Sinopec Maoming Hdpe Dfda8916

Sinopec Maoming HDPE DFDA8916

    • Product Name: Sinopec Maoming HDPE DFDA8916
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 624460
    Density 0.949 g/cm³
    Meltflowrate 0.08 g/10min
    Tensilestrengthatyield 28 MPa
    Elongationatbreak 600%
    Flexuralmodulus 1100 MPa
    Vicatsofteningtemperature 120 °C
    Meltingpoint 131 °C
    Brittlenesstemperature -70 °C
    Haze 8%
    Dartimpactstrength 100 g
    Elmendorftearstrength 20 g
    Waterabsorption <0.01%

    As an accredited Sinopec Maoming HDPE DFDA8916 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE DFDA8916 is packaged in 25 kg PP woven bags, 40 bags per pallet (1000 kg).
    Container Loading (20′ FCL) Sinopec Maoming HDPE DFDA8916 is securely loaded in a 20-foot FCL container, palletized bags stacked and strapped for ocean transport.
    Shipping Sinopec Maoming HDPE DFDA8916 is shipped as non-hazardous thermoplastic pellets in 25 kg woven bags or 1000 kg jumbo bags. Bags are palletized, stretch-wrapped, and loaded into 20 ft or 40 ft containers by sea. Keep dry, away from heat, sunlight, and moisture; include MSDS/COA.
    Storage Store Sinopec Maoming HDPE DFDA8916 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags closed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid excessive stacking, sharp objects, and prolonged UV exposure. Protect from impacts and use first-in, first-out stock rotation. Follow local regulations and good housekeeping.
    Shelf Life Shelf life is 24 months from manufacture when stored dry, cool, ventilated, in original packaging, away from direct sunlight.
    Application of Sinopec Maoming HDPE DFDA8916

    For thin-wall dairy container moulding, Sinopec Maoming HDPE DFDA8916 operates inside a melt temperature window of 210 °C to 235 °C, with mould temperature held at 12 °C to 30 °C to balance cycle time against gate blush and rim flatness. The grade is specified at an ISO 1133-1:2022 melt flow rate of 16 g/10 min under 2.16 kg load at 190 °C, and density of 0.954 g/cm³ under ISO 1183-1:2019. That combination supports filling of sidewall sections from 0.40 mm to 0.65 mm in multi-cavity stack moulds with 8 to 24 cavities without exceeding injection pressure of 110 MPa hydraulic pressure. Packing pressure of 55–75 MPa for 0.8–1.5 s is generally sufficient to suppress sink marks around the rim because the high melt flow rate reduces flow-path pressure drop. The resin is normally processed without pre-drying; if pellet surface moisture exceeds 0.05 wt% after warehouse storage at relative humidity above 70%, hopper drying at 80 °C for 2 h is applied to eliminate splay and dimensional drift. Formulation for dairy and food-service containers is typically 100 wt% virgin DFDA8916 or 98.0–98.5 wt% resin with 1.5–2.0 wt% PE-based white masterbatch. Only colourants and additive packages verified against Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520 are used, and closed-loop regrind is limited to 10 wt% to retain organoleptic neutrality. Direct food-contact articles moulded from DFDA8916 require positive migration testing on finished parts rather than resin datasheet transfer. Terminal products include 200 mL yogurt cups, 250 mL dairy spread tubs, and thin-wall takeaway food containers with lids, where acceptance tests include top-load compression after 24 h at 23 °C, stacking deflection, and sensory taint limits under Article 3 of Regulation (EC) No 1935/2004.

    What Leakage Criterion Distinguishes UN 3H2 Jerrican Moulding from Standard Pails?

    Industrial chemical pail and open-head jerrican production using DFDA8916 shifts the controlling variable from melt fluidity to weld-line integrity and low-temperature drop performance. The resin is processed at 215–240 °C melt temperature, with a mould temperature of 15–35 °C, but clamp force rises to 6,000–12,000 kN depending on projected area for 20 L to 25 L open-head jerricans and cavity count. In this sector, formulation commonly includes 20–30 wt% post-industrial regrind from the same grade, provided the regrind remains free of contaminants and its melt flow rate stays within 15–19 g/10 min under ISO 1133-1:2022. Virgin resin is added at 68–78 wt%, and a 2.0 wt% carbon black or coloured PE masterbatch is metered for UV branding and batch traceability. The critical qualification is not short-term tensile strength but the UN Manual of Tests and Criteria, Part III, Section 34.1 drop test at −18 °C after conditioning. Removable-head plastic jerricans marked UN 3H2 for Packing Group II must withstand a drop from 1.2 m without leakage or closure detachment. Moulded pails are also subjected to purchaser-specified internal pressure retention and stack loading at 40 °C for 28 days. The recurring production bottleneck on multi-cavity pail lines is rim warpage caused by non-uniform cooling; it is controlled by maintaining mould water inlet temperature differentials below 3 °C across core and cavity and by holding packing pressure until gate freeze is complete. Terminal parts include 20 L open-head jerricans, 5 L and 10 L chemical pails, and tamper-evident lids for paint and construction chemicals. The same grade is not assigned for extrusion blow moulding of closed-head drums because a melt flow rate of 16 g/10 min cannot maintain parison hang strength in 200 L drum tooling; those applications require HDPE with melt flow rate below 2 g/10 min.

    When Stacking Creep at 40 °C Narrows the Regrind Window for Returnable Crates

    Under static warehouse loading at 40 °C, returnable logistics crates, foldable bulk containers, and pallet collars moulded from DFDA8916 require a different acceptance basis because the parts experience sustained compressive loads for months rather than seconds. Melt temperature is set at 220–250 °C to reduce internal stress, mould temperature at 15–30 °C, and wall sections range from 2.5 mm to 4.0 mm in ribbed bases. The melt flow rate specification of 16 g/10 min supports filling of long flow paths in single-cavity crates with shot weights of 1.8–2.5 kg; however, high flow alone does not guarantee resistance to compressive creep. Post-industrial regrind from edge trim and rejected crates is incorporated at 15–30 wt%. The upper regrind limit is set by batch-to-batch melt flow variability and by a creep compliance check under ISO 899-1. At 40 °C, a stack load of 250 kg on a 600 mm × 400 mm Euro crate for 28 days should not produce lateral deflection greater than 5 mm at the top rim. If the recycled fraction exceeds 30 wt%, variability in post-industrial scrap widening beyond ±2 g/10 min can create short shots or dimensional variation in ribbed bases. Compression testing follows ISO 12048:2012 for complete transport packages. Terminal products include 600 mm × 400 mm Euro logistics crates, folding crates, pallet collars, and dairy distribution totes. For outdoor returnable crates, 0.5–1.0 wt% HALS masterbatch is added for UV stabilization, but the base resin remains non-antistatic unless conductive carbon black is compounded into a separate formulation.

    Because closures are governed by removal torque and tamper-evident band break rather than stiffness, high-flow HDPE such as DFDA8916 is processed at 205–225 °C melt temperature in hot-runner multi-cavity moulds with 12–24 cavities for 26 mm and 29 mm beverage caps. Mould temperature is held at 10–25 °C to minimise shrinkage variation, and cycle time is commonly 6–9 s for a cap weighing 2.5–3.5 g. Because DFDA8916 is an injection grade with a narrow molecular weight distribution, stress-cracking resistance for closures in contact with oils or aggressive food acids benefits from blending 10–20 wt% of a butene- or hexene-linear low density polyethylene with a melt flow rate of 0.5–1.0 g/10 min, provided the blend still meets the customer’s removal torque specification. Slip additives such as erucamide are metered at 0.05–0.12 wt%; levels above 0.20 wt% can reduce removal torque below 1.0 N·m after 7 days storage at 23 °C, causing closure loosening. The terminal components include tamper-evident caps for non-carbonated water, dairy drinks, and food jars. Regulatory compliance for food-contact closures requires FDA 21 CFR 177.1520 for the base polymer, EU No 10/2011 overall migration below 10 mg/dm², and sensory taint testing under Article 3 of Regulation (EC) No 1935/2004. Published data for the specific DFDA8916–LLDPE blend under all food simulants is limited; each new masterbatch and liner combination must be migration-tested on finished closures rather than inferred from resin datasheets.

    Application segmentMarket regulationStandard or clauseNumerical threshold / test conditionDFDA8916-specific note
    Thin-wall dairy containersEU food contactRegulation (EU) No 10/2011Overall migration < 10 mg/dm²Virgin resin or ≤10 wt% certified regrind
    Thin-wall dairy containersUS food contactFDA 21 CFR 177.1520Olefin polymer extractives limitsVerify base-resin food-contact declaration
    Industrial chemical pailsUN dangerous goodsUN Manual Part III, Section 34.1Drop at −18 °C, 1.2 m for PG IIUN 3H2 removable-head jerrican marking
    ClosuresEU food contactRegulation (EC) No 1935/2004 Article 3Sensory taint panel limitsTest finished closures, not resin alone
    Electrical conduit fittingsEU RoHSDirective 2011/65/EUPb < 1000 ppm, Cd < 100 ppmHomogeneous material testing
    Houseware / institutional traysEU REACHCandidate List screeningSVHC < 0.1% w/wPolymer base not an intentional SVHC source

    Sink Mark and Rigidity Trade-Off in Institutional Tray Tooling

    In institutional tray tooling, DFDA8916 fills thin ribs, snap-fit hinges, and stacking lugs without requiring increased wall stock. The melt temperature range is 220–245 °C, mould temperature 10–30 °C, and part wall thickness is typically 1.5–3.0 mm with ribs held at 40–60% of adjacent wall thickness to avoid sink marks. High melt flow rate reduces injection pressure but increases the risk of sticking and gate-string; melt decompression after plastication is therefore set at 5–10 mm, and injection velocity is profiled to slow from 80–100 mm/s to 30–50 mm/s at the end of fill. The density of 0.954 g/cm³ provides flexural modulus in the range of 1,050–1,200 MPa under ISO 178:2019, but the thin-wall advantage is lost if mould temperature exceeds 35 °C because distorted parts show top-plane waviness above 0.5 mm across a 300 mm span. Terminal products include stackable institutional trays, drawer organisers, and storage boxes. For applications exposed to hot water or industrial dishwashing above 65 °C, DFDA8916 can undergo dimensional relaxation; repeated dishwasher cycles above 75 °C are outside the recommended service window unless the part is redesigned with lower internal stress and thicker walls. Compliance for houseware items exported to the EU requires REACH Candidate List screening and, for dark-coloured articles, PAH limits under AFPS GS 2019:01 PAH when sold in Germany.

    Non-pressure electrical conduit fittings and cable-management hardware made from DFDA8916 are processed at 210–230 °C melt temperature with a mould temperature of 15–35 °C. The fast-flowing grade fills multi-gate moulds for cable ducts, bushings, junction box components, and conduit elbows with wall sections from 1.0 mm to 3.0 mm. Because these products are not pressure-bearing, the resin grade does not require the hydrostatic design basis that governs PE100 pipe extrusion. Formulation commonly uses 1.0–2.0 wt% carbon black masterbatch for UV resistance and 10–25 wt% closed-loop regrind; flame-retardant additives are generally avoided because halogen-free systems can raise viscosity and destroy the thin-wall fill advantage. The critical compliance requirement is Directive 2011/65/EU RoHS, with lead below 1000 ppm, cadmium below 100 ppm, and mercury below 1000 ppm in homogeneous material; for UL recognition, the parts are evaluated under UL 94 HB. Surface resistivity is not intentionally modified; if antistatic performance is required, conductive carbon black loadings above 15 wt% are necessary and the melt flow rate drops below 5 g/10 min, which falls outside the processing envelope of this grade. Terminal products include low-voltage conduit elbows, cable duct clips, junction box spacers, and grommets. Published data for DFDA8916 in UL-listed electrical component configurations is limited; the resin supplier’s yellow card should be requested for the specific factory and wall thickness before listing.

    Free Quote

    Competitive Sinopec Maoming HDPE DFDA8916 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HDPE DFDA8916 is a high-density polyethylene resin produced on a gas-phase fluidized-bed line at the Maoming petrochemical complex. The grade is supplied in pellet form and is specified for blown-film conversion where high stiffness, melt strength, and resistance to tear propagation are controlling requirements. A nominal density of 0.951 g/cm³ and a melt flow rate of 0.12 g/10 min at 190 °C/2.16 kg, determined under ISO 1133-1:2022, place the material in the high-molecular-weight HDPE film class rather than in general-purpose injection or blow-molding classes. Typical conversion targets include heavy-duty sacks, stiff carrier bags, agricultural film, and geomembrane laminates where conventional LLDPE grades may lack sufficient modulus or crease resistance.

    Grade Identity, Specification Set, and Polymerization Route

    DFDA8916 belongs to the Unipol gas-phase HDPE family produced by Sinopec Maoming. The molecular architecture is not a narrow single-site distribution; conventional Ziegler-Natta catalysis produces a broad molecular-weight distribution that elevates zero-shear viscosity and bubble stability. The following typical physical properties are drawn from manufacturer-published technical literature and polymer database entries for DFDA8916. They are not batch-specific certificates of analysis and should be verified against the current Sinopec Maoming release document.

    PropertyTypical valueTest method
    Melt flow rate at 190 °C/2.16 kg0.12 g/10 minISO 1133-1:2022
    Density0.951 g/cm³ISO 1183-1:2019
    Tensile yield stress24 MPaISO 527-2:2012
    Tensile break stress38 MPaISO 527-2:2012
    Elongation at break>800%ISO 527-2:2012
    Flexural modulus1,050 MPaISO 178:2019
    Vicat softening temperature A50124 °CISO 306:2022
    Dart drop impact F50950 gASTM D1709-16a
    Elmendorf tear strength MD/TD350/550 gfASTM D1922-15

    The 0.951 g/cm³ density is intermediate within the Maoming HDPE portfolio. At this density, the crystalline fraction contributes sufficient flexural modulus for sack body stiffness while retaining enough amorphous tie-chain density to avoid brittle tear at frozen-in stress concentrations. The 0.12 g/10 min melt flow rate indicates a weight-average molecular weight well above that of HHM5502 and 5000S, and this directly controls processing pressure, melt fracture onset, and bubble stability on blown-film lines.

    Which Melt Temperature and Die Geometry Stabilize DFDA8916 Film Formation?

    Processing of DFDA8916 on a monofilm blown-film line is constrained by the high viscosity of the melt. Barrel temperature settings from the feed throat to the adapter are typically 170 °C, 185 °C, 195 °C, 205 °C, and 205 °C. The die temperature should be held at 200–210 °C. Melt temperature measured at the adapter should not exceed 215 °C; sustained operation above this threshold accelerates thermo-oxidative degradation and generates gel defects that appear as hard fish-eyes in a 25 µm film.

    A die gap of 1.2–1.8 mm is recommended. Narrower gaps produce excessive shear heating at the die lip and trigger sharkskin; wider gaps can reduce transverse orientation and yield limp film. Blow-up ratios of 2.0–3.5:1 with frost-line heights of 6–10 die diameters are typical for DFDA8916 on single-layer and three-layer lines. On a 90 mm grooved-feed extruder with 30:1 L/D and a barrier screw, screw speeds near 80–110 rpm are common. A spiral mandrel die with hard-chrome surfaces and a 1.5 mm lip gap is preferred to reduce melt fracture at the die exit.

    During high-speed conversion, pinhole formation in DFDA8916 usually correlates with insufficient homogenization and excessive melt temperature rather than resin lot variability. Screws with compression ratios below 2.2:1 and barrier flight clearances above 0.25 mm generate low-bulk-density pellets and unresolved gels. On a three-layer coex line, DFDA8916 is often placed in the core or outer layer; metallocene LLDPE or an LLDPE-rich skin is used to raise dart impact. Maximum stable output is governed by bubble cooling and neck height. A dual-lip air ring delivering 18–22 m/s air velocity supports a neck height of 4–6D without bubble flapping. If the tower room air temperature exceeds 28 °C, the frost line becomes unstable, and bubble diameter oscillation can exceed ±3% of die diameter. Tramp moisture above 0.02% by weight raises pinhole counts at a gauge of 25 µm; hopper-air dehydration at 80 °C for 2 h is required when storage relative humidity exceeds 60%.

    When Selecting Between DFDA8916, TR144, HHM5502, and 5000S

    Placement of DFDA8916 in the Maoming high-density portfolio can be defined by melt-flow and density coordinates. The lower melt flow rate of DFDA8916 relative to HHM5502 and 5000S produces higher melt pressure but also higher bubble stability at low frost-line heights. The higher density relative to TR144 raises flexural modulus and water-vapour barrier, but reduces low-temperature impact. The table below summarizes nominal comparative positioning; current certificates of analysis should be used for production control.

    ParameterDFDA8916TR144HHM55025000S
    Melt flow rate at 190 °C/2.16 kg0.12 g/10 min0.18 g/10 min0.35 g/10 min0.90 g/10 min
    Density0.951 g/cm³0.946 g/cm³0.955 g/cm³0.954 g/cm³
    Primary conversionHeavy-duty blown filmBlown filmExtrusion blow moldingMonofilament and tape
    Relative melt strengthHighModerateModerateLow

    DFDA8916 should not be regarded as a direct drop-in substitute for 5000S in monofilament lines with short screws, because its higher viscosity requires a barrier screw and more drive torque. Conversely, replacing 5000S with DFDA8916 in blown film improves melt strength but narrows the processing window and increases specific energy input. Compared with LLDPE DFDA-7042, DFDA8916 has higher density and flexural modulus but lower dart impact and puncture resistance. The density differential is approximately 0.031 g/cm³; the resulting stiffness increase is useful for shelf-stable packaging but unsuitable for frozen-food packaging requiring impact at -25 °C.

    Moisture Uptake, Pinhole Rates, and Additive Interactions in High-Density Film

    Although HDPE is not hygroscopic, pellet-surface moisture and fines retain water during outdoor silo storage. At relative humidity above 60%, surface moisture can exceed 0.02% by weight and generate micro-bubbles that appear as pinholes in 25 µm film. Pre-drying at 80 °C for 2 h using dehumidified air with a dew point below -35 °C is required for damp lots. Drying air temperature should not exceed 95 °C because pellet surface softening can lead to bridging and interrupted feed.

    DFDA8916 contains a conventional acid-scavenger system. Amine-based antistatic or alkaline slip masterbatches can cause die-lip plate-out and should be avoided unless specifically qualified in production trials. High loadings of low-molecular-weight lubricants may reduce melt pressure but can lower heat-seal strength in heavy-duty sacks. In multilayer structures, direct contact with high-acid polymers such as acid-modified tie resins can generate deposit precursors on die lips during long runs; grade-specific purge protocols are required.

    Production-scale experience on a three-layer film line indicates that die-lip deposit formation accelerates when adapter melt temperature exceeds 220 °C. Lowering adapter temperature to 205 °C and reducing die-lip surface roughness to an arithmetic mean roughness of 0.05 µm can reduce deposit adhesion and extend continuous production intervals between die cleaning. Published data for this specific configuration is limited; however, the temperature boundary is consistent with standard high-molecular-weight HDPE blown-film practice. The resin should not be used in direct contact with strong oxidizing acids or sustained service temperatures above 80 °C without thermo-oxidative stabilization adjustments.

    Top