Sinopec Guangzhou Hdpe Dmda8008

Sinopec Guangzhou HDPE DMDA8008

    • Product Name: Sinopec Guangzhou HDPE DMDA8008
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 634339
    Density 0.956 g/cm³
    Meltflowrate 0.8 g/10 min
    Tensileyieldstrength ≥26 MPa
    Tensilestrengthatbreak ≥30 MPa
    Elongationatbreak ≥500%
    Flexuralmodulus ≥1100 MPa
    Notchedizodimpactstrength ≥50 kJ/m²
    Vicatsofteningtemperature ≥125 °C
    Heatdeflectiontemperature ≥75 °C
    Brittlenesstemperature ≤-70 °C
    Hardnessshored ≥60
    Environmentalstresscrackingresistance ≥1000 h
    Moistureabsorption <0.01%
    Dielectricconstant 2.3
    Volumeresistivity ≥1×10^16 Ω·cm

    As an accredited Sinopec Guangzhou HDPE DMDA8008 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Sinopec Guangzhou HDPE DMDA8008 is supplied in 25 kg polyethylene-lined woven bags, stacked on pallets for transport.
    Container Loading (20′ FCL) Sinopec Guangzhou HDPE DMDA8008, 25kg bags, loaded in 20′ FCL, palletized or floor-loaded, approx. 20 MT, securely stowed for export.
    Shipping Sinopec Guangzhou HDPE DMDA8008 is a non-hazardous thermoplastic resin. It is typically shipped in 25 kg woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped, in clean, dry containers. Store cool and dry, away from moisture, sunlight, heat, and ignition sources. Standard sea, rail, or truck transport applies.
    Storage Store Sinopec Guangzhou HDPE DMDA8008 in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, heat, flames, and strong oxidizers. Keep original bags sealed, palletized, and off the floor. Avoid prolonged UV exposure and excessive stacking. Maintain clean, dust-free conditions. Follow supplier SDS and local regulations. Shelf life may be reduced by moisture, contamination, or high temperatures.
    Shelf Life Typically 12 months from production date when stored unopened in a cool, dry, ventilated area, away from direct sunlight and heat.
    Application of Sinopec Guangzhou HDPE DMDA8008

    Sinopec Guangzhou HDPE DMDA8008 functions as an injection-molding high-density polyethylene with a melt mass-flow rate in the range of 7.0–8.5 g/10 min under ISO 1133-1:2022 at 190 °C/2.16 kg and a density of approximately 0.954–0.958 g/cm³ under ISO 1183-1:2019. In thin-wall food-storage container production, the grade is processed on high-cavitation cold-runner stack molds where wall thicknesses of 0.7–1.2 mm require near-continuous flow fronts and rapid holding-pressure transitions. The relevant compliance basis for direct food-contact articles is FDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm², and GB 4806.7-2016 when the finished article is placed on the China market. Formulation addition ratios on production lines typically include a polyolefin color masterbatch at 2–4 wt%, a processing stabilizer at 0.05–0.15 wt%, and, where demolding release is limiting, an erucamide slip additive at 0.05–0.10 wt%; recycled content is not introduced unless the converter holds a food-contact approval or a no-objection letter covering the reclaimed polymer stream. Downstream processing uses injection molding machines with clamp forces of 1,000–2,500 kN, barrel profiles from 180 °C in the feed zone to 210–240 °C at the nozzle, mold temperatures of 10–20 °C, injection velocities of 100–220 mm/s, and holding pressures of 45–65 MPa; cycle times for 0.9 mm wall containers can be held between 6–12 s. Field-scale bottlenecks are dominated by warpage across the base and flash along the rim when the holding-pressure profile decays too early, or when batch-to-batch melt-flow rate drifts toward the upper end of the specification. Terminal finished product types include 0.5–2.0 L dairy tubs, rectangular food-storage bases, and matching polyethylene lids intended for refrigerated and ambient conditions. Pre-drying at 70–80 °C for 2–3 h is required only when silo or hopper storage exceeds 60 % RH, because surface moisture causes splay in fast-fill gates.

    What Limits Impact Resistance in 1H2 Open-Top Pail Production?

    The production of UN-certified open-top pails from DMDA8008 shifts the critical control variables from cycle-time reduction to low-temperature impact retention and leakage after drop testing. The governing compliance framework is the UN Model Regulations Chapter 6.1 for rigid plastics packaging designation 1H2, with the packaging group II drop height of 1.2 m applied after low-temperature conditioning; relevant regional overlays are the ADR/RID, IMDG Code, and IATA dangerous goods regulations for air transport. Formulation addition ratios observed on pail lines include hindered amine light stabilizer at 0.2–0.5 wt%, carbon black or polyolefin color masterbatch at 2–4 wt%, and an antioxidant package at 0.05–0.15 wt%; some converters add an antistatic concentrate at 0.1–0.3 wt% for powder product service. Post-industrial regrind is commonly limited to 20–30 wt%, with the upper boundary constrained by the drop-impact and environmental stress-cracking resistance requirements of ASTM D1693 condition A. The downstream production process uses accumulator-assisted injection molding machines with clamp force capacities of 8,000–16,000 kN for 10–25 L pail bodies, hot-runner valve gates feeding multiple injection points, shot weights from 1.2–1.8 kg, melt temperatures of 200–230 °C, mold temperatures of 15–30 °C, and fill times of 0.5–1.5 s to prevent premature freeze-off of the flow front. The limiting production failure modes are sink marks at handle landings and base ribs when the mold surface temperature exceeds 35 °C, pinholes from wet regrind when hopper drying is omitted above 60 % RH, and dimensional shrinkage after ejection when the cooling cycle is shortened below 30 s for a 20 L pail. Terminal finished product types include 5 L, 10 L, 20 L, and 25 L open-top pails with tamper-evident lids for coatings, lubricants, industrial intermediates, and dry food ingredients. The operational boundary for DMDA8008 in this segment is the combination of high-flow melt behavior with thin-wall filling: above 25 L capacity, the wall thickness required to meet drop impact at low temperature may exceed 3.5 mm, and melt strength at the gate can become the limiting parameter for consistent weight distribution.

    In beverage crate manufacturing, DMDA8008 is processed as a thick-wall injection-molding feedstock that must sustain repeated stacking load without creep rupture. The relevant compliance obligations are less food-migration-specific than for primary packaging; crates that contact beverage multipacks only indirectly are assessed under REACH Regulation (EC) No 1907/2006 and, where applicable, the user company’s internal heavy-metal and PAH specifications for returnable transit packaging. Formulation addition ratios for crate stock typically combine a weathering-stabilized color masterbatch at 3–5 wt% and a processing aid at 0.1–0.3 wt%; no slip additive is used because surface friction is required for palletized stability. Downstream processing runs on large-platen injection presses with clamp forces from 12,000–25,000 kN, shot weights of 1.5–4.0 kg, melt temperatures of 200–230 °C, mold temperatures of 20–40 °C, and extended holding-pressure plateaus to pack out corners and rib intersections. Terminal finished product types are 24-bottle returnable beverage crates, 300 × 400 mm dairy crates, and 600 × 400 mm Euro logistics boxes; service life is dominated by cold-temperature impact in the distribution yard and by gate-area stress cracking when the hot-runner valve-gate vestige is not isolated from the load path.

    When Valve-Gated Closure Tooling Operates Below the Over-Slip Limit

    Closure production with DMDA8008 involves a narrow formulation window because the torque-release behavior and organoleptic neutrality of the cap must survive downstream filling lines. The compliance basis for still-beverage and food closures is FDA 21 CFR 177.1520(c), EU Regulation (EU) No 10/2011, and GB 4806.7-2016; closure torque retention is evaluated under equipment-specific internal protocols validated against ASTM D4169-22 for transport simulation where brand owners require distribution testing. Formulation addition ratios are typically restricted to an erucamide slip additive at 0.05–0.20 wt%, a color masterbatch at 1–3 wt%, and an antioxidant at 0.05–0.10 wt%; exceeding 0.30 wt% total slip additive produces surface bloom that reduces cap-to-bottle torque retention and may impart taste-and-odor defects in weakly flavored beverages. The downstream production process uses high-cavitation injection molds with 48–128 cavities, valve-gated hot runners to eliminate cold-runner regrind, melt temperatures of 200–230 °C, mold temperatures of 10–20 °C, injection velocities of 150–300 mm/s, and cycle times of 6–10 s; clamp force per cavity is generally below 20 kN, so total clamp requirements can reach 2,500–5,000 kN for large stack molds. The main process conflict is that high injection speed for thin-wall filling increases shear heating and can degrade the slip additive, while low speed leaves short shots in the tamper-evident band; a holding pressure of 35–50 MPa and rapid decompression before screw recovery are used to control gate vestige. Terminal finished product types include 28 mm screw closures for dairy and juice, 38 mm skirted closures for still beverages, and 20–24 mm flip-top lids for personal-care sachets. Published data for this specific configuration is limited for carbonated soft-drink closures, where higher environmental stress-cracking resistance and dimensional stability requirements frequently shift converter qualification toward bimodal HDPE grades instead of DMDA8008.

    Housewares and Modular Storage: The Gate-Blush Threshold in Thick-Wall Drawers

    For household storage and modular drawer systems, DMDA8008 is selected when high cavity throughput and an impact-resistant surface are the primary purchasing specification. The compliance framework for products sold in Europe is REACH Regulation (EC) No 1907/2006, particularly Annex XVII entries 50 and 51 for polycyclic aromatic hydrocarbons in consumer articles; no food-contact declaration is assigned unless the part is sold as a kitchen food canister, in which case FDA 21 CFR 177.1520(c) and EU 10/2011 apply. Formulation addition ratios include a polyolefin color masterbatch at 1–4 wt%, an antioxidant at 0.05–0.10 wt%, and, where added rigidity is required, talc or calcium carbonate filler at 2–5 wt%; filler loading above 5 wt% reduces notched impact strength under ISO 179-1 and is avoided for drawer bases. Downstream production uses conventional or stack injection molds with wall thicknesses of 2.0–3.5 mm, clamp forces of 4,000–10,000 kN, melt temperatures of 200–230 °C, mold temperatures of 15–25 °C, and holding pressures of 40–60 MPa. A process defect common to this segment is gate blush and jetting when injection velocity exceeds 140 mm/s through undersized edge gates; the corrective sequence on production lines is to enlarge the gate land to 0.8–1.0 mm and reduce first-stage injection velocity by 10–15 % while compensating with a longer hold time. Terminal finished product types include 10–50 L modular drawer trays, under-bed storage boxes, and stackable organizer units. The operational limitation is that DMDA8008 is not an inherently high-gloss grade; surface gloss specifications above 70 GU at 60° under ISO 2813 require mold polishing beyond standard SPI A2 finishes and are routinely subject to batch-to-batch variance.

    Sharps Container Wall Thickness, Puncture Resistance, and Locking-Lid Integrity

    Medical sharps containers and clinical waste bins represent a regulated downstream segment in which the injection molding cycle must not create local thin spots that permit needle penetration under service loads. The primary compliance standard is ISO 23907-1:2018 for single-use sharps containers, which sets puncture resistance, impact resistance, and handle/lid stability requirements; in the United States, devices marketed as sharps containers additionally fall under the FDA 510(k) pathway as Class II medical devices, while European placing on the market under EU MDR 2017/745 requires a technical file. Formulation addition ratios in this segment are intentionally conservative: neat DMDA8008 with color masterbatch at 2–5 wt%, UV stabilizer at 0.2–0.4 wt%, and antioxidant at 0.05–0.10 wt%; post-consumer recycled material is excluded from the cavity because the puncture-resistant floor cannot tolerate a non-uniform regrind melt history. Downstream production uses medium-to-high clamping tonnage machines of 2,000–6,000 kN, melt temperatures of 200–230 °C, mold temperatures of 15–30 °C, and injection velocities low enough to avoid jetting into the depth of a 2.0–4.0 mm wall container; cycle times for a 5 L sharps container range from 20–35 s depending on tamper-evident lid design. The critical failure mode on production lines is sidewall puncture after the cooling stage if the mold is opened before full dimensional stabilization, especially at the junction of the base and sidewall where molded-in stress concentrates; dimensional inspection after ejection is performed after 24 h at 23 ± 2 °C per ISO 291 to separate immediate shrinkage from post-molding creep. Terminal finished product types include 1 L, 5 L, and 10 L sharps disposal containers, locking-lid waste boxes, and hospital room clinical waste bins. Published data for this specific resin in sharps containers is limited, so converter validation should include a full ISO 23907-1:2018 puncture test on production samples rather than relying on generic HDPE grade data.

    Free Quote

    Competitive Sinopec Guangzhou HDPE DMDA8008 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Sinopec Guangzhou HDPE DMDA8008 is a high-density polyethylene extrusion blow moulding resin produced at the Guangzhou petrochemical complex and supplied under the resin designation DMDA8008. The grade is assigned to the blow moulding segment by its nominal melt flow rate of 0.80 g/10 min at 190 °C under a 2.16 kg load in ISO 1133-1:2022 or ASTM D1238-20, and by a nominal density of 0.956 g/cm³ determined according to ISO 1183-1:2019. These two properties position the product for containers that require melt strength to hold a parison during extrusion but also require sufficient flow to fill a shuttle or accumulator-head blow mould on a controlled cycle.

    The model DMDA8008 identifies the resin type rather than a specific additive package or lot. Certificates of analysis for this grade typically report melt flow rate, density, tensile yield stress, elongation at break, flexural modulus and environmental stress crack resistance. The published values are typical values, not specification limits, and they are generated on standard test specimens under the cited methods. Within the Guangzhou HDPE slate, the 8008 suffix distinguishes the blow moulding grade from higher-flow injection and film grades; the coding logic is proprietary and should not be interpreted as comonomer content or filler level.

    Nominal Property Benchmarks Reported Against ISO and ASTM Methods

    The table below consolidates typical resin data for DMDA8008. The values are not guaranteed release limits and should be checked against the supplier’s current certificate of analysis for each commercial specification.

    PropertyTest methodTypical valueUnit
    Melt flow rateISO 1133-1:2022 / ASTM D1238-200.80g/10 min
    DensityISO 1183-1:20190.956g/cm³
    Tensile stress at yieldISO 527-2:201224.0MPa
    Elongation at breakISO 527-2:2012600%
    Flexural modulusISO 178:2019980MPa
    Charpy notched impact strength at 23 °CISO 179-1/1eA:20235.5kJ/m²
    Environmental stress crack resistance F50, 10% Igepal CO-630ASTM D1693-15>30h
    Vicat softening point A50ISO 306:2022126°C
    Shore D hardnessISO 868:200362dimensionless

    The environmental stress crack resistance value is a comparative benchmark obtained under ASTM D1693-15, condition A; it does not predict service life against aggressive oxygenated or halogenated fill formulations. Mechanical values are generated on compression-moulded plaques prepared under ISO 293 at 180 °C. Blow-moulded wall sections may show lower elongation because of molecular orientation and weld-line discontinuities at the pinch-off zone.

    For incoming lot control, some plants monitor the flow rate ratio between the 21.6 kg and 2.16 kg loads under ISO 1133-1:2022. A change in this ratio indicates a shift in molecular weight distribution that may not be visible in a single-point melt flow test. Capillary rheometry at 190 °C across shear rates from 10 s⁻¹ to 1000 s⁻¹ is used to detect molecular structure shifts before extrusion blow moulding trials.

    What Processing Envelope Is Observed on Continuous Shuttle Blow Moulders?

    Processing of DMDA8008 on shuttle blow moulding equipment generally follows a melt temperature window of 190 °C to 210 °C at the die head. Single-screw extruders with diameters from 45 mm to 75 mm and length-to-diameter ratios of 24:1 to 30:1 are used for containers from 500 mL to 20 L. Barrel temperatures are commonly profiled from 180 °C in the feed zone to 220 °C at the metering zone, with head and die zones held at 190 °C to 210 °C. Melt temperatures above 230 °C accelerate thermo-oxidative degradation and may produce yellowing or odour; melt temperatures below 180 °C increase viscosity enough to generate melt fracture or rough parison surfaces.

    Die gaps are commonly set between 1.0 mm and 2.5 mm for bottles and small containers. A wider gap reduces shear heating but requires more parison programming to control thinning near the mould parting line. Some processors use a divergent die pin and a mandrel angle of 15° to 20° to stabilise the parison against draw-down. On accumulator-head machines, parison programming is required to delay extrusion at the parison start, enlarge the die gap in the centre section, and narrow the gap at the tail to compensate for sag.

    Blow air pressure on shuttle blow moulders is typically set at 0.6 MPa to 0.8 MPa, and cooling water is held at 8 °C to 12 °C to reduce cycle time and control warpage. Mould surface temperature should be kept below 15 °C to limit post-mould shrinkage in thick shoulder areas. Because DMDA8008 has a higher melt flow index than a 0.30 g/10 min fractional-melt HDPE, head pressure can be 10% to 20% lower on the same screw. The same higher flow index shortens the stable parison hanging time before sag becomes unacceptable; published data for this specific configuration is limited.

    Regrind incorporation in DMDA8008 is normally held below 30 wt% for general-purpose containers. Higher regrind ratios can reduce melt strength and raise gel counts if the regrind carries multiple heat histories. Colour masterbatch addition at 2 wt% to 4 wt% is common, but masterbatch carriers should be matched to the 0.80 g/10 min base resin to avoid dispersion defects in thin-walled sections. Pellets exposed to relative humidity above 80% can carry enough surface moisture to produce splay; a hopper dryer at 80 °C for 2 h is used when surface defects appear, although the resin itself is not hygroscopic.

    Screw configurations for DMDA8008 commonly include a feed zone of 5 to 7 diameters, a compression zone with compression ratio from 2.5:1 to 3.5:1, and a metering zone fitted with a Maddock mixing section. A mixing section improves thermal homogeneity and can reduce melt-temperature overshoot when screw speed is increased to meet bottle output. Screw speeds above 80 RPM on a 65 mm extruder can create excessive shear heating and should be validated by measuring melt temperature at the die entry.

    When Parison Sag Limits Wall Thickness in Containers Above 20 L

    For industrial containers with capacity above 20 L, DMDA8008 can be limited by parison sag because its melt flow rate is higher than fractional-melt blow moulding HDPE. On accumulator-head machines, the shot size and drop time may exceed the stable parison hanging time, producing thin sidewalls near the top and excessive flash at the pinch-off. Compensation involves running the die temperature at the lower end of the window, reducing melt temperature to 190 °C, and increasing parison programming steps to maintain a wall thickness differential of no more than 15% across the container height.

    When the application requires top-load strength above 300 N or long-term contact with hydrocarbon-based liquids, grade selection should be validated by full-container testing rather than by resin-level ESCR alone. DMDA8008 is suitable for non-pressurised industrial packaging, but it is not a substitute for high-molecular-weight HDPE or barrier-treated containers in applications that require low temperature impact below -30 °C or permeation resistance to aromatics.

    End-use applications for DMDA8008 include extrusion blow moulded bottles and containers in the 250 mL to 10 L range for household chemicals, personal care products, pharmaceutical closures and non-pressurised industrial packages. The grade is used where a balance of stiffness, ESCR and processability is required. For carbonated beverage bottles, the resin is generally unsuitable because the high-density polyethylene backbone provides insufficient CO₂ barrier and pressure-induced stress accelerates environmental stress cracking in the bottle base; a PET or barrier-treated HDPE structure is specified instead.

    Contrasting DMDA8008 with Fractional-Melt Blow Moulding and High-Flow Injection Grades

    The functional position of DMDA8008 is best understood against two HDPE reference categories: a fractional-melt extrusion blow moulding HDPE with a nominal melt flow rate of 0.30 g/10 min and a high-flow injection moulding HDPE with a nominal melt flow rate of 8.0 g/10 min. The comparison is based on representative category data and is not a specification for any named grade.

    AttributeDMDA8008Fractional-melt blow moulding HDPEHigh-flow injection moulding HDPE
    Nominal melt flow rate0.80 g/10 min0.30 g/10 min8.0 g/10 min
    Nominal density0.956 g/cm³0.954 g/cm³0.960 g/cm³
    Primary processExtrusion blow mouldingExtrusion blow moulding, large partsInjection moulding
    Melt strengthModerateHighLow
    Cycle time in blow mouldingFaster than 0.30 g/10 min gradeSlower but better parison hangNot used for blow moulding
    ESCR rankingModerate to highHighLow to moderate

    The higher flow index of injection moulding grades reduces injection fill pressure but makes them unsuitable for continuous parison formation. DMDA8008 retains sufficient melt strength for small and medium containers while providing lower head pressure than fractional-melt blow moulding HDPE. For very large containers or long drop times, fractional-melt high-density polyethylene remains the conventional choice; for thin-wall injection-moulded housewares or caps, a high-flow injection grade is used.

    Food-contact status for DMDA8008 should be confirmed against FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011 before use in direct food packaging. Compliance is a declaration based on the completed polymer and its additive package, and converters should verify migration testing under the actual time and temperature conditions. For industrial chemical packaging, the final container must be qualified with the specific fill formulation; resin-level ESCR data alone cannot guarantee compatibility with oxidising agents, hydrocarbons or surfactant-based products.

    Top