Sinopec Guangzhou Hdpe Dmdb8910

Sinopec Guangzhou HDPE DMDB8910

    • Product Name: Sinopec Guangzhou HDPE DMDB8910
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 758459
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.954 g/cm³
    Melt Flow Rate 10 g/10 min
    Tensile Yield Strength 26 MPa
    Elongation At Break 500%
    Flexural Modulus 1100 MPa
    Izod Notched Impact Strength 5 kJ/m²
    Vicat Softening Point 125 °C
    Brittleness Temperature -70 °C
    Hardness 65 Shore D
    Environmental Stress Cracking Resistance 30 h
    Water Absorption <0.01%
    Mold Shrinkage 1.5-3.0%
    Melting Point 130-135 °C
    Thermal Deformation Temperature 80 °C
    Volume Resistivity >10^16 Ω·cm
    Dielectric Constant 2.3
    Dielectric Strength >20 kV/mm
    Processing Temperature 200-260 °C

    As an accredited Sinopec Guangzhou HDPE DMDB8910 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg woven bags, Sinopec Guangzhou HDPE DMDB8910 is packaged as white high-density polyethylene resin pellets.
    Container Loading (20′ FCL) 20′ FCL container loading of Sinopec Guangzhou HDPE DMDB8910: 25 kg bags, palletized, shrink-wrapped, and securely stowed for sea freight.
    Shipping Sinopec Guangzhou HDPE DMDB8910 is typically shipped as a non-hazardous thermoplastic resin in 25 kg woven bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Store dry, cool, and ventilated; protect from moisture, direct sunlight, heat, and ignition sources. Not DOT/IMDG/IATA regulated.
    Storage Store Sinopec Guangzhou HDPE DMDB8910 in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags closed, palletized, and off the floor to prevent moisture and contamination. Avoid excessive stacking and rough handling. Maintain clean, dust-free conditions; use appropriate grounding to prevent static buildup. Shelf life is typically 24 months under proper storage.
    Shelf Life Shelf Life: Typically 24 months in unopened original packaging, stored cool, dry, well-ventilated, away from direct sunlight and heat.
    Application of Sinopec Guangzhou HDPE DMDB8910

    Extrusion blow molding of 200-L tight-head drums for liquid chemical transport places Sinopec Guangzhou HDPE DMDB8910 at the intersection of two critical process boundaries: melt strength sufficient to suspend a parison of 4.5–8.0 kg over a 600–900 mm drop length, and resistance to environmental stress cracking during long-term stacked storage of filled containers at 45°C ambient warehouse temperature. The compounding practice on a single-station shuttle blow molding line with a 90 mm grooved-barrel extruder and 28:1 L/D screw includes 2.5–4.0 wt% of a 40% carbon black masterbatch for UV stabilization of outdoor storage, 0.10–0.20 wt% fluoropolymer processing aid to suppress melt fracture at the die lips, and 20–30 wt% clean plant regrind from flash, rejected parisons, and cut rim scrap. Melt temperature measured with a needle pyrometer at the die entry is held at 190–210°C; mold temperature is kept at 12–18°C to remove heat from a 2.5–3.5 mm wall without inducing warpage at the lid gasket seat. Blow air follows a two-stage profile—pre-blow at 0.15–0.20 MPa for 2–3 s to stabilize the parison, full inflation at 0.65–0.75 MPa to fill the chime and top shoulder. Compliance is verified against UN Model Regulations 6.1.5.1 drop test at 1.2 m for PG II liquids, 6.1.5.2 leakproofness test, 6.1.5.3 hydraulic pressure test, and 6.1.5.4 stacking test, with terminal packaging codes UN 1H1/Y1.9/250 for tight-head drums and UN 1H2 for open-head 60-L variants used in agrochemical and detergent supply chains.

    Does Fluorination Depth on DMDB8910 Agrochemical Packaging Plateau Above 35 Minutes of Exposure?

    In low-permeation agrochemical packaging, the fluorination depth achieved on a DMDB8910-rich layer is governed by available surface fluorine radicals and the crystallinity gradient at the parison wall, not by simple exposure time. A six-layer coextrusion blow molding line with a 190–215°C die head processes the structure as 18–22 wt% virgin DMDB8910 outer skin / 30–35 wt% regrind / 1.5–2.5 wt% maleic anhydride-grafted polyethylene tie resin / 2.5–4.0 wt% EVOH with 32–38 mol% ethylene / 1.5–2.5 wt% tie resin / 18–25 wt% virgin DMDB8910 inner skin. The EVOH layer is kept below 220°C to avoid odour-generating acetic acid cleavage; the DMDB8910 skin layers carry the structural load and allow recycled content without compromising the barrier layer. Offline fluorination is run at 0.05–0.10 MPa F2/N2 partial pressure for 25–35 min; beyond 35 min, published diffusion-limited fluorination data for high-density polyethylene show diminishing barrier improvement, so the process window is bounded rather than open-ended. Published data for this specific DMDB8910/EVOH/tie-layer configuration is limited; fluorination time is therefore validated on a per-line basis. Finished containers are tested under ASTM D1693-21 condition B at 50°C with 10% Igepal CO-630; a failure time below 300 h is rejected for xylene-based emulsifiable concentrate formulations. Regulatory compliance references EC 1272/2008 CLP labeling and packaging, the FAO/WHO International Code of Conduct on Pesticide Management, and UN Model Regulations 6.1.5.1 drop plus 6.1.5.2 leakproofness verification for 0.5-L to 10-L coextruded agrochemical bottles.

    Stacking Creep and Environmental Stress-Crack Resistance in Composite IBC Inner Bottles

    The 1000-L composite intermediate bulk container inner bottle produced from DMDB8910 is the load-bearing liner inside a welded steel or wire mesh frame, and its predominant failure mode is environmental stress cracking at the bottom knuckle, not burst. The formulation uses 100% virgin DMDB8910 when the bottle is destined for UN-rated dangerous goods, or ≤10 wt% approved plant regrind, with 2.0–3.0 wt% carbon black masterbatch for outdoor storage and 0.15–0.25 wt% antioxidant masterbatch when the internal liquid is a sodium hypochlorite solution or hydrogen peroxide formula. Extrusion is performed on a 120 mm grooved-barrel extruder with 30:1 L/D feeding an accumulator head; melt temperature at the die is held at 195–215°C, mold water is maintained at 15°C, and the wall thickness profile is programmed to 4.0 mm at the bottom corners, 2.5 mm in the cylindrical body, and 3.5 mm at the top closure area. Because a 0.02 g/10 min MFR shift under ISO 1133-1:2022 at 190°C/2.16 kg can change parison sag enough to produce corner thinning, the line performs hourly parison weight checks and rejects bottles outside ±0.5% of target weight. The bottle is audited against UN Model Regulations Chapter 6.5 for composite IBCs, ASTM D1693-21 condition B for ESCR, ISO 1183-1:2019 for density, and ISO 1133-1:2022 for melt mass-flow rate; terminal output is the 1000-L composite IBC inner bottle classified under UN 31HA1 for non-flammable liquids.

    Audit pointStandard or codeCritical condition or clauseDecision rule
    Drum drop testUN Model Regulations6.1.5.1, PG II 1.2 mNo rupture or leakage
    Drum leakproofnessUN Model Regulations6.1.5.2No leakage at specified pressure
    Composite IBC stacking and dropUN Model Regulations Ch.6.5Composite IBC drop and stacking testNo rupture or leakage
    Environmental stress crack resistanceASTM D1693-21Condition B, 10% Igepal CO-630, 50°CReject below 300 h
    DensityISO 1183-1:2019Immersion methodMatch mill certificate
    Melt mass-flow rateISO 1133-1:2022190°C/2.16 kgCompare to batch certificate

    When Cosmetics Packaging Requires 0.02 mm Wall Uniformity at Low Blow Pressure

    Because low-pressure inflation reduces shear heating and preserves tint dispersion in thick-walled personal-care containers, DMDB8910 is run in continuous shuttle blow molding machines equipped with 0.02 mm resolution laser wall-thickness gauges rather than high-speed extrusion blow molding lines. The formulation for 200-mL to 1-L cosmetic and personal-care containers includes 1.5–2.5 wt% colour masterbatch, 0.5–1.0 wt% antistatic masterbatch for dust resistance in filling plants, and 15–20 wt% clean regrind from trim and start-up scrap. Melt temperature at the die exit is kept at 190–205°C, mold temperature at 10–14°C, and blow air is applied at 0.45–0.60 MPa; the lower pressure prevents abrupt mould pinning that can generate stress concentrations around threaded closures. Wall thickness is monitored on every cycle by a non-contact infrared sensor; a deviation exceeding 0.02 mm in the neck thread area triggers automatic ejection for density analysis under ISO 1183-1:2019. Compliance is checked against REACH Regulation (EC) No 1907/2006 Annex XVII for restricted phthalates and migration of plasticisers from the container wall, and against ISO 22715:2006 for cosmetic packaging labeling and primary packaging integrity. Terminal finished product types are thick-walled jars, laminated-barrel cream jars, and oval personal-care bottles where the print surface must remain dimensionally stable at 45°C warehouse conditions.

    Behind the 75 mm reciprocating screw of an intermittent extrusion blow molder producing 10-L narrow-mouth laboratory reagent containers, the dominant process variable is parison weight repeatability, because neck tolerances below ±0.15 mm determine closure torque and subsequent leakage classification for solvent-bearing liquids. The compound formulation uses 2.0–3.0 wt% carbon black masterbatch, 0.05–0.15 wt% antioxidant masterbatch for residual oxidative stability after hot-air aging, and ≤25 wt% clean regrind from rejected bottles and flash. The parison programmer applies an axial wall thickness curve of 3.2 mm at the neck, 2.0 mm in the mid-body, and 3.5 mm at the base, with melt temperature at 190–205°C and mould cooling water at 10–15°C to stabilize the ESCR-sensitive neck weld line. Containers are subjected to ASTM D1693-21 condition B in 10% Igepal CO-630 at 50°C; if the batch fails below 300 h, the lot is diverted to non-chemical packaging. Density is confirmed by ISO 1183-1:2019, and melt mass-flow rate by ISO 1133-1:2022 at 190°C/2.16 kg to capture lot-to-lot variation that can shift parison sag. Terminal packaging types are 1-L, 2.5-L, 5-L, and 10-L narrow-mouth laboratory bottles used for methanol, acetonitrile, and reagent-grade solvent shipments under UN Model Regulations 6.1.5.2 leakproofness verification for PG II liquids at 1.2 m drop height.

    Free Quote

    Competitive Sinopec Guangzhou HDPE DMDB8910 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Under the commercial designation Sinopec Guangzhou HDPE DMDB8910, Sinopec Guangzhou Petrochemical supplies a high-density polyethylene blow-moulding grade intended for thick-walled industrial hollow parts. The nominal density is 0.956 g/cm³ when measured according to ISO 1183-1:2019, and the high-load melt mass-flow rate is 10 g/10 min at 190 °C/21.6 kg according to ISO 1133-1:2022. These two properties place the grade in the medium-high molecular weight segment of the HDPE blow-moulding range, where parison hang time and top-load stiffness take precedence over rapid cycle time. Lot-level values are supplied on the certificate of analysis; incoming inspection commonly applies the producer’s release limits around the nominal density and melt-flow index rather than the full property range of the commodity high-density polyethylene family.

    Large-part blow moulding exposes the difference between a 10 g/10 min grade and a 20 g/10 min grade of the same density class. DMDB8910 exhibits a lower melt volume-flow rate and measurably higher resistance to parison sag during accumulator discharge. The effect is most visible in tooling for large containers: the 10 g/10 min grade can carry a longer, heavier parison through the pre-blow delay without forming pronounced pendulum sag or uneven wall distribution. That benefit is accompanied by higher screw torque, elevated head pressure, and a longer cooling-limited cycle because thick walls retain heat after mould closure. Published data for the exact molecular weight distribution of DMDB8910 is limited; the flow-rate ratio between the 21.6 kg and 5 kg conditions, when shown on the certificate of analysis, provides an indirect measure of shear sensitivity and melt extensibility.

    Property Test method DMDB8910 typical Higher-flow blow-moulding HDPE reference
    High-load melt mass-flow rate ISO 1133-1:2022, 190 °C/21.6 kg 10 g/10 min 20 g/10 min
    Density ISO 1183-1:2019 0.956 g/cm³ 0.954 g/cm³
    Tensile stress at yield ISO 527-2:2012, type 1B, 50 mm/min 26–28 MPa 25–27 MPa
    Environmental stress-cracking resistance, F50 ASTM D1693-15, Condition B, 100 % Igepal, 50 °C >500 h 100–300 h

    These values are representative figures from supplier technical documentation and are not batch-release specifications. The higher-flow comparator is included to illustrate the melt-flow divide; product selection should rely on the full certificate of analysis and application-specific test plaques rather than a single property.

    What separates a 10 g/10 min high-load melt index resin from 20 g/10 min grades in large-part blow moulding?

    The distinction is not simply viscosity. High-load melt index divides the polymer’s response to shear and extension. A 10 g/10 min resin has a lower population of short-chain molecules than a 20 g/10 min resin of similar density, but the molar mass distribution breadth determines how much viscosity falls in the die land. At low shear rates typical of a hanging parison, the 10 g/10 min grade retains more entanglement resistance and sags less. At high shear rates in the die land, shear thinning reduces apparent viscosity and prevents die pressure from rising in direct proportion to the low-shear viscosity.

    Oscillatory parallel-plate rheometry at 190 °C, 1 % strain, from 0.01 rad/s to 100 rad/s, shows that blow-moulding HDPE of this type has a steep storage-modulus drop at low frequency, indicating a long relaxation tail. The long tail correlates with sag resistance but can also increase recoverable strain at the die exit and cause die swell. Die swell values for high-molecular-weight blow-moulding HDPE often fall between 1.3 and 1.7 at apparent shear rates of 100–500 s−1, but the exact value must be measured on the actual die because it depends on land length and entry angle.

    Blow moulders should not interpret the lower HLMI as a universal improvement. For parts with shot volumes below 5 L or wall thickness below 2 mm, the viscosity of DMDB8910 can increase head pressure and slow the cycle without delivering a measurable top-load or ESCR advantage. In such cases a 20 g/10 min grade may be preferable.

    The selection rule changes when the container is large or aggressive contents are expected. The 10 g/10 min viscosity helps retain wall thickness in the gate and pinch-off zones, where orientation and weld-line integrity control impact failure. A drop impact test under ASTM D5276 or top-load test under ISO 12048:1994 is typically used to verify the final container, because resin tensile yield alone does not capture failure at the weld.

    Accumulator-head blow moulding parameters and pinch-off weld integrity

    For shuttle blow moulding of a 200 L tight-head drum, the resin is typically processed on a 90 mm grooved-barrier feed extruder with an L/D of 30:1 and an accumulator head fitted with a parison programmer. Barrel zone setpoints fall between 180 °C and 210 °C, with die-head setpoints between 190 °C and 210 °C. The actual melt temperature should be controlled within a narrow band, because melt-temperature drift above 230 °C can initiate thermo-oxidative degradation, visible as gel particles, yellowing, and reduced environmental stress-cracking resistance. Below 170 °C, melt fracture, rough parison skin, and excessive accumulator pressure are common failure modes.

    Because parison programming compensates for sag by opening the die gap progressively over the shot, the radial gap difference between the bottom and top portions of a large drum parison can exceed 10 % of the nominal wall thickness. If the programmer curve is too steep or the accumulator discharge speed is too high, the parison can tear at the upper weld line or show lacy melt fracture at the die exit. Processors should record the accumulator pressure-time trace and parison length at inflation, not only the extruder setpoints; batch-to-batch changes in melt strength often appear first as a change in parison length at constant time.

    Bulk HDPE is not hygroscopic, and drying is not normally required. However, if pellets are stored in an unheated silo at relative humidity above 60 % and then transferred into a warm mould shop, surface condensation can produce splay, pinholes, or inconsistent surface finish. A hopper inlet above the dew point and a purge of the first 2–5 kg after cold start reduce moisture-related surface defects.

    The pinch-off weld is the dominant failure site in closed-head drums. Pinch-off compresses two hot parison surfaces and creates a trace of unoriented material at the seam. In a properly annealed HDPE drum, the pinch-off weld should survive a drop impact at −18 °C under ASTM D5276. Inadequate melt temperature, contamination from regrind, or excessive moisture at the mould surface can create a cold weld line that passes short-term hydraulic tests but fails after environmental stress cracking.

    If chemical containers must survive long-term environmental stress cracking

    Environmental stress cracking is evaluated using ASTM D1693-15. The test uses a rectangular specimen with a controlled notch, bent in a holder, and immersed in a surfactant solution such as 100 % Igepal CO-630 at 50 °C. F50 denotes the time at which 50 % of specimens fail. For HDPE grades of the DMDB8910 molecular weight class, supplier data commonly report F50 above 500 h under Condition B, though the exact value is strongly influenced by specimen preparation, residual stresses, and comonomer distribution. Compression-moulded laboratory plaques can overestimate field ESCR relative to blow-moulded container walls; certificates of analysis and type-test reports should therefore state the specimen preparation method.

    When lower-stress slow crack growth is the concern, full-notch creep test methods such as ISO 16770:2019 provide a more discriminating measure than a single ESCR point. For blow-moulded containers, the combination of ESCR and drop impact is a more practical screen than single-point tensile data because container failures usually initiate at weld lines, not in the flat sidewall.

    For chemical compatibility, the candidate liquid should be evaluated under ISO 175:2010 or EN ISO 22088-2 on production containers. HDPE is generally resistant to aqueous acids, alkalis, and many surfactants, but it is susceptible to swelling and stress cracking in strong oxidisers, halogenated solvents, and aromatic hydrocarbons. Long-term contact with such media above ambient temperature should be validated on finished articles, not resin plaques. For food-contact applications, final articles must be evaluated under FDA 21 CFR 177.1520 or EU 10/2011; base-resin compliance alone does not address colour concentrates, processing aids, or lubricants.

    Batch-to-batch viscosity drift and incoming inspection

    Incoming inspection should measure density and high-load melt mass-flow rate on every lot and retain pellets for capillary rheometry when large containers are qualified. A change in HLMI beyond ±15 % of the process reference often shifts parison sag, accumulator pressure, and die swell enough to alter wall-thickness distribution. Density drift of ±0.002 g/cm³ can affect top-load stiffness and volumetric shrinkage, especially in rectangular containers with flat sidewalls. Rheological fingerprinting with a capillary die of L/D 20:1 at 190 °C and 210 °C provides a more sensitive indication of molecular weight distribution change than a single melt-flow point.

    Regrind can be incorporated at controlled ratios, but the amount should be limited by the accumulator pressure and the drop-impact result. In large drums, regrind levels above 25 % can reduce pinch-off weld strength and ESCR, depending on the thermal history of the scrap and the number of heat cycles. A closed-loop regrind system with tight melt filtration and a nitrogen purge on the hopper reduces gel formation.

    The product differs from injection-moulding HDPE grades in the same producer’s slate, such as DMDA-8007, because injection grades are designed for low melt viscosity and rapid mould filling rather than parison stability. Film-grade HDPE resins have a different additive package and are evaluated for dart impact and tear strength rather than top-load and ESCR. Pipe-grade HDPE grades may carry higher hydrostatic strength designations under ISO 9080:2012; DMDB8910 is not sold as a pipe-grade material, and its pressure resistance should not be inferred from hydrostatic design stress data.

    Typical end uses include 200 L tight-head and open-head drums, intermediate bulk container inner bottles, and thick-wall industrial shuttles used for chemical distribution. The final container is qualified by UN dangerous-goods tests, ASTM D1998-15 for plastic drums, or customer-specific top-load and drop-impact protocols. The resin contributes the required stiffness and crack resistance, but the drum mould, parison programming, and weld-line cooling also determine whether the finished article meets the transport test classification.

    Top