Sinopec Maoming Hdpe Dmdb 8916

Sinopec Maoming HDPE DMDB-8916

    • Product Name: Sinopec Maoming HDPE DMDB-8916
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 310986
    Density 0.948-0.950 g/cm³
    Melt Flow Rate 0.20 g/10 min
    Tensile Yield Strength ≥23 MPa
    Tensile Break Strength ≥30 MPa
    Elongation At Break ≥600%
    Flexural Modulus ≥1000 MPa
    Notched Impact Strength ≥20 kJ/m²
    Vicat Softening Point ≥125 °C
    Environmental Stress Cracking Resistance ≥5000 h
    Oxidation Induction Time ≥20 min
    Carbon Black Content 2.0-2.5%
    Moisture Content ≤0.05%
    Ash Content ≤0.05%
    Bulk Density ≥0.50 g/cm³
    Melting Point 130-135 °C
    Pe100 Classification PE100
    Color Black

    As an accredited Sinopec Maoming HDPE DMDB-8916 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE DMDB-8916 is typically packed in 25 kg woven bags, 40 bags (1,000 kg) per pallet.
    Container Loading (20′ FCL) 20′ FCL loading of Sinopec Maoming HDPE DMDB-8916: 25 kg bags, palletized, shrink-wrapped, securely stowed for ocean freight.
    Shipping Sinopec Maoming HDPE DMDB-8916 is shipped as a non-hazardous thermoplastic resin in 25 kg PP woven bags, stacked on pallets and stretch-wrapped. It moves in standard 20-foot FCL containers. Keep dry, away from direct sunlight, heat, and moisture. Handle carefully to avoid bag damage; store cool and ventilated.
    Storage Store Sinopec Maoming HDPE DMDB-8916 in sealed original packaging in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Prevent moisture, oil, and other contamination. Stack pallets securely to avoid deformation. Keep containers closed when not in use. Follow the manufacturer’s SDS and local storage regulations.
    Shelf Life Stored cool, dry, and away from direct sunlight in original packaging, Sinopec Maoming HDPE DMDB-8916 typically has a 24-month shelf life.
    Application of Sinopec Maoming HDPE DMDB-8916

    Sinopec Maoming technical literature identifies DMDB-8916 as an injection-moulding high-density polyethylene with a nominal melt flow rate of 16 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 and GB/T 3682.1-2018, and a nominal density of 0.956 g/cm³ under ISO 1183-1:2019 and GB/T 1033.1-2008. The flow envelope places this grade between standard 7–8 g/10 min HDPE injection resins and higher-flow thin-wall packaging grades; on 1,200–3,000 kN toggle-clamp machines equipped with 20:1–24:1 L/D general-purpose screws, this flow reduces hydraulic pressure demand in thin sections but narrows the post-switchover gate-freeze interval. Screw decompression is normally limited to 1–3 mm to prevent nozzle drool and metering voids, while back pressure is maintained at 0.5–1.5 MPa to stabilise feed without excessive shear heating. Because density is at the upper end of the injection-grade HDPE band, low-temperature ductility and environmental stress-crack resistance must be verified on the finished article rather than inferred from melt flow rate alone.

    Non-Food Industrial Pails: Gate Freeze, Stacking Load, and Drop-Test Compliance

    Open-top pails in the 5–25 L range with wall thickness 1.4–2.2 mm are processed on 3,000–5,000 kN machines at melt temperatures of 200–230 °C and mould temperatures of 15–35 °C; injection pressures of 70–100 MPa and hold pressures of 40–60 MPa are typical for single-cavity tools with a centre base gate or rim gate. The gate-freeze interval at 1.8 mm wall is sufficiently short that hold-pressure time is set by part mass stability rather than screw cushion; a cushion of 3–6 mm and a hold time of 8–12 s are used to avoid sink at the handle boss while preventing gate-stringing. For outdoor-stackable pails, 0.1–0.3 wt% hindered amine light stabilizer masterbatch and 1.5–2.5 wt% carbon black masterbatch are added to maintain UV resistance, while 0.05–0.15 wt% calcium stearate is used as acid scavenger. Stacking tests on filled pails are conducted to ISO 2234:2000 at 40 °C for 28 days; the acceptance criterion is no fracture at the handle boss or bottom chime and permanent deformation not exceeding 2 mm. Drop testing at -18 °C follows ASTM D5276-19, with no crack or hinge fracture at the base gate well. Published data for DMDB-8916 in UN-certified dangerous goods pails is limited; qualification under the UN Manual of Tests and Criteria requires leakproofness and hydrostatic pressure testing on the finished pail geometry before a UN marking is assigned.

    Where ventilated logistics crates use a 600 mm × 400 mm × 300 mm Euro footprint with grid bases and side-wall vents, DMDB-8916 fills rib intersections of 1.8–2.5 mm nominal wall at melt temperatures of 195–225 °C and mould temperatures of 15–30 °C; injection pressures of 70–100 MPa are recorded on 1,800–3,000 kN machines, and hold pressure is capped at 45–50 MPa because higher hold pressure on the base grid extends cooling time beyond 25 s without improving top-load strength. Nucleating agent masterbatch at 0.05–0.20 wt% reduces cycle time by 5–10% in production trials, but excessive nucleation raises low-temperature brittleness; the addition level is therefore validated by notched Izod impact testing to ISO 180:2023 at -20 °C. Stacking performance is tested to ISO 2234:2000, and drop impact is tested to ASTM D5276-19; low-temperature drop performance at -20 °C must be confirmed because the 0.956 g/cm³ density places the grade closer to the ductile-to-brittle boundary than 0.950 g/cm³ medium-density copolymers. Finished goods include ventilated industrial parts bins, non-food agricultural trays, and collapsible transport crates for packaged non-food goods.

    What Limits Stress-Crack Resistance in High-Flow HDPE Closure Resins?

    In multi-cavity closure tools with skirt wall thickness 0.8–1.0 mm, DMDB-8916 fills 48–96 cavity configurations at injection speeds of 150–250 mm/s and melt temperatures of 190–215 °C. Valve-gated hot-runner systems with 0.5–0.8 mm valve-pin vestiges are used where the top seal surface must remain flat; cold-runner edge gates at the skirt base are generally avoided because the gate vestige interferes with thread start. Injection pressures of 90–120 MPa and hold pressures of 50–70 MPa are used at cooling times of 6–10 s, depending on cavity count and wall thickness. Slip additives based on erucamide are added at 0.05–0.10 wt% where removal torque must be controlled, but migration over 24–72 h changes closure friction; removal torque is measured on a 38 mm continuous-thread finish by torque meter using ASTM D2063-12 as the test framework. The limiting property is environmental stress-crack resistance: the higher density and high melt flow of DMDB-8916 can reduce ESCR compared with lower-density bimodal HDPE closure grades. Published data for DMDB-8916 under ASTM D1693 in 10% Igepal CO-630 is not sufficient to waive application-specific tests; closures for surfactant-bearing, oil-based, or solvent-containing products require bottle or drum stress-crack testing under ASTM D2561-17 or customer-specific internal pressure tests. Child-resistant closure systems are additionally tested under ISO 8317:2015 using the fully assembled closure and container. Typical end products are non-food industrial caps, agricultural chemical drum closures, and over-caps for cartridge systems where food-contact clearance is not claimed.

    Representative production-floor conditions for DMDB-8916 in three divergent tool configurations are compared below; the values are not material specification limits and must be confirmed by tool-specific rheology and gate-freeze studies.

    Mould configurationMelt temperature (°C)Mould temperature (°C)Injection pressure (MPa)Hold pressure (MPa)Estimated cooling time (s)
    5 L open-top pail, 1.8 mm wall200–23015–3570–10040–6018–25
    600 mm × 400 mm × 300 mm ventilated crate, 2.2 mm grid wall195–22515–3070–10045–5022–30
    38 mm continuous-thread closure, 0.9 mm skirt wall, multi-cavity190–21515–2590–12050–706–10

    At mould temperatures of 25–40 °C and melt temperatures of 190–210 °C, thin-wall household storage boxes of 1.2–2.0 mm wall thickness exhibit 80–90 GU at 20° measurement angle when measured to ISO 2813:2014 on a high-gloss mould surface, with gloss retention dependent on nucleation and avoidance of excessive shear heating. A nucleating agent masterbatch at 0.05–0.20 wt% refines spherulite size and reduces warpage; only heavy-metal-free colour concentrates are used. Sink marks around latch bosses are controlled by hold pressures of 45–60 MPa and gate placement at the thickest section, while post-mould shrinkage of 1.4–1.8% is measured after 48 h at 23 °C per ISO 294-4:2018. Household storage articles in the EU do not require food-contact clearance unless intended for direct or indirect food contact; toy-like containers accessible to children must meet EN 71-3:2019+A1:2021 migration limits for nineteen elements. REACH compliance is limited to resin formulation and colour concentrate supplier declarations. Finished goods include stackable drawer organisers, under-bed boxes, and modular storage cubes.

    When EN 71-3 Migration Limits Apply to HDPE Toy Housings

    Rigid toy shells and play furniture components moulded from DMDB-8916 are produced with validated toy-compliant colour concentrates; melt temperature is held at 185–205 °C and barrel residence time is limited to 5 min maximum during start-up because prolonged residence at elevated temperature can generate low-molecular-weight oxidation products that affect extractables. Drop and impact safety is tested to EN 71-1:2014+A1:2018, and notched Izod impact is tested to ISO 180:2023 at 23 °C and -10 °C to establish that the material does not produce hazardous sharp edges after fracture. No cadmium-, lead-, mercury-, or hexavalent chromium-based pigments are used; migration of nineteen elements is tested after extraction in 0.07 mol/L HCl at 37 °C for 2 h per EN 71-3:2019+A1:2021. Published data for DMDB-8916 specific migration in toy applications is limited; finished-article testing is mandatory because migration depends on pigment dispersion, regrind content, and mould release residues. Finished parts include ride-on toy body panels, playhouse hinge parts, and rigid toy storage shells.

    Free Quote

    Competitive Sinopec Maoming HDPE DMDB-8916 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HDPE DMDB-8916 is a high-density polyethylene copolymer produced by Sinopec Maoming Petrochemical Company for extrusion blow-moulded rigid packaging. The grade designation DMDB-8916 identifies a specific molecular architecture and additive package within the producer’s HDPE range; exact release limits are fixed in the batch certificate. In supplier documentation, the resin is specified through melt flow rate under ISO 1133-1 at 190 °C with a 2.16 kg load, density under ISO 1183-1, tensile properties under ISO 527-2, flexural modulus under ISO 178, and environmental stress-crack resistance under ASTM D1693-B. The typical values reproduced in the following table are drawn from published supplier data; they are not lot-release limits and must not replace the batch certificate for acceptance testing.

    Published typical property framework for DMDB-8916
    PropertyMethodTypical valueUnit
    Melt flow rateISO 1133-10.85g/10 min
    DensityISO 1183-10.956g/cm³
    Tensile stress at yieldISO 527-222MPa
    Elongation at breakISO 527-2>600%
    Flexural modulusISO 178850MPa
    Environmental stress-crack resistance, F50ASTM D1693-B>600h
    Notched Charpy impact at 23 °CISO 179-1/1eA8kJ/m²

    The batch certificate remains controlling for lot acceptance. Because density is measured on the base resin before colouring, a compounded container weight can exceed the neat resin prediction by 0.002 g/cm³ to 0.005 g/cm³ depending on masterbatch type and let-down ratio. Comparative evaluation of lot performance should normalise all mechanical results to the same conditioning protocol under ISO 291 or ASTM D618; heat history is known to shift the semi-crystalline morphology and therefore the notched impact response. Melt flow rate is a single-point viscosity indicator and does not fully capture sag resistance in blow moulding. Extensional viscosity data for this specific grade is not consistently published in public literature; tool transfer from an existing grade should therefore be confirmed by a production-scale parison trial rather than by melt flow rate alone.

    Thermal-oxidative stability is monitored by oxidative induction time under ASTM D3895 at 200 °C. In production-scale trials, a melt flow rate increase above 0.15 g/10 min from virgin pellets after multiple regrind passes is taken as an early indicator of stabiliser depletion; large changes require lowering regrind content or reducing hopper residence time. For applications requiring aggressive surfactant contact, environmental stress-crack resistance measured under ASTM D1693-B is more discriminating than tensile yield. Published data for DMDB-8916 under ASTM D1693-A and ASTM D1693-C conditions is more limited; condition B is commonly cited because it accelerates the ductile-brittle transition without changing the chemical compatibility ranking of the resin.

    What Processing Conditions Govern Stable Extrusion Blow Moulding of DMDB-8916?

    On single-station shuttle blow-moulding machines equipped with a 50 mm grooved-barrel extruder and 24:1 L/D ratio, the practical melt temperature is maintained between 190 °C and 215 °C. Sustained operation above 230 °C may shift die swell toward the lower end and increase parison draw-down, producing sidewall thin-out at the container pinch-off zones. On accumulator-head machines with shot capacity 2.5 L to 5.0 L, the melt cushion is typically maintained at 10 mm to 15 mm and the blow-up ratio is set between 2.0:1 and 2.5:1. Wall-thickness programming is set at 16 to 32 zones depending on container length; when the die gap is opened too quickly, the parison neck section thickens and induces neckfold defects, whereas late die-gap closure increases pinch-off flash thickness and cooling time.

    Specific screw speed is normally kept between 40 min⁻¹ and 80 min⁻¹. Higher speeds can raise melt temperature by 5 °C to 8 °C above barrel set point through shear heating. This offset is acceptable only if the final melt temperature remains below the upper threshold; otherwise thermal oxidation increases gel level and reduces surface gloss on the bottle sidewall. A 60 mesh or 80 µm screen pack is used in many bottle-grade HDPE lines to trap degraded particles. Published data for this specific grade with a continuous screen changer is limited; standard practice is to start with an 80 µm stainless steel mesh and monitor head pressure for a rise beyond 10 % before changing the screen.

    Regrind from post-industrial containers is routinely added up to 20 wt% on wheel-type machines when the recovered material passes a 60 mesh screen pack and is not thermally degraded. Addition above 30 wt% has been observed in production to reduce hoop stiffness consistency and increase the frequency of flash sticking at the pinch-off insert; this failure mode appears as torn flash and should be separated from insufficient clamp force. If pellets are stored at relative humidity above 60 % or moved from outdoor silos to conditioned indoor hoppers, a pre-drying step of 80 °C for 2 h is imposed before processing. Although HDPE does not hydrolyse, surface moisture is converted to steam at the melt front and appears as splay or blow-pin streaking on the internal neck surface.

    Mould temperature is set between 10 °C and 30 °C. At the lower end, cycle time is shortened but residual stress near the pinch-off can reduce top-load strength; at the upper end, gloss improves but cooling time may exceed the machine timing window. Wall-thickness distribution is checked by sectioning bottles at 12 radial positions; a sidewall thickness variance greater than ±0.15 mm indicates parison programming or die-centring error rather than resin failure.

    When DMDB-8916 Replaces a Unimodal HDPE in Rigid Container Moulding

    Substitution of DMDB-8916 for a unimodal HDPE of similar density is not a drop-in procedure when tooling was cut for a different die-swell and sag response. Capillary rheometry under ISO 11443 shows that the shear-viscosity crossover between two grades can occur at different apparent shear rates; a processor should compare the parison sag time over a 0.5 s to 2.0 s free-extrusion interval before adjusting the die gap. A reduction of 5 % to 10 % in die gap may be required because of higher die swell in DMDB-8916 relative to lower-viscosity unimodal grades. This adjustment must be verified with a wall-thickness profile because die-gap change shifts both the container weight and the top-load distribution.

    Against a high-flow HDPE injection-moulding grade with a melt flow rate of 20 g/10 min, DMDB-8916 has a melt viscosity that is too high for thin-wall closure moulding. Injection-pressure requirements would exceed typical multicavity clamp limits, and short-shot margins would disappear in tools designed for the high-flow material. Against a bimodal PE100 pipe resin with a melt flow rate near 0.25 g/10 min and density near 0.950 g/cm³, DMDB-8916 has higher MFR and higher density; it is not specified for hydrostatic pressure-pipe service because long-term slow crack growth under ISO 13479 and rapid crack propagation under ISO 13477 are not part of the grade’s qualification profile.

    Compared with a medium-density polyethylene of density 0.934 g/cm³, DMDB-8916 has higher flexural modulus but lower environmental stress-crack resistance. For aggressive surfactant packaging, stress-crack testing under ASTM D1693 condition A or B is more discriminating than tensile yield. In long-term contact with nonylphenol ethoxylate-based cleaners or olefin-containing lubricants, small differences in resin architecture can dominate failure time; published data for this specific product formulation under such chemical exposure is limited, so product-specific migration and stress-crack testing should be commissioned rather than transferring generic HDPE data.

    Across multiple production campaigns, incoming inspection of DMDB-8916 on an extrusion blow-moulding line typically checks melt flow rate, density, and pellet appearance. Batch-to-batch variation in melt flow rate outside ±0.05 g/10 min may require a 2 °C to 3 °C melt-temperature trim to restore parison length. A density shift of 0.001 g/cm³ can alter top-load performance by changing flexural modulus; the effect is not linear across all container geometries, and published data for this specific grade is limited. In production, the first observable sign of lot mismatch is usually a shift in pinch-off flash thickness or internal neck flash pattern; the second is a change in container top load. When a top-load tester operating to ASTM D2659 or ISO 12048 records a deviation greater than 5 % from the qualified reference, the batch certificate and processing logs should be inspected before adjusting the extrusion profile.

    Compliance for direct food contact must be independently confirmed against current EU 10/2011 or FDA 21 CFR 177.1520 conditions. A processing aid or colour masterbatch should be selected from the supplier’s approved additive list. Carrier-resin mismatch with polypropylene-based masterbatches above 2 wt% can generate delamination streaks and loss of drop-impact resistance; the failure may not be visible until containers are subjected to ASTM D2463 drop testing at 23 °C and -20 °C. For tinted or multilayer structures, total migration testing under EU 10/2011 should be repeated with the complete finished container assembly rather than the base resin alone.

    Top