Sinopec Maoming Hdpe Dmdb8902

Sinopec Maoming HDPE DMDB8902

    • Product Name: Sinopec Maoming HDPE DMDB8902
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 509229
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.949 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.20 g/10 min
    Tensile Strength At Yield 26 MPa
    Elongation At Break >600%
    Flexural Modulus 1000 MPa
    Vicat Softening Temperature 125°C
    Brittleness Temperature <-70°C
    Environmental Stress Cracking Resistance >1000 h
    Hardness Shore D 60
    Melting Point 130°C
    Crystallinity 70-80%
    Water Absorption <0.01%
    Volume Resistivity >10^16 Ω·cm
    Dielectric Constant 2.3
    Thermal Conductivity 0.4 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2×10^-4 /°C

    As an accredited Sinopec Maoming HDPE DMDB8902 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE DMDB8902 packed in 25 kg PP woven bags, 1,000 kg per pallet, 20 pallets per 20-foot container.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Sinopec Maoming HDPE DMDB8902 in palletized bags, securely strapped and shrink-wrapped for sea export.
    Shipping Sinopec Maoming HDPE DMDB8902 is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg woven bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Not classified as dangerous goods. Transport in dry, clean containers or trucks. Store cool, dry, ventilated, away from sunlight, heat, and moisture.
    Storage Store Sinopec Maoming HDPE DMDB8902 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep bags or containers tightly sealed, clean, and undamaged. Protect from moisture, dust, oils, and incompatible oxidizers. Use pallets, avoid stacking damage, and follow first-in, first-out stock rotation. Maintain clear labels and good ventilation.
    Shelf Life Sinopec Maoming HDPE DMDB8902 shelf life: 24 months in unopened original packaging, stored cool, dry, ventilated, away from direct sunlight.
    Application of Sinopec Maoming HDPE DMDB8902

    In the tight-head 200 L/220 L chemical drum segment, Sinopec Maoming DMDB8902 is processed on accumulator-head extrusion blow molders with shot capacities of 8–25 kg because parison stability at wall thicknesses of 3.0–5.5 mm depends on a high-molecular-mass, broad-molecular-weight-distribution HDPE. The production process uses a grooved-feed extruder of 90–120 mm diameter and L/D 24:1–30:1, a diverging accumulator head programmed for axial wall-thickness control, melt temperature 200–225 °C, mold temperature 10–40 °C, and blow pressure 0.6–0.9 MPa. Cycle time for a 200 L tight-head drum is typically 180–300 s depending on cooling fixture design; post-mold shrinkage fixtures are used to control top and bottom thread dimensions. Typical charge formulation is 70–85 wt% virgin DMDB8902, 15–30 wt% clean post-industrial regrind from deflashed domes and pinch-off, 1.5–2.5 wt% carbon black masterbatch, and 0.3–0.6 wt% antioxidant masterbatch. If antistatic packaging is required, conductive carbon black masterbatch is added at 5–10 wt% to achieve surface resistivity below 10^6 Ω measured by IEC 61340-2-3. Drum certification follows UN Model Regulations Chapter 6.1 for performance-oriented packaging; the marking normally includes the 1H1 designation for a non-removable-head plastics drum, the packing-group rating, a specific gravity or maximum gross mass, the hydrostatic test pressure, and the year of manufacture. The relevant destructive tests include drop, leakproofness, hydraulic pressure, and stacking under 49 CFR 178.604 and corresponding ADR/RID/IMDG provisions. For chemical drums exposed to aggressive solvents, the required environmental stress-cracking resistance is commonly assessed by ASTM D1693-15 Condition B; ESCR values of 600–1,000 h are typical for this application class. Production-scale failure modes appear as cold weld lines at the pinch-off zone when mold temperature falls below 10 °C, or as thinning at the drum shoulder when the parison programmer does not compensate for the top-to-bottom diameter transition. Batch-to-batch high-load melt index variation greater than ±15% from the certificate of analysis can produce wall-thickness deviation of 0.5–1.0 mm at the bottom chime and requires adjustment of melt temperature or screw speed.

    UN package testReference clauseTypical production-scale acceptance criterion
    DropUN Model Regulations 6.1.5.3No leakage after free-fall drop from 1.2 m onto rigid target
    LeakproofnessUN Model Regulations 6.1.5.4No leakage at 20 kPa internal air pressure for 30 min
    Hydraulic pressureUN Model Regulations 6.1.5.5No rupture or leakage at designated packing group test pressure
    StackingUN Model Regulations 6.1.5.6No deformation causing leakage after 28 days at 40 °C under calculated load
    Environmental stress-cracking resistanceASTM D1693-15No cracking at 600 h minimum for hazardous-chemical grades

    When 1000L Rigid Plastics IBC Bottles Are Blow Molded in Composite Packaging

    For the 1000 L composite IBC inner bottle, DMDB8902 is processed at shot weights of 20–45 kg, which exceeds the capability of most shuttle blow molders and requires a dedicated accumulator-head machine with a 120–150 mm extruder, L/D 24:1–30:1, and a first-in first-out accumulator of 20–60 kg capacity. Melt temperature is typically 210–230 °C, mold temperature 10–30 °C, and blow pressure 0.7–1.0 MPa; the parison programmer is configured to maintain the top, center, and bottom wall sections at 2.5–5.0 mm to avoid thinning at the shoulder and bottom corners. The charging formula for black or coloured IBC bottles consists of 75–100 wt% DMDB8902, 0–25 wt% clean regrind, 1.0–2.5 wt% colour masterbatch, and 0.5–1.0 wt% UV masterbatch when the bottle is intended for prolonged outdoor storage. Regrind with surface moisture above 0.1 wt% must be dried or passed through a vented hopper; otherwise pinholes and surface splay appear on the inner bottle wall. Certification is governed by the UN Model Regulations Chapter 6.5 provisions for rigid plastics IBCs and by 49 CFR 178.705; the container is marked as 31H1 or 31H2 depending on structural configuration, with performance tests covering bottom lift, top lift, stacking, leakproofness, hydraulic pressure, and drop. Terminal products include the inner bottle of 1000 L composite IBCs for water-based emulsions, liquid fertilisers, industrial cleaners, and non-flammable chemical intermediates; the resin is not applied to high-permeation solvents without a barrier layer or surface treatment because HDPE alone does not provide sufficient permeation resistance for Class 3 flammable liquids in all UN packaging groups.

    Six-layer coextrusion blow molding of automotive fuel tanks uses DMDB8902 as the virgin HDPE skin and inner layers where high environmental stress-cracking resistance, weld-line integrity, and melt-strength stability under repeated six-layer parison formation are required. The layer distribution in a typical 6-layer structure is 15–20 wt% outer HDPE skin, 30–40 wt% regrind layer, 1.5–2.5 wt% adhesive tie, 1.5–3.0 wt% EVOH barrier, 1.5–2.5 wt% adhesive tie, and 15–20 wt% inner HDPE skin; DMDB8902 is used in the outer skin and the regrind matrix. The coextrusion blow molder uses six separate extruders feeding a multi-layer accumulator head with individual melt temperatures of 210–240 °C, a die gap of 1.5–3.0 mm, and blow pressure of 0.8–1.2 MPa; parison programming is critical because the tank wall must be 3.0–7.0 mm at corners and pinch-off areas. The regrind stream is generated from pinch-off flash, punched-out filler-neck holes, and rejected tanks; feeding regrind above 40 wt% of the total tank mass can reduce low-temperature impact strength measured by ASTM D256-10 and ESCR measured by ASTM D1693-15, so the regrind fraction is controlled gravimetrically. Fuel tank qualification follows ECE R34 Annex 4 fire-resistance requirements for plastic fuel tanks, FMVSS 301 fuel system integrity for the North American market, and SAE J2587 for automotive fuel system components; material approval also includes tensile testing per ISO 527-2:2012 and high-load melt index per ISO 1133-1:2022 on each lot. Production-scale failures observed in six-layer tank blow molding include weld-line splitting at the pinch-off when regrind exceeds 45 wt%, and pinholing near the parison seam when the accumulator head temperature drops below 200 °C. Published data for DMDB8902 in six-layer automotive fuel tank regrind structures is limited; qualification on the exact coextrusion line with production regrind is required before lot approval. Terminal products are seamless blow-molded fuel tanks for passenger cars, light commercial vehicles, and off-road equipment where monolayer HDPE would fall below hydrocarbon permeation thresholds.

    LayerMaterial functionTypical thickness shareCritical material requirement
    Outer skinImpact absorption and stone-chip resistance15–20%DMDB8902 plus 2.0–3.0% carbon black masterbatch
    Regrind coreRecycle trim and maintain stiffness30–40%Maximum 40% regrind; ESCR per ASTM D1693-15
    Tie layerAdhere EVOH to HDPE3–5%Maleic-anhydride-grafted adhesive
    BarrierHydrocarbon permeation barrier1.5–3.0%EVOH with controlled ethylene content
    Tie layerAdhere EVOH to inner HDPE3–5%Maleic-anhydride-grafted adhesive
    Inner skinChemical resistance and weld integrity15–20%DMDB8902 with no regrind for fuel-contact critical applications

    What Limits Continuous Outdoor Exposure in Blow-Molded Aquaculture Floats?

    For aquaculture cage collars, dredging pipeline floats, and pontoon flotation modules, DMDB8902 is processed at shot weights of 10–40 kg into hollow bodies with wall thicknesses of 6–15 mm; the production line uses a 90–150 mm accumulator-head blow molder and cooling fixtures that maintain internal air pressure during the first 30–60 s of cooling to control shrinkage and weld-line flatness. The charge formulation for UV-stable floats is 70–90 wt% virgin DMDB8902, 10–25 wt% regrind, 2.0–4.0 wt% hindered-amine light stabilizer/UV masterbatch, and 1.0–2.0 wt% carbon black or pigment masterbatch; carbon black dispersion is checked by ISO 18553:2002 to avoid agglomerates that form stress concentrations in the weld seam. The production process avoids direct adhesion of multiple parisons unless they are fusion-bonded in a closing mold with a defined pinch-off land; for large floats, welding is controlled by maintaining pinch-off temperature above the crystalline melting range and by avoiding contamination from oxidized regrind. Performance under wet-immersed outdoor service is assessed by ASTM D638-14 tensile yield and elongation, ASTM D256-10 notched Izod impact after 1,500–2,000 h accelerated weathering per ISO 4892-2:2013, and ASTM D1693-15 ESCR; typical validation requires less than 25% loss of elongation at break after aging. UV stabilizer overfeeding above 4 wt% can reduce interlayer weld strength, while underfeeding produces surface cracking within the first 12–24 months of tropical or high-UV exposure. Terminal products include blow-molded floating pipes, aquaculture cage collars, and modular pontoon floats used in marine and freshwater environments.

    Blow-molded water treatment and chemical storage tanks in the 30–1,000 L range are a separate downstream segment for DMDB8902 because the resin’s high melt strength permits consistent wall thickness in vertical cylindrical tanks with integrally molded fittings and baffles. The production process uses an accumulator-head machine with shot capacity matched to the tank volume; melt temperature is 200–225 °C, mold temperature 10–35 °C, blow pressure 0.6–0.9 MPa, and programmed wall thickness 3.0–8.0 mm to reinforce sidewall seams, chime areas, and threaded bungs. The formulation for potable water contact is 75–100 wt% DMDB8902, 0–20 wt% clean regrind, 1.5–2.5 wt% white or coloured masterbatch, and 0.3–0.5 wt% antioxidant masterbatch; potable-water grades must comply with NSF/ANSI/CAN 61 and with 21 CFR 177.1520 for food-contact olefin polymers, while chemical dosing tanks are assessed under ASTM D1998-15 for upright storage tanks. Terminal products include water softener brine tanks, reverse-osmosis storage tanks, chemical dosing tanks, and acid/alkali neutralization tanks used in building services and light industrial water treatment. The same blow molding line can be changed between tank sizes by replacing the mold and parison program, but the accumulator head shot capacity must be at least 1.3× the finished part weight to avoid excessive melt residence time and molecular degradation.

    Diesel Exhaust Fluid Reservoir Blow Molding and Urea Compatibility

    Diesel exhaust fluid reservoirs for selective catalytic reduction systems are blow molded from DMDB8902 where cycle-level resistance to 32.5 wt% urea solution, freeze-thaw cycling, and road-vibration loads are required. The processing window is 200–230 °C melt temperature, 10–40 °C mold temperature, 0.6–0.9 MPa blow pressure, and programmed wall thickness of 2.5–5.5 mm; 3D blow molding or suction blow molding is used for the complex routing around coolant lines and vehicle body constraints. The filling formulation is 70–90 wt% virgin DMDB8902, 10–30 wt% regrind, 1.0–2.5 wt% carbon black or grey masterbatch, and 0.3–0.5 wt% antioxidant masterbatch; bright-white reservoirs may use titanium-dioxide-based masterbatch at 2.0–4.0 wt% to improve visibility of the fluid level. Material compliance is driven by ISO 22241-1:2019 for urea solution quality, ISO 22241-3:2019 for handling, transportation, and storage components, and automotive OEM material specifications that include heat aging at 80–100 °C in air and in 32.5 wt% urea solution, followed by tensile property retention testing per ISO 527-2:2012. Terminal products are blow-molded DEF tanks integrated with fill lines, vent valves, and level sensors for commercial and light-duty diesel vehicles.

    Free Quote

    Competitive Sinopec Maoming HDPE DMDB8902 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming Petrochemical’s HDPE DMDB8902 is a pelletised high-density polyethylene injection-moulding resin. The manufacturer’s technical bulletin lists a nominal melt flow rate of 8.0 g/10 min at 190 °C under 2.16 kg load when tested according to ASTM D1238, and a nominal density of 0.956 g/cm³ when tested according to ASTM D1505. Under ISO 1872-1, this positions the material as a high-flow HDPE for multicavity thin-wall moulds where injection pressure, cycle time and part weight must be controlled simultaneously. The product is not intended for blow moulding or pressure-pipe extrusion. Its melt rheology differs from Sinopec Maoming DMDA-8008, a blow-moulding grade quoted at 0.8 g/10 min under the same 190 °C/2.16 kg conditions, by trading melt strength for lower cavity-pressure loss. Typical downstream uses include crates, totes, storage bins, pallets, caps and closures, and rigid houseware. Lot-specific certificates of analysis should be requested because thermoplastic nominal values are not guaranteed specification limits.

    What distinction separates DMDB8902 from low-MFR blow-moulding grades in cavity filling and part design?

    The primary difference is rheological. A melt flow rate of 8.0 g/10 min reduces pressure drop through sprues, runners and gates relative to 0.8 g/10 min blow-moulding HDPE. That permits thinner nominal walls, longer flow-length-to-wall-thickness ratios and lower clamp-force requirements for the same projected area. The penalty is lower extensional viscosity at parison-forming temperatures, which is why DMDB8902 is unsuitable for blow moulding where parison sag and wall-thickness control are governed by melt strength. The table below compares the two Sinopec Maoming grades using manufacturer bulletin values and intended conversion process.

    Property or attributeDMDB8902DMDA-8008
    Nominal melt flow rate, 190 °C/2.16 kg8.0 g/10 min0.8 g/10 min
    Test methodASTM D1238ASTM D1238
    Nominal density0.956 g/cm³0.957 g/cm³
    Primary conversion routeInjection mouldingExtrusion blow moulding
    Rheological design emphasisLow cavity-pressure loss, rapid fillingHigh melt strength, parison stability
    Typical article geometryThin-wall crates, totes, caps, rigid housewareBottles, containers, small drums

    Compared with PE100 pipe-grade HDPE, DMDB8902 has a much higher melt flow index and lower molar mass. Pipe resins are typically bimodal HDPE grades with melt flow rates below 0.3 g/10 min at 190 °C/5 kg, designed for long-term hydrostatic strength and slow crack growth resistance under ISO 9080 and ISO 13479. DMDB8902 does not satisfy PE100 classification and should not be used for pressure-pipe applications. Compared with high-flow injection grades such as DMDA-8920, where manufacturer bulletins cite nominal melt flow rates near 20 g/10 min, DMDB8902 offers a middle processing window with generally better stiffness retention and lower mould shrinkage sensitivity in thicker sections, although published property data for all such comparisons should be verified with the supplier.

    On hydraulically clamped injection-moulding machines of 1,200 kN to 2,500 kN, DMDB8902 is usually processed at melt temperatures from 190 °C to 220 °C and mould temperatures from 20 °C to 40 °C. These are class-typical starting conditions for HDPE with a melt flow rate near 8.0 g/10 min; published data for DMDB8902 in specific multicavity tools is limited and tool-specific optimisation is required. A general-purpose screw with 20:1 to 25:1 L/D and compression ratio of 2.5:1 to 3.0:1 provides stable metering. Pre-drying is not normally required when the original sacks remain sealed; if exposure to condensation or relative humidity above 60% occurs, drying at 75–80 °C for 2–3 h in a desiccant dryer with dew point below -20 °C reduces surface defects. Residence time above 220 °C should be kept below 5 min to suppress chain scission and yellowing. Purging after thermal excursions with a lower-MFR HDPE or general-purpose PP is recommended.

    When DMDB8902 replaces random copolymer polypropylene in rigid storage containers

    Substitution of random copolymer polypropylene with DMDB8902 changes flexural modulus, heat deflection and low-temperature impact behaviour. HDPE injection grades in this density range commonly show flexural modulus values of 1000–1200 MPa under ASTM D790 or ISO 178, whereas many random copolymer PP grades fall in the 900–1300 MPa interval depending on comonomer content. Part stiffness is also controlled by wall thickness and moulded-in stress. Heat deflection temperature under 0.455 MPa load according to ASTM D648 for HDPE is generally in the range of 65–80 °C, below polypropylene homopolymer values typically above 90 °C. Therefore stacking under load in hot environments must be revalidated if PP is replaced by DMDB8902. Low-temperature impact performance under ISO 6603 or ASTM D3763 usually favours HDPE because it retains ductile response at subzero temperatures where PP can become brittle. The replacement is therefore appropriate when low-temperature durability and processability are critical, but it is not a direct drop-in for hot-fill, retort, or elevated-temperature top-load specifications.

    Gate dimensions for this MFR class may be smaller than for low-MFR HDPE, but not as small as for high-flow PP. For crates and totes, edge gates or fan gates of 1.5–2.5 mm wall thickness are common. Caps and closures may use pin gates of 0.8–1.2 mm diameter if gate freeze-off is controlled by short hold time. Parting-line vent depths for HDPE are typically 0.02–0.03 mm. Full-round runner channels of 4–6 mm diameter reduce pressure loss in cold-runner tools. Hot-runner systems with 6–8 mm manifold channels and thermal gating require closed-loop tip temperature control to prevent drool. Packing pressure of 50–70 MPa and hold time of 0.5–2 s per mm of nominal wall are used to minimise sink marks in thick bosses. These numerical ranges are tooling rules for high-flow HDPE and are not resin-specific guarantees; mould-flow simulation with measured DMDB8902 viscosity data is necessary for final gate and runner layout.

    ESCR, chemical compatibility and quality-control verification

    Environmental stress crack resistance for HDPE is commonly tested according to ASTM D1693. DMDB8902 is an injection-moulding product and should not be compared with bimodal PE100 pipe resins, which are specifically optimised for slow crack growth resistance under ISO 13479 and long-term hydrostatic strength under ISO 9080. For crates, totes and industrial containers exposed to detergents, oils or weak acids, finished-article testing is required because moulded-in residual stress and processing history often dominate stress-crack failure more than resin selection alone. The grade is not recommended for prolonged immersion in strong oxidising acids, aromatic hydrocarbons, or chlorinated solvents at elevated temperature. Food-contact suitability must be confirmed for the specific lot and colour package; relevant standards include FDA 21 CFR 177.1520, EU 10/2011 and GB 9685. Colour masterbatch can lower stiffness and ESCR; let-down ratios above 4 wt% should be pre-tested on the intended tool.

    Incoming resin should be stored in unopened bags at 20–30 °C in a dry roofed warehouse. Bags exposed to ultraviolet radiation or moisture may need drying before processing. Certificate-of-analysis checks should include melt flow rate, density, and lot-to-lot colour shift. When DMDB8902 is run in hopper loaders with long conveying lines, pellet fracturing and dust formation can create feed instability; low-speed vacuum conveying with minimum bend radii is preferable. The material should not be blended with amine-based hindered amine light stabiliser masterbatches without evaluating additive interactions, because certain amine chemistries can generate surface bloom at high processing temperatures. Published data for this specific grade in long-term ultraviolet exposure is limited; outdoor applications generally require adequate carbon black or UV stabiliser loading verified by ISO 4892 weatherometer testing.