Sinopec Maoming Hdpe 4003

Sinopec Maoming HDPE 4003

    • Product Name: Sinopec Maoming HDPE 4003
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 863203
    Density G Cm3 0.940
    Melt Flow Rate G 10min 0.3
    Tensile Yield Strength Mpa 20
    Elongation At Break Percent 700
    Flexural Modulus Mpa 900
    Vicat Softening Point C 120
    Brittleness Temperature C -70
    Environmental Stress Cracking Resistance H >1000
    Hardness Shore D 55
    Melting Point C 130
    Dielectric Constant 2.3
    Volume Resistivity Ohm Cm >1e16
    Water Absorption Percent <0.01
    Thermal Conductivity W Mk 0.44

    As an accredited Sinopec Maoming HDPE 4003 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Maoming HDPE 4003 is supplied in 25 kg polyethylene-lined woven bags, stacked on pallets for bulk handling.
    Container Loading (20′ FCL) 20′ FCL container: Sinopec Maoming HDPE 4003 in 25 kg bags, palletized, shrink-wrapped, and secured for ocean freight.
    Shipping Sinopec Maoming HDPE 4003 is typically shipped as non-hazardous polymer pellets in 25 kg bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. A 20-foot container holds about 17–20 metric tons. Store dry, ventilated, away from heat, moisture, and direct sunlight. Standard sea freight is used.
    Storage Store Sinopec Maoming HDPE 4003 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and incompatible materials. Keep original bags sealed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Use first-in, first-out stock rotation. Maintain clean, dry conditions and follow the supplier’s SDS and local regulations.
    Shelf Life Sinopec Maoming HDPE 4003: typically 24 months when stored unopened in original packaging, cool, dry, well-ventilated, away from sunlight, moisture.
    Application of Sinopec Maoming HDPE 4003

    Narrow-neck extrusion blow moulded bottles for liquid detergents and surface disinfectants place simultaneous demands on melt strength, environmental stress crack resistance (ESCR), and colourant dispersion stability. Sinopec Maoming HDPE 4003 enters this application in a typical dry blend containing 97.0 wt% HDPE 4003, 2.5 wt% HDPE-carrier pigment masterbatch, and 0.5 wt% processing stabilizer; masterbatch levels above 4.0 wt% are not advised because they dilute ESCR and lower pinch-off seam strength. The grade’s reported melt flow index of 0.30–0.40 g/10 min at 190 °C/2.16 kg (ASTM D1238-20) and density of 0.955 g/cm³ (ASTM D1505) dictate a barrel temperature profile of 185–205 °C on a 24:1–30:1 L/D extruder to avoid parison roughness below 180 °C and oxidative viscosity shift above 210 °C. Compliance for non-food household chemical packaging rests on REACH Annex XVII, EU packaging waste directive 94/62/EC heavy-metal concentration ceilings, and ASTM D1693-21 ESCR screening in 100% Igepal CO-630 at 50 °C. Production is typically conducted on single-station shuttle blow moulders with 0.6–0.8 MPa blow pressure, mould cooling water at 15–25 °C, and cycle times of 10–15 s for 1 L containers. Finished articles include 500 mL–5 L narrow-neck bottles for liquid detergents, surface cleaners, and ready-to-use disinfectant formulations.

    Extrusion Blow Moulding of UN-Certified Chemical Jerricans and Tight-Head Containers

    Containers intended for UN Packing Group II and III liquid chemical transport are not single-layer commodity packaging items; they are design-type-tested pressure vessels. Sinopec Maoming HDPE 4003 is compounded at 97.0 wt% with 2.5 wt% carbon black masterbatch and 0.5 wt% hindered amine UV stabilizer to suppress ultraviolet embrittlement during open-yard storage. The melt flow index must remain in the 0.30–0.40 g/10 min band because lower-viscosity grades produce excessive parison sag in 20 L parisons weighing 1.4–1.8 kg, while higher-viscosity grades raise die swell beyond 55% and destabilize programmed wall-thickness control. The extrusion blow moulding line uses an accumulator head with a 24:1–30:1 L/D extruder, 190–210 °C melt temperature, and a die gap of 1.5–2.5 mm; parison programming varies wall thickness from 1.2 mm at the pinch-off to 2.0 mm at the chime. Cycle time on a 20 L tight-head jerrican is 45–70 s depending on post-cooling fixture dwell and plant ambient humidity. Batch-to-batch melt flow index variation of ±0.02 g/10 min is compatible with these settings; larger drift requires recalibration of the parison programmer. Finished products include 5 L, 10 L, 20 L, 25 L tight-head jerricans and 30 L open-top pails for solvents, agrochemical concentrates, and industrial detergents.

    Standard / methodRequirement or test conditionRelevance to HDPE 4003
    UN 3H1 / 3H2Plastic jerrican design type approval; hydrostatic pressure testConfirms pinch-off and weld-line integrity
    ADR 6.1.5.4Leakproofness and stacking load at 40 °C for 28 daysEvaluates creep deformation at closure and chime
    49 CFR §178.509Drop, vibration, pressure test for plastic packagingsDrop height 1.2 m for Packing Group II liquids
    ASTM D1693-21ESCR in 100% Igepal CO-630, 50 °CScreens resistance to surfactant and chemical stress cracking

    In five-layer coextruded barrier bottles, the Sinopec Maoming HDPE 4003 outer layer functions as both structural substrate and moisture vapour barrier while the EVOH core suppresses oxygen ingress. A representative layer mass distribution is given below; HDPE 4003 comprises 30 wt% of the total parison mass as the outer cap layer. The EVOH must be pre-dried at 80 °C for 4 h to avoid bubble formation at the tie interfaces; HDPE 4003 itself requires no pre-drying unless surface condensation is present, in which case 80 °C for 2 h is sufficient. Extrusion is performed on a continuous coextrusion blow moulding line with six extruders, each equipped with barrier screws and melt pumps to hold layer thickness fluctuation below ±5%. Interfacial instability occurs when the HDPE 4003 melt temperature exceeds 210 °C at the die, because viscosity mismatch with the EVOH layer increases interfacial wave formation and reduces oxygen barrier consistency; therefore the die head zone is maintained at 190–205 °C. Barrier performance is verified by oxygen transmission rate testing per ASTM D3985 after 100% relative humidity conditioning, while migration compliance follows EU Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520(c) for the HDPE layers. Finished articles include 250 mL–1 L multilayer bottles for solvent-based agrochemicals, oxygen-sensitive disinfectants, and flavoured industrial concentrates.

    LayerMaterialMass fraction of total parison
    Outer structural layerSinopec Maoming HDPE 400330 wt%
    Regrind layerIn-house process regrind45 wt%
    Tie layerMaleated HDPE adhesive resin4 wt%
    Barrier layerEVOH with 32–44 mol% ethylene content6 wt%
    Inner layerHDPE15 wt%

    What Are the Processing Limits When HDPE 4003 Is Used for Personal Care and Cosmetic Bottles?

    When Sinopec Maoming HDPE 4003 is selected for personal care and cosmetic bottles, the dominant processing constraint shifts from short-term mechanical strength to long-term parison repeatability and surface finish consistency. Formulation for pearlescent shampoo and body wash bottles contains 98.0 wt% HDPE 4003, 1.5 wt% pearlescent or colour masterbatch, and 0.5 wt% slip additive to reduce surface scuffing during filling-line handling. Melt temperature is deliberately held at 180–195 °C because higher temperatures reduce polymer chain orientation in the pinch-off seam and increase gloss variability, while lower temperatures generate visible weld lines around the flash zone. Mould cooling water is maintained at 10–20 °C to accelerate skin solidification and improve repeatable neck finish tolerances; blow pressure is 0.6–0.75 MPa. The extrusion blow moulding machine is typically a twin-station shuttle unit with a 24:1 L/D extruder and 0.8–1.2 m parison drop length, capable of 12–18 s cycles for 500 mL bottles. Surfactant-containing formulations impose ESCR screening per ASTM D1693-21; the surrounding packaging is evaluated under EC No 1223/2009 for cosmetic product compatibility and REACH Annex XVII for restricted substances. Finished products include 200 mL–1 L bottles for shampoos, conditioners, body washes, and viscous lotions that are filled cold below 40 °C.

    When Sheet Thermoforming Replaces Injection Moulding for Dunnage Trays and Lids

    Dry-cycle material handling trays and dunnage sheets present a different reprocessing profile from hollow containers because the trim generated during thermoforming is reground and returned upstream at high ratios. Sinopec Maoming HDPE 4003 is metered at 75.0 wt% with 25.0 wt% in-house regrind, and 0.5 wt% antioxidant masterbatch based on total feed to offset the additional heat history. The sheet die is fed by a 30:1 L/D extruder with melt temperature 190–215 °C; the melt curtain is polished through a three-roll stack maintained at 70–90 °C to produce 3.0–6.0 mm sheet without internal voids. Thermoforming requires sheet surface temperature of 165–175 °C, just above the Vicat softening threshold and below the point of excessive sag. Operational boundaries are explicit: regrind content above 30 wt% reduces melt strength and causes local thinning in draw ratios above 3:1; continuous service temperature should not exceed 60 °C under stacking load because creep deflection accelerates beyond 0.5% strain. Compliance with 94/62/EC and ISO 18601:2013 for packaging heavy-metal limits is required for cross-border automotive service parts. Mechanical acceptance tests follow ISO 178:2019 for flexural modulus and ASTM D638-14 for tensile strength at yield. Finished articles include 600 mm × 400 mm industrial dunnage trays, tote lids, conveyor-line dividers, and interlayer stacking sheets used in automotive parts logistics.

    For underhood fluid reservoirs, the critical requirement is dimensional stability under repeated thermal cycling and resistance to windshield washer solvent stress cracking. Sinopec Maoming HDPE 4003 is processed at 100.0 wt% or, for underhood exposure, at 97.6 wt% HDPE 4003 with 2.0 wt% carbon black masterbatch and 0.4 wt% heat stabilizer. Suction blow moulding or 3D sequential blow moulding is used because the parts contain three-dimensional routing geometry and require pinch lines away from fluid contact zones. Melt temperature is held at 190–205 °C; wall thickness is programmed between 2.0 mm and 3.0 mm to satisfy burst-pressure testing without exceeding part mass targets. Cycle times on 2–8 L reservoirs range from 60–120 s depending on cooling fixture capacity. The key boundary is thermal ageing: HDPE 4003 is not suitable for continuous immersion in engine coolant above 80 °C or for turbocharger reservoir placements where local wall temperatures exceed 95 °C for extended periods. Compliance relies on ASTM D638-14 tensile yield, ASTM D256-10 Izod impact at −30 °C, and OEM-specific pressure-cycle testing. Finished products include 2–8 L windshield washer fluid reservoirs, 1–5 L coolant overflow bottles, and auxiliary fluid containers for commercial vehicle engine bays.

    Free Quote

    Competitive Sinopec Maoming HDPE 4003 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Maoming HDPE 4003 is a high-density polyethylene extrusion resin supplied by Sinopec Maoming Petrochemical. The grade is positioned for thick-walled extrusion and heavy-duty blow moulding where melt strength, slow crack growth resistance, and flow-rate consistency are the controlling parameters. The designation 4003 is a producer-specific grade code; it does not directly encode melt flow rate or density, and cross-producer substitution cannot be made on nomenclature alone. Published data for this specific configuration is limited in open technical literature, so the numeric control bands below should be checked against the batch certificate of analysis and the current manufacturer datasheet before release for production.

    The resin is a high-molecular-weight ethylene copolymer; the comonomer may include 1-butene or 1-hexene depending on reactor campaign. The high-molecular-weight tail increases low-shear viscosity and provides parison stability in large blow-moulded parts. For pipe and sheet extrusion, the same molecular architecture translates into higher head pressure and higher screw torque than a general-purpose low-viscosity HDPE of equivalent density.

    What processing window governs the 4003 grade?

    On grooved-barrel single-screw extruders with an L/D ratio of at least 30:1, melt temperature measured at the adapter is commonly maintained between 200 °C and 230 °C. A barrel profile from 180 °C in the feed zone to 220 °C in the metering zone is typical for thick sheet and pipe lines. Die head temperature is normally held at 210–220 °C. Residence time above 240 °C should be avoided because oxidative chain scission may lower melt strength and shift the high-load melt flow rate outside the control band.

    Pre-drying is generally unnecessary for sealed packaging. If open-bag storage has occurred at relative humidity above 60% with visible surface condensation, drying at 80 °C for 4 h in a desiccant dryer with a dew point no higher than −20 °C is sufficient. Screen-pack configuration for pipe and sheet extrusion commonly uses 60/80/100 mesh stacked screens to remove char and agglomerates; higher back-pressure beyond 250–350 bar often indicates screen blockage or insufficient temperature in the adapter.

    For large blow-moulded industrial containers, accumulator-head machines with die gap settings from 0.6 mm to 1.2 mm and blow ratios between 2:1 and 3:1 are used. Parison sag is controlled by the high melt strength of the grade, but die swell may increase relative to lower-viscosity blow moulding HDPE. Tooling design should account for higher die swell by adjusting preform diameter and wall-thickness programming rather than by raising melt temperature excessively.

    Thermal, Rheological and Compliance Control Parameters

    The table below lists representative control bands for Sinopec Maoming HDPE 4003. These values are not guaranteed lot limits; they reflect typical grade positioning and may differ for black carbon-black-modified lots or specific additive packages.

    Property Test method Unit Control band or note
    Melt mass-flow rate, high-load ISO 1133-1:2022 g/10 min 0.25–0.45 at 190 °C/21.6 kg
    Density ISO 1183-1:2019 g/cm³ 0.940–0.945
    Tensile yield stress ISO 527-2:2012 MPa ≥ 18.0
    Elongation at break ISO 527-2:2012 % ≥ 600
    Flexural modulus ISO 178:2019 MPa 700–900
    Notched Charpy impact, 23 °C ISO 179-1:2023 kJ/m² ≥ 10.0
    Carbon-black content, black lots only ISO 6964:2019 wt% 2.0–2.5

    Rheologically, the high-load melt flow rate alone understates the processing difference. A capillary rheometer at 190 °C shows pronounced shear thinning; apparent viscosity at 10 s⁻¹ is typically more than one order of magnitude higher than apparent viscosity at 1000 s⁻¹. This behaviour is beneficial for sag resistance but it increases pressure drop through narrow die lands and spider legs. Die design should avoid sharp transitions with included angles below 30 °, because local shear heating can exceed the bulk melt temperature and produce surface melt fracture.

    For hydrostatic pressure applications requiring PE80 classification under ISO 12162, long-term hydrostatic strength data generated according to ISO 9080 and validated by ISO 1167-1:2006 are required. The grade has been positioned in trade literature for industrial pipe and sheet where a minimum required strength of 8.0 MPa at 20 °C for 50 years is a typical design basis. However, certification is batch- and formulation-specific; a natural lot without a certifying test report should not be considered a substitute for a certified black pipe compound.

    Compliance area Standard or regulation Condition
    Food-contact olefin polymer, natural lots FDA 21 CFR §177.1520 Lot-specific declaration required; clearance applies to natural resin, not final fabricated article
    Plastics intended for food contact EU 10/2011 Overall migration and specific migration limits evaluated on finished article
    Carbon-black dispersion in black lots ISO 18553:2002 Rating should be ≤ 3.0 in pipe-grade evaluations
    Restriction of hazardous substances 2011/65/EU No intentional addition of restricted heavy metals above threshold limits
    Registration, evaluation and authorisation of chemicals REACH Supplier confirmation required; the resin is not expected to require a safety data sheet under normal industrial use

    For outdoor service, natural lots should not be exposed to continuous UV irradiation for more than 12 months unless compounded with a suitable hindered-amine light stabiliser or protected by a carbon-black masterbatch. Black lots containing 2.0–2.5 wt% dispersed carbon black are preferred for pipe and sheet products requiring long-term weathering resistance. Carbon-black dispersion is critical: undispersed agglomerates larger than 70 µm can act as crack-initiation sites under hoop stress.

    Oxidative induction time measured by differential scanning calorimetry at 200 °C according to ISO 11357-6 is commonly expected to exceed 20 min for adequately stabilised extrusion lots. A lower value does not automatically reject the batch, but it indicates antioxidant depletion or contamination and should trigger supplementary melt-flow and dispersion testing.

    When the resin is substituted for general-purpose blow moulding HDPE

    Substitution of Sinopec Maoming HDPE 4003 for a lower-viscosity blow moulding HDPE changes two processing responses simultaneously: extruder back-pressure increases and parison swell increases. On a single-screw extruder with a grooved feed zone, screw speed may need to be reduced by 10–20% compared with a conventional 0.35 g/10 min high-load melt flow resin to avoid overtorque. Head pressure can rise by 15–25% at the same screw speed and barrel profile, which may exceed the mechanical pressure rating of older die clamps or screen changers.

    Compared with a unimodal general-purpose HDPE of similar density, the broader molecular weight distribution of the 4003 control band increases low-shear viscosity and improves slow crack growth resistance. In notched constant-strain testing under ASTM D1693-21, failure time in a 10% Igepal CO-630 solution at 50 °C is typically expected above 1000 h for pipe-grade formulations, although published data for this specific configuration is limited. This differentiates the grade from lower-cost HDPE variants intended for thin-wall injection moulding or low-stress packaging, where notched ESCR may be below 100 h.

    When processing on twin-screw extruders with L/D ratios near 33:1, mixing energy must be limited to prevent excessive melt temperature. High-shear kneading blocks should be placed only in the first half of the screw, while the final zones should use low-shear forwarding elements. Melt temperature probes installed after the die adapter are preferred over barrel thermocouples alone, because the first barrel thermocouple can under-report the actual melt temperature by 5–10 °C under high shear.

    Batch-to-batch variance is most visible at grade changeover from a lower-viscosity product. If the changeover is incomplete, high-load melt flow rate may appear in specification while the low-shear viscosity remains out of range, producing variable parison sag on blow moulding lines. A purge with a fractional-melt HDPE of similar density for 60–90 min at screw speeds below 40 rpm is typically required before stable 4003 lot performance is achieved.

    Chemical resistance follows general high-density polyethylene behaviour. The grade is suitable for continuous contact with dilute mineral acids, aqueous salt solutions, and many polar solvents at ambient temperature. It is not recommended for continuous exposure to strong oxidising acids, chlorinated aromatic hydrocarbons, or aliphatic hydrocarbons at elevated temperature, because swelling and oxidative attack can occur. For potable water lines with free chlorine residuals above 2.0 ppm at temperatures above 60 °C, the chlorine resistance of the stabiliser package must be validated by the pipe producer; standard compression-moulded resin data do not cover long-term chlorine-induced crack growth.

    Welding of extruded HDPE 4003 sheet is normally conducted by hot-gas welding, extrusion welding, or butt fusion. For butt fusion of pipe, interface pressure and bead size should follow the equipment manufacturer’s procedure rather than generic values. Incompatibility with amine-based surface treatments is not a principal concern for polyethylene; however, melt blending with organic peroxides above 0.1 wt% can initiate controlled crosslinking and should not be performed without a defined reactivity protocol. If the resin is stored outdoors in translucent bulk containers, moisture adsorption alone is not harmful, but UV-degraded surface layers can generate volatile carbonyl species and should be purged before high-quality extrusion.

    Top