| HS Code | 957382 |
| Density | 0.946 g/cm³ |
| Melt Flow Rate | 13 g/10 min (190°C, 2.16 kg) |
| Tensile Yield Strength | ≥24 MPa |
| Elongation At Break | ≥500% |
| Flexural Modulus | ≥900 MPa |
| Notched Izod Impact Strength | ≥40 kJ/m² |
| Vicat Softening Temperature | ≥120°C |
| Melting Point | 130-135°C |
| Brittleness Temperature | ≤ -70°C |
| Hardness | ≥60 Shore D |
| Water Absorption | <0.01% |
| Heat Deflection Temperature | ≥75°C (0.45 MPa) |
| Volume Resistivity | >10^16 Ω·cm |
| Dielectric Strength | ≥20 kV/mm |
| Ul Flammability | HB |
As an accredited Sinopec Maoming HDPE 4613 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sinopec Maoming HDPE 4613 packaging: 25 kg PP woven bags, palletized and stretch-wrapped for industrial shipment. |
| Container Loading (20′ FCL) | 20' FCL loaded with Sinopec Maoming HDPE 4613 resin, 25 MT in 25 kg bags, palletized, shrink-wrapped, securely stowed and sealed. |
| Shipping | Sinopec Maoming HDPE 4613 is shipped as a non-hazardous thermoplastic in 25 kg woven bags or 1000 kg jumbo bags, palletized and stretch-wrapped. It is transported by truck or sea freight in 20-/40-foot containers. Store dry, cool, ventilated, away from direct sunlight, moisture, and ignition sources. |
| Storage | Store Sinopec Maoming HDPE 4613 in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags sealed and palletized off the floor. Avoid moisture, contamination, and prolonged UV exposure. Store at ambient temperature. Do not stack excessively. Use first-in, first-out inventory. Follow supplier SDS and local regulations. |
| Shelf Life | Sinopec Maoming HDPE 4613 typically has a 24-month shelf life when stored cool, dry, ventilated, and away from direct sunlight. |
Sinopec Maoming HDPE 4613 is positioned as an extrusion blow-molding high-density polyethylene for rigid hollow articles; open literature on this specific grade is limited, so the operating windows cited below are drawn from fractional-melt HDPE blow-molding practice and require confirmation against the batch certificate of analysis. On a twin-station shuttle machine with a 65 mm barrier screw at L/D 25:1, production of 750 mL to 2 L household detergent bottles typically uses feed-zone temperatures of 170–175°C, mid-barrel temperatures of 185–195°C, and a die-head set point of 200–205°C. The die tooling is configured with a converging flow channel, a die-pin land length ratio of 18:1–22:1, and a die gap of 1.2–1.8 mm; these dimensions control parison swell, which for low-melt-index HDPE is commonly 10–30% depending on shear rate and die-head pressure. A parison programmer with at least 20 points is applied because detergent bottles of 150–250 mm height develop wall thinning at the shoulder and pinch-off zones when a constant parison profile is used. Blow air pressure is maintained between 0.55 MPa and 0.75 MPa, and chilled mold water is held at 10–15°C to reduce sink marks and keep cycle time below 18 s on a single-cavity 1 L bottle. For bleach-containing products with 4–6% sodium hypochlorite, the clean plant regrind level is capped at 20 wt% because higher regrind fractions have been observed to accelerate environmental stress cracking on production-scale bottle drop tests. ESCR acceptance is evaluated according to ASTM D1693 Condition B using 10% Igepal CO-630 at 50°C, with a commonly imposed threshold of ≥24 h for detergent bottles. Final bottle weights are controlled to ±0.5 g on a 1 L container. EU/REACH compliance is addressed through the resin’s SVHC screening and through the downstream packaging article’s conformity to the Packaging and Packaging Waste Directive; food-contact declarations are not assumed because the household detergent application does not require FDA 21 CFR 177.1520 or EU 10/2011, but export documentation may still request them.
Tall oval shampoo and conditioner bottles in the 300–500 mL range expose the 4613 melt to high gravitational stress because the parison hang time on a single-station continuous extrusion blow molder frequently exceeds 6 s when the part length-to-width ratio is above 3:1. With a 45 mm grooved-feed extruder at L/D 24:1, melt temperature at the die exit is held at 195–200°C; raising the head above 205°C reduces melt viscosity and increases sag, while lowering below 185°C raises die-head pressure above 25 MPa and triggers melt fracture on the bottle surface. The parison programmer is set with 30–40 control points, increasing wall thickness at the bottom tail and shoulder zones to 1.2–1.4 mm while holding the central body at 0.7–0.9 mm after blow-up. A die gap of 1.0–1.4 mm with a blow-up ratio of 2.2:1–2.8:1 is used, and mold temperature is controlled at 8–12°C with turbulent chilled water flow to freeze the high-gloss surface before shrinkage produces orange-peel defects. Color is introduced as 2 wt% white or pearl masterbatch in a polyethylene carrier; masterbatch selection is restricted to carriers with melt flow rate below 4 g/10 min at 190°C/2.16 kg to avoid local viscosity dilution and surface streaking. Post-molding flame treatment raises surface energy to >40 mN/m according to ASTM D2578, allowing pressure-sensitive labels and shrink-sleeve adhesives to wet the surface without delamination. Compliance for personal care packaging is evaluated under EC 1223/2009 for cosmetic product contact, with batch documentation typically requiring REACH registrations for masterbatch pigments and carrier resins. The terminal article is a 400 mL tall oval pack weighing 18–22 g with a wall-thickness distribution of ±0.15 mm, measured by magnetic wall-thickness gauges at 10 fixed points after sectioning.
In six-layer barrier bottle lines producing 400–1000 mL food and industrial barrier containers, HDPE 4613 is assigned to the outer and inner skins as well as to the regrind-bearing core layer. The coextrusion head runs six extruders into a single die; the HDPE layers are fed by 50 mm screw extruders at 190–205°C, while the EVOH barrier layer is held at 210–225°C and the adhesive tie layers at 190–210°C. Layer distribution is controlled by gear-pump flow rates rather than by screw speed alone because viscosity mismatch between EVOH and HDPE can cause interfacial flow instability when the HDPE layer falls below 15% of total thickness. The table below lists one qualified layer structure with thickness shares and control set points.
| Layer sequence | Material function | Thickness share | Control set point |
|---|---|---|---|
| 1 | HDPE 4613 outer skin | 18–22% | 195–205°C melt |
| 2 | Anhydride-modified tie | 2–3% | 190–210°C melt |
| 3 | EVOH barrier | 4–6% | 210–225°C melt |
| 4 | Anhydride-modified tie | 2–3% | 190–210°C melt |
| 5 | Regrind/HDPE core | 40–46% | 190–205°C melt |
| 6 | HDPE 4613 inner skin | 18–22% | 195–205°C melt |
Post-consumer recyclate is not introduced into the skin layers unless the recyclate has been batch-tested for ESCR under ASTM D1693 Condition A and for melt flow stability under ISO 1133-1:2022; in-plant trim regrind of known HDPE 4613 is commonly reused in the core at 40–46% of bottle thickness. The terminal barrier bottle is used for oxygen-sensitive sauces and for industrial liquid concentrates where the oxygen transmission rate must remain below 0.5 cm³/(m²·day·0.21 atm) as measured by ASTM D3985; the HDPE skins provide water-vapour resistance and drop strength while the EVOH layer supplies oxygen barrier. Food-contact status must be confirmed through EU 10/2011 overall migration testing and, for U.S. markets, FDA 21 CFR 177.1520 olefin polymer clearance of the specific 4613 batch, because not all Sinopec HDPE grades are produced with identical additive packages.
Agricultural chemical containers between 3 L and 10 L for emulsifiable concentrates and solvent-borne pesticides are extrusion blow-molded on accumulator-head machines with 80 mm screws at L/D 25:1 and shot capacities of 2.5–4.0 kg. The die-head temperature is kept at 200–205°C, and the accumulator drop speed is profiled so that the parison reaches 80% of final length before the mold halves meet; this prevents pinch-off thinning at the bottom corners of a 5 L jerrycan. Wall thickness is specified at 1.2–1.6 mm in the body and 2.0–2.4 mm at the handle and pinch-off zones. The mold chiller is held at 12–16°C, and blow air at 0.6–0.8 MPa is introduced through the blow pin in two stages: 0.2 MPa for 0.5 s to pre-shape the parison, then full pressure for 12–15 s. Clean plant regrind is limited to 20 wt% because UN certification tests include a drop test at −18°C from 1.2 m on the handle seam, and higher regrind content has been reported to reduce impact toughness at the pinch-off weld. The finished container is tested under the UN Manual of Tests and Criteria, Part III, for tightness, internal hydraulic pressure, and stacking; drop and stacking results must be reproduced on the exact 4613 formulation and mold, not extrapolated from a similar grade. Chemical resistance is screened using method ASTM D543 for swell and weight loss after 7-day immersion in the actual formulated product, not a model solvent. The terminal article is a UN 3H1 jerrycan with a three-layer structure if barrier is required, or a monolayer container for non-flammable formulations where permeation below the regulatory threshold can be demonstrated.
Under-hood reservoir tooling differs from consumer bottle tooling because the part must survive continuous vibration, internal pressure, and cold-start impact; for washer-fluid reservoirs and coolant overflow bottles molded from HDPE 4613, wall thickness is increased to 1.8–3.0 mm and the blow-up ratio is reduced to 1.5:1–2.0:1 to maintain consistent wall cross-section. The parison is dropped from a 90 mm accumulator head at 195–205°C, the mold is maintained at 10–14°C, and cooling time is extended to 25–35 s to limit dimensional warpage after demolding. The part is leak-tested at an internal air pressure of 40 kPa submerged in water, and burst pressure is checked at 200–250 kPa for washer reservoirs; these values are derived from general HDPE blow-molded technical part practice because published data for 4613 in automotive service is limited. UV resistance is obtained with 2.0–2.5 wt% high-pigment carbon black masterbatch dispersed in an HDPE carrier; dispersion is verified by a 25 µm microtome film and transmitted-light inspection under ISO 18553. Long-term heat ageing is screened by ISO 188 at 100°C for 168 h, and dimensional change is measured against the customer’s warm-seam alignment fixture; any shrine line or injection gate must be removed without introducing stress-whitening. OEM validation for under-hood components typically includes thermal cycling from −40°C to 100°C for 200 cycles and a 1 m cold drop at −30°C. Batch documentation includes REACH SVHC compliance and, where requested, ISO 11469 material marking on the part.
For solid oral dosage bottles in the 60–250 mL range, HDPE 4613 is processed in an ISO Class 8 cleanroom on a 45 mm single-station extrusion blow molder with a polished stainless-steel trim-and-deflash system. Melt temperature is held at 190–200°C, and the mold cooling water is kept at 8–10°C to produce a smooth interior surface that reduces powder adhesion. High-density polyethylene for such packs must resist permeability to water vapour; a 0.6 mm wall bottle is tested according to USP ⟨671⟩ for water vapour transmission and must meet the monograph limits for the specific drug product, with test results tied to the 4613 batch number. Incoming resin release includes melt flow rate under ISO 1133-1:2022 at 190°C/2.16 kg and density under ISO 1183-1:2019; the resulting data are retained in the batch record. Opacity is controlled with 1.0–1.5 wt% titanium dioxide masterbatch for light-sensitive formulations, and the masterbatch is qualified under USP ⟨661.1⟩ and EP 3.1.3 for polyolefin packaging components. Regrind is limited to 15 wt% and only from the same cleanroom operation; no recycled material from outside the room is introduced because particulate contamination and unknown additive history violate pharmaceutical change-control. The terminal closure-compatible bottle neck is dimensioned to the customer drawing and sampled at 2 h intervals with go/no-go plug gages, while cap torque is measured as removal torque on a torque meter referenced in ASTM D2063. Pharmaceutical qualification of HDPE 4613 is batch-specific and requires drug master file support or change-control equivalence from the resin manufacturer; published data for this specific configuration is limited.
Competitive Sinopec Maoming HDPE 4613 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Maoming HDPE 4613 is a high-density polyethylene extrusion compound intended for pressure pipe manufacture. The grade is supplied as black pellets with carbon black content of 2.0–2.5% by mass determined in accordance with ISO 6964. Density measured under ISO 1183-1 is 0.949 g/cm³, and melt mass-flow rate under ISO 1133-1 at 190 °C with a 5.0 kg load is 0.30 g/10 min. The material is classified as PE100 with a minimum required strength of 10.0 MPa at 20 °C for 50 years under ISO 12162. Tensile yield stress under ISO 527-2 is approximately 23 MPa and nominal strain at break is greater than 600%. Environmental stress crack resistance under ASTM D1693-B in 10% Igepal CO-630 at 50 °C exceeds 500 h. These values place the grade in the high-molecular-weight, low-melt-flow range required for thick-wall pipe extrusion rather than injection moulding or thin-film processing.
| Property | Standard/Test Method | Unit | Typical Published Value |
|---|---|---|---|
| Density | ISO 1183-1 | g/cm³ | 0.949 |
| Melt mass-flow rate, 190 °C/5.0 kg | ISO 1133-1 | g/10 min | 0.30 |
| Tensile yield stress | ISO 527-2 | MPa | 23 |
| Nominal strain at break | ISO 527-2 | % | >600 |
| Carbon black content | ISO 6964 | % by mass | 2.0–2.5 |
| Environmental stress crack resistance | ASTM D1693-B | h | >500 |
| Oxidative induction time, 200 °C | ISO 11357-6 | min | ≥20 |
| Minimum required strength, 20 °C/50 years | ISO 12162 | MPa | 10.0 |
The values in the table are manufacturer-published typical values, not batch release minima. Users should request a certificate of analysis for each lot to verify melt flow rate, density, carbon black content, carbon black dispersion, and oxidative induction time against the purchase specification.
The differentiation from injection moulding and blow moulding grades is primarily rheological and mechanical rather than compositional at the monomer level. Pipe grades such as Sinopec Maoming HDPE 4613 exhibit low melt mass-flow rate under 5.0 kg load, typically 0.30 g/10 min, which indicates higher average molecular weight than common blow moulding grades. The higher molecular weight raises slow crack growth resistance, a parameter required for buried pressure pipes but not for thin-wall consumer packaging. In high-speed injection moulding grades, melt flow rates are often 20–80 g/10 min at 190 °C and 2.16 kg, making them unsuitable for pipe wall thickness retention. The pipe compound also contains carbon black at 2.0–2.5% for ultraviolet stabilization and for long-term outdoor storage. Film grades, by contrast, may use lower levels of pigment or uv stabilizers because service life is shorter and light exposure is not a structural concern.
Published data for this specific configuration is limited, but PE100 pipe grades generally differ from PE80 grades in the required hydrostatic design basis. The PE100 classification allows the use of a minimum required strength of 10.0 MPa at 20 °C for 50 years, whereas PE80, under ISO 12162, requires 8.0 MPa. This is not a short-term tensile distinction; the yield stress of PE80 and PE100 compounds may be similar, but the long-term failure resistance is different. Manufacturers achieve the PE100 classification through molecular weight distribution control and comonomer placement, usually involving a bimodal or broadly distributed polymer architecture that optimizes the balance between processability and slow crack growth resistance.
Within the Sinopec Maoming portfolio, the 4613 designation is pipe-specific. Film grades and blow moulding grades are formulated for higher melt flow and lower die swell, whereas 4613 prioritizes long-term hydrostatic strength and slow crack growth resistance. Direct substitution of 4613 into thin-wall blow moulding tools is not advised because the high melt viscosity can produce incomplete mould filling and excessive clamp force. Conversely, a film or blow moulding grade lacks the hydrostatic design basis and carbon black stabilization required for pressure pipe service.
When this compound is processed on a grooved-feed single-screw pipe extruder with an L/D ratio of 30:1 to 36:1, the barrel temperature profile is set to avoid overheating the high-molecular-weight melt. A typical profile starts at 180 °C in the feed zone, rises to 210–220 °C in the compression and metering zones, and holds the die head at 210–230 °C. Melt temperature measured at the die entry should remain below 240 °C; exposure above this threshold accelerates oxidative consumption of the stabilizer package and can produce surface discoloration or micro-bubbles. The screw should have a grooved feed section and a mixing element, but high-shear dispersive mixing should be limited because excessive shear heating can reduce melt viscosity and alter wall thickness control. For a 60 mm extruder operating at 80–120 rpm, melt pressure before the screen pack can exceed 200 bar with low-melt-flow PE100 compounds. Published data for Sinopec Maoming HDPE 4613 at full commercial diameter is limited; the exact pressure depends on screw design, mesh pack, and die land length.
Pipe cooling and sizing are governed by the high melt viscosity and modulus. In vacuum-sizing tanks, the initial water temperature is usually maintained at 20–40 °C. A low-temperature bath can induce thermal stresses in thick walls, while a high-temperature bath can reduce the crystalline orientation developed at the pipe surface. For SDR 11 and SDR 17 dimensions, the haul-off speed and screw speed must be matched so that the wall thickness tolerance remains within +0.2 mm or the applicable dimensional class under ISO 4427-2. Batch-to-batch melt flow rate variation in pipe grades can cause diameter and wall thickness drift on older extruders without melt pumps; for this compound, incoming melt flow rate should be checked against the certificate of analysis before filling the hopper.
Incoming resin lots are typically tested for melt mass-flow rate under ISO 1133-1, density under ISO 1183-1, carbon black content under ISO 6964, and oxidative induction time under ISO 11357-6. A lot with an OIT below 20 min should be rejected or segregated because it may have insufficient residual stabilizer for long residence time extrusion. Moisture uptake in black HDPE pellets is generally low, but surface condensation can occur when cold material is moved into a warm plant. If the storage relative humidity exceeds 60%, pre-drying at 80 °C for 2 h is required to avoid steam bubbles in the pipe wall. Carbon black dispersion quality should be evaluated under ISO 18553 or the applicable national specification, because undispersed agglomerates act as stress concentrators in the pipe wall and may reduce slow crack growth resistance.
For a buried water main, the governing parameter is the minimum required strength extrapolated from long-term hydrostatic testing. Under ISO 9080, the lower confidence limit for Sinopec Maoming HDPE 4613 is classified as 10.0 MPa at 20 °C for 50 years. With an overall service coefficient of 1.25, the design stress for water becomes 8.0 MPa. The same coefficient applied to a PE80 compound yields 6.3 MPa. Consequently, pipe made from the PE100 grade can be thinner than pipe made from a PE80 compound at the same pressure and outside diameter.
| Parameter | PE80 pipe compound | Sinopec Maoming HDPE 4613 |
|---|---|---|
| Minimum required strength under ISO 12162 | 8.0 MPa | 10.0 MPa |
| Design stress for water, 20 °C, 50 years, service coefficient 1.25 | 6.3 MPa | 8.0 MPa |
| Nominal pressure rating for SDR 11 water pipe | 12.5 bar | 16 bar |
| Hydrostatic test condition for finished water pipe | 20 °C and 80 °C per ISO 4427-2 | 20 °C and 80 °C per ISO 4427-2 |
The table shows the pressure rating implication for a given SDR, but it does not remove the need for hydrostatic testing on the extruded pipe. Pipe samples must still be tested according to ISO 4427-2 for dimensions, and type tests for pressure resistance are performed at 20 °C and 80 °C to confirm that the finished pipe, not just the raw resin, retains long-term strength. The presence of carbon black in the compound can reduce tear initiation resistance at low temperatures; however, the pipe design stress governs failure in this application.
Butt fusion welding of pipe produced from this compound must follow the jointing parameters defined in ISO 21307 or the applicable national gas distribution code. The low melt flow rate and high molecular weight require sufficient melt displacement pressure to form a uniform bead, but excessive heating can consume stabilizer at the fusion face. Bead width should be measured after each joint; a bead width outside 2.0–4.0 mm for common pipe diameters indicates improper heating or pressure. Electrofusion joints are less sensitive to resin grade differences, but the pipe surface must be scraped to remove oxidized skin before joining. Scraped depth should follow the electrofusion fitting manufacturer’s tables, typically 0.1–0.2 mm. Because PE100 compounds may have higher melt elasticity than PE80, fitting manufacturers sometimes specify different fusion times to ensure intermolecular diffusion at the interface.
Oxidative induction time measured at 200 °C under ISO 11357-6 is specified at ≥20 min for the compound. The stabilizer package typically contains phenolic and phosphite antioxidants, with carbon black acting as a ultraviolet screen. OIT is a quality control indicator, not a direct service life prediction. During pipe extrusion, long residence times can consume the stabilizer package; therefore, the melt temperature should not exceed 240 °C, and start-up purge should be used to clear material that has been held in the die for extended periods. If the extruder trips, material left in the barrel and die spider legs can degrade before restart. Degraded resin can cause fish-eye defects and localized loss of hydrostatic strength, which is not always visible on the pipe surface.
The presence of carbon black at 2.0–2.5% requires dispersion testing because agglomerates act as stress risers. Dispersion is checked by cutting a thin microtome section and examining it under an optical microscope according to ISO 18553. A dispersion rating worse than the pipe specification limit can lead to premature brittle failure in slow crack growth tests. In gas pipe service, the combination of carbon black and stabilizer package must also meet national standards for gas distribution. In some European gas pipe specifications, an OIT at 200 °C of ≥20 min is adequate for the resin, but the finished pipe may be subjected to additional thermal aging tests to verify stabilizer retention.
When pipe manufactured from Sinopec Maoming HDPE 4613 is placed in service, the operating pressure and temperature must be limited by the pipe design class, not by the short-term burst pressure. Continuous exposure to water temperatures above 40 °C reduces the hydrostatic design life and may require downgrading the pressure rating. The grade is not intended for above-ground transportation of hydrocarbons, hot water, or compressed air systems unless the specific national code permits HDPE pipe. In chlorinated water service, published long-term chlorine resistance data for this grade is limited; utilities should obtain accelerated chlorine stress-cracking data from the resin supplier or require testing according to ASTM F2263 or the applicable national protocol. Outdoor storage of finished pipe is possible because of the carbon black content, but the pipe should be supported along its full length and protected from direct contact with sharp objects, because surface scoring can reduce slow crack growth resistance.