Sinopec Maoming Hdpe E4012

Sinopec Maoming HDPE E4012

    • Product Name: Sinopec Maoming HDPE E4012
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 419246
    Density 0.954 g/cm³
    Meltflowrate 0.12 g/10 min (190°C/2.16 kg)
    Tensileyieldstrength 26 MPa
    Tensilestrengthatbreak 30 MPa
    Elongationatbreak >600%
    Flexuralmodulus 1100 MPa
    Izodnotchedimpactstrength 50 kJ/m² (23°C)
    Shoredhardness 65
    Vicatsofteningtemperature 126 °C
    Heatdeflectiontemperature 75 °C (0.45 MPa)
    Brittlenesstemperature -70 °C
    Environmentalstresscrackingresistance >1000 h
    Waterabsorption <0.01%
    Volumeresistivity >10^16 Ω·cm
    Dielectricconstant 2.3 (1 MHz)
    Dielectricstrength 20 kV/mm

    As an accredited Sinopec Maoming HDPE E4012 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE E4012 is supplied in 25 kg net-weight woven polypropylene bags, palletized for industrial shipment.
    Container Loading (20′ FCL) Sinopec Maoming HDPE E4012 is loaded in 20′ FCL containers, typically 25 MT in 25kg bags, securely packed for export.
    Shipping Sinopec Maoming HDPE E4012 is shipped as non-hazardous polyethylene pellets, usually in 25 kg bags or 500–1000 kg jumbo bags on pallets. It requires clean, dry containers, protection from moisture, heat, and sunlight. Standard land or sea freight; no special Dangerous Goods classification. Handle with care to avoid bag damage and contamination.
    Storage Store Sinopec Maoming HDPE E4012 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, moisture, and ignition sources. Keep original bags sealed, palletized, and off the floor. Avoid contact with strong oxidizers and contaminants. Maintain moderate stacking heights to prevent deformation. Use first-in, first-out stock rotation. Shelf life may be reduced by prolonged UV or high-temperature exposure.
    Shelf Life Sinopec Maoming HDPE E4012: store cool, dry, ventilated, away from sunlight; shelf life typically 24 months in original unopened packaging.
    Application of Sinopec Maoming HDPE E4012

    For 10–30 L extrusion blow-moulded jerricans produced from Sinopec Maoming HDPE E4012, the parison wall distribution is governed less by a single melt temperature than by the interaction between the accumulator-head programme, the extruder throughput stability, and the die-gap setting on a continuous shuttle machine. A 90 mm grooved-barrel extruder with an L/D ratio of 30:1 feeds a shot accumulator at a metering-zone melt temperature of 205–210 °C, while the head and die zones are held at 200–208 °C. The die gap for a 25-L container with a target mass of 1,350–1,500 g is set at 1.8–2.2 mm. Pre-blow pressure is maintained at 0.25–0.40 MPa for 0.6–1.0 s, final blow pressure at 0.65–0.80 MPa, and the mould cooling water is supplied at 14–18 °C with a per-cavity flow of 60–80 L/min. When the mould supply temperature falls below 10 °C, handle-root flash freezes before relaxation and post-mould trimming produces hairline weld fracture on a percentage of containers across a typical shuttle line. Wall thickness measured at 12 points around a 25-L jerrican ranges from 1.15 mm at the sidewall to 1.85 mm at the handle base, and the drop impact pass rate at 23 °C is evaluated under ASTM D2463-15 after filling to 80% volume with water/antifreeze and dropping from 2.0 m.

    The certified-jerrican formulation generally contains 80–85 wt% E4012, 15–20 wt% closed-loop plant regrind, 1.5–2.5 wt% carbon black masterbatch at a nominal 40% loading, and 0.1–0.3 wt% antioxidant masterbatch. For food-contact jerricans, masterbatch components must comply with FDA 21 CFR 177.1520 and EU Regulation No 10/2011; overall migration is tested under EN 1186-1 and must remain below 10 mg/dm². The inclusion of 20 wt% regrind lowers environmental stress crack resistance measured under ASTM D1693-15 Condition B from 35–45 h to 15–20 h in 10% Igepal CO-630 solution at 50 °C. Consequently, jerricans used for agricultural surfactant concentrates are usually limited to 15 wt% regrind and are qualified by notched stress crack testing at 40% internal stress. Compliance with the UN Model Regulations Chapter 6.1 requires drop testing under 6.1.5.3, hydraulic pressure testing under 6.1.5.4, and stacking under 6.1.5.6. The terminal product is a stackable narrow-neck 25-L container for crop-protection chemicals, detergent concentrates, and light hydrocarbon emulsions.

    What Limits Drop-Weight Rupture Pressure in a 200-L L-Ring Drum After Outdoor Storage?

    In accumulator-head extrusion blow moulding of 200-L L-ring drums, the machine employs a 120–150 mm single-screw extruder with an L/D ratio of 30:1 to 36:1 and a shot capacity of 25–35 kg. The die melt temperature is held at 215–225 °C, higher than the jerrican route because the large parison must remain stable over a cycle time of 6–10 min. The die gap is programmed from 2.5 mm at the top segment to 3.8 mm at the bottom segment to compensate for parison draw-down; a two-stage pre-blow at 0.20–0.35 MPa for 10–15 s is followed by full inflation at 0.55–0.70 MPa. Mould cooling water is supplied at 18–22 °C to avoid frozen-in stress, and the drum wall is typically 2.0 mm at the chime and 4.5 mm at the bottom knuckle. After 12 months of outdoor storage, drop-weight rupture pressure under ASTM D2463-15 declines mainly because UV-generated surface microcracks reduce the effective wall section; 2.0–2.5 wt% carbon black masterbatch with a primary particle size below 25 nm is therefore used. The compound also contains 0.2–0.5 wt% hindered phenolic antioxidant and 0.1–0.2 wt% phosphite process stabiliser.

    For UN certification as a 1H1/Y1.8/200 drum, the closure ring, L-ring, and wall must pass a drop test onto a rigid concrete plane from 1.2 m at −18 °C, a hydrostatic pressure test at 250 kPa for 30 min, and a stack load test under UN Model Regulations 6.1.5.6 at the combined mass of the packages stacked to the transport height. The outer-surface oxygen induction time is checked under ISO 11357-6:2018 with a minimum of 20 min at 200 °C for stabilised material. Terminal products are 200-L L-ring drums for solvent-based adhesives, high-density liquid concentrates, and industrial oils. Where E4012 is used outside the supplier’s published certification envelope for very thick-walled containers, published data for this specific configuration is limited; converters typically qualify the parison drop time and die swell through a two-level factorial design before full-scale production.

    Extrusion Sheet Gauge Band and Chill-Roll Pressure in Chemical Tote Liner Fabrication

    For sheet thicknesses from 2 mm to 6 mm, E4012 is processed on a 90–120 mm single-screw extruder with an L/D ratio of 30:1 and a barrier screw. The flat die is maintained at 210–225 °C, and the die gap is set 10–15% above the target sheet thickness to offset draw-down between the die and the three-roll stack. The primary chill roll is held at 65–80 °C, the secondary roll at 75–85 °C, and the tertiary roll at 50–60 °C; nip pressure at the primary roll is set to 350–500 N/cm of sheet width to control transverse gauge variation. A 2,000 mm die is adjusted by thermo-die bolts and an automated thickness scanner to hold gauge variation within ±2.5% across the sheet. The compound contains 1.5–2.0 wt% carbon black masterbatch for UV opacity, 0.1–0.2 wt% antioxidant masterbatch, and 5–10 wt% in-house regrind. For food-contact liners, a white masterbatch at 0.5–1.0 wt% is used, and the final sheet must comply with FDA 21 CFR 177.1520 and EU Regulation No 10/2011 with overall migration below 10 mg/dm² under EN 1186-1. Chemical tote liners exposed to oxidising acids are additionally screened for surface stress cracking under ASTM D1693-15 Condition A. The sheet is post-formed into tote liners at a surface temperature of 145–155 °C using a draw ratio of 0.8:1; terminal products are acid-resistant liner trays for intermediate bulk containers and dunnage boards used in chemical logistics.

    When High-Draw Strapping Lines Push HDPE Through a 6:1 Orientation Gap

    In monofilament strapping conversion, E4012 is extruded through a 65–90 mm single-screw extruder with an L/D ratio of 30:1 and a screen pack of 80/120/80 mesh. A gear pump delivers melt at 190–215 °C to a slit die, after which the tape is quenched in water at 30–38 °C. The quenched tape is then oriented in a hot-air oven at 90–110 °C with a draw ratio between 6:1 and 9:1. The oven temperature must not drift by more than ±3 °C across the web; lower temperatures increase fibrillation at the tape edges, while higher temperatures reduce tensile strength by more than 5% per 5 °C of drift. A 12 mm wide tape with a target thickness of 0.45–0.55 mm is annealed at 100–115 °C for 1.5–2.0 s under 3–5% relaxation. The compound contains 0.5–1.0 wt% UV stabiliser masterbatch and 0.1–0.2 wt% acid scavenger masterbatch. Calcium carbonate filler above 0.1 wt% reduces elongation at break under ASTM D638-22 to values below 18%, which is below the 20–30% elongation window accepted for dynamic railcar vibration. Compliance for non-metallic strapping is evaluated under ASTM D3950-23; terminal products are palletized corrugated carton strapping and lumber bundle straps.

    Non-pressure corrugated drainage conduit and cable ducting from E4012 are processed on a 60–75 mm single-screw extruder with a vacuum calibrator and water spray tank. The melt temperature is raised to 215–230 °C because the corrugator forming cavity requires sufficiently low viscosity for full replication of the corrugation profile. A 110 mm diameter corrugated pipe with a 1.2 mm wall thickness is formed in a mould block system with 12–16 blocks per loop, and the vacuum level in the corrugator is held at −0.06 to −0.08 MPa. The black conduit compound contains 2.0–2.5 wt% carbon black masterbatch; dispersion is verified by ring stiffness testing under ISO 9969:2016. The resulting duct is not qualified for pressure service under ISO 4427 because the long-term hydrostatic strength class for E4012 has not been established for pressure piping; use is limited to non-pressure buried conduit standards such as EN 61386-1 for cable management. Terminal products are buried cable protection ducts and perforated drainage pipes for brownfield sites.

    Parison Sag, Die Swell, and Bottleneck Weight Repeatability in 500 mL Personal Care Bottles

    For 500 mL mouthwash bottles, the E4012 parison is extruded at 195–210 °C through a 35–55 mm extruder with an L/D ratio of 24:1 to 28:1 and a die diameter of 8–12 mm. Measured die swell at the recommended throughput is 25–35%, so the die gap is set at 0.8–1.0 mm to produce a finished sidewall of 0.55–0.70 mm. The target bottle mass is 28–32 g, and shot-to-shot weight repeatability on a 12-cavity long-stroke blow-moulding machine must remain within ±0.75% over 50 consecutive shots. Pre-blow pressure is 0.15–0.25 MPa and final blow is 0.45–0.60 MPa; mould chiller supply is set at 8–12 °C. If the chiller supply falls below 6 °C, condensation forms on the neck rings and the 24/410 neck inner diameter becomes unstable, leading to elevated lot rejection in vacuum decay leak testing under ASTM D4991-07. The formulation contains 0.5–1.0 wt% white titanium dioxide masterbatch, 0.05–0.10 wt% slip agent masterbatch, and 0.02–0.05 wt% antioxidant masterbatch. For a fluoride-containing mouthwash, the bottle is evaluated as a pharmaceutical primary component under USP <661.1>, and food-contact compliance is assessed under FDA 21 CFR 177.1520 and EU Regulation No 10/2011. Published data for E4012 at this parison diameter and die swell range is limited; processors establish the die gap through a design-of-experiments protocol using the batch certificate melt flow rate determined under ISO 1133-1:2022. Terminal product is a 500 mL personal care bottle with a 24/410 neck finish.

    Downstream routeExtruder/equipmentMelt temperatureCritical settingTest anchor
    10–30 L jerrican90 mm grooved-barrel, L/D 30:1205–210 °C meteringDie gap 1.8–2.2 mmASTM D2463-15
    200-L L-ring drum120–150 mm accumulator head215–225 °C dieProgrammed die gap 2.5–3.8 mmASTM D1693-15
    Chemical tote liner sheet90–120 mm barrier screw210–225 °C flat dieNip 350–500 N/cmEN 1186-1
    Monofilament strapping65–90 mm, 80/120/80 mesh190–215 °C meltDraw ratio 6:1–9:1ASTM D3950-23
    Corrugated conduit/ducting60–75 mm with corrugator215–230 °CVacuum −0.06 to −0.08 MPaISO 9969:2016
    500 mL personal care bottle35–55 mm, L/D 24:1–28:1195–210 °CDie gap 0.8–1.0 mmUSP <661.1>
    Free Quote

    Competitive Sinopec Maoming HDPE E4012 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HDPE E4012 is a high-density polyethylene grade produced at the Maoming petrochemical complex of China Petroleum & Chemical Corporation. The E4012 code identifies a grade within the manufacturer’s HDPE portfolio that is directed to extrusion blow moulding of rigid hollow articles, including industrial containers, chemical packaging, and automotive fluid reservoirs. Specification compliance is governed by the certificate of analysis issued with each production lot; certified melt mass-flow rate, density, mechanical properties, and additive stabilisation are the binding values rather than a single fixed literature datasheet. Under REACH Regulation (EC) No 1907/2006, the polymer molecule is not subject to registration, while monomers and additives are registered by their respective suppliers. Where food-contact use is intended, the converter is responsible for verification under Commission Regulation (EU) No 10/2011 or FDA 21 CFR 177.1520 as applicable.

    What Standardised Property Set Should a Converter Request for E4012?

    The specification benchmark for E4012 should be defined through internationally recognised test methods. Certified values supplied by the manufacturer are preferred over generic HDPE range tables because melt index and density are regulated within narrow production tolerances that are not always published for export grades. The following property fields form a standard technical acceptance plan.

    PropertyTest standardOperational relevance
    Melt mass-flow rateISO 1133-1:2022 at 190 °C and 2.16 kgControls extruder throughput, head pressure, and parison hang time in blow moulding.
    DensityISO 1183-1Affects stiffness, stacking resistance, and permeability of the finished container.
    Tensile stress at yieldISO 527-2Provides a short-term load-bearing benchmark for wall sections and handle geometries.
    Flexural modulusISO 178Correlates with top-load and panel stiffness in rigid packaging.
    Charpy notched impact strengthISO 179-1/1eAIndicates low-speed impact toughness and ductile-brittle behaviour at service temperature.
    Vicat softening temperatureISO 306/A50Sets an upper boundary for hot-fill, wash-down, and stacking under elevated temperature.
    Environmental stress-cracking resistanceASTM D1693Ranks resistance to detergent, bleach, and chemical stress-cracking in container service.

    Typical HDPE blow-moulding class ranges reported in public literature are density 0.950 g/cm³ to 0.965 g/cm³, tensile yield 22 MPa to 30 MPa, flexural modulus 900 MPa to 1500 MPa, and ESCR F50 values above 100 h in 10% Igepal under ASTM D1693 condition B. Melt mass-flow rates for extrusion blow moulding HDPE grades typically fall below 2.0 g/10 min at 190 °C and 2.16 kg. These ranges do not replace the supplier’s certified E4012 lot data.

    For extrusion blow moulding, the melt mass-flow rate alone is insufficient for process control. Capillary rheometry under ASTM D3835 can provide shear viscosity data at relevant die shear rates, while extensional or melt-strength data should be obtained for critical parison lengths above 500 mm. Typical HDPE melts in the conversion shear-rate range of 100 s⁻¹ to 1000 s⁻¹ exhibit pseudoplastic flow with a power-law index between 0.3 and 0.6. The exact value for E4012 varies with lot and temperature and should be obtained from the supplier or measured by capillary rheometry.

    Melt Strength, Parison Sag, and Accumulator-Head Boundary Conditions

    On an accumulator-head extrusion blow moulder with a grooved-barrel extruder from 80 mm to 120 mm diameter and an L/D ratio of 25:1, E4012 should be processed with the primary objective of maintaining parison geometry. Typical barrel setpoints for high-molecular-weight HDPE blow moulding are 180 °C to 210 °C, with head zones at 190 °C to 210 °C and mould temperatures at 10 °C to 30 °C. For a hang length of 600 mm, melt-temperature uniformity across the parison circumference must remain within ±2 °C to avoid wall-thickness drift. If surface melt temperature exceeds 215 °C, die-lip oxidation, gel streaks, and loss of parison uniformity become increasingly probable.

    Die swell is a controlling parameter. On a shuttle-type machine with a 60 mm extruder, a die swell change of 10 percentage points can move a 1.0 mm target wall by approximately ±0.1 mm. Higher-swell lots may require a smaller die gap or faster accumulator speed to prevent over-thick pinch-off welds and under-thick sidewalls. Lower-swell lots often require a wider die gap to maintain the desired wall after parison inflation.

    An extruder screw with L/D 24:1 to 30:1 and compression ratio 3.0:1 to 3.5:1 is typical for blow moulding HDPE. The use of a grooved feed section can increase output by 15% to 25% relative to a smooth-bore feed in high-molecular-weight HDPE processing. Screw speed and die gap should be adjusted so that melt pressure at the head remains stable; a variation of more than ±2.5 bar at constant screw speed may indicate feedstock moisture, feed-bridge blockage, or inconsistent screw temperature.

    Pre-drying is not normally required when the resin is stored in sealed hoppers at relative humidity below 60%. If surface moisture exceeds 0.05 wt%, a desiccant dryer at 80 °C for 2 h to 4 h is typical. Storage should avoid direct sunlight and repeated condensation cycling because surface moisture becomes entrained in the pellet feed and can generate splay, voids, or internal porosity in thick container walls.

    The interaction between processing conditions and environmental stress-cracking resistance is particularly significant for E4012 when articles are intended for surfactant-based liquids, agricultural chemicals, or bleach-containing formulations. ASTM D1693 condition B in 10% Igepal CO-630 provides a comparative ranking of stress-crack resistance, but it is not a quantitative service-life prediction. Frozen-in orientation from a low melt temperature can raise ESCR while reducing sidewall impact; elevated melt temperature can improve surface gloss but may lower ESCR. Converters should therefore qualify the final bottle, not the raw resin, using full-container hydraulic or stack-load testing and, where regulated, UN packaging protocols for dangerous goods.

    When E4012 Is Compared with Pipe and Injection-Moulding HDPE Grades

    The E4012 grade occupies a different specification space from pressure-pipe grades such as 5000S produced at the same site. A PE100 pipe resin is classified under ISO 9080 and ISO 12162 with long-term hydrostatic strength as the primary fitness-for-service criterion; E4012 is not supplied against hydrostatic design stress data and is not intended for pressure piping. Compared with high-flow injection-moulding HDPE grades with melt mass-flow rates above 4 g/10 min, E4012 is specified for lower-melt-index performance to retain parison stability. Compared with high-density film grades, E4012 does not need the same gel-count control or bubble-stability qualification, and it is not typically qualified under ASTM D1709 dart impact or ISO 527-3 film tensile protocols.

    HDPE categoryPrimary acceptance standardsE4012 positioning
    Pressure pipeISO 9080, ISO 12162Not specified; no long-term hydrostatic design classification.
    Injection mouldingISO 1133-1, ISO 527-2Lower target melt flow for melt strength; not suitable for high-speed injection filling without re-qualification.
    Blown filmASTM D1709, ISO 527-3Not optimised for thin-film bubble stability or gel control.
    Extrusion blow mouldingASTM D1693, ASTM D3835, ISO 527-2Primary application space; ESCR, melt strength, and die swell are controlling properties.

    Commercial use of E4012 is concentrated in extrusion blow moulding of containers from approximately 1 L to 200 L. Typical articles include detergent and cleaner bottles, agrochemical containers, automotive fluid reservoirs, and industrial pails. For a 5 L to 25 L container, wall thickness commonly ranges from 0.6 mm to 2.5 mm; the selected die gap and accumulator speed are adjusted to the melt-strength data of the incoming lot. In thick-wall industrial containers above 10 L, cooling time is governed by wall thickness, mould temperature, and polymer thermal diffusivity. Blow moulder output is therefore closely linked to the chosen mould cooling circuit and not solely to the resin melt index.

    Cooling time is dominated by wall thickness. For steel moulds at 15 °C, a 1.5 mm HDPE wall section commonly requires 40 s to 70 s cooling depending on tonne size and part geometry; a 4.0 mm wall can require 180 s or longer. Poor mould cooling circuit design, not polymer selection, is the principal cause of warpage in thick-wall containers.

    Production-scale failure modes reported in HDPE blow moulding include parison thinning caused by misaligned head tooling, pinch-off weld splitting due to excessive melt temperature, and cold slugs from low head-zone temperature. These are process-induced and can be resolved by die-centering, head-temperature correction, or accumulator-speed changes before rejecting the resin lot. Batch-to-batch variance in melt flow rate and density should be tracked against an internal reference lot. A shift in MFR greater than 10% relative to the reference may require adjustment of extruder screw speed, die gap, or accumulator pressure to maintain container weight.

    For bleach, detergent, and agrochemical formulations, full-bottle compatibility testing is required because ASTM D1693 class data cannot account for all bottle-processing effects. Published data for E4012 in specific chemical formulations may be limited, and no generic HDPE datasheet should be interpreted as a filled-container warranty. HDPE blow moulding grades of this class are typically run with clean regrind levels up to 20% to 30%; validation is required for E4012 because lot additive levels differ. Higher regrind levels may alter ESCR and impact and should be validated on the finished container. The feedstock should be free of paper, metal, and incompatible polymer contamination, particularly polypropylene and PVC, because these can create delamination or brittle welds.

    If the resin is converted on a line previously running PVC or acetal, a purge sequence with a lower-viscosity HDPE or MDPE purge compound is recommended because residual acidic decomposition products can catalyse polyethylene degradation and form carbonaceous deposits. E4012 should not be combined with pro-oxidant transition-metal stearates or with certain amine-containing additives that can interfere with the stabilisation package and accelerate colour change. Store E4012 in sealed containers or silos at ambient temperature below 35 °C and relative humidity below 60%. Avoid contact with copper, cobalt, or manganese stearates at elevated temperature, because transition-metal ions can catalyse oxidative degradation and reduce ESCR.

    During shutdown, purge the extruder and die head with a lower-viscosity HDPE or MDPE purge compound; do not allow molten E4012 to stagnate in the head at high temperature for extended periods, because gel formation and char can occur. The die head should be brought to a reduced holding temperature according to the machine builder’s procedure.