Sinopec Maoming Hdpe Hhm5202m2

Sinopec Maoming HDPE HHM5202M2

    • Product Name: Sinopec Maoming HDPE HHM5202M2
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 241196
    Material Type High Density Polyethylene (HDPE)
    Density 0.952 g/cm³
    Melt Flow Rate 0.2 g/10 min (190°C/2.16 kg)
    Tensile Yield Strength ≥26 MPa
    Elongation At Break ≥600%
    Flexural Modulus ≥1000 MPa
    Vicat Softening Temperature ≥125°C
    Brittleness Temperature ≤-70°C
    Environmental Stress Cracking Resistance ≥1000 h
    Hardness 60 Shore D
    Impact Strength ≥30 kJ/m²

    As an accredited Sinopec Maoming HDPE HHM5202M2 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE HHM5202M2 is packed in 25 kg PP woven bags, 40 bags per pallet, 1000 kg per pallet.
    Container Loading (20′ FCL) Sinopec Maoming HDPE HHM5202M2 loaded in 20′ FCL, 25 kg bags, palletized, stretch-wrapped, securely braced for ocean export.
    Shipping Sinopec Maoming HDPE HHM5202M2 is shipped as a non-hazardous solid polymer resin in 25 kg bags or jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks. Store in a cool, dry, ventilated area, away from heat, moisture, and sunlight. Keep packaging sealed.
    Storage Store Sinopec Maoming HDPE HHM5202M2 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags sealed on pallets, off the floor, to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Do not store near foodstuffs or incompatible chemicals. Ensure adequate ventilation.
    Shelf Life Shelf life is typically 24 months when stored in original packaging, cool, dry, well-ventilated area, away from direct sunlight.
    Application of Sinopec Maoming HDPE HHM5202M2

    Monolayer bottom-seal T-shirt sack production with Sinopec Maoming HDPE HHM5202M2 places constraints on bubble stability that are not observed with fractional-melt LLDPE feedstocks. The resin is typically charged as received without predrying at ambient humidity below 50 % RH; above that threshold, hopper moisture condensation can produce surface defects on the film bubble. A common monolayer formulation for outlet-bound retail sacks is 96–98 wt% HHM5202M2, 1.0–2.0 wt% silica-based antiblock masterbatch, and 0.5–1.5 wt% erucamide slip masterbatch. The slip fraction is reduced to 0.5 wt% when the film is printed with water-based inks because bloom migration is accelerated at slit-seal temperatures above 120 °C. Extrusion is performed on a single-screw grooved-feed extruder with L/D 25:1–30:1 and a 100–160 mm dual-lip air ring die. Die gap is held at 0.9–1.1 mm, blow-up ratio at 3.5:1–4.5:1, and frost line height at 6–8 die diameters. Die temperature is controlled at 210 °C ± 5 °C. A high-stalk bubble configuration is preferred; the stalk diameter should remain below 80 % of die diameter to avoid helical instability. Downstream conversion uses bottom-seal machines with 500–650 mm film width and T-shirt bag punch units operating at 120–180 cycles/min. The film is tested according to ISO 1133-1:2022 for melt flow rate, ISO 1183-1:2019 for density, ASTM D1709-15ae1 for dart impact, ASTM D1922-23 for Elmendorf tear, and ISO 527-3:2018 for tensile properties. Finished sacks are evaluated for heavy metals under Directive 94/62/EC Annex II, with a total Cr VI, Pb, Cd, and Hg limit of 100 mg/kg. End-product forms include bottom-seal T-shirt bags, loop-handle retail sacks, and die-cut header sacks for non-food merchandise.

    What Limits Drawdown Below 12 µm in High-Molecular-Weight HDPE Film Processes?

    Sub-12 µm film from HHM5202M2 is governed by the melt strength of the bubble, not by the extruder plasticating capacity. The critical processing conflict is that increasing melt temperature to lower melt pressure promotes shear thinning and improves die flow, but reduces bubble load-bearing capacity and raises the probability of bubble rupture above 215 °C. Conversely, die temperatures below 200 °C produce shark-skin melt fracture on the outer bubble surface. The operational window is therefore 205 °C ± 5 °C at the die, and this must be maintained across the full die circumference within 3 °C. To reduce gauge to 12–15 µm, converters typically use 85–90 wt% HHM5202M2 and 10–15 wt% C4 or C6 LLDPE with a melt index of 0.8–1.0 g/10 min; if gauge falls to 10 µm, LLDPE addition is raised to 20 wt% and 0.5 wt% polymer processing aid masterbatch based on a fluoroelastomer is added. The bubble is run with a high-stalk configuration, blow-up ratio 3.0:1–3.8:1, frost line height 8–10 die diameters, and die gap 0.8–1.0 mm. A twin-lip air ring with lower lip flow at 60–70 % of total air volume stabilizes the stalk. Gauge variation across the web must remain below ±5 % at 12 µm; otherwise film thickness variations create weak points in perforation lines during roll-bag conversion. Tests are performed under ISO 7765-1:1988 or ASTM D1709-15ae1 Method A, with 66 cm dart height. Elmendorf tear values in MD and TD are obtained under ASTM D1922-23. Tear anisotropy above 1.5:1 MD/TD indicates excessive stalk elongation and is rejected because it causes bag splitting at cut-outs. End products include 10–12 µm perforated roll bags, star-sealed banana-liner sacks, and compactor bin liners.

    Control parameterTargetTest/equipment
    Die temperature profile200–210 °CInsulated die with 3-zone heating
    Blow-up ratio3.0:1 to 3.8:1Bubble cage with ultrasonic diameter sensors
    Frost line height8–10 die diametersInfrared frost line sensor
    Film gauge10–15 µmCapacitance gauge scanner, ±5 % tolerance
    LLDPE addition10–20 wt%Loss-in-weight gravimetric feeding

    Because the conversion window for industrial refuse sacks is narrower than for commodity film grades, the use of HHM5202M2 in this segment is concentrated in heavy-gauge sacks above 25 µm where high melt strength reduces sag and allows haul-off speeds above 40 m/min. A typical compound is 80–90 wt% HHM5202M2, 8–15 wt% post-industrial HDPE trim regrind, and 2–4 wt% carbon black masterbatch with 40–50 wt% pigment loading. The regrind fraction must be screened to remove particles above 250 µm, since high-molecular-weight tails in the regrind cause gel specks and dart impact variability. These sacks are classified under EN 13592:2017 for household waste collection and are also subjected to tensile seam strength evaluation under ISO 527-3:2018 at a jaw separation speed of 500 mm/min. Heavy metal restrictions follow Directive 94/62/EC Article 11, and the carbon black masterbatch must comply with its supplier REACH registration under Regulation (EC) No 1907/2006. Film is blown on a 65–90 mm extruder with L/D 28:1 and die diameter 200–300 mm. Die gap is set at 1.2–1.5 mm. The bubble is cooled with ambient or chilled air; frost line is maintained at 5–7 die diameters to produce balanced dart and tear. Blow-up ratio is 3.0:1–3.5:1. After slitting, tubing passes through a star-seal bottom former or a draw-tape insertion unit. Perforations are introduced by a rotary pin wheel. Winding tension is maintained at 4–6 N per 100 mm film width to prevent blocking. Finished types include star-sealed construction refuse sacks, draw-tape yard waste sacks, and perforated roll liners for 50–200 L containers.

    When a High-Density Core Is Coextruded with Metallocene LLDPE Skins

    Coextrusion of a HHM5202M2 core with metallocene LLDPE skins is used where stiffness from the HDPE core must be combined with lower seal initiation temperature and higher dart impact from the skins. The core layer contains 65–80 wt% HHM5202M2, with 10–20 wt% mLLDPE added to reduce bubble stress and 10–15 wt% regrind trim. Skin layers are each 10–15 wt% of total thickness, formulated from mLLDPE or a plastomer, with slip/antiblock masterbatch at 0.5–1.0 wt% in the skin only. Because all layers are polyethylene, no tie resin is required, but viscosity ratios must remain below 1.5:1 at 250 s⁻¹ to avoid interfacial instability. The structure is tested under ASTM D1894-14 for skin coefficient of friction, ASTM D1709-15ae1 for dart impact, and ASTM D1003-21 for haze if the application uses clear skins. If inks or adhesives are used, the converter should verify that ultraviolet-curing primers meet the specific migration limits of Regulation (EC) No 1935/2004 only when packaging contact is predicted; for industrial mailers, this is not a mandatory framework. Production uses a three-layer blown-film die with a spiral mandrel design. Die gap is 1.4–1.6 mm, die temperature 215 °C ± 5 °C, blow-up ratio 3.0:1–3.5:1, frost line 6–8 die diameters. The higher die gap is required because the core layer is highly viscous; below 1.2 mm, shear rates exceed 1500 s⁻¹ and trigger melt fracture at the skin/core interface. Bubble cage stabilization is employed to limit gauge bands. After treatment to 38–42 mN/m by corona discharge, the film is converted on a form-fill-seal line. End products include courier mailers, industrial wrap films, and heavy-duty appliance dust covers.

    Refuse Sack Compression Stress Retention Under EN 13592 Loading

    Household refuse sacks manufactured from HHM5202M2 are characterized less by tensile yield than by the ability of the bottom seal and side folds to retain contents under impact and compression. The governing test is EN 13592:2017, which specifies capacity, drop resistance, and seal integrity requirements for sacks intended for household waste collection. A typical formulation for 20–30 µm household sacks is 88–93 wt% HHM5202M2, 5–10 wt% LLDPE extrusion-grade modifier, and 1–2 wt% black or grey masterbatch. The LLDPE fraction is essential below 25 µm because it raises dart impact under ASTM D1709-15ae1 from below 80 g to above 100 g, a shift that determines whether sacks pass a 66 cm loaded drop test. Extrusion is performed on a single-layer blown-film line with L/D 25:1, die diameter 150–250 mm, die gap 1.0–1.2 mm, blow-up ratio 3.5:1, and frost line 6 die diameters. The bubble is collapsed through a V-guide after 5–8 m of haul-off height. The tube is slit, perforated, and formed into star-seal sacks at 120–160 cycles/min. Sealing temperature for star seals is 140–155 °C with dwell 0.35–0.60 s; above 160 °C, thin-gauge sections exhibit seal burn-through. Besides EN 13592:2017, the converter may apply ISO 527-3:2018 for tensile ultimate elongation, which typically must exceed 400 % in MD for draw-tape sack mouth retention. Heavy metal concentrations are controlled under Directive 94/62/EC Annex II to a total of 100 mg/kg. Product forms include star-sealed pedal bin liners, draw-tape refuse sacks, and grey kitchen waste bags with tie handles.

    For temporary containment panels welded from 0.5 mm sheet, HHM5202M2 is used as the primary ply because the low melt flow range of 0.15–0.25 g/10 min under ISO 1133-1:2022 provides high zero-shear viscosity for extrusion stability at wide widths. The formulation is 100 wt% HHM5202M2 with 2.5–3.0 wt% carbon black UV stabilizer masterbatch; no mineral fillers are included because calcium carbonate loading above 5 wt% reduces hot-wedge weld peel strength. Panels are produced on a wide-width blown-film line with 600–1200 mm die diameter, die gap 1.5–1.8 mm, blow-up ratio 2.5:1–3.0:1, and die temperature 210 °C ± 5 °C. The lower blow-up ratio yields preferred MD tensile strength and limits web wander during panel assembly. Performance is evaluated under ISO 527-3:2018 for tensile yield and break, ASTM D882-18 for thin-sheet tensile, and ISO 12236:2006 for static puncture resistance. Welded seam peel is assessed under ASTM D6392-12. The carbon black masterbatch is selected with a UV rating for 12-month outdoor exposure; published data for this specific grade in multi-year weathering is limited. Hot-wedge welding is performed at 300–350 °C with seam overlap 40–60 mm and roller pressure 0.5–0.7 MPa. Ultrasonic thickness gauges check for thickness reduction below 10 % at the seam. Panels are joined by hot air welding if the onsite temperature is below 5 °C, with preheating of the weld track to 30 °C to prevent brittle fracture. End products are temporary construction containment curtains, dust-control partitions, and non-critical waste transfer pit liners.

    Free Quote

    Competitive Sinopec Maoming HDPE HHM5202M2 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HHM5202M2 is a high-density polyethylene (HDPE) extrusion blow moulding grade designed for large-volume industrial containers. The producer datasheet lists a nominal density of 0.952 g/cm³ as measured by ISO 1183-1:2019 and a melt flow rate of 0.30 g/10 min to 0.35 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022. The high-load melt flow rate at 21.6 kg is typically 30 g/10 min to 38 g/10 min, yielding a melt flow ratio of approximately 100 to 115 that indicates a broad molecular weight distribution tailored for parison stability. The product is supplied as translucent white pellets containing a hindered phenolic phosphite antioxidant package and an acid scavenger. It is used primarily in accumulator-head and continuous-extrusion blow moulding lines for 200 L and 250 L tight-head drums, open-top containers, and chemical packaging requiring high environmental stress crack resistance.

    For large-drum production, the molecular architecture of HHM5202M2 differs from standard HDPE grades in the distribution of comonomer and high molar mass chains. In 1-butene-modified HDPE, short-chain branches are located preferentially in lower molar mass fractions; the M2 modification increases tie molecule formation in the high molar mass fraction, which enhances slow crack growth resistance. Under ASTM D1693-15, condition B, 100% Igepal CO-630, the F50 value is reported above 1000 h. The grade is specified for cargoes that contain surface-active agents, alkali solutions, and non-oxidizing inorganic salts. The same property shifts the grade away from injection moulding and film processes, where rapid crystallisation and drawdown are more important than parison hold-up.

    Compared with chromium-catalysed bimodal HDPE film grades, HHM5202M2 has substantially lower drawdown capability and higher melt strength. Capillary rheometry at 190 °C typically shows a shear viscosity near 8000 Pa·s at 100 s⁻¹ and 1200 Pa·s at 1000 s⁻¹, placing the grade between pipe resins and high-melt-flow-rate injection moulding resins. Published data for this specific configuration is limited outside the standard melt flow parameters, and end users should generate rheological curves on the actual accumulator head. The grade should not be processed on a vented extruder without a melt seal unless the feed zone is kept below 170 °C to prevent additive volatilisation and yellowing.

    What Distinguishes HHM5202M2 from Other Maoming HDPE Blow Moulding Grades?

    Compared with the smaller-container blow moulding grade HHM5502, HHM5202M2 has a lower density and a higher environmental stress crack resistance. HHM5502 is typically selected for 1 L to 20 L bottles because its density near 0.955 g/cm³ provides higher top-load strength and faster cooling in thin walls. In contrast, HHM5202M2 is selected for large drums because the lower crystallinity from a density of approximately 0.952 g/cm³ improves resistance to stacking fatigue and chemical cracking. Against the standard HHM5202 variant, the M2 suffix indicates an ESCR-optimised molecular design; the improvement is observed as a shift in F50 from roughly 300 h to above 1000 h in producer comparisons, while the melt flow and density remain nearly unchanged.

    PropertyHHM5202M2Standard HHM5202HHM5502Test standard
    Density0.951–0.953 g/cm³0.951–0.953 g/cm³0.954–0.956 g/cm³ISO 1183-1:2019
    Melt flow rate0.30–0.35 g/10 min0.30–0.40 g/10 min0.25–0.35 g/10 minISO 1133-1:2022
    ESCR F50, 100% Igepal>1000 h300–500 h50–150 hASTM D1693-15
    Tensile yield strength26–28 MPa25–27 MPa28–30 MPaISO 527-2:2012
    Flexural modulus1050–1150 MPa1000–1100 MPa1150–1250 MPaISO 178:2019
    Vicat softening point A/50126–130 °C125–129 °C127–131 °CISO 306:2022

    The difference between HHM5202M2 and standard HDPE blow moulding grades is not visible in the melt flow rate alone. The M2 modification changes the high molar mass tail, shifting the storage modulus transition and slow crack growth resistance, but it also reduces crystallisation rate because of the lower density and higher short-chain branch content. In practice, converters observe slower solidification of the chime by 5 s to 10 s compared with HHM5502. Mould cooling time may need to be increased by 5% to 10% when switching from HHM5502 to HHM5202M2 to maintain the same moulded drum weight and flatness.

    Extruder Barrel Profile, Melt Temperature Limits, and Accumulator Head Settings

    On a single-screw extruder with L/D 24:1 to 30:1 and a screw diameter of 90 mm to 120 mm, the barrel zones are set from 170 °C in the feed section to 210 °C in the metering section. The accumulator head and die are maintained at 195 °C to 205 °C. For a 200 L parison with a length close to 1.8 m, the practical die melt-temperature window is 195 °C to 205 °C; below 185 °C, sharkskin and head-pressure excursions above 35 MPa are observed on production lines, and above 220 °C, parison sag increases to the point that sidewall thickness variation exceeds 2 mm. The extruder melt pressure at the breaker plate is normally controlled between 15 MPa and 25 MPa. Screw speed is adjusted to maintain a filled feed zone, and the accumulator fill time is typically 10 s to 20 s depending on shot size.

    Parison programming is mandatory for large drums. The die gap is opened to 70–80% of maximum for the bottom chime, reduced to 20–30% at the neck, and ramped through 20 or more points to compensate for gravitational thinning. Blow-up ratio is maintained at 2.2:1 to 2.8:1; blow air pressure is held at 0.6 MPa to 0.8 MPa, with preblow delayed by 1.5 s to 2.5 s after parison closure. The mould coolant temperature is set at 8 °C to 12 °C using a chiller sized for 45 kW to 75 kW per 200 L tool. Total cycle time is normally 150 s to 180 s; cycles forced below 120 s produce under-cooled demoulded chime sections that shrink after extraction and fail the UN leakage test.

    Accumulator-head machines require a decompression stroke after fill to prevent drool. The programmed decompression distance is usually 3 mm to 5 mm; excessive decompression above 8 mm can draw air into the melt and create void inclusions in the parison wall. The head tooling for a 200 L drum uses a die diameter of 80 mm to 100 mm and a mandrel-core assembly with 15° to 20° divergence angles. Wall thickness around the drum shoulder is set at 5.5 mm to 6.5 mm, tapering to 3.5 mm in the sidewall. These values provide top-load ratings above 2500 kg in laboratory compression tests.

    If Carbon Black Masterbatch Is Added for UV-Stabilized Outdoor Storage

    For drums stored outdoors, addition of a 40 wt% carbon black polyethylene masterbatch is required at 2.0 wt% to 2.5 wt% final carbon black content. This raises the density by less than 0.003 g/cm³ and reduces the melt flow rate by approximately 5% to 10%. The masterbatch must be metered with a gravimetric feeder at the hopper throat, and a static mixer or melt pump is advised to avoid aggregate formation. Dispersion is evaluated by a pressure-rise test on a 325-mesh screen pack; a rise above 0.5 MPa over 30 min indicates poor dispersion and possible microvoid formation. Addition above 4 wt% carbon black can reduce ESCR F50 by 20% to 30% and should be avoided unless specific outdoor weathering data are available.

    HHM5202M2 is compatible with aqueous acids, alkalis, and non-oxidizing salts at ambient temperature. It is not recommended for continuous contact with aromatic hydrocarbons, chlorinated solvents, ethers, or strong oxidizing acids such as concentrated nitric acid and hydrogen peroxide; these media cause swelling, permeation, or oxidative chain scission. Detergent and agricultural chemical formulations containing ethoxylated alkylphenols or high-HLB surfactants can induce environmental stress cracking even when the neat chemical is benign; compatibility must be tested by drum or bottle tests under ASTM D543 and ISTA 7D conditioning. For food-contact use, the converter must obtain a producer compliance statement; HDPE olefin polymers can fall under FDA 21 CFR 177.1520 when end-use extractables are below the specified limits, but this grade is normally supplied for industrial packaging and is not automatically food-contact certified in every region.

    Mechanical qualification of fabricated drums is usually performed to EN 15426 and UN 6.1.5.3.5 protocols for hazard classes. Drop tests are executed after conditioning at -18 °C for 48 h; a 200 L drum at 1.2 m drop height must not leak or rupture. Stacking tests under 40 °C and 28 days load simulate 2.5 times the gross mass. In production trials, the resin exhibits consistent wall thickness at the chime, but process capability depends on the parison programmer and mould alignment. Published data for the specific effect of regrind levels above 30 wt% on ESCR of this grade is limited; therefore, regrind use above 20 wt% should be validated in the end-use packaging qualification.

    Standard or regulationScopeRelevant condition or limit
    ASTM D1693-15Environmental stress crack resistanceF50, 100% Igepal CO-630, 50 °C
    ISO 1133-1:2022Melt flow rate190 °C, 2.16 kg
    ISO 1183-1:2019DensityImmersion method, 23 °C
    ISO 527-2:2012Tensile yield strengthType 1B, 50 mm/min
    ISO 178:2019Flexural modulusThree-point bending
    FDA 21 CFR 177.1520Olefin polymers in food contactExtractables determined by end use; verification required
    EU Regulation No 10/2011Plastics intended for food contactOverall migration < 10 mg/dm²
    GB 4806.7-2016Food contact plastic articlesMigration and sensory requirements
    REACH (EC) No 1907/2006SVHC declarationSVHC not present above 0.1% w/w per producer SDS
    RoHS Directive 2011/65/EUHazardous substance limitsPb, Hg, Cd, Cr(VI), PBB, PBDE below directive limits

    Batch-to-batch control on production lines is supported by certificate-of-analysis data. The producer typically reports melt flow rate, density, tensile yield strength, and antioxidant content for each lot. In compounding and blow moulding operations, pellet moisture should be maintained below 0.05 wt%. Pre-drying at 80 °C for 2 h to 4 h is required if silo storage has exceeded 60% relative humidity or if the pellet temperature has fallen below the dew point during outdoor unloading. The grade is not suitable for pressure pipe applications under ISO 12162 and lacks a PE100 hydrostatic strength classification.

    For the production of large tight-head drums, the critical processing boundaries are the 5 °C melt-temperature control band, the 20 wt% regrind ceiling, and the 2.0–2.5 wt% carbon black dosage window. These boundaries, rather than the nominal melt flow rate alone, determine whether HHM5202M2 can replace general-purpose HDPE blow moulding grades in a given industrial packaging line.

    Top