| HS Code | 372984 |
| Density | 0.953 g/cm3 |
| Meltflowrate | 0.16 g/10min |
| Tensileyieldstrength | ≥25 MPa |
| Tensilebreakstrength | ≥30 MPa |
| Elongationatbreak | ≥500% |
| Flexuralmodulus | ≥1100 MPa |
| Notchedizodimpactstrength | ≥50 kJ/m2 |
| Vicatsofteningtemperature | ≥123 °C |
| Brittlenesstemperature | ≤-70 °C |
| Environmentalstresscrackingresistance | ≥1000 h |
| Shoredhardness | 62 |
| Waterabsorption | <0.01% |
| Thermalexpansioncoefficient | 1.2E-4 /°C |
| Ashcontent | ≤0.05% |
| Moisturecontent | ≤0.1% |
As an accredited Sinopec Guangzhou HDPE DMDB8916 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Typically packed in 25 kg PE-lined PP woven bags, Sinopec Guangzhou HDPE DMDB8916 pellets are palletized for transport and storage. |
| Container Loading (20′ FCL) | 20′ FCL loads about 17.5 MT of Sinopec Guangzhou HDPE DMDB8916, packed in 25 kg bags (700 bags per container). |
| Shipping | Sinopec Guangzhou HDPE DMDB8916 is shipped as a non-hazardous thermoplastic resin in 25 kg woven bags or 500/1000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks. Store cool, dry, away from sunlight, moisture, heat, and incompatible chemicals. |
| Storage | Store Sinopec Guangzhou HDPE DMDB8916 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep bags closed to prevent moisture, dust, and contamination. Avoid strong oxidizers. Store on pallets off the floor with adequate aisle space and no excessive stacking. Use FIFO stock rotation; protect from physical damage. Follow local regulations and the safety data sheet. |
| Shelf Life | Typically 12 months from production when stored unopened in a cool, dry, ventilated area, away from direct sunlight. |
For edible oil and sauce bottles produced on single-station shuttle blow molders, Sinopec Guangzhou HDPE DMDB8916 is processed as a high-density polyethylene with a nominal density of 0.958 g/cm³ and a melt mass-flow rate of 0.6 g/10 min at 190°C/2.16 kg under ISO 1133-1:2022. Food-contact status rests on FDA 21 CFR 177.1520(c) 2.1, China GB 4806.6-2016, and EU No 10/2011 for overall migration limits of 10 mg/dm² in applicable food simulants. A grooved feed extruder with L/D 30:1 and compression ratio 3.0:1 to 3.5:1 delivers a homogenized melt to a diverging die head. Barrel zone temperatures are set at 170°C, 180°C, 190°C, and 195°C, with the head maintained at 200°C to 210°C. The die gap is held at 1.2 mm to 1.6 mm, and parison programming with an 8-point axial wall thickness controller reduces corner thinning in handleware to less than 20% of nominal wall. Mold temperatures between 20°C and 30°C and blow air pressure of 0.7 MPa to 0.9 MPa produce a 500 mL bottle with a cycle time of 12 s to 15 s. Average top-load resistance ranges from 220 N to 320 N for a 500 mL container with 0.7 mm to 0.9 mm wall thickness under ASTM D2659 at 23°C. Only in-house regrind from the same food-contact production campaign may be reintroduced at up to 30 wt%; post-consumer recycled material is prohibited unless the recycling process has an applicable authorization. Hot-fill use is not recommended above 70°C because HDPE paneling and creep at the neck finish can compromise seal integrity. The grade is also not a barrier layer for oxygen-sensitive edible oil products unless a coextruded or coated barrier is engineered into the bottle structure.
Sodium hypochlorite bleach containers and heavy-duty detergent bottles impose stress-cracking demands that cannot be evaluated by tensile yield alone. Slow crack growth at the handle weld and base flash is the dominant field failure in this segment, and ASTM D1693 condition B with 100% Igepal CO-630 at 50°C is the standard screening method. For an HDPE homopolymer of 0.958 g/cm³ density, the grade typically exhibits F50 values in the range of 40 h to 100 h; the lower bound should be used for detergent and hypochlorite packaging because oxidative formulations accelerate crack propagation. Continuous shuttle machines with 80 mm extruder diameter and 24:1 to 30:1 L/D are common on production lines. Wall thickness around handle sections is kept above 0.7 mm, and a die gap of 1.5 mm to 2.0 mm is used for 1 L containers. The mold pinch-off land width is set at 1.5 mm; below 1.0 mm, cracked weld defects at the knit line can exceed 3% of production after drop testing from 1.2 m. Melt temperatures above 220°C oxidize the surface and produce gel particles visible as black specks in unpigmented bottles. Bleach bottle validation requires a filled-bottle drop test at 23°C and a post-drop inspection of the handle pinch area under 10× magnification for microcracks. Post-consumer reclaim must be excluded from oxidative packaging because uncontrolled polyethylene grades lower ESCR and introduce stress risers.
At a parison temperature of 195°C, a die gap wider than 1.6 mm increases sag rate above 12 mm/s for a 300 mm parison length. The resulting bottom-wall thinning on a 300 mL cylindrical bottle reaches 25% to 30% relative to the label panel. Narrow-neck cosmetic bottles therefore require a converging die with a land length of 12 mm to 16 mm, a die gap of 1.0 mm to 1.4 mm, and a diverging tip angle of 15° to 20°. A parison programmer with 16-point radial adjustment controls the upper shoulder and base pinch-off zones where wall thinning is most severe. Mold polish of SPI A2 or A3 is required for high-gloss external surfaces, and mold temperature is held at 25°C to 35°C to avoid sink marks around the neck insert. Blow pressure is set at 0.8 MPa for 100 mL to 400 mL oval and cylindrical bottles. When a pearlized or pearlescent masterbatch is added at 2 wt% to 3 wt%, the melt temperature must not exceed 205°C to avoid titanium dioxide-catalyzed oxidation and surface streaking. In-house regrind is limited to 20 wt% to retain surface gloss and reduce black specks. The grade’s density of 0.958 g/cm³ supports drop performance at 1.5 m for a 100 mL bottle when minimum wall thickness remains above 0.5 mm. Processing above 210°C creates parison draw marks and die lines that cannot be corrected by downstream flame treatment.
Pharmaceutical-grade extrusion blow molding of DMDB8916 requires segregation of production campaigns and documented additive composition. Primary packaging for oral syrup dropper bottles and non-implantable pharmaceutical devices is evaluated under USP <661.1> and Ph.Eur. 3.1.3. The resin does not contain slip additives unless explicitly declared on the clean-room production record. Tooling for 20 mL dropper bottles uses 12-cavity shuttle systems. Core pin temperature is controlled at 10°C to 15°C, cavity temperature at 20°C to 25°C, and the neck finish requires an insert surface roughness below 0.8 µm to achieve reliable sealing with rubber teats and screw caps. Blow air pressure of 0.6 MPa to 0.8 MPa is sufficient for the thin wall sections because the cavity is small and the parison is short. Gamma sterilization at doses up to 25 kGy is generally tolerated by HDPE packaging; above 40 kGy, elongation at break may decrease and discoloration can be visible. Packaging validation should include post-irradiation seal torque and axial crush testing because neck thread embrittlement can occur if excessive oxidation is present. DMDB8916 is not appropriate for parenteral primary containers unless extractables and leachables data for the finished packaging system support the specific clinical application. Clean-room molding at ISO Class 8 or better reduces particulate contamination in the threaded closure area.
| Standard or regulation | Test focus | Application boundary for DMDB8916 |
|---|---|---|
| FDA 21 CFR 177.1520(c) 2.1 | Olefin polymer identity and total extractables | Food-contact primary bottle; in-house regrind only |
| EU No 10/2011 | Overall migration limit | 10 mg/dm² overall migration for applicable simulants |
| GB 4806.6-2016 | China food-contact plastics | Bottles and closures for edible oils and sauces |
| USP <661.1> | Plastic packaging physico-chemical evaluation | Oral dosage dropper bottles and auxiliary packaging |
| Ph.Eur. 3.1.3 | Polyolefin packaging materials | Non-parenteral pharmaceutical containers |
| ASTM D1693 condition B | Environmental stress crack resistance | Detergent, bleach, and short-term oxidative liquid packaging |
Windshield washer fluid bottles require a weld line at the tail flash that does not fail under sub-zero impact. Mold closing speed is set at 150 mm/s to 250 mm/s; a slower speed allows the parison to fold and creates an incomplete weld at the parting line. The pinch-off insert is made from H13 tool steel with a land width of 1.5 mm to 2.0 mm and a vent slot height of 0.02 mm to 0.05 mm. Blow air pressure at 0.8 MPa to 1.0 MPa forces flash into the vent, leaving a flash thickness of 0.2 mm to 0.4 mm. The trimmed weld is tested by drop impact at -30°C from 1.2 m using a 50% methanol-water load; accepted bottles contain no cracks at the weld region. For cold-fill windshield washer fluid bottles, the resin’s density of 0.958 g/cm³ provides adequate panel stiffness, but service temperature must remain below 75°C. Coolant expansion reservoirs are restricted to non-pressurized cold-fill designs because continuous exposure to ethylene glycol above 120°C is outside the grade’s long-term thermal capability. Hot plate welding of filler necks and handle supports requires a heated tool temperature of 220°C to 240°C and a weld displacement of 0.8 mm to 1.2 mm to achieve consistent burst strength. Regrind from automotive flash can be reintroduced at up to 35 wt% if the material is dry, free of oil contamination, and screened through a 6 mm granulator screen.
Converting DMDB8916 into UN-rated jerry cans for agrochemical emulsifiable concentrates requires compounding with carbon black masterbatch at 2.0 wt% to 3.0 wt% carbon black content and screening for ESCR under ASTM D1693 condition C at 50°C. UN Model Regulations Packing Group II impose a drop height of 1.2 m, while Packing Group III requires 0.8 m. The stacking test is conducted at 1.5 times gross mass for 28 days at 40°C. Accumulator head machines with 2.0 mm to 2.8 mm die gap and 600 mm to 800 mm parison length are used for 5 L jerry cans. The resin alone is not a barrier for xylene, cyclohexanone, or aromatic solvents; monolayer containers are limited to aqueous suspension concentrates and water-based formulations. Surface fluorination reduces hydrocarbon permeation for solvent-based formulations but changes food-contact status and must be specified before compounding. Flash regrind is added at up to 35 wt%, but outdoor UV exposure demands that carbon black concentration in the final article be maintained above 2.0 wt%. Welding of jerry can handles requires that the pinch-off weld be visually inspected for fiber pull-out and thickness variation because freeze-thaw cycling of water-based agrochemical formulations can open incomplete welds.
Competitive Sinopec Guangzhou HDPE DMDB8916 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Sinopec Guangzhou HDPE DMDB8916 is a high-density polyethylene blow-moulding grade produced at Sinopec Guangzhou Petrochemical and classified in manufacturer technical bulletins as a hexene-1–modified high-molecular-weight resin. The grade is distinct from general-purpose HDPE because the melt flow rate reported under ISO 1133-1:2022 is nominally 0.16 g/10 min at 190 °C with a 2.16 kg load, while density measured under ISO 1183-1:2019 is reported as 0.949 g/cm³. This combination places DMDB8916 in the high-molecular-weight HDPE range used for large rigid containers, where parison hang stability and slow-crack growth resistance govern the fitness of the moulded article, rather than in the low-viscosity injection-moulding or small-bottle HDPE range where flow length and cycle time dominate.
The product is typically specified for monolayer extrusion blow moulding of 120–220 L tight-head and open-top drums, intermediate bulk container inner bottles, agrochemical containers and industrial packaging. The hexene comonomer is selected to disrupt crystallinity sufficiently to increase tie-molecule density, which improves environmental stress-cracking resistance relative to homopolymer HDPE of similar melt flow. Because the grade is not formulated as a food-contact-specific grade by default, food-contact status must be confirmed against the manufacturer’s declaration and finished-article migration testing under the relevant food-contact regulation. Industrial use for dangerous goods packaging is governed by article-level UN drop and stacking certification rather than by resin properties alone.
| Property | Test method | Reported typical value |
|---|---|---|
| Melt flow rate, 190 °C / 2.16 kg | ISO 1133-1:2022 | 0.16 g/10 min |
| Density, 23 °C | ISO 1183-1:2019 | 0.949 g/cm³ |
| Tensile yield stress | ISO 527-2:2012 | 26 MPa |
| Nominal tensile elongation at break | ISO 527-2:2012 | >600 % |
| Flexural modulus | ISO 178:2019 | 1050 MPa |
| Notched Charpy impact strength, 23 °C | ISO 179-1:2010 | 25 kJ/m² |
| Environmental stress-cracking resistance, F50, 100 % Igepal CO-630 | ASTM D1693-15 condition B | >500 h |
The tabulated values are typical values from published supplier bulletins and do not constitute specification limits. Certificate-of-analysis values should be used for lot acceptance, and finished article properties should be validated on the intended production tool.
Accumulator-head extrusion blow moulding of DMDB8916 is constrained by two competing failure modes. The lower boundary is set by high melt viscosity and surface defects; if head and die zones are kept below approximately 185 °C, the high-molecular-weight fraction increases die pressure and can produce sharkskin melt fracture on the parison surface. The upper boundary is set by parison drawdown; above 220 °C the melt strength decreases to a level at which large shot weights can sag before mould closure. Production machines producing 200 L drums therefore typically operate with melt temperatures of 190–220 °C, die heads at 185–210 °C, and mould surfaces at 10–30 °C, with blow air pressure between 0.6 MPa and 0.8 MPa.
The grade’s low melt flow means that general-purpose single-screw extruders with shallow screws and short L/D ratios may struggle to generate stable output. Technical guidance for high-molecular-weight HDPE blow-moulding grades of this class recommends grooved-feed extruders with L/D ratios of 24:1 to 30:1, barrier screws, and high-torque drives. The grooved barrel increases solids conveying and allows higher head pressure without excessive melt temperature. On accumulator-head machines, the shot pot capacity is matched to the article weight; for 220 L tight-head drums, shot weights in the range of 8–12 kg are typical, although published product-specific shot-weight data for DMDB8916 are limited.
Moisture control for HDPE is not a primary processing variable because the resin is not hygroscopic. Under ambient storage below 60 % relative humidity, pre-drying is not required. If pellet surfaces become wet through cold-to-warm transfer condensation, hopper drying at 70–80 °C for 1–2 h prevents surface splay, but drying temperatures above 90 °C risk pellet softening and feed-throat bridging. Batch-to-batch MFR variation within the certificate of analysis should be checked before switching lots on a running accumulator-head machine because a shift of 0.02 g/10 min in low melt flow can alter parison hang time and require head temperature adjustment.
No product-specific chemical incompatibility is listed in the safety data sheet. The usual HDPE compatibility limits apply: prolonged exposure to strong oxidizing acids, halogens, and aromatic or chlorinated hydrocarbons at elevated temperature swells and accelerates cracking. Concentrated nonylphenol-based surfactants and certain agricultural emulsifiers can reduce environmental stress-cracking resistance in stressed bottle shoulders and pinch-off welds. When concentrates are added, letdown ratios for blue, black, or antistatic masterbatch should be verified by melt-flow stability and ESCR testing under ASTM D1693-15 rather than by visual dispersion alone.
Article qualification for dangerous goods packaging requires testing of the finished container, not the resin alone. The typical route includes UN 6.1.5.3 drop testing, leakproofness testing under UN 6.1.5.4, hydraulic pressure testing under UN 6.1.5.5, and stacking under UN 6.1.5.6, with filled weights determined by the article design. DMDB8916 is selected for such containers because its ESCR performance at the resin level supports longer life under chemically aggressive lading when the container design avoids sharp pinch-off notches. For UV-exposed outdoor storage, carbon black or UV stabilizer masterbatch is required because unpigmented HDPE embrittles after prolonged ultraviolet exposure; the dosage of carbon black masterbatch is typically 2–3 wt% but must be validated for impact retention at -20 °C using ISO 179-1:2010 or instrumented drop testing.
The difference between DMDB8916 and a conventional unimodal HDPE blow-moulding grade is not fully captured by density and melt flow alone. In a unimodal resin with the same 0.16 g/10 min MFR and 0.949 g/cm³ density, the molecular weight distribution is narrower and the high-molecular-weight tail is reduced. Supplier technical descriptions commonly classify DMDB8916 as a hexene-1–modified HDPE with a broad or bimodal molecular weight distribution, in which the lower-molecular-weight fraction contributes processability while the high-molecular-weight fraction contributes tie molecules between lamellae. The practical result is higher slow-crack growth resistance at comparable stiffness, as measured by ESCR testing under ASTM D1693-15 and by notched Charpy impact under ISO 179-1:2010. In direct substitution on an existing tool, unimodal HDPE may cycle faster at lower head pressure, but the article may fail earlier under the same aggressive lading, particularly at pinch-off seams and around handle inserts.
At the same density, an injection-moulding HDPE with MFR 7–20 g/10 min has a much lower melt strength and cannot be suspended as a parison on large tools; it is limited to high-speed injection moulds where wall thickness is generally below 5 mm. Conversely, a high-molecular-weight film HDPE with MFR 0.05–0.12 g/10 min may exhibit even higher melt strength, but its additive package and die swell characteristics are not optimized for blow moulding; the parison can show excessive weight swell variability across the die circumference. DMDB8916 is therefore positioned as a large-part blow-moulding grade rather than a general-purpose extrusion or injection grade.
| HDPE processing family | Typical melt flow rate, ISO 1133-1:2022 | Typical density, ISO 1183-1:2019 | Main blow-moulding implication |
|---|---|---|---|
| DMDB8916 high-molecular-weight blow moulding | 0.16 g/10 min | 0.949 g/cm³ | Large-part parison stability and ESCR; requires high head pressure |
| General small-bottle HDPE | 0.30–0.50 g/10 min | 0.954–0.958 g/cm³ | Higher output; reduced melt strength; lower ESCR |
| Injection-moulding HDPE | 7–20 g/10 min | 0.956–0.964 g/cm³ | Thin-wall flow length; unsuitable for parison-suspended blow moulding |
| Bimodal film HDPE | 0.05–0.12 g/10 min | 0.947–0.952 g/cm³ | High bubble stability and downgauging; not optimized for blow-moulding die swell |
The values in the table are family-level ranges, not certificates for specific commercial grades; they illustrate the processing and property trade-offs relevant to grade substitution.
In multi-layer extruder lines where DMDB8916 is combined with polyamide or ethylene-vinyl alcohol barrier layers, the processing limits become more complex than in monolayer operation. The HDPE layers provide structural stiffness and ESCR, while the barrier layer controls oxygen or hydrocarbon permeation. Because HDPE is nonpolar, direct adhesion to EVOH or polyamide is insufficient; a maleic anhydride–grafted tie resin is required. The rheological match between DMDB8916 and the tie layer is important: if the tie layer has a higher MFR and lower melt strength than the HDPE skin, the parison may exhibit interfacial instability during inflation. The recommended approach is to select a tie resin with a melt flow rate within approximately 0.1–0.3 g/10 min or to use a dedicated high-melt-strength tie grade, but published data for DMDB8916-specific coextrusion are limited.
Weld-line integrity in the pinch-off region is a greater risk in multi-layer structures because the barrier layer can be displaced at the weld line, creating a localized reduction in barrier function. Blow moulders compensate by increasing die temperature and by adjusting tool pinch-off land geometry; however, if the melt temperature is raised beyond 220 °C to improve weld fusion, parison sag and wall-thickness variation increase. A process-sensitive balance is to run near 210 °C at the die while increasing blow delay only enough to allow the melt fronts to fuse. This balance is recognized in accumulator-head coextrusion of 220 L barrier drums, though article-specific data require tool trials.
Chemical incompatibilities are more restrictive in multi-layer packaging because the lading may contact the HDPE skin through imperfections in the barrier layer. For aggressive agrochemicals, oils, and solvent-based formulations, the finished container must pass ESCR testing after storage at 40 °C for 14 days or equivalent, depending on the lading. DMDB8916’s value in these structures is the retention of ESCR in the regrind layer; however, regrind content should not exceed 30 wt% unless validated by drop impact and ESCR tests on the finished part, because repeated heat history degrades the high-molecular-weight tail and narrows the process window.