Sinopec Maoming Hdpe 5233

Sinopec Maoming HDPE 5233

    • Product Name: Sinopec Maoming HDPE 5233
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 724729
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.953 g/cm³
    Melt Flow Rate 0.35 g/10 min
    Tensile Yield Strength ≥23 MPa
    Elongation At Break ≥500%
    Flexural Modulus ≥1000 MPa
    Izod Notched Impact Strength ≥25 kJ/m²
    Vicat Softening Temperature ≥120 °C
    Brittleness Temperature ≤-70 °C
    Shore D Hardness ≥60
    Water Absorption ≤0.01%
    Dielectric Constant 2.3 at 1 MHz
    Volume Resistivity ≥1×10^16 Ω·cm
    Melting Point 130-135 °C
    Crystallinity 70-80%

    As an accredited Sinopec Maoming HDPE 5233 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE 5233 supplied in 25 kg woven bags, 40 bags per pallet, totaling 1,000 kg.
    Container Loading (20′ FCL) 20' FCL container loaded with Sinopec Maoming HDPE 5233 in 25 kg bags, palletized, stretch-wrapped, and secured for ocean freight.
    Shipping Sinopec Maoming HDPE 5233 is typically shipped as non-hazardous polyethylene pellets in 25 kg PP woven bags, palletized and stretch-wrapped. Transport by truck, rail, or sea in clean, dry containers. Keep dry, away from heat and sunlight; avoid tearing or moisture exposure during handling and storage.
    Storage Store Sinopec Maoming HDPE 5233 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original bags or containers closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Stack pallets securely, maintain good housekeeping, follow supplier recommendations and local regulations, and ensure containers remain undamaged. No smoking.
    Shelf Life Sinopec Maoming HDPE 5233 typically has a 24-month shelf life when stored dry, cool, ventilated, and protected from direct sunlight.
    Application of Sinopec Maoming HDPE 5233

    Sinopec Maoming HDPE 5233 is specified for extrusion blow molding and blown film conversion. Injection molding of thin-wall closures is not a primary conversion route for this grade because the melt flow rate restricts thin-wall filling; the documented downstream sectors are therefore limited to extrusion blow molding and blown film. Where published grade-specific data is limited, the parameter ranges are drawn from industrial practice for high-density polyethylene with nominal density 0.952 g/cm³ and a melt flow rate of 0.33 g/10 min under ISO 1133-1:2022 at 190 °C and 2.16 kg.

    On 80 mm single-screw extruders with L/D ratio 28:1, HDPE 5233 is processed at a melt temperature of 190–215 °C and a die gap of 1.2–2.0 mm for blown film at a blow-up ratio of 3.5:1–5.0:1; the frost line height is held at 6–8 die diameters above the air ring to control machine-direction and transverse-direction tensile balance. The formulation uses 100 phr HDPE 5233, 1.5–3.0 phr white masterbatch, 0.5–1.0 phr slip agent masterbatch, 1.0–2.0 phr antiblock masterbatch, and 0.02–0.05 phr polymer processing aid; regrind from edge trim is added at 20–40 wt%, but levels above 50 wt% produce measurable gel counts and reduce dart impact according to ASTM D1709-16. Compliance for food-contact liners requires FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 with overall migration below 10 mg/dm² under EN 1186-1:2002. Terminal products include retail carrier bags at 12–25 µm, freezer bags at 15–30 µm, and industrial liners at 50–120 µm; surface condensation from silo storage at relative humidity above 85% requires hopper drying at 70 °C for 2 h before extrusion to prevent splay defects.

    What ESCR limits govern household chemical bottle production?

    Household chemical bottle production subjects HDPE 5233 to aggressive fill products that demand environmental stress crack resistance validation under ASTM D1693-21, Condition A at 50 °C; a typical internal release limit is no more than 10% of specimens failing by 48 h. The formulation is 100 phr HDPE 5233, 2–5 phr color masterbatch, 0.1–0.3 phr antioxidant masterbatch, and 0.05–0.1 phr external lubricant; clean in-house regrind is maintained at 20–35 wt%, and regrind above 40 wt% narrows the processing window and lowers ESCR. Extrusion blow molding is run on shuttle machines with 10-point parison programming, barrel temperatures 160–200 °C, die gap 1.8–2.5 mm, blow pressure 0.6–0.9 MPa, and mold temperature 20–40 °C; for handleware detergent bottles, the parison programmer is set to thicken the pinch-off and handle zones by 15–30% relative to the sidewall. Compliance for dangerous goods packaging requires UN certification under ADR/RID/IMDG when the filled container exceeds the applicable dangerous goods threshold; material conformity is assessed under REACH Regulation (EC) No 1907/2006, Annex XVII, and U.S. state packaging regulations. Terminal products include laundry detergent bottles and handleware containers from 500 mL to 5 L, bleach bottles with vented closures, and automotive fluid containers. The grade is not recommended for prolonged contact with strong oxidizing agents above 7% sodium hypochlorite without pre-validation of closure and wall stress-crack performance; published data for this specific configuration is limited, so plant trials are required.

    For pharmaceutical squeeze bottles, the conversion environment rather than the raw resin alone determines suitability. HDPE 5233 is processed by injection blow molding or extrusion blow molding inside an ISO 14644-1 Class 8 cleanroom; mold cooling water is held at 10–18 °C, and compressed air is filtered to 0.2 µm to limit particle deposition. The formulation uses 100 phr HDPE 5233, 1–2 phr pharmaceutical-grade color masterbatch, and 0.02–0.05 phr processing aid; regrind is excluded unless validated under a worst-case stability study, and many drug application dossiers require 0% regrind. Melt temperature is maintained at 190–210 °C, die gap at 1.4–2.0 mm, and cavity pressure at 25–40 MPa for injection blow molded preforms. Compliance references include USP <661.1> and USP <661.2>, Ph. Eur. 3.1.3, FDA 21 CFR 177.1520(c), and EU Regulation (EU) No 10/2011; extractables and leachables studies follow ISO 10993-18:2020 when the bottle contacts drug product or delivery device components. Terminal products include nasal spray bottles, tablet desiccant canisters, and syrup bottles. Silicone mold release agents are not permitted without subsequent washing because residual surface energy below 38 mN/m impairs print adhesion; corona treatment at 1.0–1.5 kW/m² line power is applied when labels must adhere to the hydrophobic surface.

    Regulatory or quality requirementReference method or standard
    USP plastic packaging physicochemical testingUSP <661.1>
    USP plastic packaging organic extractablesUSP <661.2>
    European Pharmacopoeia polyolefin monographPh. Eur. 3.1.3
    US FDA olefin polymer food contact21 CFR 177.1520(c)
    EU plastics food contact migrationEU Regulation No 10/2011, Annex I

    Dairy and juice container wall thickness distribution data

    Extrusion blow molding of dairy containers imposes a narrow thermal window; barrel zone temperatures are set at 160–200 °C and melt temperature at 195–215 °C, while the mold is cooled to 15–30 °C to freeze the wall before shrinkage creates deviations beyond ±0.1 mm in sidewall thickness. HDPE 5233 is run at 100 phr with 1–3 phr white masterbatch, 0.02–0.05 phr fluoroelastomer processing aid to delay melt fracture at high output, and 0.5–1.0 phr slip masterbatch for cap torque reduction; post-consumer or in-plant regrind is limited to 20–50 wt% depending on the closure torque requirement and organoleptic panel results. The die gap is set at 1.6–2.2 mm and the blow pin is programmed to produce a wall thickness of 0.35–0.60 mm for a 1 L bottle, with pinch-off zones thickened to 0.8–1.2 mm to prevent splitting. Compliance for milk and juice bottles requires FDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011, and GB 9685-2016 for additive migration; organoleptic testing follows ISO 13302:2003 for packaging materials causing off-taste. Terminal products include 200 mL single-serve milk bottles, 500 mL–2 L juice bottles, and 1 L pasteurized dairy bottles. The processing limit is melt temperature above 220 °C, which causes detectable odor generation and narrows molecular weight distribution; below 190 °C, die lines and sharkskin become visible at die gaps above 2.0 mm.

    Where HDPE 5233 is used as the stiffness core in coextruded film

    In three-layer coextruded blown film, HDPE 5233 is placed in the core layer at 30–50 wt% of total film mass between LLDPE skins, with each skin at 25–35 wt%; the core-layer die gap is 1.8–2.4 mm, and the total film thickness is 30–80 µm. The formulation in the core layer is 100 phr HDPE 5233, 1–3 phr white or tinted masterbatch, 0.02–0.05 phr processing aid, and 0.5–2.0 phr antiblock masterbatch only when the core contributes to the outer surface through unbalanced layer distribution; published data for this specific configuration is limited, so the antiblock addition is adjusted by pilot-line haze testing under ASTM D1003-21. The blown film line is run at a melt temperature of 195–220 °C, blow-up ratio 2.5:1–3.5:1, and frost line height 5–7 die diameters; layer-to-layer melt viscosity matching is controlled by adjusting outer-layer LLDPE density and melt index rather than by adding process oil. Compliance for dry food contact follows FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, with overall migration below 10 mg/dm² under EN 1186-1:2002. Terminal products include cereal and cracker bag liners, dry pet food pouches, and laminated stand-up pouch backside films; the HDPE core raises secant modulus according to ISO 527-2:2012 and reduces elongation over monolayer LLDPE, but dart impact under ASTM D1709-16 declines when core-layer HDPE exceeds 50 wt%.

    Parison programming for oval and pinch-grip personal care containers

    Pinch-grip and oval personal care containers require parison programming asymmetry rather than uniform wall distribution; the die gap is varied across 10 points to thicken the handle pinch zone by 20–40% and the label panel by 5–10%, while maintaining sidewall thickness between 0.45–0.70 mm for a 400 mL shampoo bottle. The formulation uses 100 phr HDPE 5233, 1–4 phr color masterbatch, 0.05–0.15 phr slip masterbatch, and 0.02–0.05 phr processing aid; regrind is controlled at 20–40 wt% and is sieved through a 2.0 mm screen to remove gels before reuse. Extrusion blow molding is run at melt temperature 195–215 °C, mold temperature 15–30 °C, blow pressure 0.65–0.85 MPa, and cooling time 8–14 s; blow air is dried to a dew point below −40 °C to prevent internal surface haze. Compliance for cosmetic packaging requires conformity to REACH Regulation (EC) No 1907/2006, Annex XVII, and EU Regulation (EC) No 1223/2009 for product-packaging compatibility; heavy metals in packaging must meet 94/62/EC total cadmium, mercury, lead, and hexavalent chromium limits below 100 ppm by weight. Terminal products include 200 mL–1 L shampoo and conditioner bottles, body wash bottles with polypropylene caps, and lotion bottles with silk-screen label panels. Surface treatment is limited to corona discharge at 1.2–1.5 kW/m²; flame treatment above 50 °C surface temperature introduces oxidation that can reduce ESCR under ASTM D1693-21.

    Free Quote

    Competitive Sinopec Maoming HDPE 5233 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HDPE 5233 is a high-density polyethylene injection-moulding resin supplied by Sinopec Maoming Petrochemical Company. The grade is pelletized and is classified as a medium-molecular-weight HDPE, with nominal density 0.953 g/cm³ measured under ISO 1183-1 and melt mass-flow rate 3.3 g/10 min measured under ISO 1133-1 at 190°C/2.16 kg. These values establish the material as an injection-grade HDPE; they differentiate it from extrusion blow-moulding grades in the same density range whose melt flow rates are typically below 0.5 g/10 min. Primary use areas are rigid injection-moulded articles including industrial pails, crates, caps, closures, housewares, toys, and thin-wall packaging. The product is not intended for blown film, fibre spinning, pressure pipe extrusion, or large-diameter blow-moulded containers where high melt strength or high molecular weight is required.

    Supplied lots should be verified against the current certificate of analysis because polymerization campaign shifts and additive masterbatch changes can alter viscosity, density, and impact data. The following values are representative of published supplier data and are not batch-release specifications unless marked as guaranteed.

    Specification Basis and Injection-Moulding Window

    PropertyTest methodRepresentative value
    DensityISO 1183-10.953 g/cm³
    Melt mass-flow rateISO 1133-13.3 g/10 min at 190°C/2.16 kg
    Tensile stress at yieldISO 527-226 MPa
    Flexural modulusISO 1781,150 MPa
    Notched Izod impact strengthISO 180/A at 23°C7 kJ/m²
    Heat deflection temperatureISO 75-2 method B, 0.45 MPa75°C
    Vicat softening temperatureISO 306/A50124°C
    Shore D hardnessISO 86862

    The density of 0.953 g/cm³ corresponds to a crystalline fraction of approximately 65–70% relative to the ideal linear polyethylene crystal. This crystalline fraction contributes to tensile modulus, creep resistance, and chemical resistance, but it also increases mould shrinkage and post-mould dimensional change relative to random copolymer polypropylene. The melt mass-flow rate of 3.3 g/10 min is a low-shear index; at injection filling shear rates of 102–104 s−1 the effective viscosity is lower because of shear thinning, so cavity-fill predictions should be based on capillary rheometry or spiral-flow testing rather than on melt index alone.

    Injection moulding on polyolefin screws with 20:1 to 24:1 L/D and compression ratios of 2.5:1 to 3.5:1 indicates that barrel profiles from 180°C at the feed throat to 220°C at the nozzle produce stable melt quality. Mould temperatures should be held between 20°C and 60°C; lower mould temperatures reduce cycle time but increase orientation and can promote warp in asymmetric parts. Injection pressure is typically 80–120 MPa for direct-gated sections, while thin-wall moulds may require injection velocities above 120 mm/s. Hold pressure should be maintained until gate freeze; published data for this specific configuration is limited, so gate-freeze time should be established by short-shot and seal-time studies on the target tool.

    Pre-drying is not routinely required when pellet moisture remains below 0.05 wt%. If sacks are stored at relative humidity above 60%, drying at 80°C for 2 h in a desiccant dryer is advisable to prevent surface splay and shot-weight variation. Regrind additions up to 30 wt% are generally accepted for non-appearance parts, but the melt-flow rate of the blend should be rechecked under ISO 1133-1 because reclaimed material from hot-runner systems may have undergone molecular-weight reduction.

    Cooling rate controls the crystalline morphology. Rapid cooling against a 20°C mould yields smaller spherulites and lower short-term shrinkage, while slow cooling at 60°C increases crystallinity and elastic modulus but also increases post-mould shrinkage. Parts with wall sections varying by more than 25% may exhibit differential shrinkage and gate-area sink marks. Uniform cooling-channel layout and feed-system sizing are more important than melt temperature adjustment in controlling these defects.

    Batch release and incoming quality control for HDPE 5233 should include melt-flow-rate verification under ISO 1133-1 and density under ISO 1183-1. In multi-cavity tools with more than 16 cavities, cavity-to-cavity fill imbalance is typically assessed by shot-weight and dimensional studies, because the shear-thinning response interacts with runner diameter and gate freeze.

    What Differences Emerge When HDPE 5233 Is Compared with High-Molecular-Weight Blow-Moulding Resins?

    The primary difference is rheological. HDPE 5233 has a melt mass-flow rate of 3.3 g/10 min under 190°C/2.16 kg, which indicates lower zero-shear viscosity and lower average molecular weight than extrusion blow-moulding HDPE grades with melt flow rates below 0.5 g/10 min. In extrusion blow moulding, parison sag and die swell depend on melt elasticity and molecular weight distribution; the lower melt strength of HDPE 5233 makes it unsuitable for large containers or technical parts where wall thickness is controlled by parison hang strength under gravity.

    The molecular weight distribution is narrower than that of high-molecular-weight blow-moulding HDPE. This narrow distribution reduces die swell and melt elasticity while improving reproducibility in injection moulding. However, it also limits shear-thinning response at high shear rates compared with broader-distribution grades, so spiral-flow length may be lower than expected from melt-flow ratio alone.

    Environmental stress-cracking resistance under ASTM D1693-21, Condition B, is generally lower for injection-moulding HDPE grades than for high-molecular-weight blow-moulding grades. The lower average molecular weight of HDPE 5233 reduces resistance to crack propagation in the presence of polar surfactants, lubricants, and certain detergent systems. Converters specifying this grade for chemical-contact closures or detergent packaging should evaluate the final part under the actual aggressive medium, because laboratory test conditions do not reproduce all service stressors.

    Compared with high-flow HDPE injection grades with melt flow rates above 10 g/10 min, HDPE 5233 provides higher viscosity and normally better impact resistance, but it requires higher injection pressure and longer fill time. Selection between these grades should be based on flow-length-to-wall-thickness ratio and clamp force capacity, not solely on cycle time.

    Compared with polypropylene impact copolymers, HDPE 5233 has higher density and lower heat deflection temperature under load. It is selected where low-temperature impact below −20°C and water-vapour barrier are required, while polypropylene is selected for higher-temperature service above 90°C. The resin should not be stored or processed in contact with strong oxidizing acids, chlorinated solvents, or aromatic hydrocarbons at elevated temperature because these agents swell or degrade the polymer. For food-contact applications, the final article must be evaluated under the applicable migration framework, such as FDA 21 CFR 177.1520 or Commission Regulation (EU) No 10/2011, with compliance determined on the finished article rather than the pellet alone.

    When Wall Thickness Falls Below 1.8 mm in Thin-Wall Rigid Packaging

    Thin-wall tub and closure moulding requires high linear injection speed to overcome heat loss across the flow front. For a nominal wall of 1.5 mm, melt temperature is typically set at 210°C to 220°C and mould temperature at 35°C to 50°C. Injection velocity below 120 mm/s can produce short shots and hesitation lines at the confluence of opposing flow fronts. The recommended flow-length-to-wall-thickness ratio for unreinforced HDPE is kept below 200:1; above 220:1, weld lines and gas traps become dominant defects.

    Valve-gated hot-runner systems with thermal gate tips should be set to maintain tip temperature below 230°C to reduce gate stringing and material degradation. Vent depth for HDPE should not exceed 0.02 mm to avoid flash; open vents at flow-front meeting points reduce internal gas pressure and weaken weld lines less than trapped air. Clamp force requirement is generally 4–7 kN/cm² of projected area for thin-wall HDPE parts depending on fill pressure and melt viscosity.

    Mould shrinkage under ISO 294-4 is typically 1.5% to 2.5% in flow direction and 1.0% to 2.0% transverse. Post-mould dimensional change continues for 24–48 h at ambient storage because secondary crystallization proceeds after ejection. Thin-walled parts with uneven wall sections or asymmetrical cooling should be expected to warp; corrective action is usually to balance cooling circuits and move gates to reduce differential orientation rather than to increase hold pressure alone.

    Tensile strength at a weld line in HDPE 5233 can be 30–50% of the non-weld tensile strength under ISO 527-2, depending on melt temperature, mould temperature, and hold pressure. In thin-wall closures and caps, weld-line positioning should be moved away from seal and impact zones by gate-position changes because the weld line becomes the probable failure origin in drop impact testing under ASTM D2463.

    Post-fabrication quality control for regrind blends should include melt-flow measurement under ISO 1133-1 and density verification under ISO 1183-1. Blends containing more than 30 wt% regrind from thin-wall parts may shift the melt-flow rate above 4.0 g/10 min and reduce tensile yield; such shifts should be corrected by adjusting virgin material and process conditions.