| HS Code | 762197 |
| Density | 0.952 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.05 g/10 min |
| Melt Flow Rate 190 C 5 0 Kg | 0.25 g/10 min |
| Tensile Strength At Yield | 24 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 1000 MPa |
| Izod Notched Impact Strength 23 C | 300 J/m |
| Vicat Softening Temperature | 124°C |
| Brittleness Temperature | -70°C |
| Environmental Stress Cracking Resistance | >1000 h |
| Hardness Shore D | 60 |
| Melting Point | 130°C |
| Crystallinity | 70% |
As an accredited Sinopec Maoming HDPE HHM5220 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Maoming HDPE HHM5220 is supplied in 25 kg polyethylene woven bags, palletized and shrink-wrapped for bulk handling. |
| Container Loading (20′ FCL) | Sinopec Maoming HDPE HHM5220 loaded in 20′ FCL: 25 kg bags, palletized, shrink-wrapped, secured, approximately 20–22 MT. |
| Shipping | Sinopec Maoming HDPE HHM5220 is shipped as non-hazardous polyethylene resin pellets, typically in 25 kg woven bags, jumbo bags, or bulk trucks/containers. Store in a cool, dry, ventilated area, away from direct sunlight, moisture, heat, and contaminants. Handle with care to avoid bag damage and spillage. |
| Storage | Store Sinopec Maoming HDPE HHM5220 in a cool, dry, well-ventilated warehouse away from direct sunlight, rain, heat, and ignition sources. Keep original bags sealed and pallets off the floor to prevent moisture and contamination. Stack securely, avoid sharp objects, and follow first-in, first-out rotation. Maintain clean handling; avoid prolonged UV exposure and temperatures above 40°C. |
| Shelf Life | Sinopec Maoming HDPE HHM5220 shelf life is typically 24 months under cool, dry, ventilated storage, away from direct sunlight and heat. |
| Parameter | Vest Carrier Bag | Agricultural Mulch | Refuse Sack | Coextruded Structural Ply | Drum Liner |
|---|---|---|---|---|---|
| Die gap range | 1.0–1.6 mm | 0.8–1.4 mm | 1.2–2.0 mm | 1.0–1.8 mm | 1.5–2.5 mm |
| Blow-up ratio | 4.0:1–6.0:1 | 2.5:1–3.5:1 | 3.0:1–4.5:1 | 2.0:1–3.0:1 | 1.8:1–2.5:1 |
| Frost line height (die diameters) | 6–10 | 4–7 | 8–12 | 5–8 | 3–5 |
| Melt temperature range | 180–210°C | 170–200°C | 180–215°C | 190–230°C | 185–220°C |
| Target film gauge | 7–15 μm | 10–40 μm | 15–60 μm | 35–80 μm (total structure) | 100–250 μm |
| Extruder L/D ratio | 25:1–33:1 | 24:1–30:1 | 25:1–30:1 | 28:1–36:1 | 24:1–28:1 |
| Primary test standard | ASTM D1709 Method A | ISO 4892-2 | ASTM D1709 Method B | ASTM F904 | ASTM D543 |
| Regulation / Standard | Test Method | Simulant / Condition | Limit | Applicable Segment |
|---|---|---|---|---|
| FDA 21 CFR 177.1520 | Extraction per 21 CFR 177.1520(c) | n-Hexane, 50°C, 2 h | Max 5.5% extractables | Food packaging |
| EU 10/2011 | EN 1186-1 | D2 synthetic triglyceride, 40°C, 10 days | 10 mg/dm² | Food packaging |
| 94/62/EC | Heavy metal digestion | Pb, Cd, Hg, Cr(VI) | 100 ppm combined | All packaging |
| IEC 61340-2-3 | Surface resistivity | 23°C, 50% RH | 10¹¹ Ω/sq | Drum liners, FIBC inserts |
| ASTM D7371 | Fluorine surface content | FTIR attenuated total reflectance | 2–5% surface F | Fluorinated drum liners |
Competitive Sinopec Maoming HDPE HHM5220 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Maoming HDPE HHM5220 is a high-density polyethylene grade supplied in pellet form within the Maoming HHM series. The grade is positioned for injection moulding of rigid industrial articles where controlled melt flow, stiffness, and resistance to shelf-load deformation are required. Published distributor technical data sheets list the product with a melt flow rate of approximately 2.0 g/10 min under ISO 1133-1:2022 conditions at 190 °C and 2.16 kg, and a nominal density of 0.954 g/cm³ under ISO 1183-1:2019. These values place HHM5220 between low-melt-flow blow moulding grades and high-melt-flow thin-wall injection grades; the practical consequence is that the material fills moderate-flow-length moulds without the excessive cavity pressure associated with lower-MFR grades, but it does not behave as a high-flow polypropylene substitute in thin sections.
Table 1 consolidates representative values from distributor literature for HHM5220. The data are typical rather than contractual minima or maxima; lot release is governed by the producer’s certificate of analysis. Tensile, flexural, and impact values are sensitive to specimen preparation, cooling rate, and conditioning at 23 °C and 50% relative humidity according to ISO 291:2008.
| Property | Test method | Representative value |
|---|---|---|
| Melt flow rate | ISO 1133-1:2022, Procedure A | 2.0 g/10 min |
| Density | ISO 1183-1:2019 | 0.954 g/cm³ |
| Tensile yield strength | ISO 527-2:2012 | 24 MPa |
| Elongation at break | ISO 527-2:2012 | >600% |
| Flexural modulus | ISO 178:2019 | 1000 MPa |
| Charpy notched impact strength | ISO 179-1:2010 | 4.0 kJ/m² |
| Vicat softening temperature | ISO 306:2022 | 125 °C |
Conversion of HHM5220 is routinely carried out on injection moulding machines equipped with general-purpose HDPE screws having an L/D ratio of 20:1 to 25:1 and a compression ratio of 2.5:1 to 3.0:1. Initial melt temperatures are typically set between 200 °C and 240 °C. The lower boundary is controlled by excessive melt viscosity, elevated screw torque, and poor non-return valve sealing; the upper boundary is controlled by oxidative degradation, odour generation, and colour shift. At 220 °C, the melt exhibits sufficient flowability for thick-section filling, but ejection clearances and sealing surfaces may still flash if clamp force is insufficient or if the mould parting line is worn. Back pressure for initial trials should be held below 1.0 MPa. Higher back pressure improves melt homogeneity but increases residence time and screw recovery time.
Pre-drying is not normally required for HDPE unless pellet surfaces are wet from outdoor storage or ambient relative humidity exceeds 60%. Surface moisture can produce splay, internal voids, and surface streaks. When moisture is suspected, a desiccant hopper dryer set at 70–80 °C for 1–2 h is sufficient. Vented barrels are not required for this grade, and regrind from sprues and runners may be incorporated at low levels in non-critical parts provided that particle size distribution and bulk density remain stable.
The primary distinction is rheological and conversion-specific. HHM5220 is specified for injection moulding, whereas Maoming HHM5502 is positioned for extrusion blow moulding. HHM5502 exhibits lower melt flow and higher melt strength, which maintains parison stability during extrusion blow moulding. That same high melt strength becomes a processing liability in injection moulding because it increases filling pressure and restricts flow length. Conversely, HHM5220 has lower melt strength and is generally unsuitable for large-parison blow moulding because the parison may sag before mould closing. Converters moving from HHM5502 to HHM5220 should reduce injection pressure and cushion, shorten hold time, and verify gate freeze before ejecting the part. Table 2 summarizes the differentiation without implying that one grade is universally superior to the other.
| Characteristic | HHM5220 | HHM5502 |
|---|---|---|
| Primary conversion route | Injection moulding | Extrusion blow moulding |
| Melt-flow class | Higher MFR | Lower MFR |
| Melt-strength requirement | Moderate, cavity-fill dominated | High, parison-stability dominated |
| Typical processing failure | Flash, jetting, post-mould shrinkage | Parison sag, weld-line weakness |
HHM5220 is used in industrial containers, transport packaging, crates, agricultural trays, and thick-walled technical parts. The grade is not the first candidate for packaging with wall sections below 1.0 mm, because higher-MFR high-density polyethylene or polypropylene grades fill high flow-length-to-thickness ratios with lower injection pressure. Published spiral-flow data for HHM5220 under production conditions is limited; mould-filling simulation should be calibrated with in-house spiral-flow tests for tools with flow ratios above 150:1. Linear mould shrinkage in HDPE commonly ranges from 1.0% to 2.5% depending on thickness, cooling rate, and additive package, so tight-tolerance parts require post-mould shrinkage verification rather than reliance on generic shrinkage tables.
Hot runner systems for HHM5220 must be designed without dead spots, because thermally degraded HDPE can adhere to manifold walls and produce black specks in otherwise continuous production. Melt temperatures in the manifold should remain within the same 200–240 °C window as the barrel. If hot runner temperature exceeds 250 °C, local oxidative chain scission may reduce viscosity and generate discoloration, acrid odour, and surface defects. Total melt residence time at 240 °C should be held below 10 min; at 230 °C, residence times up to 15 min may be tolerable for non-food industrial parts, but colour stability should be monitored. When producing clear or white articles, purging with a high-viscosity HDPE or a commercial purge compound before shutdown reduces severe brown streaking on restart. If the barrel temperature drops below 200 °C, unmelted pellets can damage the non-return valve and create screw recovery variability.
Gate geometry should also be matched to the grade. Edge gates or direct sprue gates are suitable for thick sections. Pinpoint gates smaller than 1.0 mm can cause jetting and surface flow marks unless the melt temperature is raised and the injection speed is reduced. Mould vent depths should be maintained at 0.02 mm to 0.03 mm to allow gas escape without creating flash. Screw speed during plastication should be set conservatively, typically 60–80 rpm for a 50 mm screw diameter; larger screws require tip-speed matching rather than identical rotational speed. If melt temperature during recovery exceeds 245 °C, reducing back pressure or screw speed is usually more effective than lowering late-barrel temperature alone because shear heating dominates the final melt temperature in high-output cycles.
Environmental stress-cracking resistance in HHM5220 follows the general trend for high-density polyethylene with density near 0.954 g/cm³: it is lower than a butene-hexene copolymer and lower than low-density polyethylene. Parts exposed to polar surfactants, detergents, fatty acids, or aggressive cleaning agents should be tested under ASTM D1693-15b or ISO 22088-3:2006 at the target service stress. Incompatible residues from polyamide, polycarbonate, or acetal in the same barrel can cause delamination at weld lines and part failure. A dedicated HDPE screw and barrel are recommended, or a rigorous purge sequence should be used after processing those polymer families. Moisture on pellets or regrind combined with high melt temperature can generate hydrolytic degradation of contaminant residues, further reducing weld-line strength.
Quality control of incoming HHM5220 should include melt flow rate and density verification before lot acceptance. For critical parts, tensile yield strength and notched Charpy impact should be tested on conditioned specimens because these properties respond strongly to crystallization history, mould cooling rate, and part thickness. A single raw-resin datasheet value does not guarantee identical properties in a finished moulded article. If the part is intended for food contact, the specific additive package and the supplier’s declaration under relevant food-contact legislation must be obtained; general HDPE compliance does not transfer automatically to all formulations and colour masterbatches. REACH and RoHS declarations for this grade are typically issued by the distributor, and users should request the current safety data sheet for their region. The grade is not supplied for implantable medical use; conversion into medical packaging requires separate regulatory assessment.