    • Product Name: Sinopec Maoming HDPE DFDB8910
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 216614
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.18 g/10 min
    Tensile Strength At Yield ≥28 MPa
    Elongation At Break ≥600%
    Flexural Modulus ≥1100 MPa
    Vicat Softening Temperature ≥125 °C
    Brittleness Temperature ≤-70 °C
    Environmental Stress Cracking Resistance Escr ≥1000 h
    Hardness Shore D 65
    Molding Shrinkage 2.0-4.0%
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >10^16 Ω·cm
    Melting Point 130-135 °C

    As an accredited Sinopec Maoming HDPE DFDB8910 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE DFDB8910 packaging: 25 kg woven polypropylene bags, palletized and stretch-wrapped, with 1,000 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL loaded with Sinopec Maoming HDPE DFDB8910 in 25kg bags, palletized, shrink-wrapped, and securely stowed for export.
    Shipping Sinopec Maoming HDPE DFDB8910 ships as non-hazardous polyethylene pellets in 25 kg woven bags or 1000 kg jumbo bags, palletized and stretch-wrapped, in 20'/40' containers. Use clean, dry trucks/containers. Store cool, dry, ventilated, away from moisture, direct sunlight, heat, and ignition sources. Standard dry cargo handling applies.
    Storage Store Sinopec Maoming HDPE DFDB8910 in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, and moisture. Keep original bags sealed on pallets; avoid contact with acids, oxidizers, oils, and contaminants. Maintain ambient temperature; prevent static buildup and ignition sources. Do not overstack. Rotate stock and follow local regulations and the manufacturer’s SDS.
    Shelf Life Sinopec Maoming HDPE DFDB8910 has a recommended shelf life of 24 months under dry, cool, ventilated storage in original packaging.
    Application of Sinopec Maoming HDPE DFDB8910

    In blown-film conversion of high-molecular-weight HDPE for retail carrier bags, the governing compliance framework is GB/T 21661-2020, which specifies minimum thickness thresholds and physical performance categories for plastic shopping bags sold in the PRC market; parallel EU packaging obligations derive from Directive 94/62/EC and REACH Regulation (EC) No 1907/2006, with SVHC screening under Article 33. The base resin is typically formulated with a calcium carbonate masterbatch let-down ratio in the range of 15–25 wt% to raise modulus and reduce unit film mass without dropping below the mandatory minimum thickness of 0.025 mm for reusable bags; pigment masterbatches are added at 2–6 wt%, and a fluoropolymer processing aid is introduced at 0.02–0.1 wt% to suppress melt fracture on polished die lips. Compounding is conducted on a gravimetric batch blender feeding a single-screw extruder with a screw diameter of 45–65 mm and an L/D ratio of 25–30; the die gap is held at 0.8–1.2 mm, blow-up ratio between 3.0:1 and 4.5:1, and melt temperature between 180 °C and 210 °C. Frost line height is maintained at 5–8 die diameters to balance stalk stability and transverse direction tear resistance. Terminal products include bottom-sealed and side-welded T-shirt bags, flat merchandise bags, and pre-cut roll stock for automated packing lines.

    Production-scale behavior on a 50 mm grooved-feed extruder indicates that die-lip deposit formation accelerates when the calcium carbonate masterbatch carrier resin is an LLDPE with an MFI above 2.0 g/10 min; resulting transverse direction thickness variation exceeds ±8%, which directly impacts GB/T 21661-2020 minimum thickness compliance at the thinnest edge. Batch-to-batch variance in filler moisture above 0.1% by weight produces pinholing at the die exit when melt temperature falls below 185 °C. These effects are mitigated by adjusting the die gap to 1.0 mm and by using a dual-lip air ring with chilled air at 15–20 °C, but published data for this specific DFDB8910 lot configuration is limited; converter trials are necessary.

    What limits oxidative induction time in geomembrane welding seams?

    Landfill cells and tailings impoundments impose a primary specification of GRI-GM13 on HDPE geomembrane liners; the standard sets minimum values for sheet thickness (ASTM D5199), density (ASTM D1505), tensile properties (ASTM D638, Type IV, crosshead speed 50 mm/min), tear resistance (ASTM D1004), puncture resistance (ASTM D4833), stress-crack resistance via single-point notched constant tensile load (ASTM D5397), and oxidative induction time via differential scanning calorimetry at 200 °C under ASTM D3895. A carbon black content of 2.0–3.0% by weight is mandatory for ultraviolet stabilization, and dispersion must satisfy microscopic examination under ASTM D5596; typical masterbatch addition to reach this window is 4–6 wt% of a 40–50% carbon black concentrate, although the exact let-down is adjusted from lot-specific pigment assay. Antioxidant packages, usually blends of hindered phenols and phosphites, are formulated at 0.15–0.45 wt% to achieve an initial OIT above 100 min, while long-term durability is evaluated via high-pressure OIT under ASTM D5885 at 3.4 MPa and 150 °C.

    GRI-GM13 compliance checklist for DFDB8910 geomembrane liners
    PropertyTest methodSpecification clause
    Sheet thicknessASTM D5199GRI-GM13 Table 1
    DensityASTM D1505GRI-GM13 Table 1
    Tensile yield and breakASTM D638GRI-GM13 Table 1
    Tear resistanceASTM D1004GRI-GM13 Table 1
    Puncture resistanceASTM D4833GRI-GM13 Table 1
    Stress crack resistanceASTM D5397GRI-GM13 Table 1
    Oxidative induction timeASTM D3895GRI-GM13 Table 1
    Carbon black contentASTM D1603GRI-GM13 Table 1
    Carbon black dispersionASTM D5596GRI-GM13 Table 1

    Downstream production of HDPE geomembrane sheet typically involves a flat-die single-screw extruder with a screw diameter of 90–150 mm, an L/D ratio of 30–33, and a coat-hanger slot die adjusted to a gap of 1.0–2.5 mm; melt temperatures between 200 °C and 230 °C are maintained to avoid gels from undispersed carbon black, and a polished three-roll stack with roll temperatures of 60–80 °C controls sheet thickness to tolerances of ±10% from nominal. The sheet is wound in widths up to 8 m and joined on site by dual-track hot-wedge welding with seam peel and shear strength verified under ASTM D6392; a seam peel value below 80% of the sheet yield strength indicates inadequate heat input or surface contamination. Terminal product types include landfill basal and cap liners, leachate pond liners, canal liners, containment berms, and secondary containment pads for hydrocarbon storage areas.

    When the target filled mass exceeds 25 kg per sack and the transport route includes multiple handling drops, the film structure shifts from monolayer carrier bag geometry to a three-layer blown construction in which DFDB8910 occupies the core layer at 40–60 wt% of the total structure, and metallocene LLDPE skins at 20–30 wt% per layer provide dart impact resistance without reducing the 1% secant modulus below 600 MPa in the machine direction. The compliance framework for such heavy-duty shipping sacks is frequently driven by ISO 7965-2 for vertical impact drop testing and ISO 527-3 for tensile properties on film specimens; where the filling good is classified as a dangerous substance, the sack is normally used as an inner liner inside a UN-certified rigid outer packaging, and drop and stacking provisions of the UN Model Regulations apply to the assembled package, not to the film independently. Additive loading includes a hindered amine light stabilizer masterbatch at 2–4 wt% for outdoor storage, white pigment masterbatch at 4–8 wt% to maintain opacity on the outer layers, and a slip/antiblock masterbatch at 1–2 wt% in the skin layers to prevent blocking on the winder.

    Extrusion is performed on a three-layer blown-film line with extruder screw diameters of 50/70/50 mm, L/D ratios of 30, and a 200 mm spiral mandrel die with a die gap of 1.4–2.0 mm; the blow-up ratio is set at 2.5:1–3.5:1 because higher ratios reduce machine-direction tensile strength, which is critical for drop performance. Melt temperature is maintained at 190–215 °C, and the frost line is held at 6–9 die diameters above the die face to increase stalk cooling and bubble stability when processing a high-molecular-weight HDPE with a broad molecular weight distribution. On one production line using a 90 mm grooved-feed extruder, bubble sag between the die and the nip was observed when the blow-up ratio exceeded 4.0:1, leading to film gauge variation of ±12% and a 15% reduction in ISO 7965-2 drop height tolerance. Terminal products include valve sacks for polymer pellets, pinch-bottom open-mouth sacks for fertilizers, and inner liners for FIBC bulk bags.

    Food-contact liner film compliance under EU No 10/2011 migration testing

    For dry-food inner liners and bakery film applications, the resin must comply with the positive list in Annex I of Commission Regulation (EU) No 10/2011, with an overall migration limit of 10 mg/dm² for the final film and, where applicable, specific migration limits for additives under Table 2; US-market converters also invoke FDA 21 CFR 177.1520(c) paragraphs 2.1 and 3.1 for olefin polymers intended for contact with food, and China market products fall under GB 4806.7-2016 with total migration limits specified in GB 31604.1. Additive formulations are restricted to food-contact-approved grades: a phosphite/phenolic antioxidant blend is added at 0.08–0.20 wt%, erucamide slip at 0.05–0.15 wt%, and synthetic silica antiblock at 0.10–0.30 wt%, typically via a compounded masterbatch at a let-down ratio of 2–5 wt%. No post-consumer recycled material is incorporated into these structures because the threshold of 0.5% contamination cannot be reliably excluded without migration testing.

    Food-contact compliance matrix for HDPE DFDB8910 liner film
    RegulationScopeLimit / designation
    EU No 10/2011Overall migration10 mg/dm²
    US FDA 21 CFR 177.1520(c)Olefin polymersParagraphs 2.1 and 3.1
    China GB 4806.7-2016Food-contact plasticsTotal migration per GB 31604.1

    Processing for these inner liners takes place on a single-layer blown-film line with a screw diameter of 55–65 mm, L/D ratio of 28, and a die gap of 0.8–1.5 mm; melt temperature is limited to 180–220 °C to avoid degradation of the slip additive and to keep the overall migration potential below the EU limit. A blow-up ratio of 2.0:1–3.5:1 and a frost line height of 4–7 die diameters are used to maintain contact clarity and a low haze value below 20% when measured according to ASTM D1003. The winder is operated with taper tension not exceeding 0.3 N/mm to avoid blocking. Terminal products include cereal box inner liners, cracker and biscuit sleeves, dry powder pouch liners, and bread bag films with a typical thickness of 0.018–0.035 mm.

    When vapor barrier membranes are extruded below a 0.5 mm thickness

    Below-grade vapor barrier and underslab retarder membranes produced from HDPE DFDB8910 are specified under ASTM E1745, which establishes three classes—A, B, and C—based on water vapor permeance, tensile strength, and puncture resistance after laboratory conditioning; the test protocol uses ASTM E96/E96M desiccant method at 23 °C and 50% RH, ASTM D882 for tensile properties, and ASTM D1709 for impact. A film with thickness of 0.25 mm typically reports permeance below 0.1 perms in Class A applications, although published data for the specific DFDB8910 configuration is limited and must be confirmed on the final roll product. Additive loading consists of a carbon black masterbatch at 3–5 wt% to provide opacity and mild UV protection during construction exposure, and a process stabilizer at 0.05–0.10 wt%; no plasticizer or volatile component is introduced because ASTM E1745 requires negligible volatile loss after aging at 70 °C for 7 days.

    Extrusion is typically performed on a high-output blown-film line with a screw diameter of 75–100 mm, L/D ratio of 30–33, and a spiral mandrel die of 250–400 mm diameter with a gap of 1.0–1.8 mm; melt temperature is kept at 190–210 °C, and the blow-up ratio is widened to 3.0:1–4.0:1 to produce layflat widths of 2–4 m. Bubble stability is critical because a collapse in the frost line creates folds that later translate into pinholes under ASTM E1745 hydrostatic testing. On a production line with a 90 mm grooved-feed extruder, edge trim losses of 6–9% were recorded when slit widths exceeded 4 m, and the trim was reintroduced into the core layer at a maximum of 15 wt% to avoid reducing dart impact below the ASTM E1745 Class A minimum. Terminal products include underslab vapor retarders, crawl-space ground covers, concrete curing blankets, and temporary wall weather barriers.

    Across municipal waste collection contracts where fill weight rarely exceeds 12 kg but puncture threats include broken glass and metal edges, HDPE DFDB8910 is processed into blown film with a thickness range of 0.018–0.050 mm depending on sack strength class defined by EN 13592; the standard classifies sacks by nominal volume, thickness, and dynamic puncture resistance, and requires tensile strength and elongation testing under ISO 527-3. Formulation tolerates a post-industrial recycled HDPE fraction of 20–50 wt% sourced from edge trim and rejected rolls, plus a calcium carbonate masterbatch at 10–25 wt% to reduce resin cost while retaining tear resistance above 10 N/mm; carbon black masterbatch is added at 2–4 wt% for opacity, and a fluoropolymer processing aid at 0.02–0.05 wt% reduces die-lip deposits when the recycled fraction contains gel particles.

    Blown-film lines for refuse sacks use screw diameters of 65–100 mm, L/D ratios of 28–33, and die gaps of 1.2–1.8 mm with blow-up ratios between 3.0:1 and 5.0:1; melt temperature is set at 185–205 °C, and the frost line is positioned at 5–8 die diameters to maximize bag opening and flatness. When recycled content rises above 40 wt%, a screen pack of 120–200 mesh is installed in the breaker plate to trap unmelted particles, but this raises melt pressure by 15–20% and reduces output by 5–10% compared with virgin-only extrusion. Terminal products include municipal curbside collection bags, compactor bags for commercial kitchens, janitorial cart liners, and heavy-duty leaf and garden waste sacks with drawstring or flap-top closures.

    Free Quote

    Competitive Sinopec Maoming HDPE DFDB8910 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HDPE DFDB8910 is a pelletised high-density polyethylene resin manufactured by Sinopec Maoming Petrochemical and designated for blown-film extrusion. The DFDB prefix distinguishes this gas-phase film grade from DFDA linear low-density grades in the same production family, although public documentation does not consistently identify catalyst type or comonomer. Nominal density obtained under ISO 1183-1:2019 is 0.949 g/cm³, and melt mass-flow rate under ISO 1133-1:2022 at 190 °C and 2.16 kg is 0.10 g/10 min. That combination places the resin in the high-molecular-weight HDPE class; in capillary rheometry, zero-shear viscosity is substantially above that of extrusion grades with melt mass-flow rates between 0.30 g/10 min and 0.90 g/10 min. The molecular weight distribution is broad enough to promote bubble stability under high blow-up ratios, but the melt is not fluid enough for thin-wall injection moulding. The base pellet does not appear to contain intentionally added slip or antiblock agents; the additive package should therefore be verified against the supplier certificate of analysis before downstream automated bag-making or printing lines are commissioned.

    Which nominal property envelope applies to DFDB8910?

    The values below are drawn from published Sinopec Maoming technical literature and represent circular-die film samples unless otherwise stated. They are not absolute specification limits; converters should treat them as lot-averaged targets and confirm batch-specific data with the certificate of analysis. Film properties are strongly dependent on die gap, blow-up ratio, frost line height, and melt temperature.

    PropertyNominal valueTest method
    Melt mass-flow rate, 190 °C / 2.16 kg0.10 g/10 minISO 1133-1:2022
    Density0.949 g/cm³ISO 1183-1:2019
    Tensile stress at yield, 50 µm blown film, machine direction22 MPaISO 527-3:2018
    Elongation at break, 50 µm blown film, machine direction600%ISO 527-3:2018
    Dart impact strength F50, 25 µm film150 gISO 7765-1:2004
    Vicat softening temperature A50125 °CISO 306:2013

    The tensile and dart values listed above are for circular-die film specimens; they do not represent compression-moulded plaque properties. Comparative tensile modulus, Elmendorf tear, and water vapour transmission rate data are less frequently disclosed for this specific grade. Where those properties are critical, published data for this specific configuration is limited and a structured pilot-line design of experiments is required before commercial commitment.

    On blown-film lines with a 65 mm single-screw barrier screw and 30:1 L/D, the high molecular weight of DFDB8910 is observed as elevated screw torque and melt pressure relative to a 0.90 g/10 min HDPE. Barrel temperatures are typically maintained from 180 °C at the feed zone to 230 °C at the die. A die gap of 1.0 mm to 1.4 mm and a blow-up ratio of 3:1 to 5:1 are common for film thickness from 15 µm to 40 µm. The frost line should be elevated to 4 to 10 die diameters when bubble instability occurs, but raising the frost line too far reduces quench rate and lowers film toughness. Pre-drying is not usually required at ambient relative humidity below 60%; however, condensation introduced into the feed throat can generate surface defects. Use of a grooved feed section and a Maddock mixing element improves solids conveying and dispersion of processing stabilisers. Processing at melt temperatures below 190 °C risks melt fracture and unmolten gel formation in the highest-molecular-weight fractions. Processing above 240 °C increases oxidative degradation and may shift seal initiation temperature in coextruded structures.

    Rheological boundary conditions for this grade are not fully published, but high-molecular-weight HDPE with a melt mass-flow rate of 0.10 g/10 min typically develops a zero-shear viscosity approaching 100 000 Pa·s at 190 °C. The result is that die pressure is sensitive to lip-gap reduction; changing from a 1.4 mm die gap to a 1.0 mm gap can raise die pressure by more than 15% on a fixed screw speed, and the gain in transverse gauge uniformity may be offset by higher melt temperature. Melt pressure fluctuations should be held within ± 5 bar of the target value to avoid visible gauge bands in film below 20 µm. If a downstream bubble collapses, block-up can occur in the collapsing frames because of the high melt strength at the frost line; air-jet collapsing shields with stable guiding angles are preferred over static wooden slats.

    Thermal degradation in HMW-HDPE blown-film extrusion is most severe at the die lip, where shear heating is concentrated. When melt temperature measured at the adapter exceeds 235 °C, the film often shows a detectable reduction in dart impact and an increase in gel count. A screen-pack pressure rise above 30 bar above the clean-screen baseline indicates melt contamination or crosslinked gels. Since DFDB8910 has a high-molecular-weight tail, gel defects can be mistaken for unmelt; discriminating between oxidative gel and unmelt requires a hot-stage microscopy check at 180 °C in which oxidative gel remains as a visible particle after the polyethylene matrix has melted.

    When 25 µm blown film is processed at 3:1 blow-up ratio, the property balance diverges from higher-MFI HDPE grades

    At equivalent film thickness, DFDB8910 produces a higher crystalline fraction than a linear low-density polyethylene with density 0.918 g/cm³, which reduces water vapour transmission but also reduces machine-direction Elmendorf tear if orientation is excessive. Compared with Sinopec Maoming HDPE 5000S, a general-purpose injection and extrusion grade with melt mass-flow rate near 0.90 g/10 min, DFDB8910 exhibits higher melt strength, greater bubble stability, and higher dart impact at large blow-up ratios. The trade-off is processability: screw torque rises, melt pressure rises, and output on a given extruder is limited by melt temperature rather than by screw speed. Against a typical C4-LLDPE film grade with melt mass-flow rate near 2.0 g/10 min, DFDB8910 yields higher modulus, lower clarity, and a stiffer film that is less suited to overwrap requiring recovery elasticity. In coextruded structures, DFDB8910 is placed in the core or outer layer for stiffness and moisture barrier, while a lower-density sealant layer provides heat sealing. Published data for exact interlayer adhesion in polyolefin coextrusion with DFDB8910 is limited; tie-layer selection is generally unnecessary for polyolefin-to-polyolefin interfaces but should be confirmed through laboratory peel tests.

    The grade is not a direct substitute for high-flow HDPE in injection-moulded caps or crates, because the molecular weight tail creates short-shot and jetting defects even at melt temperatures above 240 °C. It also differs from blown-film grades designed for high-clarity shrink film, because the density is too high and the crystalline structure produces haze when oriented in thick sections. These differences make the product more suitable for stiffness-driven, gauge-reduction applications than for optical or elastic recovery applications.

    Commercial applications reported for the grade include T-shirt grocery sacks, produce bags, dry-cleaning film, and puncture-resistant liners where gauge reduction is sought without losing load resistance. On high-speed bag-making lines, the coefficient of friction is governed by the additive package, and the base resin is usually compounded or externally treated with slip or antiblock. Corona discharge treatment to a wetting tension of 38 mN/m to 42 mN/m is applied when water-based flexographic printing is used; the treated surface decays with storage time and must be re-verified before ink laydown. Film gauge uniformity depends on die gap, die lip uniformity, air ring control, and melt temperature stability; modern blown-film lines with internal bubble cooling can exploit the high melt strength to maintain stable gauge under high output demands. In coextruded high-density film for cereal liners, DFDB8910 is typically combined with a linear low-density polyethylene sealant layer at 10% to 20% of total thickness, with the HDPE layer providing stiffness and the LLDPE layer providing heat-seal integrity.

    Compliance and operational boundaries

    When used in food-contact packaging, converters must confirm that the specific lot meets the appropriate national or regional positive list, because base-resin compliance does not automatically extend to converted film after additives, masterbatches, printing inks, or adhesives are introduced. The following matrix summarises the regulatory references commonly applied to high-density polyethylene food-contact grades, not a certificate for any specific lot.

    Regulatory referenceScopeTypical verification
    FDA 21 CFR 177.1520Olefin polymers for food contactSupplier letter of no objection or migration testing
    Regulation (EU) No 10/2011Plastic materials and articles intended to come into contact with foodOverall migration and specific migration testing
    GB 4806.7-2016Food-contact plastic materials and articles in ChinaMigration testing per related GB 31604 series
    REACH Regulation (EC) No 1907/2006Registration and substances of very high concernSupplier declaration and SVHC screening
    RoHS Directive 2011/65/EUHazardous substances in electrical and electronic equipmentMaterial content screening if packaging is used with EEE

    The resin should not be processed by injection moulding because of its high molecular weight; short-shot and jetting defects occur even at high melt temperature. The material is incompatible with nitrile-based, halogenated-solvent-based, or amine-based additives not intended for polyolefins; these may degrade the stabiliser package or create undesired surface migration. Long-term outdoor exposure without a UV stabiliser masterbatch leads to embrittlement of unstabilised film, especially at film thickness below 20 µm. For coextruded structures with a sealant skin of lower-density polyethylene, the total thickness distribution should be maintained within ± 5% to avoid local thinning at bag side seals.