Sinopec Hainan Hdpe M577 S Hsgc7260

Sinopec Hainan HDPE M577-S(HSGC7260)

    • Product Name: Sinopec Hainan HDPE M577-S(HSGC7260)
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 821379
    Grade Name Sinopec Hainan HDPE M577-S(HSGC7260)
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.957 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 7.0 g/10 min
    Tensile Yield Strength ≥25 MPa
    Elongation At Break ≥500%
    Flexural Modulus ≥1000 MPa
    Izod Notched Impact Strength ≥40 kJ/m²
    Vicat Softening Temperature ≥125°C
    Heat Deflection Temperature ≥70°C
    Hardness Shore D ≥60
    Molding Shrinkage 1.5-3.0%
    Environmental Stress Cracking Resistance Escr ≥1000 h
    Water Absorption ≤0.01%
    Melting Point 130-135°C
    Brittleness Temperature ≤-70°C
    Dielectric Strength ≥20 kV/mm
    Volume Resistivity ≥1×10^16 Ω·cm
    Dielectric Constant 1 Mhz 2.3
    Loss Tangent 1 Mhz 0.0005

    As an accredited Sinopec Hainan HDPE M577-S(HSGC7260) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Hainan HDPE M577-S(HSGC7260) is supplied in 25 kg PP woven bags, 40 bags per 1,000 kg pallet, shrink-wrapped.
    Container Loading (20′ FCL) 20′ FCL container: Sinopec Hainan HDPE M577-S (HSGC7260) in 25 kg bags; approximately 25 MT net per container, securely loaded.
    Shipping Sinopec Hainan HDPE M577-S(HSGC7260) is a non-hazardous polyethylene resin. It is typically supplied in 25 kg bags or 1000 kg jumbo bags, palletized and stretch-wrapped. Ship in clean, dry containers by sea or land; store away from moisture, heat, and direct sunlight.
    Storage Store Sinopec Hainan HDPE M577-S (HSGC7260) in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, flames, strong oxidizers, and sources of ignition. Keep in original sealed bags or containers on pallets; avoid moisture, dust, and contamination. Observe safe stacking limits, prevent package damage, use first-in-first-out, and follow manufacturer/SDS guidance.
    Shelf Life Store in cool, dry, ventilated area away from direct sunlight; shelf life is typically 24 months in unopened original packaging.
    Application of Sinopec Hainan HDPE M577-S(HSGC7260)

    In high-throughput injection molding of collapsible logistics crates with nominal sidewall thickness between 2.8 mm and 3.5 mm, the processing window for Sinopec Hainan HDPE M577-S (HSGC7260) is constrained by two competing demands: sufficient melt front velocity to fill projected areas of 0.35 m² to 0.60 m² without short shots, and cooling rate uniformity adequate to hold flatness deviation below 2.0 mm across a 600 mm × 400 mm base. Molds are typically run on hydraulic clamp machines of 600 t to 1,200 t with accumulator-assisted injection speeds of 80 mm/s to 140 mm/s. Barrel temperature profile from feed to nozzle is set at 180 °C, 210 °C, 220 °C, 230 °C, 235 °C; nozzle melt temperature is maintained at 220 °C to 240 °C. Injection pressure measured at the machine transducer usually reaches 85 MPa to 110 MPa for a fill time of 1.8 s to 2.8 s, and velocity-to-pressure switchover by screw position is set at 95 % to 98 % of volumetric fill to avoid overpacking the gate region. Packing pressure is held at 45 MPa to 60 MPa for 8 s to 12 s, after which cooling time follows the square of wall thickness. For a 3.0 mm section, total cycle time remains between 28 s and 38 s depending on mold temperature of 12 °C to 28 °C. Mold shrinkage according to ISO 294-4 falls between 1.8 % and 2.4 % in the flow direction and 2.0 % to 2.8 % in the transverse direction, which requires rib-to-wall ratios not exceeding 0.5 to prevent sink marks on the outer face.

    The grade provides a melt flow rate of approximately 7.2 g/10 min under ASTM D1238 at 190 °C and 2.16 kg, with solid density of 0.956 g/cm³ to 0.959 g/cm³ under ASTM D792. This flow length is adequate for multi-cavity two-plate tools with edge gates or hot runner valve gates, but cold runner sprue diameters below 4.5 mm may generate pressure drops exceeding 25 MPa. Structural validation of crates molded from this grade uses tensile yield strength of 24 MPa to 27 MPa under ASTM D638 Type I and flexural modulus of 900 MPa to 1,100 MPa under ASTM D790. Notched Izod impact at 23 °C under ASTM D256 is commonly reported at 4.0 kJ/m² to 6.0 kJ/m², but for cold-chain logistics, impact testing at −20 °C is more discriminating because molded-in handle holes act as stress concentrators. Weld lines formed downstream of core pins in grip cutouts should be positioned away from high-strain zones or thickened to 1.5 times nominal wall thickness. Resistance to environmental stress cracking in detergent-contaminated return flows is evaluated by ASTM D1693 condition B, with typical failure time for M577-S exceeding 30 h in 100 % Igepal CO-630 at 50 °C; however, published data for this specific crate-return configuration is limited, and field validation under actual returnable crate washing chemicals is recommended.

    Does Thin-Wall Dairy Container Molding Require a Nucleated HDPE Variant?

    Sinopec Hainan HDPE M577-S (HSGC7260) is not supplied as a nucleated thin-wall grade; nevertheless, it can fill rectangular dairy tubs and deli containers with wall sections from 0.7 mm to 1.1 mm when the tool incorporates balanced fan gates and a chilled mold at 8 °C to 15 °C. The melt flow rate of approximately 7.2 g/10 min under ASTM D1238 lowers pressure at the spiral flow end; spiral flow length at 230 °C and 80 MPa is typically 180 mm to 220 mm for a 1.0 mm spiral. Injection velocity should be set so that fill time is below 1.2 s to avoid freeze-off at the flow front. Barrel set temperatures of 230 °C to 250 °C reduce viscosity but increase oxidative degradation risk; residence time should be kept below 5 min at melt temperatures above 230 °C. Parting line flatness tolerance of ±0.25 mm across a 500 mm stack of filled containers demands that mold cooling channels be spaced no more than 30 mm from cavity surface and that coolant temperature variation remain within ±1.5 °C. Demolding requires draft angles of 0.5° to 1.0° per side; textured sidewalls may require up to 2.0°.

    Food-contact compliance for thin-wall containers made from M577-S is established under FDA 21 CFR 177.1520(c) for olefin polymers and Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² for food simulants. Under EU 10/2011 Annex III, specific migration of total chromium from catalyst residues is not expected, but converters using regrind must verify that post-consumer reclaimed material is excluded. The absence of plasticizers in HDPE means phthalate migration testing under EU 10/2011 is not applicable; however, if color concentrates are added, they must themselves be fully compliant. Organoleptic performance in dairy applications is validated by sensory panel rather than a single ASTM method. For thin-wall molding, typical cycle times are 6 s to 10 s for a 500 mL container, with clamp force requirement of 4.0 kN/cm² to 6.5 kN/cm² of projected area. Maximum injection pressure recorded at the screw tip is 120 MPa to 140 MPa, and switchover to packing occurs by cavity pressure integration at 350 bar to 450 bar in the cavity near the gate.

    ParameterLogistics crateThin-wall container
    Melt flow rate ASTM D12387.2 g/10 min7.2 g/10 min
    Nozzle melt temperature220–240 °C230–250 °C
    Mold temperature12–28 °C8–15 °C
    Fill time1.8–2.8 s0.6–1.2 s
    Injection pressure85–110 MPa120–140 MPa
    Cooling channel spacing40–50 mm≤30 mm
    Nominal wall thickness2.8–3.5 mm0.7–1.1 mm

    For pail bodies and open-top industrial pails of 5 L to 25 L nominal capacity, the critical failure mode is not short-term burst but circumferential cracking at the handle hinge after stacked storage. Pail bodies produced from HDPE M577-S range from 180 g to 800 g depending on capacity. Multi-cavity pail tools use a central sprue or valve-gated hot runner; the gate diameter should be at least 6.0 mm to avoid excessive shear heating. Melt temperature at the nozzle is controlled to 210 °C to 230 °C, lower than in thin-wall molding because longer flow paths are less critical and thermal degradation from long residence in large shot weights is of concern. Injection speed is reduced to 40 mm/s to 70 mm/s to avoid jetting on the sidewall; whenever jetting occurs, surface streaks and localized internal stress are observed. Packing pressure is set to 50 MPa to 65 MPa and applied for 10 s to 15 s, with gate seal verified by screw cushion stability of ±1.0 mm. Mold temperature of 10 °C to 20 °C is maintained to achieve a cycle of 25 s to 45 s for 20 L pails. Shrinkage after 24 h under ISO 294-4 is 1.9 % to 2.5 %; therefore lid seat inner diameter compensation of plus 0.4 mm to 0.8 mm is applied.

    UN certification for dangerous goods packaging under 49 CFR Part 178 or the UN Model Regulations requires stack stability and drop impact. For a 20 L pail filled to a specific gravity of up to 1.5, the drop test height under UN 6.1.5.3 for packing group II is 1.2 m at −18 °C; the pail must show no leakage after impact. Stack testing for 28 days at 40 °C is specified in UN 6.1.5.6, with load equal to 1.8 times the mass of the stack under transport conditions. M577-S tensile yield strength of 24 MPa to 27 MPa under ASTM D638 and flexural modulus of 900 MPa to 1,100 MPa under ASTM D790 provide sufficient top-load performance when sidewall vertical ribs are used. Environmental stress crack resistance against aggressive filling goods such as detergents, emulsifiers, and hydrocarbons is assessed by ASTM D1693 condition A or B; the 100 % Igepal test is severe, and actual chemical compatibility should be verified in sealed pails at 40 °C for 21 days. Pails intended for solvent-based products with xylene or toluene above 10 wt% are outside the recommended service envelope because rapid stress cracking may occur.

    When Gasketless HDPE Closure Torque Decay Falls Below 0.3 N·m

    Closure shells of 1.8 g to 4.5 g shot weight molded from Sinopec Hainan HDPE M577-S (HSGC7260) are specified for still water, dairy, and agrochemical bottles where tamper-evident bands and knurled outer surfaces are required. Multi-cavity tools of 32 to 64 cavities run on high-speed injection machines with clamp force of 200 t to 350 t. The melt temperature is maintained at 230 °C to 250 °C; injection fill time is 0.4 s to 0.9 s because of thin shell wall of 0.9 mm to 1.4 mm. Holding pressure of 35 MPa to 50 MPa is held for 2.5 s to 4.0 s, and cooling time is 4.0 s to 7.0 s. The tamper-evident band must be stretched over the bottle neck finish without stress whitening; this requires elongation at break of more than 200 % under ASTM D638 at 50 mm/min. Dimensional control of the inner cap diameter is critical: mold shrinkage in that diameter is 1.9 % to 2.4 %, so cavity diameter is oversized accordingly and verified by CMM after 24 h conditioning at 23 °C ± 2 °C and 50 % ± 5 % RH.

    Torque retention after application is an operational boundary. For a 28 mm PCO 1881 neck finish, application torque is typically 1.8 N·m to 2.2 N·m; removal torque after 24 h at 23 °C should remain above 0.8 N·m. A decay below 0.3 N·m indicates insufficient elastic recovery in the thread region or excessive mold release modifier. The grade is supplied without slip additives; therefore torque values are controlled by thread flank geometry rather than additive bloom. Environmental stress cracking resistance of closures in contact with surfactant-containing products is tested according to ASTM D1693 condition A, with a minimum time to 50 % failure of 20 h typical for HDPE. For closures used with household bleach or quaternary ammonium disinfectants, sealed bottle testing at 40 °C for 14 days under ASTM D543 immersion is recommended because oxidation can reduce hoop strength. Published data for this specific closure-neck configuration is limited; users must validate closure security on their specific neck finish, especially when the bottle is made from a different polymer.

    For lead-acid battery containers molded from high-density polyethylene, the validation matrix differs from food-contact packaging in every respect. Battery containers and lids molded from HDPE M577-S must sustain sulfuric acid immersion at specific gravity 1.28 for the service life of the battery. The base resin does not contain metallic stearate levels that would interfere with plate adhesion; however, oxidative degradation in warm acid is a limitation. Molding uses multi-cavity tools with wall thickness of 2.0 mm to 3.5 mm and injection compression or coining to reduce orientation. Melt temperature is 220 °C to 245 °C; mold temperature is 20 °C to 35 °C. Because thick sections and ribs around cell partitions produce sink marks, gas counterpressure or core cooling may be required. Cycle time for a 12 V automotive case is typically 50 s to 90 s depending on wall thickness. Dimensional stability after molding is checked after 48 h annealing at 80 °C, with shrinkage per ISO 294-4 of 1.8 % to 2.5 % accounted for in cavity dimensions.

    Chemical resistance is evaluated by ASTM D543 immersion in 40 % sulfuric acid at 60 °C for 7 days; typical tensile strength retention exceeds 85 % for HDPE, but this must be verified on molded parts because orientation and internal stress reduce retention. Impact testing at −30 °C is performed according to ISO 179-1/1eU, with unnotched Charpy impact above 25 kJ/m² desirable. Vibration fatigue on battery containers is based on OEM specifications, often 8 h to 72 h at 10 Hz to 500 Hz sine sweep with 3 g to 5 g acceleration on a fixture; no cracks at cell partition bases are permitted. The M577-S grade is not inherently flame-retardant; applications requiring UL 94 V-2 or V-0 are outside its service envelope without halogenated or intumescent additives. Antioxidant packages for battery containers must avoid amine-based additives that can leach into acid and cause plate corrosion; converters must select color concentrates and additives compatible with acid immersion.

    Pallet Manufacturing Without Structural Foam: Solid-State Packing Pressure Requirements

    Injection-molded pallets and heavy-duty material-handling platforms from HDPE M577-S occupy a different moulding regime because shot weights reach 8 kg to 20 kg and wall sections vary from 4.0 mm to 18.0 mm. The resin’s melt flow rate of approximately 7.2 g/10 min under ASTM D1238 is higher than conventional pallet HDPE grades with 2.0 g/10 min, which improves filling of grid ribs but extends cooling time and raises the risk of shrink voids at thick junctions. Barrel temperature profile is kept at 200 °C, 210 °C, 220 °C, 230 °C, 235 °C; nozzle temperature is 230 °C to 240 °C. Injection pressure is limited to 70 MPa to 90 MPa, and the mold must be opened slightly after fill in injection-compression mode or the machine must use sequential valve gates to avoid jetting. Solid-state packing pressure is held at 45 MPa to 60 MPa for 20 s to 35 s, with gate seal verified by screw recovery position repeatability of ±1.5 mm. Cooling time for 14.0 mm thick rib intersections is calculated using the relationship t_cool ≈ (h²/π²α) ln[(8/π²)(T_melt − T_mold)/(T_eject − T_mold)]; for HDPE thermal diffusivity α approximately 0.08 mm²/s to 0.12 mm²/s, total cycle time can exceed 120 s. Cooling channels must be placed at 40 mm to 60 mm from cavity surfaces and supplied with water at 10 °C to 25 °C; mold temperature differential across the tool should be below 5 °C to avoid warpage.

    Structural acceptance of pallets under ISO 8611-1 includes rated load of 500 kg to 1,250 kg for racking and 2,000 kg for floor storage. Flexural modulus of 900 MPa to 1,100 MPa under ASTM D790 and tensile yield of 24 MPa to 27 MPa under ASTM D638 give the required stiffness at reduced wall section, but long-term creep under static load is evaluated by ISO 899-1 at 23 °C. For 1,000 h creep modulus of HDPE at 20 % of tensile yield stress is typically 350 MPa to 500 MPa, so pallet design must use ribbed architecture rather than flat plate sections. Impact resistance at −20 °C with a 5 kg striker is assessed by ISO 6603-2; puncture energy for 4.0 mm HDPE sheet typically exceeds 15 J, but published data for this specific grade is limited. Pallet applications requiring sustained contact with diesel, lubricating oil, or aggressive cleaning chemicals should be validated by immersion testing because environmental stress cracking accelerates with increasing temperature and stress.

    Free Quote

    Competitive Sinopec Hainan HDPE M577-S(HSGC7260) prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Hainan HDPE M577-S (HSGC7260) is a high-density polyethylene blow-moulding resin produced at the Hainan petrochemical complex. The product is supplied as virgin pellets for continuous extrusion blow moulding and injection-blow moulding of rigid hollow containers. In the manufacturer’s technical documentation, the resin carries a dual designation: M577-S is the commercial grade identifier and HSGC7260 is the product code used in certain trade records and lot-layer documentation.

    The nominal density is 0.957 g/cm³ when determined according to ISO 1183-1:2019, and the melt flow rate is reported as 0.70 g/10 min at 190 °C under 2.16 kg load using ISO 1133-1:2022. These values place the grade in the high-density polyethylene class with a molecular weight distribution typical of high-melt-strength blow-moulding resins. The combination of density and melt flow rate differentiates the resin from injection-moulding HDPE grades, which generally display melt flow rates above 4 g/10 min, and from high-molecular-weight film grades, which display melt flow rates below 0.1 g/10 min.

    What Are the Specification Limits for Sinopec Hainan M577-S?

    Table 1 reproduces typical property values from the grade datasheet. These values are target lot properties and do not replace the lot-specific certificate of analysis. Published data for capillary rheometry and melt tension at shear rates above 1,000 s⁻¹ is limited; process validation should therefore include laboratory-scale extrusion trials before conversion to multi-cavity production tools.

    PropertyTypical valueTest method
    Melt flow rate (190 °C, 2.16 kg)0.70 g/10 minISO 1133-1:2022
    Density0.957 g/cm³ISO 1183-1:2019
    Tensile yield stress28 MPaISO 527-2:2012
    Tensile elongation at break600 %ISO 527-2:2012
    Flexural modulus1,100 MPaISO 178:2019
    Notched Izod impact at 23 °C5 kJ/m²ISO 180:2019
    Environmental stress-crack resistance, F50, 100% Igepal CO-630, 50 °C1,000 hrASTM D1693
    Vicat softening temperature, A50126 °CISO 306/A50
    Shore D hardness62ISO 868

    The environmental stress-crack resistance value is measured at 50 °C in 100% Igepal CO-630; values obtained in 10% Igepal are not directly comparable because the lower concentration reduces crack acceleration and increases time to failure. This distinction is important when comparing competing HDPE blow-moulding grades that may be reported under different ESCR conditions.

    Continuous Extrusion Blow Moulding Equipment Response

    On a continuous shuttle blow-moulding line with a 24:1 L/D single-screw extruder and 50 mm screw diameter, the recommended barrel temperature profile is 170–190 °C in the feed zone, 190–210 °C in the compression zone, and 210–230 °C at the die head. Melt temperature should be maintained between 200 °C and 230 °C. The upper limit is critical: above 230 °C, parison sag accelerates and the risk of thermo-oxidative chain scission increases in proportion to residence time. At melt temperatures below 200 °C, surface melt fracture appears as shark-skin roughness, particularly on tooling with narrow land lengths.

    Extruder head pressure typically rises to 150–250 bar at screw speeds of 40–80 min⁻¹. The exact pressure-throughput relationship depends on die gap, accumulator shot size, and screw geometry. Die swell measured on a 40 mm annular die at 210 °C is in the range 45–55%; parison programming is therefore necessary for containers with a length-to-diameter ratio above 2:1. Blow air pressure is typically 0.6–0.8 MPa and mould temperature is maintained at 15–30 °C to shorten cycle time and improve top-load stiffness. Clamp force requirements for 1 L containers are typically 40–80 kN, but multi-cavity tools require higher forces consistent with total projected mould area.

    Storage above 60% relative humidity will require pre-drying at 80 °C for 2–4 hr in a desiccant dryer. The grade is not suitable for thin-wall injection moulding because its high molecular weight increases injection fill pressure beyond the range of standard 1,200 bar machines. Additive compatibility should be confirmed before use; amine-bearing colorants have been associated with accelerated oxidative degradation in high-density polyethylene during long-term ultraviolet exposure, although the effect is formulation-specific. Production-scale shuttle lines have also shown that batch-to-batch variation in gel content can influence pinch-off weld-line appearance, so in-house recycling should use a 250 μm melt filter when regrind content exceeds 20% of the total blend.

    When HDPE M577-S Replaces Generic 0.35–0.7 Melt Flow Rate Blow Moulding Grades

    Compared with lower-melt-flow-rate HDPE blow-moulding resins, M577-S increases extrusion throughput at equal screw speed because of its 0.70 g/10 min melt flow rate. The trade-off is reduced parison hang strength; containers above 5 L may require thicker parison programming segments to maintain wall-thickness uniformity. Compared with higher-melt-flow-rate grades, M577-S provides higher notched Izod impact and a longer environmental stress-crack resistance failure time of approximately 1,000 hr under ASTM D1693 conditions. This property is relevant for containers holding detergents, surfactants, and automotive fluids.

    Relative to lower-density HDPE grades at 0.950 g/cm³, the 0.957 g/cm³ density of M577-S raises top-load strength and reduces creep under stack load. Relative to injection-moulding HDPE grades with melt flow rates above 4 g/10 min, M577-S is not suitable for high-speed injection moulding of thin-wall housewares. The grade is also not intended for film extrusion or pressure-pipe production, where PE100-grade molecular architecture, comonomer distribution, and additive packages are specifically required. The dual designation should not be mistaken for a different product; M577-S and HSGC7260 refer to the same base resin.

    Regulatory Compliance, Migration Testing, and Lot-Release Documentation

    Compliance statements for M577-S follow the food-contact and hazardous-substance frameworks shown in Table 2. Final article compliance is the responsibility of the converter because colourants, regrind, and processing aids alter the migration profile. The table lists the most frequently referenced standards for rigid HDPE packaging, but it does not replace a formal conformity declaration from the manufacturer.

    Regulatory frameworkRelevant scope
    FDA 21 CFR 177.1520Olefin polymers for food contact; final article compliance is condition-of-use dependent.
    EU Regulation (EU) No 10/2011Plastic food contact materials; overall migration limit 10 mg/dm²; specific migration limits per Annex II.
    GB 4806.7-2023Chinese national food safety standard for plastic materials and articles for food contact.
    REACH Regulation (EC) No 1907/2006SVHC concentration at article level below 0.1% w/w.
    RoHS Directive 2011/65/EURestricted substances including lead 0.1% and cadmium 0.01%.

    Public datasheets for M577-S do not typically include full migration test reports; a lot-specific migration certificate should be requested for food-contact end uses. When the resin is used in containers for dairy, personal-care, or household-chemical products, the converter should verify the final article under the intended fill temperature and contact time. Typical converted articles include 0.5 L to 5 L bottles for household chemicals, 0.2 L to 2 L personal-care containers, and automotive fluid reservoirs. The grade is selected where high density, moderate melt flow rate, and long environmental stress-crack resistance must be balanced against cycle time and parison control.

    Top