    HS Code 113863
    Melt Flow Rate 190c 2 16kg 0.25 g/10 min
    Density 0.952 g/cm³
    Tensile Yield Strength 25 MPa
    Elongation At Break >600 %
    Flexural Modulus 1100 MPa
    Vicat Softening Temperature 125 °C
    Brittleness Temperature < -70 °C
    Environmental Stress Cracking Resistance >1000 h
    Hardness Shore D 60
    Notched Izod Impact Strength 300 J/m
    Dielectric Constant 2.3
    Volume Resistivity >10^16 Ω·cm
    Water Absorption <0.01 %

    As an accredited Sinopec Maoming HDPE HHM5202 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE HHM5202 is supplied in 25 kg PP woven bags, 40 bags per pallet, or 1000 kg jumbo bags.
    Container Loading (20′ FCL) Sinopec Maoming HDPE HHM5202 loaded in 20′ FCL, 25 kg bags, palletized, shrink-wrapped, moisture-protected, securely stacked and lashed for transport.
    Shipping Sinopec Maoming HDPE HHM5202 ships as non-hazardous polyethylene pellets in 25 kg PP woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Use clean, dry containers by sea, truck, or rail. Store away from moisture, heat, and direct sunlight. Handle with care and keep sealed until use.
    Storage Store Sinopec Maoming HDPE HHM5202 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep original bags closed, palletized, and off the floor to prevent moisture, dust, and contamination. Protect from weather, oils, acids, alkalis, and strong odors. Avoid excessive stacking. Maintain first-in, first-out rotation and follow the supplier’s SDS.
    Shelf Life Store in a cool, dry, ventilated area in original packaging, away from direct sunlight; shelf life approximately 24 months.
    Application of Sinopec Maoming HDPE HHM5202

    Sinopec Maoming HHM5202 is classified as a high-molecular-weight high-density polyethylene blow molding grade with a nominal density of 0.952 g/cm³ and melt flow rate controlled within the producer’s low-melt-index envelope, nominally 0.35 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022. The downstream routes presented here are restricted to established conversion processes: extrusion blow molding, injection blow molding, coextrusion blow molding, and post-molding fluorination. Each route identifies the compliance anchor, addition ratio, production process, and terminal article without extrapolating beyond documented industrial use.

    UN 3H1/Y1.9 Drop-Test Conditioning for HHM5202 Jerricans

    For Packing Group II and III liquid chemicals, the converter blends 100 parts virgin HHM5202 with 0.5–1.5 parts carbon black masterbatch and, where outdoor storage is required, 0.2–0.4 parts UV stabilizer. The barrel temperature profile on a shuttle blow molding machine equipped with a 24:1 L/D grooved-feed extruder is normally set from 180 °C at the feed zone to 210 °C at the die head, while the accumulator is held at 195–210 °C to prevent melt fracture at the parison surface. A 20 L jerrican usually requires a clamp force of 300–600 kN, blow air pressure of 0.7–0.9 MPa, and mold temperature of 15–30 °C; cycle time is 45–65 s depending on wall thickness and cooling circuit layout. Batch-to-batch variance in carbon black masterbatch moisture above 0.05 wt% can generate surface splay at the die lip, so closed-loop hopper drying at 80 °C for 2 h is applied before processing. Compliance is demonstrated through UN Model Regulations Chapter 6.1 design-type tests, including drop impact from 1.2 m at -18 °C for Packing Group II liquids, leakproofness at 30 kPa, and hydrostatic pressure testing at 100 kPa for 30 min where the design mark requires it. Terminal articles are 10–30 L UN-marked HDPE jerricans used for corrosive, flammable, and water-miscible chemical shipments.

    In automotive diesel exhaust fluid reservoir conversion, the HHM5202 parison is processed on a 3D blow molding machine because the serpentine part geometry requires coordinated mold movement and parison manipulation rather than straight shuttle molding. The addition ratio is 100 parts natural virgin HHM5202 with 0.1–0.3 parts thermal processing stabilizer for natural tanks; black variants use 2.0–2.5 parts carbon black masterbatch to meet UV resistance targets under ISO 4892-2. The extruder is typically a 24:1 L/D grooved-feed unit with melt temperature of 195–215 °C, and blow air pressure is set at 0.8–1.0 MPa. Pinch-off weld lines are inspected at section thicknesses of 8–12 mm, and the tank is leak-tested at 30–50 kPa with pressure decay limits of ≤0.5 kPa/min. ISO 22241-3 restricts material migration into diesel exhaust fluid, and ISO 16750-4 thermal cycling from -40 °C to +60 °C is used to validate weld line integrity. Terminal products are 10–60 L on-board diesel exhaust fluid reservoirs and urea dosing system tanks for heavy-duty trucks and off-highway machinery.

    What ESCR Shift Occurs When 30 wt% Post-Industrial Regrind Returns to the Blow Molding Line?

    When non-food industrial container production returns clean post-industrial regrind to the extrusion blow molding line, the injection point for regrind is normally placed after the gravimetric dosing unit and before the feed throat. The formulation is 70 parts first-pass HHM5202, 30 parts same-line regrind, 0.5–1.0 parts processing stabilizer, and, if required, 0.5–1.5 parts color masterbatch. Melt temperature is held at 190–210 °C, and the accumulator head die gap is increased by 0.2–0.5 mm relative to virgin-only operation to compensate for the slight viscosity reduction caused by regrind shear history. Environmental stress-cracking resistance is re-qualified under ASTM D1693-15 Condition B, with acceptance criteria set by the container manufacturer; published F50 data for HHM5202-specific regrind at 30 wt% is limited, so converters must establish lot-specific baselines rather than extrapolating from virgin-grade datasheet values. The production process remains accumulation extrusion blow molding with a 60–80 mesh screen pack, mold temperature 15–25 °C, and blow air pressure 0.7–0.9 MPa. Compliance for non-food industrial containers is anchored to REACH and EU Regulation (EC) No 1272/2008 for classification, labeling and packaging; UN transport marks apply only when the final container is qualified as dangerous goods packaging. Terminal products are 5–25 L industrial bottles for non-food lubricants, detergents, and maintenance chemicals.

    Cleanroom production of oral solid dose containers from HHM5202 is managed as a rigid-wall extrusion blow molding process rather than blow-fill-seal molding, because blow-fill-seal lines typically require polymers with different parison elongation characteristics and higher melt strength. The formulation is 100 parts virgin HHM5202 with 0–0.1 parts external processing aid; post-consumer regrind is excluded, and any colorant or additive must be prequalified before use. Melt temperature is 185–205 °C, and mold cooling water is held at 10–20 °C to minimize surface haze and improve wall thickness uniformity. The bottle leak test is performed at 20–40 kPa after trimming, and wall thickness at the neck, shoulder, and base is measured against a ±0.2 mm tolerance band. Regulatory compliance uses FDA 21 CFR 177.1520 for olefin polymers, USP <661.1> for plastic packaging systems, Ph.Eur. 3.1.3 for polyethylene containers, and EU Regulation (EU) No 10/2011 for overall migration. Terminal products are 30–500 cm³ oral solid dose tablet bottles and secondary packaging for ophthalmic preparations where only indirect drug contact occurs.

    When Six-Layer Coextrusion Forces Layer Ratio Adjustments in Agrochemical Packaging

    Six-layer coextrusion blow molding of agricultural chemical containers uses HHM5202 as the structural inner and outer skin layers, with a functional barrier layer of EVOH inserted between adhesive tie layers. The total HHM5202 content is 55–70 wt% of the wall mass; EVOH is 2–3 wt%, tie resin is 1–2 wt%, and the remaining regrind layer can reach 25–30 wt% of the wall mass. The accumulator head is specified with six layer channels and a die gap of 2.0–3.0 mm; melt pumps control each layer stream, while melt temperatures are held at 190–215 °C because EVOH degrades above 220 °C and forms gel defects. Layer-to-layer viscosity mismatch is managed by maintaining melt pressure variation of ≤1.0 MPa between adjacent channels. The regrind layer may be incorporated only after the barrier structure is qualified, because reprocessing EVOH-containing trim can form uncontrolled gel particles and delamination defects. Die lip temperature is maintained at 205–215 °C, blow air pressure at 0.7–0.9 MPa, and mold temperature at 15–25 °C. Permeation testing is performed under ISO 15105-2 using oxygen at 23 °C and 50% RH, with an acceptance target of ≤0.5 cm³/(m²·day·atm) for the complete sidewall. Terminal articles are 1–20 L agrochemical barrier bottles for emulsifiable concentrates, solvents, and adjuvants requiring UN Packing Group II or III transport qualification.

    Post-molding fluorine treatment of HHM5202 containers is applied to reduce permeation of volatile organic solvents and non-polar liquids in cosmetic removers, specialty adhesives, and laboratory chemicals. The base bottle is blow molded from 100 parts HHM5202 with 0.5–1.0 parts color masterbatch at melt temperature 190–210 °C, mold temperature 15–25 °C, and blow air pressure 0.7–0.9 MPa. The finished container is subsequently exposed to a fluorine-nitrogen gas mixture at 0.1–1.0% F₂ by volume for a period determined by the required barrier level; the resulting fluorinated surface layer is typically 10–50 nm thick and must be free of unreacted fluorine residue before filling. Permeation resistance is validated gravimetrically or by ASTM D3985 oxygen transmission, and total migration into fill contents is assessed under EU Regulation (EU) No 10/2011 where food or cosmetic contact is claimed. Compliance for non-food solvent containers is anchored to REACH and the ADR/RID transport requirements for volatile flammable liquids. Terminal products are 50–1000 mL fluorinated HDPE bottles for acetone-based cosmetic removers, specialty bonding agents, and reagent-grade solvent packaging.

    Compliance standards and test designations across HHM5202 blow molding routes
    Downstream routePreferred addition ratioPrimary compliance anchorQualification test
    UN jerrican100 parts HHM5202 + 0.5–1.5 parts carbon blackUN Model Regulations 6.1Drop, leakproofness, hydrostatic pressure
    Diesel exhaust fluid tank100 parts HHM5202 + 0.1–0.3 parts stabilizerISO 22241-3, ISO 16750-4Leak decay, thermal cycling, weld line inspection
    Post-industrial regrind container70 parts HHM5202 + 30 parts same-line regrindREACH, CLP 1272/2008ASTM D1693-15 Condition B
    Pharmaceutical bottle100 parts virgin HHM5202USP <661.1>, Ph.Eur. 3.1.3Leak test, migration, thickness mapping
    Six-layer agrochemical container55–70 wt% HHM5202, 2–3 wt% EVOHUN Packing Group II/III, ISO 15105-2Oxygen transmission, layer ratio verification
    Fluorinated solvent bottle100 parts HHM5202 + 0.5–1.0 parts masterbatchREACH, ADR/RIDASTM D3985, residual fluorine test

    Cold-Fill Edible Oil Container Wall Thickness and Drop Impact Trade-Off

    Edible oil bottle conversion from HHM5202 is configured as a cold-fill extrusion blow molding route with wall thickness reduced in the label panel to conserve material while maintaining drop impact resistance at the base and shoulder. The addition ratio is 100 parts HHM5202 with 0.5–1.0 parts food-grade color masterbatch and 0.05–0.15 parts antioxidant; no post-consumer regrind is used in direct food contact layers. Melt temperature is 185–205 °C, mold temperature is 10–20 °C, and blow air pressure is 0.7–0.9 MPa; the top-load strength is evaluated under ISO 8113, and drop impact is tested at 1.2 m after conditioning at 4 °C. Wall thickness distribution is controlled by parison programming with 10–30 point axial profiling, and the resulting containers are leak-tested at 20–30 kPa. Compliance is anchored to FDA 21 CFR 177.1520, EU Regulation (EU) No 10/2011, and EN 1186-1 overall migration testing. Terminal products are 500 mL–5 L edible oil bottles for cold-filled vegetable oils and blended cooking oils.

    Free Quote

    Competitive Sinopec Maoming HDPE HHM5202 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HDPE HHM5202 is a high-molecular-weight high-density polyethylene resin supplied by Sinopec Maoming Petrochemical Company. The grade is positioned for extrusion blow molding of large industrial containers, jerrycans, and thick-walled hollow parts where melt strength, environmental stress crack resistance, and pinch-off weld integrity are process-critical. Publicly available datasheets and distributor records characterise the material as a broad molecular weight distribution ethylene-based resin with a nominal density of 0.952 g/cm³ and a high-load melt flow rate of 2.0 g/10 min at 190 °C under 21.6 kg. Those values place HHM5202 in a lower-density segment of the high-molecular-weight blow molding HDPE family, distinguishing it from both higher-density 0.955 g/cm³ blow molding grades and lower-viscosity injection molding HDPE grades.

    What Are the Verified Solid-State and Melt Boundaries for HHM5202?

    The nominal property envelope for HHM5202 is defined by standardised melt-state and solid-state measurements. Density is reported as 0.952 g/cm³ when determined according to ISO 1183-1 or ASTM D1505. Melt flow rate under ISO 1133-1 and ASTM D1238 condition 190 °C/21.6 kg is typically 2.0 g/10 min, while the 190 °C/2.16 kg value is typically reported near 0.05 g/10 min. The resulting flow rate ratio near 40 indicates a broad molecular weight distribution. In HDPE, that distribution is consequential because the high-molecular-weight fraction increases tie-molecule concentration between lamellae, improving environmental stress crack resistance and impact toughness, while the lower-molecular-weight fraction improves melt processability.

    PropertyUnitNominal ValueTest Method
    Densityg/cm³0.952ISO 1183-1, ASTM D1505
    Melt flow rate, 190 °C/21.6 kgg/10 min2.0ISO 1133-1, ASTM D1238
    Melt flow rate, 190 °C/2.16 kgg/10 min0.05ISO 1133-1, ASTM D1238
    Tensile yield stressMPa25ISO 527-2
    Elongation at break%600ISO 527-2
    Flexural modulusMPa950ISO 178
    Charpy notched impact, 23 °CkJ/m²18ISO 179-1/1eA
    Vicat softening temperature°C124ISO 306/A50
    Environmental stress crack resistance, F50, 100 % Igepal CO-630, 50 °Ch300ASTM D1693 condition B
    Melting temperature, DSC°C131ISO 11357-3

    The tabulated values are nominal values collected from publicly available distributor literature and should not replace lot-specific certificate-of-analysis data. The flexural modulus near 950 MPa and Charpy notched impact of 18 kJ/m² reflect a balance between stiffness and ductility. The F50 environmental stress crack resistance value above 300 h under ASTM D1693 condition B is significant for detergent, agricultural chemical, and UN-type packaging, although field performance remains dependent on bottle geometry, pinch-off weld quality, and processing history.

    When a Converter Replaces a 0.955 g/cm³ Blow Molding Grade with HHM5202

    Substitution of a higher-density 0.955 g/cm³ blow molding grade with HHM5202 is a formulation change rather than a drop-in replacement. A 0.955 g/cm³ HDPE typically provides higher elastic modulus, higher top-load stiffness, and slightly higher Vicat softening temperature, but slower crack growth resistance may be reduced. HHM5202 at 0.952 g/cm³ shifts the property balance toward environmental stress crack resistance and low-temperature ductility. Published datasheets for HHM5202 report flexural modulus near 950 MPa, whereas a 0.955 g/cm³ blow molding grade would ordinarily be expected to exceed 1,000 MPa. For UN-certified jerrycans requiring stack load retention, the difference should be evaluated by creep testing under ISO 899-1 at 40 °C or 60 °C rather than by short-term tensile data alone.

    Compared with a standard injection molding HDPE of similar density and a melt flow rate above 0.5 g/10 min at 190 °C/2.16 kg, HHM5202 has far lower fluidity. Thin-wall sections below 1.5 mm may show short shots, flow marks, or excessive orientation if an injection mold is attempted without redesign. The high-molecular-weight fraction that reduces melt flow also provides greater parison hang strength, which is essential in large extrusion blow molding but undesirable in multicavity injection molding. Comparative data for any specific tool should be generated experimentally because published generic comparisons are orientation only.

    Chemical containment applications expose HHM5202 to environmental stress crack resistance, top load, drop impact, leakproofness, and hydraulic pressure. The pinch-off weld is normally the controlling feature in blow molded tight-head drums. HHM5202 is selected because its high-molecular-weight fraction can produce a tougher weld when clamp pressure, parison temperature, and die gap are correctly set. Drop impact testing per ASTM D2463 is commonly conducted at -18 °C for UN dangerous goods packaging. A passing result depends as much on wall thickness distribution, weld geometry, and mold venting as on the base resin. The grade has no inherent chemical resistance to strong oxidising acids, aromatic solvents, or halogenated hydrocarbons; such substances require barrier treatment or an alternative polymer system. For UN certification, the final article must meet the requirements of the applicable UN Model Regulations Chapter 6.1 performance tests, including hydraulic pressure retention, drop impact, stacking, and leakproofness.

    Extrusion Blow Molding Equipment Settings and Parison Programming Constraints

    Production-scale accumulator-head blow molders used for HHM5202 typically employ screw diameters from 90 to 120 mm and L/D ratios from 24:1 to 30:1. Barrel temperatures commonly begin near 170 °C and rise to a head temperature of 195 °C to 205 °C. The die gap is usually set between 2 and 4 mm for large containers, with parison programming adjusted to compensate for sag on shot sizes above 5 kg. Blow air pressure is typically 0.6 to 0.8 MPa, and mold temperature is maintained between 10 °C and 30 °C to limit cycle time without producing surface defects.

    At melt temperatures above 215 °C, parison sag becomes difficult to control on large shot sizes, and the proportion of drawdown can increase sharply. Below 180 °C, melt pressure rises, die-lip melt fracture may appear, and pinch-off weld interdiffusion may be incomplete. The practical processing window for large containers is therefore approximately 185 °C to 210 °C. Parison programming should use a pre-programmed wall-thickness profile that thickens the pinch-off zone and the shoulder region while reducing thickness along the body to maintain top load and drop impact performance.

    Regulatory qualification is application-specific and must not be assumed from resin selection alone. HHM5202 is an olefin polymer and may fall within the scope of FDA 21 CFR 177.1520 when the finished article meets the relevant density, extractable, and end-use limitations; however, the converter must obtain a food-contact statement from the resin supplier for the intended food type and temperature condition. For industrial packaging, compliance with the EU Packaging and Packaging Waste Directive 94/62/EC heavy-metal limits and REACH candidate list obligations applies to additives, colorants, and final articles rather than the base polyethylene resin. The base polymer is generally exempt from REACH registration as a polymer under Article 3(5), but imported additive formulations and masterbatches may require separate registration or authorisation. RoHS Directive 2011/65/EU applies to electrical and electronic equipment, not to bulk industrial packaging.

    Post-industrial regrind from flash and rejected containers can be incorporated if the material is clean and free of incompatible purge compounds. Regrind concentrations up to 25 to 30 wt% are common in large-container blow molding. Each extrusion pass reduces the high-molecular-weight fraction, raises gel count, and can lower environmental stress crack resistance. Melt flow rate, flow rate ratio, and gel count should therefore be measured on each regrind lot, and ESCR should be re-qualified when regrind content exceeds 20 wt%. Material contaminated with polyvinyl chloride, polyacetal, or aromatic solvent residues should be excluded because thermal decomposition products can degrade the melt and create surface defects.

    Moisture management is governed by surface moisture rather than bulk hygroscopicity. HHM5202 stored in outdoor silos or unsealed octabins at relative humidity above 60 % can carry surface moisture into the extruder, producing splay, bubbles, and reduced weld strength. If moisture-related defects appear, drying at 70 °C for 2 to 3 hours in a desiccant hopper dryer is generally sufficient. Hopper temperatures above 90 °C should be avoided because particle softening can cause bridging and feed instability. For outdoor chemical packaging, UV stabiliser concentration and carbon black dispersion should be verified against the end-use specification because published data for this specific grade under multi-year UV exposure is limited.