:2018. The high crystallinity contributes to resistance against aliphatic hydrocarbons and dilute acids, but swelling in aromatic solvents above 60 °C limits use in aggressive hydrocarbon service. Typical mechanical property values reported for this grade are shown below; they are not specification limits and may vary by lot and sample preparation.
| Property | Test Method | Typical Value | Unit |
|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.956 | g/cm³ |
| Melt flow rate (190 °C, 2.16 kg) | ISO 1133-1:2022 | 0.25 | g/10 min |
| Tensile yield stress (50 mm/min) | ISO 527-2 | 26 | MPa |
| Nominal elongation at break | ISO 527-2 | >600 | % |
| Flexural modulus (2 mm/min) | ISO 178 | 1100 | MPa |
| Izod notched impact strength (23 °C) | ISO 180/A | 30 | kJ/m² |
| Environmental stress crack resistance (F50, Condition B) | ASTM D1693 | >1000 | h |
| Vicat softening temperature (A50) | ISO 306 | 127 | °C |
| Shore hardness, D scale | ISO 868 | 62 | — |
Compared with lower molecular weight blow moulding grades having melt flow rates of 0.7–2.0 g/10 min, HHM5502LW offers higher melt strength and ESCR but lower throughput and higher extruder torque. The lower MFR increases cycle time in small mouldings; in large-part production, however, the resin permits thinner wall sections through improved parison stability. The ESCR test condition B uses 10% Igepal CO-630 at 50 °C; a value above 1000 h indicates that the high molecular weight fraction effectively ties crystalline lamellae and suppresses slow crack growth. This is particularly relevant for packaging of surfactant-based cleaners, agricultural chemicals, and industrial liquids. The notched Izod impact value of 30 kJ/m² at 23 °C supports ductile failure suppression at pinch-off weld lines. At temperatures below -20 °C, impact strength may decrease, and burst pressure ratings should be re-evaluated for outdoor storage. Relative to chromium-catalysed unimodal HDPE at similar density, the bimodal distribution narrows the processing window for gloss while broadening the acceptable range for ESCR and impact resistance. The grade is not designed for injection moulding; long flow paths and thin walls below 2 mm are difficult to fill at a melt index this low.
In converting a 200 L tight-head drum line from a unimodal 0.7 g/10 min blow moulding grade, the die melt temperature is commonly reduced by 5–10 °C to limit parison drawdown. Accumulator-head machines with screw diameters from 80 mm to 120 mm and 24:1 to 30:1 L/D ratios are employed. Melt temperature measured at the die is maintained between 180 °C and 210 °C. Die gap settings between 2.0 mm and 3.5 mm are selected according to part weight and parison length. Mould temperature is held at 10–40 °C for rapid solidification and cycle time reduction. The low melt flow rate requires a screw with deeper metering channels and higher torque; barrel temperatures are often set in a reverse profile from 200 °C at the feed zone to 180 °C at the metering zone to avoid excessive shear heating. Screws with 24:1 L/D and a compression ratio of 2.5:1 to 3.0:1 are preferred; high-shear barrier screws can generate excessive melt temperature at speeds above 60 rpm. The use of a gear pump may reduce pressure fluctuation to below ±0.5 MPa and improve parison weight consistency. Published data for this specific configuration is limited; on-site trials are recommended to establish exact set points.
Parison weight consistency is controlled by the accumulator head drop speed. Drop speeds above 2.0 m/min may introduce melt fracture and reduce weld-line strength at the pinch-off region. Back pressure between 0.5 MPa and 1.0 MPa improves homogenization but increases shear heating; therefore screw speed should be adjusted to maintain a melt temperature below 210 °C. The melt pressure at the head inlet is generally held below 35 MPa to prevent premature wear of accumulator head seals. Blow pressure is typically set at 0.6–0.8 MPa for large drums. At this pressure, the parison is expanded against the mould without excessive flash formation. Blow time may exceed 120 s for a 200 L drum depending on mould temperature and wall thickness. Throughput on an 80 mm 24:1 extruder is typically 120–200 kg/h depending on screw speed and head pressure; specific energy consumption ranges from 0.25 kWh/kg to 0.35 kWh/kg for similar high molecular weight HDPE grades.
Starting torque on a cold extruder is higher for bimodal HDPE than for unimodal grades of similar density. The resin should not be re-stabilized with high levels of metal stearates because this may affect colour and ESCR. Colouring can be accomplished with high-density polyethylene-based masterbatches at 2–4 wt%. Use of polypropylene-based masterbatches should be avoided because immiscibility reduces impact strength. Regrind from trimmed flash and rejected containers can be re-introduced at 10–20 wt%, provided the material is ground and dried. Higher regrind content increases gel specks and may reduce ESCR below 600 h in thin-wall sections.
Standard unimodal HDPE grades with melt flow rates of 0.7–2.0 g/10 min generally exhibit lower ESCR and lower melt strength than HHM5502LW. At equal part weight and die temperature, the parison from HHM5502LW can be hung for 3–6 s without significant drawdown, whereas lower molecular weight grades may fail within 1–2 s. This difference permits a broader die gap and more uniform wall thickness in deep parts. The flexural modulus of 1100 MPa is comparable to or higher than many 1-butene unimodal HDPE grades of similar density. The notched Izod impact value of 30 kJ/m² at 23 °C indicates a high-molecular-weight tail that suppresses brittle failure at the pinch-off weld line.
Relative to HDPE grades intended for small bottle blow moulding with melt flow rates above 0.7 g/10 min, HHM5502LW requires higher melt temperature to reduce melt fracture and higher torque at start-up. However, its melt strength permits weight reduction in large containers without downgauging below a critical wall thickness that would compromise ESCR. The material is less suitable for multi-layer structures requiring low melt viscosity for thin inner layers; a high-flow layer material should be selected for the inner layer. Oxygen and water vapour permeation are typical for HDPE, and barrier properties are inferior to polyamide or fluorinated HDPE. For fuel tank inner layers requiring high hydrocarbon barrier, fluorination or polyamide tie-layer technology is necessary.
Food-contact status for this olefin polymer is governed by the general provisions of 21 CFR 177.1520 and EU Regulation 10/2011. The grade is classified as a high-density polyethylene copolymer; no specific migration limit applies to the base polymer, but overall migration into food simulants must meet the 10 mg/dm² limit for plastic materials under EU 10/2011. Finished article testing is required because processing additives, regrind, and colourants can alter migration behaviour. The producer’s lot-specific certificate of analysis should be consulted for compliance verification.
| Requirement | Standard or Regulation | Typical Status |
|---|---|---|
| Food-contact olefin polymer | 21 CFR 177.1520 | Complies at temperature limitations specified in paragraph (c) |
| EU plastic materials for food contact | EU 10/2011 | Conformance to be verified by migration testing on finished article |
| REACH SVHC declaration | Regulation (EC) No 1907/2006 | No SVHC above 0.1 wt% in typical lot data |
| RoHS hazardous substances | Directive 2011/65/EU | Not expected to contain Pb, Cd, Hg, Cr(VI), PBB, PBDE above limits |
Production-scale experience with similar high molecular weight HDPE grades indicates that the most frequent failure modes are pinhole formation at the pinch-off weld line and surface pitting from excessive moisture. Both defects are minimised by maintaining die temperature between 190 °C and 210 °C, avoiding regrind levels above 20 wt%, and preventing water droplets from entering the feed throat. Degradation at processing temperatures above 220 °C is characterized by chain scission and increased low molecular weight species; residence time above 15 min at melt temperature above 210 °C can initiate oxidative chain scission and yellowing. When these process boundaries are maintained, the resin performs consistently in large blow moulded containers. Published quantitative case-study data for HHM5502LW specifically is limited; qualification on the target production line remains mandatory for UN certification of hazardous material packaging.